• 제목/요약/키워드: Piezoelectric coefficient $d_{33}$

검색결과 66건 처리시간 0.021초

강유전체 고분자의 음의 압전 물성 및 상공존경계(MPB)에 대한 고찰 (Perspective on Ferroelectric Polymers Presenting Negative Longitudinal Piezoelectric Coefficient and Morphotropic Phase Boundary)

  • 임성빈;부상돈;정창규
    • 한국전기전자재료학회논문지
    • /
    • 제35권6호
    • /
    • pp.523-546
    • /
    • 2022
  • Morphotropic phase boundary (MPB), which is a special boundary that separates two or multiple different phases in the phase diagram of some ferroelectric ceramics, is an important concept in identifying physics that includes piezoelectric responses. MPB, which had not been discovered in organic materials until recently, was discovered in poly(vinylidene fluoride-co-trifluoroethylene (P(VDF-TrFE)), resulting from a molecular approach. The piezoelectric coefficient of P(VDF-TrFE) in this MPB region was achieved up to -63.5 pC N-1, which is about two times as large as the conventional value of -30 pC N-1 of P(VDF-TrFE). An order-disorder arrangement greatly affects the rise of the piezoelectric effect and the ferroelectric, paraelectric and relaxor ferroelectric of P(VDF-TrFE), so the arrangement and shape of the polymer chain is important. In this review, we investigate the origin of negative longitudinal piezoelectric coefficients of piezoelectric polymers, which is definitely opposite to those of common piezoelectric ceramics. In addition to the mainly discussed issue about MPB behaviors of ferroelectric polymers, we also introduce the consideration about polymer chirality resulting in relaxor ferroelectric properties. When the physics of ferroelectric polymers is unveiled, we can improve the piezoelectric and pyroelectric properties of ferroelectric polymers and contribute to the development of next-generation sensor, energy, transducer and actuator applications.

디스크형 압전 변압기의 전기적 특성 (Electric Characteristics of Disk-type Piezoelectric Transformer)

  • 김동수;김광일;김흥락;정우철;남효덕
    • 한국전기전자재료학회논문지
    • /
    • 제18권11호
    • /
    • pp.1007-1013
    • /
    • 2005
  • In this study, a step-down piezoelectric transformer was fabricated to utilize as an adapter for charging batteries of mobile electronic appliances. The ceramic part of the transformer is $Pb[(Mn_{1/3}Sb_{2/3})_{_0.05}Zr_{0.475}Ti_{0.475}]O_3$ with mechanical quality factor of 1600, electromechanical coupling coefficient $59\%$, and piezoelectric constant $d_{33}$ 1300, which can be utilized as a piezoelectric transformer. A simply fabricated disk-typed test pattern of diameter 28 mm and thickness 2 mm was used to characterize output voltage, step-down ratio as a function of electrode area with the input remained constant, and power, efficiency as a function of input voltage, and temperature-dependent electric characteristics were evaluated. The sample APT1 showed the best properties. The highest admittance, effective electromechanical coupling coefficient and an appropriate mechanical quality factor were obtained at the sample with the input/output area ratio of 1:1.5 at the common electrode, and the condition of 20 $V_{rms}$, $50\;\Omega$ made the maximum efficiency of $95\%$. The temperature was increased by 14.7'E as the input voltage was increased for $50\;V_{rms},\;50\;\Omega$.

