• Title/Summary/Keyword: PSNY-6

Search Result 2, Processing Time 0.023 seconds

Conservation of Dry Lacquer Wares Excavated from Daho-ri, Changwon (다호리 출토 건조상태 칠기의 보존)

  • Kim, Soochul;Cho, Seokmin
    • Conservation Science in Museum
    • /
    • v.11
    • /
    • pp.43-48
    • /
    • 2010
  • Excavated lacquer wares can be divided into waterlogged lacquer wares supersatuated with moisture and dry lacquer wares with little moisture. This conservation was done with dry damaged lacquer wares excavated from Daho-ri. Lacquer ware artifacts with lacquer fragments and no surface material remaining were processed using the three following methods. The three methods are reinforcing while sustaining three-dimensional form; reinforcing with earth after cleansing so that fragments are revealed due to weak lacquer fragments; and reinforcing the whole lacquer ware or parts by connecting and supporting missing parts with rayon paper, an artificial fiber paper, if the form cannot be sustained only with lacquer fragments.

Conservation of artifacts excavated from Imdang, Kyǒngsan Province-Metals and Lacquerware (경산시 임당유적 출토 유물 보존처리-금속 및 칠기유물을 중심으로)

  • Yu, Jae-Eun;Shin, Ui-Kyoung;Hwang, Jin-Ju;Goh, Dong-Ha
    • 보존과학연구
    • /
    • s.19
    • /
    • pp.109-132
    • /
    • 1998
  • According to excavation of Imdang site, these sites were excavated place to a various of sites from Early lron period to the Koryo Kingdom. Artifacts to be conserved were excavated from A, D and E district. Metal artifacts were excavated from D and E district and lacquer ware artifacts were excavated from Adistrict. Metal artifacts including lacquer ware iron sword, imitative bronze mirror, Osujen and bronze artifact with letter and so on. Bronze artifacts were covered with soil and rust and performed consolidation after passivation treatment with Benzotriazole solution. Also, iron artifacts performed desalting treatment with 0.1M sesquicarbonate solution. After desalinization, adhesive of these artifacts were processed with Araldite(rapid type) after consolidation with20%∼30% NAD-10 solution. Lacquer ware artifacts remained fragments of lacquer to be all corroded and soiled. Therefore these artifacts retained its original form. Fragments of lacquer joined with Caparol 1%∼3% solution and the soil of relics coated with PSNY 3%∼6% solution. There were many kinds of lacquer were. Lacquer ware artifacts presumed to a string instrument that provide important clues for lacquer ware research. As for lacquer fragments inquire, paints grain size were $2∼5\mum$ and conformed to vanished three times.

  • PDF