• Title/Summary/Keyword: PW laser

Search Result 7, Processing Time 0.021 seconds

Fabrication of Micro Conductor Pattern on Polymer Material by Laser Induced Surface Activation Technology

  • Lee, Sung-Hyung;Yashiro, Hitoshi;Kure-Chu, Song-Zhu
    • Korean Journal of Materials Research
    • /
    • v.30 no.7
    • /
    • pp.327-332
    • /
    • 2020
  • Laser induced surface activation (LISA) technology requires refined selection of process variables to fabricate conductive microcircuits on a general polymer material. Among the process variables, laser mode is one of the crucial factors to make a reliable conductor pattern. Here we compare the continuous wave (CW) laser mode with the pulse wave (PW) laser mode through determination of the surface roughness and circuit accuracy. In the CW laser mode, the surface roughness is pronounced during the implementation of the conductive circuit, which results in uneven plating. In the PW laser mode, the surface is relatively smooth and uniform, and the formed conductive circuit layer has few defects with excellent adhesion to the polymer material. As a result of a change of laser mode from CW to PW, the value of Ra of the polymer material decreases from 0.6 ㎛ to 0.2 ㎛; the value of Ra after the plating process decreases from 0.8 ㎛ to 0.4 ㎛, and a tight bonding force between the polymer source material and the conductive copper plating layer is achieved. In conclusion, this study shows that the PW laser process yields an excellent conductive circuit on a polymeric material.

Topics on Power Photonics for High-Power Solid-state Laser

  • Nakatsuka, Masahiro
    • Proceedings of the Optical Society of Korea Conference
    • /
    • 2003.07a
    • /
    • pp.6-7
    • /
    • 2003
  • The inertial fusion research at ILE, Osaka moves to the fast ignition scheme with using PW laser system to achieve hot core plasma of keV-temperature by heating additionally the dense plasma imploded by the multi-beam Gekko laser system. The solid-state lasers have been developed of the peak-power from TW to PW region with the chirped pulse amplification (CPA) and optical parametric amplification (OPA) technology. (omitted)

  • PDF

Design of a Femtosecond Ti:sapphire Laser for Generation and Temporal Optimization of 0.5-PW Laser Pulses at a 0.1-Hz Repetition Rate

  • Sung, Jae-Hee;Yu, Tae-Jun;Lee, Seong-Ku;Jeong, Tae-Moon;Choi, Il-Woo;Ko, Do-Kyeong;Lee, Jong-Min
    • Journal of the Optical Society of Korea
    • /
    • v.13 no.1
    • /
    • pp.53-59
    • /
    • 2009
  • A chirped-pulse amplification Ti:sapphire laser system has been designed using a 10-Hz 100-TW Ti:sapphire laser to generate 0.1-Hz 0.5-PW laser pulses and optimize their temporal qualities such as temporal contrast and pulse duration. A high-energy booster amplifier to be added is expected to produce an energy above 30 J through the parasitic lasing suppression and the efficient amplification. To improve the temporal contrast of the laser pulses, a high-contrast 1-kHz amplifier system is used as a front-end. A grating stretcher which makes the laser pulse have 1-ns duration is used to prevent optical damages due to high pulse energy during amplification. A grating compressor has been designed with group delay analysis to obtain the recompressed pulse duration close to the transform-limited pulse duration. The final laser pulses are expected to have energy above 20 J and duration below 40 fs.

Manufacture of Optical fiber probe Using $CO_2$ Laser Heating Pulling Method ($CO_2$ Laser Heating Pulling Method를 이용한 광섬유 탐침 제작)

  • Shin, Soo-Yong;Park, June-Do;HwangBo, Seung;Kang, Yong-Chel
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.468-470
    • /
    • 2005
  • 본 연구에서는 NSOM(Near-field Scanning Optical Microscope)에서 정밀도의 중요한 요소로 작용하는 100 ~ 200nm Scale의 Optical aperture를 제작하기 위해 Optical Fiber를 이용하여 $CO_2$ Laser Heating Pulling Method에 의하여 제작하고자 한다. Heating Pulling Method 에서 Fiber Tip의 정밀도 및 제작 재현성에 영향을 미치는 중요한 기존의 여러 Fiber Tip 구현방법 중 본 연구에서는 Pulse Width[$PW_{(SEC)}$] 와 Pulling Force 두 요소에 있어서 상호관계를 연구하였으며, 연구 결과 두 변수간의 최적화된 파라미터인 PW 0.07 ~ $0.10_{(SEC)}$ 와 Pulling force 0.2 ~ 0.81b의 구간에서 error율이 최소화되는 범위를 찾을 수 있었고, 그 결과 최적의 상태는 $0.08_{(SEC)}$와 0.21b에서 팁들은 첨예화 되었고 95% 이상의 재현성 및 신뢰성을 얻을 수 있었다.