Effect of Bias Magnetic Field on Magnetoelectric Characteristics in Magnetostrictive/Piezoelectric Laminate Composites

  • Chen, Lei;Luo, Yulin
    • Journal of Magnetics
    • /
    • 제20권4호
    • /
    • pp.347-352
    • /
    • 2015
  • The magnetoelectric (ME) characteristics for Terfenol-D/PZT laminate composite dependence on bias magnetic field is investigated. At low frequency, ME response is determined by the piezomagnetic coefficient $d_{33,m}$ and the elastic compliance $s_{33}^H$ of magnetostrictive material, $d_{33,m}$ and $s_{33}^H$ for Terfenol-D are inherently nonlinear and dependent on $H_{dc}$, leading to the influence of $H_{dc}$ on low-frequency ME voltage coefficient. At resonance, the mechanical quality factor $Q_m$ dependences on $H_{dc}$ results in the differences between the low-frequency and resonant ME voltage coefficient with $H_{dc}$. In terms of ${\Delta}E$ effect, the resonant frequency shift is derived with respect to the bias magnetic field. Considering the nonlinear effect of magnetostrictive material and $Q_m$ dependence on $H_{dc}$c, it predicts the low-frequency and resonant ME voltage coefficients as a function of the dc bias magnetic field. A good agreement between the theoretical results and experimental data is obtained and it is found that ME characteristics dependence on $H_{dc}$ are mainly influenced by the nonlinear effect of magnetostrictive material.

압전 특성의 보호층을 통한 리튬 금속 전지의 전기화학적 특성 개선 (The Enhanced Electrochemical Performance of Lithium Metal Batteries through the Piezoelectric Protective Layer)

  • 박대웅;신원호;손희상
    • 멤브레인
    • /
    • 제33권1호
    • /
    • pp.13-22
    • /
    • 2023
  • 리튬 금속 기반 전극의 높은 용량에도 불구하고, 제어가 어려운 덴드라이트 성장은 낮은 쿨롱 효율, 안전 문제를 야기해, 리튬금속 배터리의 상용화를 제한한다. 본 연구에서는 압전 복합체인 BaTiO3/PVDF (BTO@PVDF) 기반 보호층을 리튬금속에 코팅, 덴드라이트에 의한 부피팽창으로 발생한 변형을 분극을 이용하여, 리튬 금속 전극의 안정성 및 성능을 향상하고자 한다. 이를 통해, 균일한 리튬이온의 증착이 가능해졌으며, BTO@PVDF 전극은 100 사이클 동안 약 98.1% 이상의 쿨롱 효율을 나타내었다. 또한, CV를 통해 향상된 리튬이온의 확산계수(DLi+) 증가를 보였으며, 본 연구에서 제시된 전략은 리튬 금속 전극의 성능 향상에 새로운 길을 나타내준다.

Zr/Ti 몰비에 따른 PZT-PCNS 압전 세라믹의 압전 및 유전 특성 (The Dielertric and Piezoelectric Properties of PZT-PCNS Piezoelectric Ceramics with Zr/Ti Mole Ratio)

  • 이시용;이용회;이문주;이종섭;임기조
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.100-102
    • /
    • 2001
  • In this paper, the piezoelectric and dielectric properties of $Pb(Zr_xTi_{1-x)O_3$ - $Pb(Co_{1/3}Nb_{1/3})O_3)$ piezoelectric ceramics have been investigated as a function of Zr/Ti mole ratio. From the results, when Zr/Ti mole ratio is 49/51, electromechanical coupling coefficient($k_p$), piezoelectric strain constant($d_{33}$) mechanical quality factor($Q_m$), and Permittivity(${{\varepsilon}_{33}}^T/{\varepsilon}_0$) is 64[%], 469[PC/N], 360 and 2000, respectively. Morphotropic Phase Boundary is Zr/Ti mole ratio(49/51) from XRD analysis. Also. From SEM observation, when sintering temperature is 1150[$^{\circ}C$], grain size is about $1{\sim}2[{\mu}m]$ and maximum sintering density is 7.85[$g/cm^3$].

