탄산염 성분이 포함된 사질토의 장기침하 예측 (Prediction of Long-Term Settlement of Sands Containing Carbonates)

  • 황웅기;이용수;황중호;김태형
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2009년도 춘계 학술발표회
    • /
    • pp.993-998
    • /
    • 2009
  • This study was conducted to propose the model that is able to predict long-term settlement of sands containing carbonates. We can observe that in addition to the initial elastic compression, a considerable additional compression occurs with long-term period in some sands. The compressibility of sands is significantly dependent on particle characteristics. Some sands have many pores and particularly has an angular shape. To predict of long-term settlement of these sands which contain carbonates, first of all a variety of tests which are to assess chemical, physical and compression characteristics of these sands were conducted. Second, in order to know settlement with time, the time parameter was determined by analyzing the measured data obtained from $\bigcirc\bigcirc$ area. The measured settlement of this area shows that in addition to the initial elastic compression, a considerable additional compression occurring with time. It was caused by the crushing, shattering, and rearrangement of particles, which were real phenomena in sandy soils under loading condition. Based on this case study, we proposed that a simple method is able to predict settlement with time of sandy soil containing carbonates.

  • PDF

WC/Co 초경 스크랩 산화물의 고체탄소에 의한 환원/침탄 (Carbothermal Reduction of Oxide Powder Prepared from Waste WC/Co Hardmetal by Solid Carbon)

  • 이길근;하국현
    • 한국분말재료학회지
    • /
    • 제12권2호
    • /
    • pp.112-116
    • /
    • 2005
  • In the present study, the focus is on the analysis of carbothermal reduction of oxide powder prepared from waste WC/Co hardmetal by solid carbon under a stream of argon for the recycling of the WC/Co hard-metal. The oxide powder was prepared by the combination of the oxidation and crushing processes using the waste $WC-8 wt.\%Co$ hardmetal as the raw material. This oxide powder was mixed with carbon black, and then this mixture was carbothermally reduced under a flowing argon atmosphere. The changes in the phase structure and gases discharge of the mixture during carbothermal reduction was analysed using XRD and gas analyzer. The oxide powder prepared from waste $WC-8wt.\%Co$ hardmetal has a mixture of $WO_{3} and CoWO_{4}$. This oxide powder reduced at about $850^{\circ}C$, formed tungsten carbides at about $950^{\circ}C$, and then fully transformed to a mixed state of tungsten carbide (WC) and cobalt at about $1100^{\circ}C$ by solid carbon under a stream of argon. The WC/Co composite powder synthesized at $1000^{\circ}C$ for 6 hours from oxide powder of waste $WC-8wt.\%Co$ hardmetal has an average particle size of $0.3 {\mu}m$.

토목 발파가 소음, 진동, 부유 분진에 미치는 영향 (Effects of Civil Blasting on Noise, Vibration and Total Suspended Particles)

  • 정진도;정영국
    • 한국환경과학회지
    • /
    • 제13권1호
    • /
    • pp.99-107
    • /
    • 2004
  • This research is to determine the level of environmental pollution at a blasting construction area which is the origin of noise, vibration, and suspended particle, and to compare the results with other domestic and international standard data. This experiment is also to find out the effects resulting from blasting construction and to propose a plan that can decrease environmental pollution. The blasting construction area is a factory site which is about one and half million square meter and sewage disposal plant is about ninety thousand square meter. Both were selected as the areas for the tests to be conducted in determination test. The test to determine the level of noise, vibration, and total suspended particle was conducted thirty times around the blasting construction area by comparing measurement results and numerical analysis. However, as the test was not conducted in the laboratory but in the actual blasting construction area, it was not possible to do the test with the same exact conditions each true. Therefore, the test was not ideal as conditions could change from test to test. For the most part, the level of noise was below the standard level of 70dB. Every vibration test was under the standard limitation. For example, a house, 200m away was tested for noise and vibration and the level was found to be under the 0.2 cm/sec which is the standard for specialty designed cultural sites., i.e very low level. Also a buried oil pipeline that was 30m away also marked under 2.0cm/sec which is the norm for an industrial area. However, if there were an oil pipeline under the house, the amount of charging gunpowder per hole should be decreased compared to the amount used in the test. The test result for suspended particles under the standard limitation which is 24hour average 300$\mu\textrm{g}$/㎥ at a distance from blasting wavelength, but at detonator, total suspended particle from the blast origin exceeded the standard limitation. If explosion occurs when it detonates in the hole, most of the energy would be absorbed in the crushing of rocks, but some remaining energy would make noises and vibration inevitable. So the important thing is how to minimize the environmental pollution from the blasting. There should be regulations in order that the standard limitation is not exceeded, and to decrease the environmental pollution from the blasting.

