Lee, Dong Hun;Choi, Jisu;Oh, Young Se;Kim, Yoong Ahm;Yang, Kap Seung;Ryu, Ho Jin;Kim, Yong Jung
Carbon letters
/
v.24
/
pp.28-35
/
2017
We demonstrated an effective way of preparing melt spinnable mesophase pitches via catalytic hydrogenation of petroleum residue (fluidized catalytic cracking-decant oil) and their subsequent thermal soaking. The mesophase pitches thus obtained were analyzed in terms of their viscosity, elemental composition, solubility, molecular weight, softening point and optical texture. We found that zeolite-induced catalytic hydrogenation under high hydrogen pressure contributed to a large variation in the properties of the pitches. As the hydrogen pressure increased, the C/H ratio decreased, and the solubility in n-hexane increased. The mesophase pitch with entirely anisotropic domains of flow texture exhibited good meltspinnability. The mesophase carbon fibers obtained from the catalytically hydrogenated petroleum residue showed moderate mechanical properties.
Pitch is an attractive raw material for carbon fiber precursors due to its low cost stemming from its availability as a residue of coking and petroleum processes. Ford Motor Company reported a carbon fiber target price of $11.0/kg by using a fast cycle-time manufacturing method with carbon fiber in an inexpensive format, allowing for an average retail price of gasoline of $3.58/gallon. They also recommended the use of carbon fiber with strength of 1700 MPa, modulus of 170 GPa, and 1.5% elongation. This study introduced a ca. $5.5{\mu}m$ carbon fiber with 2000 MPa tensile strength obtained from a precursor through simple distillation of petroleum residue. Petroleum pitch based carbon nanofibers prepared via electrospinning were characterized and potential applications were introduced on the basis of their large specific surface area and relatively high electrical conductivity.
U, Hui Gwon;Hong, Ran Yeong;Park, Jin Yeong;Jeong, Yeong Tae;Park, Hyeong Ryun;Ham, Hui Seok
Bulletin of the Korean Chemical Society
/
v.17
no.1
/
pp.16-19
/
1996
The bulk photopolymerization of methyl methacrylate (MMA) with disilanes such as 1,2-diphenyldisilane and 2-phenyl-1,3-disilapropane was carried out to yield poly(MMA)s containing the corresponding disilyl moiety presumably as an end group. It was found that while the polymerization yields and the polymer molecular weights decreased as the relative disilane concentration increased, the TGA residue yields and the relative intensities of SiH IR stretching bands increased with increment of molar ratio of disilane over MMA. The photopolymerization of MMA with 2-phenyl-1,3-disilapropane produced higher-molecular-weight polymer with lower TGA residue yield when compared to the photopolymerization of MMA with 1,2-diphenyldisilane. The disilanes seemed to significantly influence on the photopolymerization as both chain initiation and chain transfer agents.
The poly(methylsilene) (1) was modified with the group 4 metallocene Cp2MCl2/Red-Al (M = Ti, Zr, Hf) combination catalyst and with the group 6 metal carbonyl M(CO)6 (M = Cr, Mo, W) catalyst, producing the highly cross-linked isoluble polymer and the lowly cross-linked soluble polymer, respectively. An interrelationship between molecular weight and percent ceramic residue yield with metal within the respective group was not found. The polymers modified with the group 4 metallocene combination catalysts have higher molecular weight and lower percent ceramic residue yield than the polymers modified with the group 6 metal carbonyl catalysts do. The catalytic activity of group 4 metallocene combinations appears to be higher at ∼100 ℃, but to be lower at very high temperature than those of group 6 metal carbonyls. The pyrolysis of the modified 1 yielded SiC ceramic.
U, Hui Gwon;O, Eun Mi;Park, Jong Hak;Kim, Bo Hye;Kim, Yong Nam;Yun, Chan Ho;Ham, Hui Suk
Bulletin of the Korean Chemical Society
/
v.21
no.3
/
pp.291-294
/
2000
The bulk photopolymerization of methyl methacrylate(MMA) with bis(silane)s such as 1,4-$C_6H_4(SiH_3)_2$ (1) and 1,4-$C_6H_4(SiH_2Me)_2$ (2) was performed to produce poly(MMA)s possessing the corresponding bis(silyl) moiety as an end group. For the bis(silane)s, while the polymerizaiton yields and the polymer molecular weights decreased, the TGA residue yields and the relative intensities of Si-H IR stretching bands increased as the relative bis(silane) concentration over MMA increased. The polymerizaion yield, polymer molecular weight, and TGA residue yield of MMA with 1 were found to be higher than those with 2. The bis(silane)s appears to influence significantly upon the photopolymerization of MMA as both chain initiation and chain transfer agents.
