핵 융합로 구조재료의 예민화 열처리에 따른 극저온 파괴거동 및 분극특성 (Cryogenic fracture behaviors and polarization characteristics according to sensitizing heat treatment on structural material of the nuclear fusion reactor)

  • 권일현;정세희
    • 대한기계학회논문집A
    • /
    • 제22권2호
    • /
    • pp.311-320
    • /
    • 1998
  • The cryogenic fracture behaviors of austenitic stainless steel HN2 developed for nuclear fusion reactor were evaluated quantitatively by using the small punch(SP) test. The electrochemical polarization test was applied to study thermal aging degradation of HN2 steel. The X-ray diffraction(XRD) analysis was conducted to detect carbides and nitrides precipitated on the grain boundary of the heat treated HN2 steel. The mechanical properties of the HN2 steel significantly decreased with increasing time and temperature of heat treatment or with decreasing testing temperature. The integrated charge(Q) obtained from electrochemical polarization test showed a good correlation with the SP energy(ESP) obtained by means of SP tests. From the results observed in the x-ray diffraction and anodic polarization curve, it was known that the material the grain boundary. Combining SP test and electrochemical polarization test, it could be useful tools to non-destructively evaluate the cryogenic fracture behaviors and the aging degradation for cryogenic structural material.

침지시험법 및 전기화학적 분극법에 의한 2205 이상 스테인리스강의 임계공식온도 측정 비교 (Critical Pitting Temperature of 2205 Duplex Stainless Steels Using Immersion and Electrochemical Polarization Test Methods)

  • 신재호;이재봉
    • 한국표면공학회지
    • /
    • 제39권1호
    • /
    • pp.18-24
    • /
    • 2006
  • Although stainless steels have the excellent corrosion resistance by passive film, they are susceptible to pitting corrosion in the environment containing halogen elements such as chloride ions. The resistance to pitting corrosion can be evaluated by measuring the critical pitting temperature (CPT). CPT values can be obtained using immersion, potentiodynamic and potentiostatic polarization test methods. Results on duplex 2205 stainless steels showed that CPT values were measured as $50^{\circ}C,\;55^{\circ}C\;and\;61^{\circ}C$, respectively for immersion, potentiodynamic and potentiostatic polarization test methods, depending upon the different test methods, even though the difference between CPT values are not much.

플라즈마 질화처리한 중, 고탄소저합금강의 내식성에 관한 연구 (Characteristics on Corrosion Resistance of Medium High Carbon Low Alloy Steels using Plasma Nitriding Process)

  • 이병찬
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제22권5호
    • /
    • pp.702-711
    • /
    • 1998
  • The characteristics of corrosion resistance for the surface of medium high carbon steels and low alloy steels utilizing as manufacturing the machinery structures and machining tools and treating by plasma/ion nitriding process have been studied in terms of electrochemical polarization behav-iors including corrosion potential(Ecorr) anodic polarization trends and polarization resistance(Rp) The seven base materials showed a clear passivation behavior for the polarization tests in the ASTM standard solution 1N ${H_2){SO_4}$ Although the treated surface by plasma nitriding for the seven test materials showed a significant increase in hardness the treatment gave a detri-mental effect in corrosion resistance. The various characteristics including corrosion potential polarization curves microstructures corrosion current polarization resistance among non-treat-ed nitriding and/or soft-nitriding treated specimens have been investigated and some of the mechanisms discussed.

  • PDF

보일러용 STS 444재 용접부의 수소취성에 미치는습기의 영향 (Effect of Humidity on the Hydrogen Embrittlement of STS 444 Weld Zone for Boiler)

  • 임우조;최병일;윤병두
    • 수산해양교육연구
    • /
    • 제18권1호
    • /
    • pp.58-64
    • /
    • 2006
  • In order to examine the effect of humidity on hydrogen embrittlement of STS 444 weld zone for boiler with dry and wet welding conditions, this paper was carried out the accelerated hydrogen osmosis test and the electrochemical Tafel polarization test. In 0.5M $H_2SO_4$ + 0.01M $As_20_3$ solution, this test is added to load of $1400kg/cm^2$ together with hydrogen osmosis by current of $50 {mA/cm^2}$ for 60 min.. The electrochemical Tafel polarization test was carried out in 0.5M $H_2SO_4$ + 0.01M $As_20_3$ solution. Therefore, the effect of humidity on hydrogen embrittlement of STS 444 was considered. The main results are as following: On the basis of hydrogen embrittlement mechanism, that is, integrated electrochemical polarization characteristics with the established mechanism of hydrogen embrittlement, the reduction rate of corrosion current density of weld zone in the wet weld condition is larger than in the dry condition. We can nondestructively predict the degree of hydrogen embrittlement of STS 444 weld zone for boiler through the reduction rate of electrochemical corrosion current density.

