• Title/Summary/Keyword: Poly styrene

Search Result 355, Processing Time 0.029 seconds

Studies on the Styrenic Polymers(1), Imidization of Poly(styrene-co-maleic anhydrides) and Their Thermal Properties (Styrenic Polymers연구(1), Poly(styrene-co-maleic anhydride)의 이미드화와 열적 성질)

  • Ahn, Tae-Oan;Park, Lee-Soon;Lee, Sang-Soo;Kim, Gi-Heon
    • Applied Chemistry for Engineering
    • /
    • v.3 no.1
    • /
    • pp.179-187
    • /
    • 1992
  • Poly(styrene-co-maliec anhydride) was reacted with aromatic amines such as aniline, p-toluidine, and p-chloroaniline in 10% (w/w) DMF solution to convert maleic anhydride units into maleimides. Optimum reaction conditions for cyclodehydration step of imide ring formation were : (a) reaction temp. of $80^{\circ}C$ (b) mole ratios of cyclodehydration agents : anhydride units in SMA/acetic anhydride/sodium acetate/triethyl amine= 1.0/2.0/0.2/1.1. $T_g$of SMI(imide modified SMA) was increased with increasing degree of imidization, but $T_g$leveled off in the early stage of imide content. And $T_g$of SMI was increased with the following order of amines used for imidization reagents : aniline < p-toluidine < p-chloroaniline.

  • PDF

Effects of Zinc Stearates on the Thermal and Rheological Properties of Polystyrene Ionomers (폴리스티렌 이오노머의 열적·유변학적 성질에 미치는 스테아린산 아연의 영향)

  • Kim, Jong-sang;Doo, Jun Kil;Lee, Dai Soo
    • Applied Chemistry for Engineering
    • /
    • v.10 no.8
    • /
    • pp.1216-1220
    • /
    • 1999
  • Different amounts of zinc stearate were incorporated as a plasticizer into poly(styrene-co-sodium methacrylate) ionomers prepared by bulk-suspension plymerization and neutralization with sodium hydroxide and effects of the zinc stearate on the thermal and rheological properties were investigated. It was obseved that the crystallization of zinc stearate in the ionomers were partially suppressed depending on the content of ionic moieties. It is postulated that the ionic moieties dissolved zinc stearate and suppressed crystallization of the zinc stearates. We speculated that 0.4~0.6 mole of zinc stearate was dissolved by one mole of the ionic moiety. Poly(styrene-co-sodium methacrylate) containing only the dissolved zinc stearates showed typical rheological properties of homogeneous systems in Cox-Mertz plots. However, poly(styrene-co-sodium methacrylate) containing crystallizable zinc stearates as well as dissolved ones showed typical rheological properties of heterogeneous systems.

  • PDF

The Effects of Blend Composition and Compatibilizer on the Mechanical Properties of the PP/SAN and the PP/ABS Blends (블렌드 조성과 상용화제가 PP/SAN과 PP/ABS 블렌드의 기계적 물성에 미치는 영향)

  • 박정훈;성운모;현재천;김우년;홍병권;홍존희;임양수
    • Polymer(Korea)
    • /
    • v.26 no.1
    • /
    • pp.53-60
    • /
    • 2002
  • Polypropylene(PP : continuous phase)/poly (styrene-co-acrylonitrile)(SAN : dispersed phase) blends, and PP/poly(acrylonitrile-butadiene-styrene) (ABS : dispersed phase)blends, containing various amounts of compatibilizer(PP-SAN graft copolymer), were prepared at various shear rates by using twin-screw extruder. In the PP/SAN blend, the average size of the dispersed particles(SAN) was increased with SAN content, while the flexural strength and tensile strength were decreased with SAN content. When the screw rpm was increased from 10 to 60 rpm, the size of the dispersed phase was decreased while the flexural strength and the tensile strength were increased. Maximum mechanical strength and minimum droplet size were observed when the 5 phr compatibilizer was added to the PP/SAN blends. The mechanical strength of PP/ABS blends such as flexural strength and tensile strength increased by adding compatibilizer was reached maximum when blends contained 5 phr compatibilizer.

