Characteristics of Bending Strength on Coating Condition of Metal Surface Polyurethan Coating Material (금속표면에 폴리우레탄코팅한 소재의 코팅조건 변화에 따른 굽힘강도 특성)

  • 이강길
    • Journal of Ocean Engineering and Technology
    • /
    • v.15 no.2
    • /
    • pp.124-129
    • /
    • 2001
  • The research on anticorrosive of valve for ship, waterworks, and drainage system is very important. The purpose of this paper is to develop the metal/polyurethan adhesive technique at insider of the value to prevent corrosion in the value. It is performed to the bending strength test by using metal /polyurethan in the metals (SB41, Al6061). It is investigated to the effects of bending strength on curing temperature, preheating time and curing time, and to the fracture mechanism of metal/polyurethan adhensived specimen. As a results, we find that the bending strength is the highest at curing temperature of 11$0^{\circ}C$ and the curing time is 60 minutes in metal/polyurethan adhesive specimen.

  • PDF

Removal of Hydrogen Sulfide using Reticulated Polyurethan Carrier in Biofilter (망상구조 폴리우레탄 담체를 이용한 황화수소 제거)

  • Jeong, Gwi-Taek;Lee, Gwang-Yeon;Cha, Jin-Myoung;Park, Don-Hee
    • Korean Chemical Engineering Research
    • /
    • v.45 no.4
    • /
    • pp.372-377
    • /
    • 2007
  • In order to assess its capability as biofilter bed material under variable conditions of two parameters (inlet gas concentration and inlet gas flow rate), reticulated polyurethan was applied to remove hydrogen sulfide via a biological process. We detected a maximal elimination capacity (critical loading rate) of $488.3(330.1)g-H_2S/m^3{\cdot}hr$, when reticulated polyurethane was employed as supporting material of biofilter. This study show that the application of reticulated polyurethane carrier might be a favorable choice as a packing material in biofilter for the biological removal of hydrogen sulfide.

A Study on materials and manufacturing process of polyurethan fairing parts for F-5E/F 15% spar kit (F-5E/F 15% SPAR KIT 용 폴리우레탄 캐스팅 윙 페어링 소재 및 공정개발)

  • 김국진;문영진;한중원;김영생;곽준영;최재성
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2002.10a
    • /
    • pp.193-197
    • /
    • 2002
  • Polyurethane casting wing fairings included in F-5E/F 15% spar kit are to be installed on aircraft wing surfaces and used for compensating the changes of the aerodynamic configuration by the leading edge extension fairings. These fairing are mandatory items in repairing wing areas and was imported from foreign supplier with long term delivery and high cost. Accordingly, local manufacturing is necessary to get rid of above disadvantages such as long term delivery and high cost. Basic properties test of specimen to be developed and part's requirements after localization was taken and its values were similar or higher when comparing with the original's even in low temp test at -55C. Casting mold process was used to manufacture the polyurethane fairings and its demensional stability & physical condition was proper and met to the related specification and drawing's requirements

  • PDF

A Study on Characteristics of Coated Films on Wood Surface by Nitrocellulose Lacquer, Aminoalkyd, Polyester, and Polyurethan (니트로셀룰로오스락카, 아미노알키드, 폴리에스테르 및 폴리우레탄 도료(塗料)의 도막성능(塗膜性能)에 관(關)한 고찰(考察))

  • Lee, Phil-Woo;Kim, Hyun-Joong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.17 no.1
    • /
    • pp.12-21
    • /
    • 1989
  • This experiment was executed to investigate the characteristics of gloss and color difference in coated films by N.C. Lacquer, Aminoalkyd, Polyester. and Polyurethan coating after chemical (distilled water, ethyl alcohol. acetic acid, and sodium hydroxide) and heating ($120^{\circ}C$) treatments, cold-check test, and U.V. radiation. The results obtained were summarized as follows 1. The gloss decreasing rate by water resistance test was the least among chemicals treated on coated films. 2. The color difference of coated films chemical treatments highly and similarly increased, except the alkali treatment showing a little increase. 3. In the color difference by U.V. radiation, the polyester coated film showed generally large difference compared with the other coated films.