  • PDF

다공질 PZT 세라믹의 압전 및 음향 특성 (Piezoelectric and Acoustic Properties of Porous PZT Ceramics)

  • 박정학;최헌일;사공건
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1994년도 추계학술대회 논문집
    • /
    • pp.183-186
    • /
    • 1994
  • Porous piezoelectric ceramics of P7T have been newly developed to apply for transducers in an echo sounder PZT powders were prepared by the molten salt synthesis method. The porous PZT was prepared from a mixture of PZT and polyvinylalcohol(PVA) powders by BURPS(Burnout Plastic Sphere) technique. The piezoelectric and acoustic properties with various PVA wt.% have studied. The density of porous PZT ceramics was decreased linearly with increasing the PVA sphere wt.%. Piezoelectric coefficient d$\_$33/ of porous PZT ceramics was almost same to that of single phase PZT ceramics. The thickness mode coupling factor k$\_$t/ was ranged over 0.53∼0.59 comparable with the single phase PZT ceramics(k$\_$t/=0.7).

온도 및 압축응력 변화에 따른 PIN-PMN-PT 단결정의 유전 및 압전 특성 (Effect of Temperature and Compressive Stress on the Dielectric and Piezoelectric Properties of PIN-PMN-PT Single Crystal)

  • 임재광;박재환;이정호;이상구
    • 마이크로전자및패키징학회지
    • /
    • 제26권4호
    • /
    • pp.63-68
    • /
    • 2019
  • 온도 및 압축응력 변화에 따른 PIN-PMN-PT계 압전 단결정의 유전 특성과 압전 특성을 조사하였다. 단결정의 결정상은 110℃ 영역에서 강유전 rhombohedral 구조에서 tetragonal 구조로, 190℃ 영역에서 tetragonal 구조로부터 상유전 cubic 구조로 변화하였다. 전계 인가에 따른 분극 및 변위의 변화율로부터 압전상수와 비유전율을 계산하였으며, 이는 계측기로부터 측정된 값과 유사한 수준을 나타내었다. 샘플에 인가되는 압축응력이 증가할수록 압전상수 d33과 비유전율값은 증가하는 경향성을 나타내었다. 측정 온도 5℃에서 샘플에 인가되는 압축응력이 60 MPa인 경우 d33 값이 4500 pC/N로 계산되었으며, 측정 온도 60℃인 경우, 샘플에 인가되는 압축응력이 40 MPa 일 때 비유전율 62000이 계산되었다. 압축응력이 높아질 때 압전상수와 비유전율 값이 상승한 것은 rhombohedral 상에서 orthorhombic 상으로의 전이에 기인한 것으로 판단된다.

Two-Step 소결법을 통한 0.96(K0.456Na0.536)Nb0.95Sb0.05-0.04Bi0.5(Na0.82K0.18)0.5ZrO3 무연 압전 세라믹의 밀도 및 압전 특성 향상 (Enhancement of Density and Piezoelectric Properties of 0.96(K0.456Na0.536)Nb0.95Sb0.05-0.04Bi0.5(Na0.82K0.18)0.5ZrO3 Lead-Free Piezoelectric Ceramics through Two-Step Sintering Method)

  • 유일열;박상현;최성희;조경훈
    • 한국재료학회지
    • /
    • 제34권2호
    • /
    • pp.116-124
    • /
    • 2024
  • In this study, we investigated the microstructure and piezoelectric properties of 0.96(K0.456Na0.536)Nb0.95Sb0.05-0.04Bi0.5(Na0.82K0.18)0.5ZrO3 (KNNS-BNKZ) ceramics based on one-step and two-step sintering processes. One-step sintering led to significant abnormal grain (AG) growth at temperatures above 1,085 ℃. With increasing sintering temperature, piezoelectric and dielectric properties were enhanced, resulting in a high d33 = 506 pC/N for one-step specimen sintered at 1,100 ℃ (one-step 1,100 ℃ specimen). However, for one-step 1,115 ℃ specimen, a slight decrease in d33 was observed, emphasizing the importance of a high tetragonal (T) phase fraction for superior piezoelectric properties. Achieving a relative density above 84 % for samples sintered by the one-step sintering process was challenging. Conversely, two-step sintering significantly improved the relative density of KNNS-BNKZ ceramics up to 96 %, attributed to the control of AG nucleation in the first step and grain growth rate control in the second step. The quantity of AG nucleation was affected by the duration of the first step, determining the final microstructure. Despite having a lower T phase fraction than that of the one-step 1,100 ℃ specimen, the two-step specimen exhibited higher piezoelectric coefficients (d33 = 574 pC/N and kp = 0.5) than those of the one-step 1,100 ℃ specimen due to its higher relative density. Performance evaluation of magnetoelectric composite devices composed of one-step and two-step specimens showed that despite having a higher g33, the magnetoelectric composite with the one-step 1,100 ℃ specimen exhibited the lowest magnetoelectric voltage coefficient, due to its lowest kp. This study highlights the essential role of phase fraction and relative density in enhancing the performance of piezoelectric materials and devices, showcasing the effectiveness of the two-step sintering process for controlling the microstructure of ceramic materials containing volatile elements.