Preparation of Poly(styrene-co-(trimethoxysilyl)propyl methacrylate)-grafted ETFE Films by a Simultaneous Irradiation Grafting Method (방사선을 이용한 스티렌-TMSPM 공중합체가 그래프트된 ETFE 필름의 제조)

  • Sung, Hae-Jun;Sohn, Joon-Yong;Song, Ju-Myung;Shin, Jun-Hwa;Nho, Young-Chang
    • Polymer(Korea)
    • /
    • v.35 no.5
    • /
    • pp.478-482
    • /
    • 2011
  • In this study, several poly(styrene-co-(trimethoxysilyl)propyl methacrylate)-grafted ETFE films were prepared by a simultaneous irradiation grafting method. After mixing of styrene/(trimethoxysilyl)propyl methacrylate(TMSPM) monomers with various solvents, the effects of various irradiation conditions such as total dose, dose rate and monomer concentration on the degree of grafting of the prepared membranes were investigated. Results indicated that the higher degree of grafting was obtained when acetone was used as a solvent. The formation of poly(styrene-co-TMSPM) grafts on the ETFE films was verified using FTIR spectrometry and the distribution of the poly(PTMSPM) graft polymer over the cross-section of the grafted film was confirmed using SEM-EDX instrument.

Synthesis of Sulfonated Poly(styrene-co-DVB) Hyper Branched Cationic Exchange Resin and Its Properties (하이퍼브랜치 Poly(styrene-co-DVB) 설폰화 양이온교환 수지의 합성 및 특성)

  • Baek, Ki-Wan;Yeom, Bong-Yeol;Hwang, Taek-Sung
    • Polymer(Korea)
    • /
    • v.32 no.1
    • /
    • pp.43-48
    • /
    • 2008
  • In this study, the hyper branched poly (styrene-co-divinylbenzene) (PSD) was synthesized by bulk polymerization and the cationic exchanger with high ion exchange capacity was prepared by sulfonation. The structure of hyper branched PSD ion exchanger was investigated by FT-IR, $^1H-NMR$ spectroscopy, and GPC analysis. The molecular weight, viscosity of hyper branched PSD increased with DVB content, which have the maximum values of 9410g/mol and 338 cP, respectively. And the reaction rate also increased with cross-linker content. As DVB content increased, the solubility of PSD decreased having the maximum value of 22 g with 0.1 mol% DVB. The water content and ion exchange capacity of the hyper branched PSD ion exchanger increased with the amount of sulfuric group. Their maximum values were 18.2% and 4.6 meq/g, respectively. The adsorption of copper and nickel ion was completed within 40 min.

Thermodynamic Characteristics of PMMA/PVME Blends Containing Compatibilizer and Their Gas Transport Properties (상용화제를 포함한 PMMA/PVME 블렌드의 열역학적 특성과 기체 투과 특성)

  • 최해욱;문유진;정병조;김창근
    • Polymer(Korea)
    • /
    • v.26 no.2
    • /
    • pp.245-252
    • /
    • 2002
  • Thermodynamics and gas transport properties of polymethylmethacrylate (PMMA) blends with polyvinylmethylether (PVME) containing various amount of poly (styrene-b-methylmethacrylate) copolymer (P(S-b-MMA)) as a compatibilizer were studied. To extract interaction energies of binary pairs involved in the blends from the phase separation temperatures using an equation-of-state theory, PVME blends with methylmethacrylate copolymers containing various amount of styrene (SMMA) were prepared. PVME formed miscible blends with methylmethacrylate copolymers containing more than 70 wt% styrene and these miscible blonds showed a LCST-type phase separation behavior. Based on the interaction information obtained here, P(S-b-MMA) copolymer was added to the PMMA/PVME blends to enhance their compatibility. The average diameter of the dispersed rubber particles was gradually decreased for the blends of containing P(S-b-MMA) from 0 to 5 phr and then leveled off at a fixed size. At a fixed bland composition, the gas permeation was also increased as the P(S-b-MMA) content increased from 0 to 5 phr and then leveled off when the P(S-b-MMA) content was higher than 5 phr.

Synthesis of Poly(Styrene-co-GMA) and its Application as in situ Reactive Compatabilizer (Poly(Styrene-co-GMA)의 합성과 in situ Reactive Compatabilizer 로서의 응용)

  • Kim, Ju-Young;Suh, Kyung-Do
    • Applied Chemistry for Engineering
    • /
    • v.3 no.3
    • /
    • pp.499-506
    • /
    • 1992
  • Copolymer of Styrene and GMA(glycidyl methachylate), having reactive ratios of $r_1=0.53$, $r_2=0.44$, was synthesized in dioxane using AIBN as free radical initiator. Followed by the reaction of ethylene diamine with copolymer PGS, amine groups were introduced to the PGS(NPGS). The composition of copolymer was determined by elemental analyzer. Poly(glycidyl methacrylate) (PGMA) was obtained in benzene using AIBN as free radical initiator. The NPGS-PGMA blend of 50/50 composition was prepared by mixing these polymers in THF at $65^{\circ}C$. Glass transition temperature (Tg) of NPGS-PGMA blend was measured by DSC. The blend showed a single Tg. Accordingly, it was clear that the NPGS was compatible with PGMA. An intermolecular reaction between amine groups of NPGS and epoxy groups of PGMA imparts compatibility in the NPGS-PGMA blend. When the NPGS-PGMA blend was added to the incompatible PS-PGMA blend, PS-PGMA blend showed Tg change. Scanning Electron Micrograph(SEM) showed a fine morphology in this blend. Consequently, it was apparent that the NPGS-PGMA blend acted as a compatibilizer for the PS-PGMA blend.

