• Title/Summary/Keyword: PL spectrum

Search Result 238, Processing Time 0.026 seconds

Synthesis and Application of Bluish-Green BaSi2O2N2:Eu2+ Phosphor for White LEDs (백색 LED용 청록색 BaSi2O2N2:Eu2+ 형광체의 합성 및 응용)

  • Jee, Soon-Duk;Choi, Kang-Sik;Choi, Kyoung-Jae;Kim, Chang-Hae
    • Korean Journal of Materials Research
    • /
    • v.21 no.5
    • /
    • pp.250-254
    • /
    • 2011
  • We have synthesized bluish-green, highly-efficient $BaSi_2O_2N_2:Eu^{2+}$ and $(Ba,Sr)Si_2O_2N_2:Eu^{2+}$ phosphors through a conventional solid state reaction method using metal carbonate, $Si_3N_4$, and $Eu_2O_3$ as raw materials. The X-ray diffraction (XRD) pattern of these phosphors revealed that a $BaSi_2O_2N_2$ single phase was obtained. The excitation and emission spectra showed typical broadband excitation and emission resulting from the 5d to 4f transition of $Eu^{2+}$. These phosphors absorb blue light at around 450 nm and emit bluish-green luminescence, with a peak wavelength at around 495 nm. From the results of an experiment involving Eu concentration quenching, the relative PL intensity was reduced dramatically for Eu = 0.033. A small substitution of Sr in place of Ba increased the relative emission intensity of the phosphor. We prepared several white LEDs through a combination of $BaSi_2O_2N_2:Eu^{2+}$, YAG:$Ce^{3+}$, and silicone resin with a blue InGaN-based LED. In the case of only the YAG:$Ce^{3+}$-converted LED, the color rendering index was 73.4 and the efficiency was 127 lm/W. In contrast, in the YAG:$Ce^{3+}$ and $BaSi_2O_2N_2:Eu^{2+}$-converted LED, two distinct emission bands from InGaN (450 nm) and the two phosphors (475-750 nm) are observed, and combine to give a spectrum that appears white to the naked eye. The range of the color rendering index and the efficiency were 79.7-81.2 and 117-128 lm/W, respectively. The increased values of the color rendering index indicate that the two phosphor-converted LEDs have improved bluish-green emission compared to the YAG:Ce-converted LED. As such, the $BaSi_2O_2N_2:Eu^{2+}$ phosphor is applicable to white high-rendered LEDs for solid state lighting.

Sol-gel Derived-highly Transparent c-axis Oriented ZnO Thin Films (졸-겔법에 의한 c-축 배향성을 가진 고투과율 ZnO 박막의 제조)

  • Lee, Young-Hwan;Jeong, Ju-Hyun;Jeon, Young-Sun;Hwang, Kyu-Seog
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.13 no.1
    • /
    • pp.71-76
    • /
    • 2008
  • Purpose: A simple and efficient method to prepare nanocrystalline ZnO thin film with pure strong UV emission on soda-lime-silica glass substrates by low-temperature annealing was improved. Methods: Crystal structural, surface morphological, and optical characteristics of nanocrystalline ZnO thin films deposited on soda-lime-silica glass substrates by prefiring final annealing process at 300$^{\circ}C$ were investigated by using X-ray diffraction analysis, field emission-scanning electron microscope, scanning probe microscope, ultraviolet-visible-near infrared spectrophotometer, and photoluminescence. Results: Highly c-axis-oriented ZnO films were obtained by prefiring at 300$^{\circ}C$. A high transmittance in the visible spectra range and clear absorption edge in the ultra violet range of the film was observed. The PL spectrum of ZnO thin film with a deep near band edge emission was observed while the defect-related broad green emission was nearly quenched. Conclusions: Our work will be possibly adopted to cheaply and easily fabricate ZnO-based optoelectronic devices at low temperature, below 300$^{\circ}C$, in the future.

