  • In this experimental investigation, various plasma-sprayed zirconia contained coatings and a kind of alumina-zirconia coating were studied to gain a better understanding of their tribological behaviour under dry contact condition in a reciprocating motion at temperature of 200℃. Particular attention was made for finding appropriate coatings in cylinder liner/piston ring application with an emphasis on the antiwear property. In order to identify the wear mechanism, SEM(Scanning Electron Microscope), optical micrograph, and roughness tester were used. Alumina-zirconia and 8% yttria-zirconia were found to be most appropriate for the application to the cylinder liner/piston ring and, especially, alumina-zirconia exhibited highest wear-resistance and also showed good friction characteristics. Wear mechanisms of ceramic coatings identified.

  • PDF

THE EFFECTS OF SEALING ON THE PLASMA-SPRAYED OXIDE-BASED COATINGS

  • Kim, Hyung-Jun;Sidoine Odoul;Kweon, Young-Gak
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.53-58
    • /
    • 2002
  • Electrical insulation and mechanical properties of the plasma sprayed oxide ceramic coatings were studied before and after the sealing treatment of the ceramic coatings. Plasma sprayed A1$_2$O$_3$-TiO$_2$ coating as the reference coating was sealed using three commercial sealants based on polymer. Penetration depth of the sealants to the ceramic coating was evaluated directly from the optical microscope using a fluorescent dye. It is estimated that the penetration depth of the sealants to the ceramic coating is from 0.2 to 0.5 mm depending on the sealants used. The preliminary test results with a DC puncture tester imply that the dielectric breakdown voltage mechanism of plasma sprayed ceramic coatings has been determined to be a corona mechanism. Dielectric breakdown voltage of the as-sprayed and as-ground samples have shown a linear trend with regard to the thickness showing an average dielectric strength of 20 kV/mm for the thickness scale studied. It is also shown that grinding the coating before sealing and adding fluorescent dye do not agent the penetration depth of sealants. All of the microhardness, two-body abrasive wear resistance, bond strength, and surface roughness of the ceramic coating after the sealing treatment are improved. The extent of improvement is different from the sealants used. However, three-point bending stress of the ceramic coating after the sealing treatment is decreased. This is attributed to the reduced micro-crack toughening effect since the cracks propagate easily through the lamellar of the coating without crack deflection and/or branching after the sealing treatment.

  • PDF

고속가스플래임 용사법을 이용한 광촉매 $TiO_2$-생분해성 플라스틱 복합재료의 개발 (The Development of Functional Photocatalytic $TiO_2$-Biodegrdable Plastic Composite Material by HVOF Spraying)

  • 방희선;방한서
    • Journal of Welding and Joining
    • /
    • 제24권5호
    • /
    • pp.57-61
    • /
    • 2006
  • For the production of functional $TiO_2$-biodegradable plastic (polybutylene succinate:PBS) composite material with photocayalytic activity, we attempted to prepare $TiO_2$ coatings on PBS substrate by HVOF and plasma spraying techniques under various conditions. The microstructures of coatings were characterized with SEM and XRD analysis, and the photocatalytic efficiency of coatings was evaluated by the photo degradation of gaseous acetaldehyde. The effects of primary particle size and spraying parameters on the formation behavior, photocatalytic performance of the coatings have been investigated. The results indicated that for both the HVOF sprayed $P_{200}$ and $P_{30}$ coatings, the high anatase ratio of 100% can be achieved regardless of fuel gas pressure. On the other hand, the HVOF sprayed $P_7$ coating exhibited a largely decreased anatase ratio (from 100% to 49.1%) with increasing the fuel gas pressure, which may be attributed to much higher susceptibility of heat for 7 nm agglomerated powder. HVOF sprayed $P_{200}$ and $P_{30}$ coatings show better performance as compared to that of plasma sprayed $P_{200}$ coatings owing to the higher anatase ratio. However, the HVOF sprayed $P_7$ coatings did not show the photocatalytic activity, which may result from the extremely small reaction surface area to the photocatalytic activity and low anatase ratio.

Plasma-Sprayed $Al_2O_3-SiO_2$ Multi-Oxide Films on Stainless Steel Substrate

  • Korobova, N.;Soh, Deawha
    • 한국항해항만학회:학술대회논문집
    • /
    • 한국항해항만학회 2000년도 추계학술대회논문집
    • /
    • pp.116-119
    • /
    • 2000
  • The advantage of plasma-sprayed coating is their good resistance against thermal shock due to the porous state of the coated layer with a consequently low Youngs modulus. However, the existence of many pores with a bimodal distribution and a laminar structure in the coating reduces coating strength and oxidation protection of the base metals. In order to counteract these problems, there have been many efforts to obtain dense coatings by spraying under low pressure or vacuum and by controlling particle size and morphology of the spraying materials. The aim of the present study is to survey the effects of the HIP treatment between 1100 and 130$0^{\circ}C$ on plasma-sprayed oxide coating of A1$_2$O$_3$, A1$_2$O$_3$-SiO$_2$on the metal substrate (type C18N10T stainless steel). These effects were characterized by phase identification, Vickers hardness measurement, and tensile test before and after HIPing. These results show that high-pressure treatment has an advantage for improving adhesive strength and Vickers hardness of plasma-sprayed coatings.