There are many methods of obtaining butadiene described in the literature. In the america it is produced largely from petroleum gases, i.e., by catalytic dehydrogenation of butene of butene-butane mixtures. Butadiene can be recovered from the $C_4$ residue of an olefin plant by distilling off a fraction containing most of the butadiene, catalytically hydrogenating the higher acetylenes to olefins and separating the product from other olefins and isobutane by extraction. Also it can be obtained by cracking naphtha and light oil. Among the individual dienes of commercial importance, 1, 3-butadiene is of first importance. It is used primarily for the production of polymers.In the present paper, it was investigated for a effect of the formation and the growth inhibition of popped corn polymer in butadiene extraction unit. As a result of study, inhibitors, $NaNO_2$ and TBC were good effective for inhibition of the formation and growth in popcorn polymer. The rational formula of popcorn polymer obtained was $(C_4H_6)_x$.
Journal of the Korean Institute of Telematics and Electronics A
/
v.30A
no.1
/
pp.31-43
/
1993
Thermal behavior and $O_{2}$ plasma effects on residue and penetrated impurities formed by reactive ion etching (RIE) in CHF$_{3}$/C$_{2}$F$_{6}$ have been investigated using X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectrometry (SIMS) techniques. Decomposition of polymer residue film begins between 200-300.deg. C, and above 400.deg. C carbon compound as graphite mainly forms by in-situ resistive heating. It reveals that thermal decomposition of residue can be completed by rapid thermal anneal above 800.deg. C under nitrogen atmosphere and out-diffusion of penetrated impurities is observed. The residue layer has been removed with $O_{2}$ plasma exposure of etched silicon and its chemical bonding states have been changed into F-O, C-O etc.. And $O_{2}$ plasma exposure results in the decrease of penetrated impurities.
Proceedings of the Korean Fiber Society Conference
/
1998.04a
/
pp.329-333
/
1998
The major classes of antimicrobial agents for textiles include organo-metallics, phenols, quaternary ammonium salts, and organo-silicones. These finishes should be durable, have selective activity towards undesirable organisms, be compatible with other finishes and dyes, and be nontoxic to man [1]. Chitosan, as a deacetylated derivative of chitin, is a natural, non-toxic and biodegradable polymer. Chitosan is also known as an antimicrobial polysaccharide due to antimicrobial action of the amino group at the C-2 position of the glucosamine residue.(omitted)
Journal of the Korean institute of surface engineering
/
v.32
no.2
/
pp.93-99
/
1999
Surface polymer layer formed on the silicon wafer during the oxide overetching using $C_4F_8$/ helicon wave plasmas and their characteristics were investigated using spectroscopic elipsometry, X-ray photoelectron spectroscopy, and secondary ion mass spectrometry. Overetch percentage and dc-self bias voltage were varied to investigate the effects on the characteristics of the polymers remaining on the overetched silicon surface. The increase of bias voltage from -80 volts to -120 volts increased the C/F ratio and carbon bondings such as C-C, $C-CF_x$/, and C-Si in the polymer while reducing the thickness of the polymer layer. However, the increase of the overetch percentage from 50% to 100% did not change the composition of the polymer layer and the carbon bondings in the polymer layer remained same even though it increased the polymer thickness. The polymer layer formed at the higher dc-self bias voltage was more difficult to be removed by the following various post-etch treatments compared to that formed at the longer overetch percentage.
Park, E-Joon;Park, Bong-Ku;Kim, Jae-Hoon;Lee, Sang-Chul;David J. T. Hill
Macromolecular Research
/
v.8
no.1
/
pp.12-18
/
2000
Six aromatic polyesters with ether-linkages were prepared from 4,4'-oxybis(benzoic acid) and naphthalenediol (ND) isomers which were 1,4-, 1,5-, 1,6-, 2,3-, 2,6- and 2,7-derivatives. The solution viscosity numbers ranged from 0.23 to 0.65 dL/g. The glass transition temperatures ranged from 142 to 179$\^{C}$. The initial decomposition temperatures were all above 400$\^{C}$, and the residue weights at 600$\^{C}$ were in the range of 50-64%. Only the polyesters derived from 1,5- and 2,6-NDs, which have a linear linking mode, were found to be semicrystalline and could form thermotropically nematic phase. Multiple melting phenomena and annealing of the polyester derived from 1,5-ND and related polymers are described. The experimental results show that the polyester derived from 1,4-ND of linear shape was amorphous and non-liquid crystalline. Particularly, the polyester derived from 2,3-ND could form a smectic mesophase as banana-shaped molecules, and this is ascribed to the C/sub_2v/ symmetry where highly kinked molecules are packed in the same direction.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.