  • PDF

Characteristics of InGaAs/GaAs/AlGaAs Double Barrier Quantum Well Infrared Photodetectors

  • Park, Min-Su;Kim, Ho-Seong;Yang, Hyeon-Deok;Song, Jin-Dong;Kim, Sang-Hyeok;Yun, Ye-Seul;Choe, Won-Jun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.324-325
    • /
    • 2014
  • Quantum wells infrared photodetectors (QWIPs) have been used to detect infrared radiations through the principle based on the localized stated in quantum wells (QWs) [1]. The mature III-V compound semiconductor technology used to fabricate these devices results in much lower costs, larger array sizes, higher pixel operability, and better uniformity than those achievable with competing technologies such as HgCdTe. Especially, GaAs/AlGaAs QWIPs have been extensively used for large focal plane arrays (FPAs) of infrared imaging system. However, the research efforts for increasing sensitivity and operating temperature of the QWIPs still have pursued. The modification of heterostructures [2] and the various fabrications for preventing polarization selection rule [3] were suggested. In order to enhance optical performances of the QWIPs, double barrier quantum well (DBQW) structures will be introduced as the absorption layers for the suggested QWIPs. The DBWQ structure is an adequate solution for photodetectors working in the mid-wavelength infrared (MWIR) region and broadens the responsivity spectrum [4]. In this study, InGaAs/GaAs/AlGaAs double barrier quantum well infrared photodetectors (DB-QWIPs) are successfully fabricated and characterized. The heterostructures of the InGaAs/GaAs/AlGaAs DB-QWIPs are grown by molecular beam epitaxy (MBE) system. Photoluminescence (PL) spectroscopy is used to examine the heterostructures of the InGaAs/GaAs/AlGaAs DB-QWIP. The mesa-type DB-QWIPs (Area : $2mm{\times}2mm$) are fabricated by conventional optical lithography and wet etching process and Ni/Ge/Au ohmic contacts were evaporated onto the top and bottom layers. The dark current are measured at different temperatures and the temperature and applied bias dependence of the intersubband photocurrents are studied by using Fourier transform infrared spectrometer (FTIR) system equipped with cryostat. The photovoltaic behavior of the DB-QWIPs can be observed up to 120 K due to the generated built-in electric field caused from the asymmetric heterostructures of the DB-QWIPs. The fabricated DB-QWIPs exhibit spectral photoresponses at wavelengths range from 3 to $7{\mu}m$. Grating structure formed on the window surface of the DB-QWIP will induce the enhancement of optical responses.

  • PDF

Fabrication and Scintillation Characteristics of LiPO3 glass scintillators with the lanthanides activators (란탄계열 원소를 활성체로 첨가한 LiPO3 유리 섬광체의 제작과 섬광특성)

  • Whang, J.H.;Lee, J.M.;Jung, S.J.;Choi, S.H.;Sumarokov, S. Yu.
    • Journal of Sensor Science and Technology
    • /
    • v.12 no.3
    • /
    • pp.139-148
    • /
    • 2003
  • $LiPO_3$ glass scintillators were fabricated, and lanthanides(except Pm) oxides or chlorides were used as an activator. For the fabrication of $LiPO_3$ glasses, optimum heating conditions were obtained, and the photoluminescence of the glasses was measured by the monochromator. For the best transparency of the glass samples, optimum heating temperature and time are $950^{\circ}C$ and 90 min, respectively. It was found that Pr, Nd, Gd, Ho, Er, Tm, Yb and Lu do not work as activator; emission spectrums of samples with them were equal to those of samples without activators. In the case of samples with Europium, the peaks of emission spectrum of $Eu^{2+}$ and $Eu^{3+}$ were 420 nm and 620 nm respectively. And samples with $Ce^{3+}$ were about 380 nm, and $Tb^{3+}$ were about 550 nm. Glass scintillators with $Be^{3+}$, $Eu^{2+}$, and $Ce^{3+}$ were found to be more applicable to neutron detection. The result of neutron detection by Ra-Be sources showed that $Ce^{3+}$ was found to be the best activator of $LiPO_3$.

