  • Laser induced surface activation (LISA) technology requires refined selection of process variables to fabricate conductive microcircuits on a general polymer material. Among the process variables, laser mode is one of the crucial factors to make a reliable conductor pattern. Here we compare the continuous wave (CW) laser mode with the pulse wave (PW) laser mode through determination of the surface roughness and circuit accuracy. In the CW laser mode, the surface roughness is pronounced during the implementation of the conductive circuit, which results in uneven plating. In the PW laser mode, the surface is relatively smooth and uniform, and the formed conductive circuit layer has few defects with excellent adhesion to the polymer material. As a result of a change of laser mode from CW to PW, the value of Ra of the polymer material decreases from 0.6 ㎛ to 0.2 ㎛; the value of Ra after the plating process decreases from 0.8 ㎛ to 0.4 ㎛, and a tight bonding force between the polymer source material and the conductive copper plating layer is achieved. In conclusion, this study shows that the PW laser process yields an excellent conductive circuit on a polymeric material.

Topics on Power Photonics for High-Power Solid-state Laser

  • Nakatsuka, Masahiro
    • 한국광학회:학술대회논문집
    • /
    • 한국광학회 2003년도 하계학술발표회
    • /
    • pp.6-7
    • /
    • 2003
  • The inertial fusion research at ILE, Osaka moves to the fast ignition scheme with using PW laser system to achieve hot core plasma of keV-temperature by heating additionally the dense plasma imploded by the multi-beam Gekko laser system. The solid-state lasers have been developed of the peak-power from TW to PW region with the chirped pulse amplification (CPA) and optical parametric amplification (OPA) technology. (omitted)

  • PDF

Design of a Femtosecond Ti:sapphire Laser for Generation and Temporal Optimization of 0.5-PW Laser Pulses at a 0.1-Hz Repetition Rate

  • Sung, Jae-Hee;Yu, Tae-Jun;Lee, Seong-Ku;Jeong, Tae-Moon;Choi, Il-Woo;Ko, Do-Kyeong;Lee, Jong-Min
    • Journal of the Optical Society of Korea
    • /
    • 제13권1호
    • /
    • pp.53-59
    • /
    • 2009
  • A chirped-pulse amplification Ti:sapphire laser system has been designed using a 10-Hz 100-TW Ti:sapphire laser to generate 0.1-Hz 0.5-PW laser pulses and optimize their temporal qualities such as temporal contrast and pulse duration. A high-energy booster amplifier to be added is expected to produce an energy above 30 J through the parasitic lasing suppression and the efficient amplification. To improve the temporal contrast of the laser pulses, a high-contrast 1-kHz amplifier system is used as a front-end. A grating stretcher which makes the laser pulse have 1-ns duration is used to prevent optical damages due to high pulse energy during amplification. A grating compressor has been designed with group delay analysis to obtain the recompressed pulse duration close to the transform-limited pulse duration. The final laser pulses are expected to have energy above 20 J and duration below 40 fs.

$CO_2$ Laser Heating Pulling Method를 이용한 광섬유 탐침 제작 (Manufacture of Optical fiber probe Using $CO_2$ Laser Heating Pulling Method)

  • 신수용;박준도;황보승;강용철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.468-470
    • /
    • 2005
  • 본 연구에서는 NSOM(Near-field Scanning Optical Microscope)에서 정밀도의 중요한 요소로 작용하는 100 ~ 200nm Scale의 Optical aperture를 제작하기 위해 Optical Fiber를 이용하여 $CO_2$ Laser Heating Pulling Method에 의하여 제작하고자 한다. Heating Pulling Method 에서 Fiber Tip의 정밀도 및 제작 재현성에 영향을 미치는 중요한 기존의 여러 Fiber Tip 구현방법 중 본 연구에서는 Pulse Width[$PW_{(SEC)}$] 와 Pulling Force 두 요소에 있어서 상호관계를 연구하였으며, 연구 결과 두 변수간의 최적화된 파라미터인 PW 0.07 ~ $0.10_{(SEC)}$ 와 Pulling force 0.2 ~ 0.81b의 구간에서 error율이 최소화되는 범위를 찾을 수 있었고, 그 결과 최적의 상태는 $0.08_{(SEC)}$와 0.21b에서 팁들은 첨예화 되었고 95% 이상의 재현성 및 신뢰성을 얻을 수 있었다.

  • PDF

시뮬레이션을 통한 레이저 융삭 추진의 우주 쓰레기 제거 응용 가능성 연구 (Research on Applicability of Laser Ablation Propulsion to Space Debris Removal by Simulations)

  • 유성문;이승민
    • 한국군사과학기술학회지
    • /
    • 제25권2호
    • /
    • pp.169-176
    • /
    • 2022
  • Laser ablation propulsion(LAP) is the method to create impulse by laser ablation. It can be used to deorbit the space debris(SD), as its long-range property and versatility on any material. In this paper, we find out several requirements of the LAP system(LAPS) to deorbit the SD by simple numerical calculations of the SD orbit and laser beam flux. As a result, minimum operable altitude angle turned out to be a crucial variable to the LAPS. Moreover, if minimum operable altitude angle is 10°, and if the minimum distance between the LAPS and the SD is below 450 km, 1 m/s2 is sufficient to deorbit the SD by once. With 18 kJ/3 ns pulsed laser and cube shaped 100 kg SD, 1 m/s2 acceleration can be achieved by increasing the pulse repetition rate over 34~53 Hz, depending on the size of the SD. This capability could compare with the conceptual design of the Japan Establishment for a Power-laser Community Harvest(J-EPoCH) facility, which include 8 kJ, 5 PW@100 Hz laser.