해체·제거 작업 시 석면함유 건축자재에서 발생되는 섬유 및 입자상 물질의 특성 (Characteristics of Generated Fibrous/Particulate Matters from Asbestos-Containing Building Materials(ACBMs))

  • 최성원;장광명;박경훈;김대종;김현욱
    • 한국산업보건학회지
    • /
    • 제25권2호
    • /
    • pp.184-193
    • /
    • 2015
  • Objectives: This study focused on three aspects: characterizing concentrations of airborne particles by size distributions and asbestos fibers generated by various building materials; analyzing the characteristics of fibers produced by each simulation and asbestos fibers released from ACBMs; and investigating correlations of airborne asbestos fibers and particles generated and association of particle and asbestos concentrations. Methods: We selected three ACBMs including an insulation board, cement asbestos slate and wallboard. We constructed 4 scenarios; a) crushing with a hammer; b) cutting with a industrial knife; c) brushing with a metal brush; and d) tightening & loosening with a hand drill. We implemented one simulation for 30 seconds followed by 30 seconds resting period. We repeated a total of 5 cycles for 5 minutes. Results: The highest concentration of particulate & fibrous matters was from crushing with a hammer in each scenario followed by brushing with a metal brush, cutting with a industrial knife, and tightening & loosening with a hand drill. For ACBMs studied, asbestos concentrations were highest from an insulation board followed by cement asbestos slate, and wallboard. No difference in terms of concentration was found between an insulation board and asbestos slate. Fibers with $5{\sim}20{\mu}m$ in length were included in 76~90% of total fibrous matters. The distribution of the straight form fibers was greater than that of the curl form. About 90% of $PM_{Total}$ released from ACBMs was consisted of $PM_{10}$ while only 10% of $PM_{Total}$ was $PM_{2.5}$. Particulate matters like $PM_{2.5}$ was significantly correlated with fibrous matters($R^2=0.81$). Conclusions: We found ACBMs can significantly release asbestos fibers as well as $PM_{2.5}$. Concentrations of asbestos generated by ACBMs were well correlated with $PM_{2.5}$.

이산화탄소의 탄산화 반응을 이용한 되메움재용 순환골재의 품질 개량: 5kg급 프로토타입 반응조 개발 (Quality Enhancement of Recycled Concrete Aggregates for Backfill Materials by CO2 Carbonation: Development of a 5-kg-scale Prototype Reactor)

  • 김진우;전민경;권태혁;김남룡
    • 한국지반공학회논문집
    • /
    • 제40권1호
    • /
    • pp.29-37
    • /
    • 2024
  • 본 연구에서는 이산화탄소 처리를 통한 순환골재의 지반공학적 성능 개량을 평가하기 위하여 5kg급 프로토타입 반응조를 제작하였다. 제작된 반응조를 이용하여 이산화탄소 처리한 순환골재와 미처리 순환골재의 골재 파쇄값과 노상토지지력비를 측정하였다. 이산화탄소 처리를 통해 골재 파쇄값은 35.6%에서 33.2%로 2.4% 감소하고 노상토지 지력비는 97.5%에서 102.4%로 4.9% 증가하는 것이 관찰되었다. 탄산화 반응을 통해 생성된 탄산칼슘 염으로 인해 순환골재의 세립분 생성이 감소하고 지지력이 증가함을 알 수 있었다. 또한 교반을 함께할 경우 추가적인 역학적 개량 효과를 통해 골재 파쇄값이 30.3%로 감소하고 노상토지지력비는 137.7%로 증가하였다. 본 연구에서 기술된 이산화탄소 처리 기술의 현장 적용 시 건설 산업의 탄소배출을 효과적으로 줄일 수 있을 것으로 보인다.