Synthesis and Anaiysis of Photohnninescence Properties of $^5D_1$$^7F_1$ Transition in $LaGaO_3$:$Eu^{3+}$ Red Phosphor ($LaGaO_3$:$Eu^{3+}$형광체의 합성 및 발광 특성)

  • Kim, Kyoung Hwa;Choi, Yoon Young;Sohn, Kee Sun;Kim, Chang Hae;Park, Hee Dong;Choe, Se Young
    • Journal of the Korean Chemical Society
    • /
    • v.44 no.5
    • /
    • pp.453-459
    • /
    • 2000
  • FED has deserved an intensive attentioD as a new flat panel display. The present investigationaims at undemtanding the photoluminescence and cathodoluminescent properties of hGaO$_3$: $Eu^{3+}$ phosphor bytaking into account the possibility that this phosphor could be applied for FED. In onler to investigate on.sucha detailed behavior; 8everM experimental skil18 Je conducted to the LaGaO$_3$:$Eu^{3+}$ phosphoL The excimtion srectrum artd emission spectmn were rnezsured in the UV range and then decay curve of $^5D_0$+$^7F_j$transitions\vas examined. The decay behavior of $^5D_0$ emission was anMyzed by a newly Iuoposed cross-relaxation mech-ani8In in asswiation with inteFwnter di1ffision (or migration). The cross-mlaxation from $^5D_0$ to CTB (Cha'geTransfer Band) wuld be a quite retsonable by considering the excitation spectrum. It could be also found thatthe quenching type was changed from ditfrsion controlled process to the direct quenching process -s inJeasing $Eu^{3+}$ oncntration.

  • PDF

The study of growth and characterization of CuGaTe$_2$single crystal thin films by hot wall epitaxy (Hot wall epitaxy(HWE) 방법에 의한 CuGaTe$_2$단결정 박막 성장과 특성에 관한 연구)

  • 홍광준;이관교;이상열;유상하;정준우;정경아;백형원;방진주;신영진
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.10 no.6
    • /
    • pp.425-433
    • /
    • 2000
  • The stochiometric mix of evaporating materials for the $CuGaTe_2$single crystal thin films was prepared from horizontal furnance. Using extrapolation method of X-ray diffraction patterns for the $CuGaTe_2$polycrystal, it was found tetragonal structure whose lattice constant $a_0 and c_0$ were 6.025 $\AA$ and 11.931 $\AA$, respectively. To obtain the single crystal thin films, $CuGaTe_2$mixed crystal was deposited on throughly etched semi-insulator GaAs(100) substrate by the Hot Wall Epitaxy (HWE) system. The source and substrate temperature were $670^{\circ}C$ and $410^{\circ}C$ respectively, and the thickness of the single crystal thin films is 2.1$\mu\textrm{m}$. The crystalline structure of single crystal thin films was investigated by the photoluminescence and double crystal X-ray diffraction (DCXD). Hall effect on this sample was measured by the method of van der Pauw and studied on carrier density and mobility dependence on temperature. The carrier density and mobility of $CuGaTe_2$single crystal thin films deduced from Hall data are $8.72{\times}10{23}$$\textrm m^3$, $3.42{\times}10^{-2}$ $\textrm m^2$/V.s at 293K, respectively. From the photocurrent spectrum by illumination of perpendicular light on the c-axis of the $CuGaTe_2$single crystal thin film, we have found that the values of spin orbit coupling $\Delta$s.o and the crystal field splitting $\Delta$cr were 0.0791 eV and 0.2463 eV at 10 K, respectively. From the PL spectra at 10 K, the peaks corresponding to free bound excitons and D-A pair and a broad emission band due to SA is identified. The binding energy of the free excitons are determined to be 0.0470 eV and the dissipation energy of the donor-bound exciton and acceptor-bound exciton to be 0.0490 eV, 0.0558 eV, respectively.