랩스케일 정삼투실험을 통한 정삼투막의 수투과도 평가 (Evaluation of water permeability of forward osmosis membranes using osmotically driven membrane test)

  • 이준서;김수한
    • 상하수도학회지
    • /
    • 제30권4호
    • /
    • pp.417-425
    • /
    • 2016
  • Desalination is a key technology to overcome water shortage problem in a near future. High energy consumption is an Achilles' heel in desalination technology. Osmotically driven membrane processes like forward osmosis(FO) was introduced to address this energy issue. Characterizing membrane properties such as water permeability(A), salt permeability(B), and the resistance to salt diffusion within the support layer($K_{ICP}$) are very important to predict the performance of scaled-up FO processes. Currently, most of researches reported that the water permeability of FO membrane was measured by reverse osmosis(RO) type test. Permeating direction of RO and FO are different and RO test needs hydraulic pressure so that several problems can be occurred(i.e. membrane deformation, compaction and effect of concentration polarization). This study focuses on measuring water permeability of FO membrane by FO type test results in various experimental conditions. A statistical approach was developed to evaluate the three FO membrane properties(A, B, and $K_{ICP}$) and it predicted test result by the internal and external concentration polarization model.

INTERPRETATION OF POLARIZATION RESPONSES OF URBAN AREA

  • Kang Moon-Kyung;Yoon Wang-Jung;Kim Kwang-Eun;Choi Hyun-Seok
    • 대한원격탐사학회:학술대회논문집
    • /
    • 대한원격탐사학회 2005년도 Proceedings of ISRS 2005
    • /
    • pp.534-537
    • /
    • 2005
  • Polarization of the radar wave refers to the ellipticity angle and orientation angle of the polarization ellipse. An evaluation of the polarization response can help understand the scattering mechanisms involved for a particular area of interest or provide information for image classification and algorithm section. C- and L-band polarization responses measured at urban area show the results that the polarization behavior for dihedral comer reflector or short, thin cylinder reflector appears at located in city streets or buildings site which are lined up and the polarization behavior for a large conducting sphere appears at parts of test site particularly river, flat, and vegetated areas. Also, the co- and cross-polarized response graphs and polarimetric parameters are discussed.

  • PDF

전기화학기법에 의한 슈퍼 오스테나이트 스테인리스강의 열화손상 평가 (An Evaluation of Degraded Damage for Superaustenitic Stainless Steel by Electrochemical Polarization Technique)

  • 권일현;이송인;백승세;이종기;;유효선
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 추계학술대회논문집A
    • /
    • pp.143-148
    • /
    • 2001
  • This research was undertaken to clarify effects of thermal aging on electrochemical and mechanical properties of superaustenitic stainless steel. The steel was artificially aged at $300{\sim}650^{\circ}C$ for $240{\sim}10,000hrs$. and investigated at $-196{\sim}650^{\circ}C$ using small punch(SP) test. Also, the change in electrochemical properties caused by effects of thermal aging was investigated using electrochemical anodic polarization test in a KOH electrolyte. Carbides and ${\eta}-phase(Fe_2Mo)$ precipitated in the grain bounderies seem to deteriorate the mechanical properties by decreasing cohesive strength in the grain bounderies and promote the current density observed in electrochemical polarization curves. The electrochemical and mechanical properties of superaustenitic stainless steel was drastically decreased in the specimen aged at $650^{\circ}C$.