적층형 PMN-PZT 세라믹 압전 액추에이터의 열화특성 (Aging Phenomena of Multilayered PMN-PZT Ceramic Actuator)

  • 송재성;정순종;김인성;이원재;이동윤
    • 한국전기전자재료학회논문지
    • /
    • 제18권5호
    • /
    • pp.445-449
    • /
    • 2005
  • Aging phenomena of 0.2PMN-0.8PZT multilayered ceramic actuators(MCA) have been investigated at the room temperature. The piezoelectric materials were synthesized as conventional ceramic process, and MCA were fabricatedby tape casting methods. The crystalline structures and lattice parameters were investigated by X-ray diffraction analysis, showing the structure was tetragonal and c/a was about 1.01. And, the effective electromechanical coupling coefficient keff and pseudo-piezoelectric constant $d_{33}$were measured. Variable unipolar electric fields, $2{\sim}4kV/mm$, were applied to MCh to investigate the aging characteristics. After 2 kV/mm unipolar electric field, keff and $d_{33}$ were 0.454 and 4.44 respectively. The measured and simulated values using for aging phenomena analysis, had a good fit to the linear logarithmic stretched exponential law.

PMWN-PZT계 압전세라믹의 압전 및 유전특성 (Characteristics of Piezoelectric and dielectric of PMWN-PZT Ceramics)

  • 홍종국;이종섭;채홍인;윤만순;정수현
    • 한국전기전자재료학회논문지
    • /
    • 제14권6호
    • /
    • pp.455-459
    • /
    • 2001
  • In this paper, the dielectric and pizoelectric properties of 0.05Pb(M $n_{04}$ $W_{0.2}$N $b_{0.4}$) $O_3$-0.95(PbZ $r_{x}$ $Ti_{1-x}$ ) $O_3$+yN $b_2$ $O_{5}$ , are investigated as a function of the mole ratio of Zr and the amount of N $b_2$ $O_{5}$ . Also, the phase is analyzed by XRD. When the mole ratio of Zr is 0.51, the electromechanical coupling coefficient( $k_{p}$ ), relative dielectric constant ($\varepsilon$$^{T}$ $_{33}$ /$\varepsilon$$_{0}$ ), piezoelectric stain constrain ( $d_{33}$ and dielectric loss tangent show maximum, while the mechanical quality factor shows minimum value ; $k_{p}$ =56.5%, $d_{33}$ =258pC/N, $\varepsilon$$^{T}$ $_{33}$ /$\varepsilon$$_{0}$ =1170, $Q_{m}$ =1150, tan$\delta$=0.51%. At that composition, MPB which rhombohedral and tetragonal phase coexist in this ternary system is shown by the results of XRD analysis. Also, when the amount of N $b_2$ $O_{5}$ is 0.3wt%, the mechanical quality factor is increased to about 2000. The phase transition temperature of the ternary piezoelectric ceramic system showed about 35$0^{\circ}C$.TEX>.>.>.

  • PDF