  • PDF

Permeation Characteristics of Water Vapor Through PVA/PSSA_MA/THS-PSA Membranes (PVA/PSSA-MA/THS-PSA 막의 수증기 투과특성에 관한 연구)

  • Rhim, Ji-Won;Cho, Hyun-Il;Kim, Dae-Hoon;Ha, Seong-Yong;Nam, Sang-Yong
    • Membrane Journal
    • /
    • v.17 no.2
    • /
    • pp.140-145
    • /
    • 2007
  • In this study, 3-(trihydroxysilyl)-1-propanesulfonic acid (THS-PSA) was added to poly(vinyl alcohol) (PVA) membranes crosslinked with poly(styrene sulfonic acid-co-maleic acid) (PSSA_MA) to improve the separation characteristics toward water vapors in the air. The prepared membranes varying both PSSA_MA and THS-PSA amounts were also synthesized at different cross linking temperatures. Then, in order to investigate the separation characteristics of the resulting membranes, the dynamic vapor sorption (DVS) and vapor permeation experiments were carried out. The increase of cross-linking temperature showed longer time to reach the equilibrium sorption state from the dynamic vapor sorption experiments. PVA/PSSA_MA (3%)/THA-PSA(7%) prepared at $120^{\circ}C$ gave the highest permeability of 480 barrer at $35^{\circ}C$.

Pervaporation Separation of Water/Alcohol Mixtures Using PVA/SSA/PSSA_MA Ion Exchange Membranes (PVA/SSA/PSSA_MA 이온교환막을 이용한 물-알코올 계의 투과증발 분리)

  • Jeon, Yi Seul;Rhim, Ji Won
    • Membrane Journal
    • /
    • v.25 no.4
    • /
    • pp.327-331
    • /
    • 2015
  • Poly(vinyl alcohol) (PVA) membranes cross-linked with sulfosuccinic acid (SSA) in which poly(4-styrene sulfonic acid-co-maleic acid) (PSSA_MA) was blended to endow more ion exchange capacity were prepared to measure the permselectivities of water-alcohol mixtures by pervaporation separation technique. The feed mixtures of binary aqueous methanol, ethanol and iso-propyl alcohol solution by 90 wt% alcohol portion were used. Typically, for PVA10/SSA9/PSSA_MA90 membrane, the flux of 202.6, 47.8, $20.2g/m^2hr$ for aqueous methanol, ethanol and iso-propyl alcohol solutions was shown while the best separation factors of 34.2, 291 and 991 were given by PVA10/SSA11/PSSA_MA80 membrane. More details are discussed in main text of this article.

Pervaporation Separation of Water-Ethanol Mixture Using Crosslinked PVA/PSSA_MA/TEOS Hybrid Membranes (PVA/PSSA_MA/TEOS 막을 이용한 물/에탄올 계의 투과증발 분리)

  • Rhim, Ji-Won;Lee, Byung-Seong;Kim, Dae-Hoon;Yoon, Seok-Won;Im, Hyeon-Soo;Moon, Go-Young;Nam, Sang-Yong
    • Membrane Journal
    • /
    • v.18 no.1
    • /
    • pp.44-52
    • /
    • 2008
  • Pervaporation separation for water-ethanol mixtures has been carried out using crosslinked poly(vinyl alcohol) (PVA) membranes with poly(styrene sulfonic acid-co-maleic acid) (PSSA_MA) and at which tetraethylorthosilicate (TEOS) was introduced. The concentration of PSSA_MA was fixed 7 wt% over PVA and the TEOS contents, 3, 5, and 7 wt%, were varied against PVA. The composition of the feed mixtures were 10, 20, 30 and 50 wt% of water in it. PVA/PSSA_MA/5 wt% TEOS membrane showed the separation factor, 1730 and the permeability, $16.3g/m^2{\cdot}hr$ for water : ethanol = 10 : 90 at $50^{\circ}C$.