다짐 풍화잔적토의 거동특성 연구 (Behavioral Characteristics of Decomposed Residual Solis)

  • 이인모;이승철;김용진
    • 한국지반공학회지:지반
    • /
    • 제12권6호
    • /
    • pp.115-126
    • /
    • 1996
  • 삼축압축시험의 결과를 이용해 2차광물성분을 많이 포함하고 있는 모앙이 편마암인 풍화잔적토의 압축 및 강도특성을 분석하여, 모암 및 광물성분비가 다른 기존의 연구결과와 비교하여 풍화잔적토의 모암과 광물성부네 따른 강도정수의 차이 및 거동특성을 파악하기 위한 근간을 제시하고자 본 연구를 수행하였으며, 치를 위하여 CIV, CID, CKoU, CKoD 등의 삼축압축시험을 실시하였다. 기원 및 광물성분이 다른 풍화잔적토라도 정규압축곡선(NCL)의 기울기는 유사한 양상을 보이며, 압축시 입자파쇄효과로 인하여 약 85%의 소성변형량을 나타냈다. 전단시 또이동 시료는 김천 및 안동 시료와는 다르게 응력연화현상을 나타내 기원 및 구성광물에 따라 다른 거동을 보여줌을 알 수 있었다. 펀단저항각은 시료가 석영과 장석성분 등의 1차 광물과 2차광물의 구성성 분에 따라 달라짐을 알 수 있었으며, 반면에 간극수압계수는 기원 및 광물성분을 막론하고 1 이상의 큰 값을 나타냈다.

  • PDF

플라이애시와 폐유리분말을 사용한 외단열용 마감모르타르의 고온 특성 (High Temperature Properties in Finishing Mortars of Exterior Insulation Finishing System Using Fly Ash and Waste Glass Powder)

  • 송훈;신현욱
    • 자원리싸이클링
    • /
    • 제28권6호
    • /
    • pp.64-72
    • /
    • 2019
  • 플라이애시는 발전소의 탄종 및 품질에 따라 화학조성이 다르고 품질 변화가 크며 탄소함량과 입경에 따라 분류하며, 폐유리분말은 파유리를 분쇄하여 제조하고 분쇄정도에 따라 분류한다. 건축물의 외단열 공법은 경제적이면서 단열성능이 우수한 폴리스티렌 폼 단열재를 활용한 공법이 일반적이다. 하지만 유기계 단열재는 단열성능이 우수하나 화재에 취약하고 다수의 문제점이 지적되었다. 본 연구에서는 플라이애시와 폐유리분말을 사용하여 고온에서 안정한 외단열용 마감모르타르를 제작하고 고온 강도 및 난연 특성을 검토하였다. 실험 결과, 플라이애시와 폐유리분말을 이용한 마감모르타르는 고온에서의 안전성이 높았다. 하지만 강도감소의 폭이 크므로 적절한 배합조건의 선정이 필요하다.

분뇨잔사(糞尿殘渣)를 이용(利用)한 유기종합비료(有機綜合肥料) 개발(開發) (Development of Organic Compound Fertilizer Based on Treated Human Waste)