헤테로폴리산 촉매를 이용한 TAME, ETBE 및 MTBE 합성반응의 연구 (Synthesis of TAME, ETBE, and MTBE Using Heteropolyacid Catalyst)

  • 박진화;이용우
    • 공업화학
    • /
    • 제8권4호
    • /
    • pp.582-588
    • /
    • 1997
  • 고체산 촉매인 헤테로폴리산 촉매를 이용하여 대기오염 방지를 위한 옥탄가 향상제인 TAME, ETBE 및 MTBE 합성반응에 대한 실험을 고정층 상압유통식 반응장치에서 수행하였다. 일반적으로 TAME, ETBE 및 MTBE 합성반응에서 헤테로폴리산에 hetero원자와 poly원자를 치환시켜 비교한 결과, 배위된 poly원자가 W, hetero원자가 Si인 $H_4SiW_{12}O_{40}$ 촉매의 활성이 가장 우수하였고, 또한 치환된 금속에 따라 촉매의 활성이 달랐으며 이는 촉매의 산성질과 관련이 있음을 알 수 있었다. 헤테로폴리산 촉매를 이용한 합성반응에서 TAME 경우는 $FeHPW_{12}O_{40}$$K_3PM_{o12}O_{40}$이 비교적 활성이 좋았으나, ETBE나 MTBE 경우에 비해서는 다소 활성이 낮았다. 그리하여 본 연구에서는 활성이 좋은 헤테로폴리산 촉매들을 선정하여 각각에 대하여 1:1로 다음과 같이 혼합하여 $H_4SiW_{12}O_{40}$ : $Sr_2SiW_{12}O_{40}$, $H_4SiW_{12}O_{40}$ : $NaH_2PW_{12}O_{40}$, $Fe_{1.5}PW_{12}O_{40}$ : $Mg_2SiW_{12}O_{40}$$Mg_2SiW_{12}O_{40}$ : $Ba_2SiW_{12}O_{40}$ 실험한 결과, 혼합촉매들이 각각의 단일성분 촉매때보다 TBA의 전화율과 ETBE나 MTBE의 선택율이 더욱 향상되었음을 알 수 있었다.

  • PDF

이종금속간의 결합방법에 따른 결합강도에 관한 비교 연구 (Comparative analysis on mechanical properties of gold and Co-Cr dental alloys due to joining methods)

  • 박성규;최부병;권긍록
    • 구강회복응용과학지
    • /
    • 제19권2호
    • /
    • pp.75-86
    • /
    • 2003
  • The purpose of this study was to evaluate their mechanical properties after laser-welding or soldering of precious and non-precious dental alloys. For this study, 30 Co-Cr alloy specimens, 15 gold alloy specimens, 15 palladium alloy specimens were casted and seperated on the middle area. 15 sperated Co-Cr specimens and 15 seperated gold alloy specimens were laser welded (GW Group). 15 sperated Co-Cr specimens and 15 sperated gold alloy specimens were soldered by coventional soldering method (GS Group). 15 sperated Co-Cr specimens and 15 seperated palladium alloy specimens were laser welded (PW Group). 15 sperated Co-Cr specimens and 15 sperated palladium alloy specimens were soldered by coventional soldering method (PS Group). Tensile strength, 0.2% yield strength, % elongation were recorded in nine specimens of each group. Bending strength were record in six specimens of each group. These data for four groups were subjected to a two-way analysis of variance(ANOVA). The fracture locations, fractured surfaces were examined by SEM(scanning electron microscope). The results were as following: 1) In the same alloy combination, the tensile strength and 0.2% yield strength and of the laser welded group with same metal combination were significantly less than soldered groups(p<0.05). 2) In the combination of Co-Cr/Palladium, the bending strength of laser welded group were significantly less than that of soldered groups(p<0.05). In the combination of Co-Cr/Gold, the bending strength of laser welded group were significantly higher than that of soldered groups(p<0.05). 3) In the same method of joint, the tensile strength and 0.2% yield strength and bending strength of the Co-Cr/gold were significantly higher than Co-Cr/palladium(p<0.05). 4) There was no significantly statistical difference between each group in the % elongation(p>0.05). 5) The fracture of the laser welded specimens occured in the welding area and a large void was observed at the center of the fracture surface. 6) The fracture of the soldered specimens occured also inthe soldered area and many porpsities were showed at the fracture sites.