  • PDF

저온분사코팅구리의 틈새부식 특성 평가 (Crevice Corrosion Evaluation of Cold Sprayed Copper)

  • 이민수;최희주
    • 방사성폐기물학회지
    • /
    • 제8권3호
    • /
    • pp.247-260
    • /
    • 2010
  • 한국원자력연구원 처분시스템개발과제에서는 처분용기 재료로 개발중인 저온분사코팅 구리에 대한 틈새부식(Crevice Corrosion) 시험을 실시하였다. 본 시험을 통하여 틈새에서의 부식의 발생여부와 발생되는 시점인 재부동태 전위(Repassivation Potential)를 측정하고자 하였다. 틈새부식 시험 방법으로 (1) ASTM G61-86 : Cyclic Potentiodynamic Polarization Measurements, (2) SWRI의 Potentiodynamic Polarization plus intermediate Potentiostatic Hold method, 그리고 (3) ASTM G192-08 (THE method) :Potentiodynamic- Galvanostatic -Potentiostatic Method 등의 3가지 방법을 소개하였다. 실제 저온분사 코팅구리의 부식시험에서는 ASTM G61-86에 따라서 틈새부식장치를 설치하고, 저온분사코팅구리가 KURT 지하수를 모사한 용액에서 어떻게 틈새부식이 일어나는지 살펴보았다. 전기적 부식조건으로는 Cyclic Polarization Test, Potentiostatic Polarization Test, 및 Electrochemical Impedance Spectroscopy 등을 사용하였다. 그리고 부식이 된 시편에 대해 Profilometer Measurement를 통해 실제 부식표면의 높낮이를 조사하여 틈새부식 유무를 관찰하였다. 최종적인 결론에서는 저온분사코팅구리는 틈새부식을 나타나지 않는다는 것을 확인할 수 있었다. 그리고 시험에 사용된 세종류의 구리에 대한 상대적인 부식평가를 한 결과, 부식전위를 나타내는 개방회로(Open Cell)에서의 전위는 구리의 제조방식과 상관없이 구리의 순도가 높을수록 높은 값을 보이는 것을 확인할 수 있었다. 결론적으로 KURT 심층지하수 조건에서는 구리는 틈새부식이 발생되지 않는다고 결론지었다.

치과주조용 Ti-20%Zr(-5%Cr)합금의 양극분극특성 (Anodic Polarization Characteristics in Ti-20%Zr(-5%Cr) Alloys for Dental Castings)

  • 정종현;한석윤
    • 대한치과기공학회지
    • /
    • 제26권1호
    • /
    • pp.41-48
    • /
    • 2004
  • Ti-20%Zr(-5%Cr) alloys not containing harmful Al and V were newly designed in order to reveal their possibility for dental casting and melted in an arc melting and casting furnace under Ar atmosphere. The corrosion resistance was studied by anodic polarization test. From the observation of anodic polarization behavior, it was found that the corrosion resistance was markedly increased by the addition of Cr. The corrosion resistance of Ti-20%Zr-5%Cr alloy was superior to that in Ti-6%Al-4%V alloy but almost similar to that in CP Ti using in market place today.

  • PDF

전기화학적 재활성화 분극시험에 의한 터빈부재의 열화손상 평가 (Degradation Damage Evaluation for Turbine Structural Components by Electrochemical Reactivation Polarization Test)

  • 권일현;백승세;류대영;유효선
    • 대한기계학회논문집A
    • /
    • 제26권7호
    • /
    • pp.1241-1249
    • /
    • 2002
  • The extent of materials deterioration can be evaluated accurately by mechanical test such as impact test or creep test. But it is almost impossible to extract a large test specimen from in-service components. Thus material degradation evaluation by non-destructive method is earnestly required. In this paper, the material degradation for virgin and several aged materials of a Cr-Mo-V steel, which is an candidated as structural material of the turbine casing components for electric power plant, is nondestructively evaluated by reactivation polarization testing method. And, the results obtained from the test are compared with those in small punch(SP) tests recommended as a semi-nondestructive testing method using miniaturized specimen. In contrast to the aged materials up to 1,000hrs which exhibit the degradation behaviors with increased ${\Delta}[DBTT]_{SP}$, the improvement of mechanical property can be observed on the 2,000hrs and 3,000hrs aged materials. This is because of the softening of material due to the carbide precipitation, the increase of ferritic structures and the recovery of dislocation microstructure by long-time heat treatment. The reactivation rates($I_R/I_{Crit},\;Q_R/Q_{Crit}$) calculated by reactivation current densityt ($I_R$) and charge($Q_R$) in the polarization curves exhibit a good correlation with ${\Delta}[DBTT]_{SP}$ behaviors.