  • 신제성;성기석;임동규
    • 한국토양비료학회지
    • /
    • 제17권1호
    • /
    • pp.55-59
    • /
    • 1984
  • 습식(濕式) 분뇨잔사중(糞尿殘渣中)의 인산(燐酸) 및 유기물(有機物)을 주축(主軸)으로하여 유기종합비료(有機綜合肥料)를 제조(製造)하였다. 분뇨잔사중(糞尿殘渣中)의 인산(燐酸) 가용율(可溶率)을 증가(增加)시키기 위하여 황산 및 당밀폐액을 처리(處理)하여 후숙시켰으며 황산 0.1N처리후(處理後) 24시간(時間) 후숙시킨 것이 인산(燐酸)의 가용율(可溶率)이 가장 높았다. 시제품(試製品)의 입도분포(粒度分布)는 접착제(接着劑)로 첨가(添加)된 당밀폐액양(量)에 따라 차이(差異)가 있었으며 양(量)이 증가(增加)될수록 입도(粒度)가 증가(增加)되었다. 시제품(試製品)의 입도(粒度)가 클수록 경도(硬度)는 증가(增加)되었으며 접착제(接着劑)로 처가(添加)된 당밀페액양(量)이 12.5%일 때 입자(粒子)의 경도(硬度)가 가장 높게 나타났다. 시제품(試製品)의 흡습도(吸濕度)는 요소(尿素)에 비(比)하여 대단(大端)히 높았으며 이는 시제품(試製品)의 물리(物理) 화학적(化學的) 특성(特性)에 기인(起因)되었다.

  • PDF

천연 Zeollte로부터 열수합성에 의한 주상 Na-P Zeolite합성 (Synthesis of Columnar Na-P Zeolite by Hydrothermal Process from Natural Zeolite of Korea)

  • 장용선;정필균;김상효
    • 한국토양비료학회지
    • /
    • 제36권6호
    • /
    • pp.357-366
    • /
    • 2003
  • 본 연구는 천연 zeolite를 파쇄하여 일정크기의 입제를 생산하는 과정에서 부산물로 생산되는 다량의 미분을 이용하여 양이온치환용량이 높은 입상의 흡착제를 개발할 목적으로 수행하였다. 천연 zeolite를 알카리 용액의 열수합성법을 활용하여 Na-P zeolite로 전환시켰다. 반응시간별 합성과정 중 광물학적 특성 변화를 X-선회절, 주사전자현미경, 화학조성 및 CEC의 변화를 통하여 구명하였다. 주상 Na-P zeolite의 입단은 천연 zeolite-숯혼합물을 약 3 mm 두께로 압축성형한 후 열처리하였으며, 연속적인 3 M NaOH 처리로 천연 zeolite의 주요구성광물인 climoptile, moderite, 장석 등의 광물이 파괴되고 새로이 구형의 Na-P zeolite가 24시간 처리에서 관찰되었다. 반응시간이 증가함에 따라 잔류용액 중 Si/AI비는 감소하였으며, 입단 크기의 증가에도 불구하고 Na-P zeolite의 CEC는 출발물질로 사용된 미분의 천연 zeolite에 비하여 2배 이상 증가하였다.

무기안료의 제조 및 특성에 관한 연구 (Preparation and Characteristics of Inorganic Pigments)

  • 오세중
    • 한국산학기술학회논문지
    • /
    • 제14권6호
    • /
    • pp.3102-3107
    • /
    • 2013
  • $Al_2O_3$, CoO, $Cr_2O_3$, ZnO, $SrO_2$ 및 Kaolin을 이용하여 무기안료를 제조하였다. 제조방법은 원료분말들을 일정비율로 배합하고 분쇄한 후 소성을 시키고 분쇄 및 건조과정을 거쳐 제조하였다. 안료의 원료 중 $Cr_2O_3$의 비율이 증가할수록 청색에서 녹색으로 발현되는 것을 알 수 있었으며 안료의 조성에 관계없이 소성시킨 안료의 입자크기가 작아질수록 색도가 밝아지는 것을 알 수 있었다. 그리고 소성시 최고온도는 $1,250^{\circ}C$정도가 가장 적합한 것으로 조사되었다. 안료의 유약적합성 실험에서는 안료 성분 중 $Cr_2O_3$의 비율이 증가할수록 녹색에 가까워졌으며 CoO의 비율이 증가할수록 청색감이 증가하였다.