  • PDF

Plasma-Sprayed $Al_{2}O_{3}-SiO_{2}$ Multi-Oxide Films on Stainless Steel Substrate

  • Korobova, N.;Soh, Deawha
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 추계학술대회 논문집
    • /
    • pp.116-119
    • /
    • 2000
  • The advantage of plasma-sprayed coating is their good resistance against thermal shock due to the porous state of the coated layer with a consequently low Youngs modules. However, the existence of many pores with a bimodal distribution and a laminar structure in the coating reduces coating strength and oxidation protection of the base metals. In order to counteract these problems, there have been many efforts to obtain dense coatings by spraying under low pressure or vacuum and by controlling particle size and morphology of the spraying materials. The aim of the present study is to survey the effects of the HIP treatment between 1100 and 130$0^{\circ}C$ on plasma-sprayed oxide coating of A1$_2$O$_3$, A1$_2$O$_3$-SiO$_2$ on the metal substrate (type C18N10T stainless steel). These effects were characterized by phase identification, Vickers hardness measurement, and tensile test before and after HIPing, These results show that high-pressure treatment has an advantage for improving adhesive strength and Vickers hardness of plasma- sprayed coatings.

  • PDF

플라즈마 용사 Al2O3 코팅의 특성에 미치는 CrO3 봉공처리의 영향 (Influence of CrO3 Sealing Treatment on Properties of Plasma Sprayed Al2O3 Coating)

  • 조경식;이현권;권정철
    • 한국세라믹학회지
    • /
    • 제48권2호
    • /
    • pp.160-167
    • /
    • 2011
  • Plasma sprayed ceramic coatings inherently contain pores and usually also cracks. Post-treatment of the plasma sprayed coatings is a way to close the connected pores and cracks. In this study, post-sealing treatment in plasma sprayed $Al_2O_3$ coatings was employed to overcome the reduction of coating properties. $Al_2O_3$ plasma thermal spray coating was made on aluminum alloys plate, $CrO_3$ post coating and heat treatment at $550^{\circ}C$ was carried out in order for final $Cr_2O_3$ to be saturated through phase transformation. Chromia sealing began at the fine defect in coated microstructure, while larger pores were permeated later. The increase in concentration and treatment frequency of sealing solution resulted in the decrease of porosity of coating layer, while cracks occurred partially after the third treatment. After twice treatment of 10M $CrO_3$ solution, microhardness and breakdown voltage of $Al_2O_3$ coatings were found to increase by ${\fallingdotseq}$ 50% and ${\fallingdotseq}$ 390% respectively than without post-treatment.

Wear Mechanism of Plasma-Sprayed Coating in Mo- and Co-Based Alloy

  • Lee, Soo W.
    • Tribology and Lubricants
    • /
    • 제11권5호
    • /
    • pp.108-113
    • /
    • 1995
  • Wear and friction behavior of plasma-sprayed coatings in Mo- and Co-based alloy were studied for the application of piston-ring automobile engine. The plasma-sprayed coatings were varied with gun current density, gas flow, and distance. The surface roughness, microhardness, and wear volume were measured depending on the spray distances. The high temperature hardness value were also measured as a function of temperature. Ball-on-disc geometry configuration tribometer was utilized in air. The wear tests were performed in the temperature ranges from room temperature to 825$^{\circ}$C to investigate the tribological trend of the piston-ring materials in the lack of lubricant. The cross sections of wear track were investigated, using microscopy.

크롬탄화물 용사피막의 접착력 및 잔류응력측정에 관한 연구 (A Study on the Adhesion Strength and Residual Stress Measurement of Plasma Sprayed Cr$_3$C$_2$-NiCr Coating)

  • 김의현;김종영
    • Journal of Welding and Joining
    • /
    • 제14권4호
    • /
    • pp.43-52
    • /
    • 1996
  • The plasma sprayed Cr$_{2}$C$_{2}$-NiCr coatings are widely used as wear-resistant and corrosion-resistant materials. The mechanical properties of the plasma sprayed Cr$_{2}$C$_{2}$-NiCr coatings were examined in this study. The distribution of the residual stress with the coating thickness was also examined by X-ray diffraction method. The pore in the coatings could be classified into two types ; one is the intrinsic pore originated from the spraying powder, the other is the extrinsic pore formed during spraying. During the tensile adhesion test, the fracture occurred at the interface of top coat and substrate or top coat and bond coat depending on the existence of bond coat. It was found that the compressive residual stress near the interface decreased with the increase of the top coat thickness. The tensile adhesion strength of the coating without bond coat was higher than that with bond coat, because the coating with bond coat has higher horizontal crack density near the interface between bond coat and top coat.

  • PDF

MoS$_2$$Fe_2O_3$ 첨가제가 지르코니아계 용사코팅층의 마모마찰 특성에 미치는 영향 (Effect of MoS$_2$ and $Fe_2O_3$ Additives on the Tribological Behavior of the Plasma Sprayed Zirconia Based Coatings)

  • 신종한;임대순;안효석
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1997년도 제26회 추계학술대회
    • /
    • pp.93-99
    • /
    • 1997
  • High Temperature wear behavior of plasma sprayed ZrO$_2$ and MoS$_2$, $Fe_2O_3$ coatings were investigated for high temperature wear resistance applications. The MoS$_2$, $Fe_2O_3$ added powders containing 2.5, 5.0, 7.5, 10.0 mol% of $MoS_2$, $Fe_2O_3$ for plasma spray were made by spray drying method. Wear test were performed at temperature ranges from room temperature to 600$\circ$C. The microstructural change of coatings and the worn. surface were examined by SEM and XRD. In ZrO$_2$ coating, the coefficient of friction and wear amount of room temperature to 400$\circ$C was increased with temperature and decreased with temperature over 400$\circ$C. The coefficient of friction and wear amount of MoS$_2$ added coatings were increased with temperature, but those of $Fe_2O_3$ added coatings had lower coefficient of friction and higher wear resistance than ZrO$_2$ coating.

  • PDF