  • PDF

Research on Applicability of Laser Ablation Propulsion to Space Debris Removal by Simulations (시뮬레이션을 통한 레이저 융삭 추진의 우주 쓰레기 제거 응용 가능성 연구)

  • Yoo, Seong-Moon;Lee, Seung-Min
    • Journal of the Korea Institute of Military Science and Technology
    • /
    • v.25 no.2
    • /
    • pp.169-176
    • /
    • 2022
  • Laser ablation propulsion(LAP) is the method to create impulse by laser ablation. It can be used to deorbit the space debris(SD), as its long-range property and versatility on any material. In this paper, we find out several requirements of the LAP system(LAPS) to deorbit the SD by simple numerical calculations of the SD orbit and laser beam flux. As a result, minimum operable altitude angle turned out to be a crucial variable to the LAPS. Moreover, if minimum operable altitude angle is 10°, and if the minimum distance between the LAPS and the SD is below 450 km, 1 m/s2 is sufficient to deorbit the SD by once. With 18 kJ/3 ns pulsed laser and cube shaped 100 kg SD, 1 m/s2 acceleration can be achieved by increasing the pulse repetition rate over 34~53 Hz, depending on the size of the SD. This capability could compare with the conceptual design of the Japan Establishment for a Power-laser Community Harvest(J-EPoCH) facility, which include 8 kJ, 5 PW@100 Hz laser.

Synthesis of TAME, ETBE, and MTBE Using Heteropolyacid Catalyst (헤테로폴리산 촉매를 이용한 TAME, ETBE 및 MTBE 합성반응의 연구)

  • Park, Jin-Hwa;Yi, Yong-Woo
    • Applied Chemistry for Engineering
    • /
    • v.8 no.4
    • /
    • pp.582-588
    • /
    • 1997
  • Synthetic reaction of TAME, ETBE, and MTBE compounds used largely for gasoline octane number enhancer to prevent air pollution was investigated using heteropolyacid catalyst in a fixed bed flow reactor. In the synthetic reaction of TAME, ETBE and MTBE, after hetero atom being replaced with poly atom, the activity of the catalyst, $H_4SiW_{12}O_{40}$ with coordinated bond with W and an hetero atom of Si was the highest among the catalysts tested. Also the activity depended upon the metals replaced which are related to the catalyst acidity. $FeHPW_{12}O_{40}$ and $K_3PM_{o12}O_{40}$ catalysts showed high activity in TAME synthesis, while they were not effective in ETBE and MTBE synthesis. In this study catalysts showing high activity were selected and mixed with equal weight combination of $H_4SiW_{12}O_{40}$ and $Sr_2SiW_{12}O_{40}$ ;$H_4SiW_{12}O_{40}$ and $NaH_2PW_{12}O_{40}$ ; $Fe_{1.5}PW_{12}O_{40}$ and $Mg_2SiW_{12}O_{40}$ ; $Mg_2SiW_{12}O_{40}$ and $Ba_2SiW_{12}O_{40}$. The mixed heteropolyacid catalysts showed higher TBA conversion rate and better selectivity of ETBE and MTBE than the single catalysts.

  • PDF

Comparative analysis on mechanical properties of gold and Co-Cr dental alloys due to joining methods (이종금속간의 결합방법에 따른 결합강도에 관한 비교 연구)

  • Park, Seong-Kyu;Choi, Boo-Byung;Kwon, Kung-Rock
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.19 no.2
    • /
    • pp.75-86
    • /
    • 2003
  • The purpose of this study was to evaluate their mechanical properties after laser-welding or soldering of precious and non-precious dental alloys. For this study, 30 Co-Cr alloy specimens, 15 gold alloy specimens, 15 palladium alloy specimens were casted and seperated on the middle area. 15 sperated Co-Cr specimens and 15 seperated gold alloy specimens were laser welded (GW Group). 15 sperated Co-Cr specimens and 15 sperated gold alloy specimens were soldered by coventional soldering method (GS Group). 15 sperated Co-Cr specimens and 15 seperated palladium alloy specimens were laser welded (PW Group). 15 sperated Co-Cr specimens and 15 sperated palladium alloy specimens were soldered by coventional soldering method (PS Group). Tensile strength, 0.2% yield strength, % elongation were recorded in nine specimens of each group. Bending strength were record in six specimens of each group. These data for four groups were subjected to a two-way analysis of variance(ANOVA). The fracture locations, fractured surfaces were examined by SEM(scanning electron microscope). The results were as following: 1) In the same alloy combination, the tensile strength and 0.2% yield strength and of the laser welded group with same metal combination were significantly less than soldered groups(p<0.05). 2) In the combination of Co-Cr/Palladium, the bending strength of laser welded group were significantly less than that of soldered groups(p<0.05). In the combination of Co-Cr/Gold, the bending strength of laser welded group were significantly higher than that of soldered groups(p<0.05). 3) In the same method of joint, the tensile strength and 0.2% yield strength and bending strength of the Co-Cr/gold were significantly higher than Co-Cr/palladium(p<0.05). 4) There was no significantly statistical difference between each group in the % elongation(p>0.05). 5) The fracture of the laser welded specimens occured in the welding area and a large void was observed at the center of the fracture surface. 6) The fracture of the soldered specimens occured also inthe soldered area and many porpsities were showed at the fracture sites.