  • PDF

Fitness and Physical Properties in Current Stretch Fabrics for Bottoms -Focused on the Tight Skirt- (하의용 시판 신축성 소재의 물리적 특성과 맞음새에 과한 연구 -스커트를 중심으로-)

  • 이진희;최혜선;도월희
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.26 no.10
    • /
    • pp.1467-1477
    • /
    • 2002
  • This study was investigated physical properties of stretch fabrics by KES-FB system to show suitable basic data to making skirts of excellent capacity and develop more organized basic skirt pattern by fitness evaluation. 1. The results of T. H. V.(Total Hand Value) were as followa: In the kind of blending fiber, cotton/spandex was more excellent than nylon/spandex and polyester/spandex, in the direction of stretch, one-way(weft inserted polyurethan yarn) polyester/spandex and cotton/spandex were higher than two-way(warp and wet inserted polyurethan yarn) polyester/spandes and cotton/spandex, two-way nylon/spandex was higher than one-way nylon/spandex. 2. The results of calculating the variance between sample stretch fabrics and Japanese s/s women's suit fabrics after standardizing were as follows: Stretch fabrics has 2 range of tensile, bending, shearing, compression, surface, thickness and weight as compared with Jpanese s/s women's suit fabrics. In the tensile property, one-way stretch fabrics were almost the same with Japanese s/s women's suit fabrics, only two-way polyester/spandex had+1~+2 range. In the bending, shear property, there was no difference between sample fabrics and Japanese s/s women's suit fabrics 3. In the total fitness of the skirt, nylon/spandex is the best in the fabrics and one-way stretch fabric is better than two-way strethch fabric.

Solar Energy Utilization in a Greenhouse Bulk Curing and Drying System(I) (Greenhouse Bulk건조기에 의한 태양열이용에 관한 연구 (제I보))

  • 진정의;이승철;이상하
    • Journal of the Korean Society of Tobacco Science
    • /
    • v.2 no.1
    • /
    • pp.61-67
    • /
    • 1980
  • The greenhouse hulk curing and drying system utilizing the direct solar energy was tested to see how much fuel could be saved for curing flue-cured tobacco at the Daegu Experiment Station, Korea Tobacco Research Institute (North latitute: 35$^{\circ}$49'), in 1979. The structure consists of transparent fiberglass exterior, polyurethan boards covered with galvanized iron as the heat absorbers and insulation boards, air duct in which the air is introduced to the furnace room of bulk curing barn, and gravel heat storage system. All exterior surface of heat absorbers, air duct, and gravels were coated with black paint. The air temperature and total radiation were 20.5 to 35.5$^{\circ}C$ and 1004.2 to 1436.2 cal/$\textrm{cm}^2$ during the 3 replicated curing tests, respectively. The greenhouse bulk curing and drying system was able to cut fuel consumption by 25 percent compared with the conventional bulk curing barn. The maximum temperatures for the top absorber and the inlet air of the system were 89$^{\circ}C$ and 64$^{\circ}C$, respectively, and the average temperature of inlet air was higher than that of conventional one by 18$^{\circ}C$.

  • PDF

A Study on the Physiological Responses and the Microclimate in Girdle (Girdle 착용이 인체생리반응과 의복기후에 미치는 영향)

  • Kim Hyun Sik;Choi Jeong Wha
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.11 no.2 s.24
    • /
    • pp.57-67
    • /
    • 1987
  • The purpose of this study was to confirm the effects of girdle on the physiological responses and the microclimate in summer. The measuring points were rectal temperature, skin temperature, pulse rate and sweat volume as physiological responses and the inside clothing temperature, relative humidity as microclimate when the subjects wore girdle (girdle A; polyurethan+nylon, girdle B; polyurethan+cotton) for the period of rest and exercise in climate chamber. The enviromental conditions were at $25^{\circ}C$ ($65{\pm}5\%$ RH) and $30^{\circ}C$ ($75{\pm}5\%$ RR). The results were as followings. 1. Mean skin temperature increased in girdle during the exercise at $30^{\circ}C$. 2. The pulse rate decreased in girdle during the rest at $25^{\circ}C$. In the case of girdle A, it was remarkably decreased. Rectal temperature increased in girdle A and B during the exercise at $25^{\circ}C$. But the kinds of girdle didn't affect the pulse rate and rectal temperature. 3. The total sweat volume in girdle was larger than in control. 4. The difference between skin temperature and inside clothing temperature of abdomen had a tendency to increase at all experiment condition. 5. The relative humidity of inside ($RH_1$) and outside ($RH_2$) of girdle increased in girdle during the rest at $25^{\circ}C$ and $30^{\circ}C$. And the relative humidity of wearing girdle B was hig-her than girdle A during the rest at $25^{\circ}C$ and $30^{\circ}C$. The $RH_1$ after stepping at $30^{\circ}C$ was the highest in girdle A and the lowest in control. From this point of view, we concluded that physiological responses and the microclimate were affected by wearing girdle. And mean skin temperature and relative humidity of inside clothing were affected by the materials of girdle.

  • PDF