  • PDF

Growth and Opto-electric Characterization of ZnSe Thin Film by Chemical Bath Deposition (CBD(Chemical Bath Deposition)방법에 의한 ZnSe 박막성장과 광전기적 특성)

  • Hong, K.J.;You, S.H.
    • Journal of Sensor Science and Technology
    • /
    • v.10 no.1
    • /
    • pp.62-70
    • /
    • 2001
  • The ZnSe sample grown by chemical bath deposition (CBD) method were annealed in Ar gas at $45^{\circ}C$. Using extrapolation method of X-ray diffraction pattern, it was found to have zinc blend structure whose lattice parameter $a_o$ was $5.6687\;{\AA}$. From Hall effect, the mobility was likely to be decreased by impurity scattering at temperature range from 10 K to 150 K and by lattice scattering at temperature range from 150 K to 293 K. The band gap given by the transmission edge changed from $2.700{\underline{5}}\;eV$ at 293 K to $2.873{\underline{9}}\;eV$ at 10 K. Comparing photocurrent peak position with transmission edge, we could find that photocurrent peaks due to excition electrons from valence band, ${\Gamma}_8$ and ${\Gamma}_7$ and to conduction band ${\Gamma}_6$ were observed at photocurrent spectrum. From the photocurrent spectra by illumination of polarized light on the ZnSe thin film, we have found that values of spin orbit coupling splitting ${\Delta}so$ is $0.098{\underline{1}}\;eV$. From the PL spectra at 10K, the peaks corresponding to free bound excitons and D-A pair and a broad emission band due to SA is identified. The binding energy of the free excitons are determined to be $0.061{\underline{2}}\;eV$ and the dissipation energy of the donor -bound exciton and acceptor-bound exciton to be $0.017{\underline{2}}\;eV$, $0.031{\underline{0}}\;eV$, respectively.

  • PDF

Studies on the Biological Effects of Chemosterilant, Hempa, on the Rice Weevil (Sitophilus oryzae 1.) and Transmission of Sterility (화학적 불임유기물질 Hempa가 쌀바구미(Sitophilus oryzae L.)에 미치는 생물학적 영향 및 불임성의 전달에 관한 연구)

  • Shim Jai Wook
    • Korean journal of applied entomology
    • /
    • v.12 no.1
    • /
    • pp.1-21
    • /
    • 1973
  • Some experiments were conducted to investigate the effects of the chemosterilant, hempa, on the biology of the rice weevil, Sitophilus oryzae L., and the transmission of the lethal factors in the progeny. One to three days old adult males were fed on the wheat grains treated with concentrations of 0.0625, 0.125, 0.25, and $0.5\%$ of hempa water solution. The effects of the treatment on the mortality, longevity, and the performance of oviposition were examined for the Pl generation, and the hatchability and mortality in the postembryonic development were also tested in the $F_1,\;F_2,\;BC_1,\;F_3,\;and\;BC_2$ generations to analyze the inheritance of the lethal factors. The results obtained were summarized as follows. (1) The average longevity of the treated males were ranged from 26.6 to 30.4 days, and indicated no statistical differences. (2) The mortality of the treated males were ranged between $3.3\%\;and\;13.3\%$ and showed no statistical significance. (3) The overall mean number of eggs laid by a female mated to a treated male with concentrations of 0.0625, 0.125, 0.26 and $0.5\%$ were 3.78, 4.05, 3.75 and 3.61 for the respective treatments, and they were not differ significantly from those of control which were 3.60 per female per 3 day period. The unmated female laid 1.91 in the same period, and significantly differ from those in other experimental groups. (4) The overall mean hatchability of the eggs laid by the females mated with males that had been treated with various concentrations of hempa were 86.82, 64.77, 53.47, 40.33 and $24.78\%$ for the respective concentrations of 0, 0.0625, 0.125, 0.25 and $0.5\%$. The hatchability decreased with the increasing concentrations. (5) The minimum hatchabilities were obtained from the eggs laid in the period of 10-12 days after treatment, then the hatchability increased showing some recovery. The recovery seemed to be very much delayed for the males which had been treated with the greater concentrations. Such a difference in hatchability might be related with the sensitivity of the developmental stages of the sperms, and broader spectrum in the stages and severer effects seemed to be associated with the increased concentrations. (6) The overall mean of larval mortality in the $F_l$ generation were 6.55, 17.89, 27.40, 35.42 and $52.17\%$ for the respective concentrations of 0,0.0625, 0.125,0.25 and $0.5\%$. And there was a tendency to increase in the mortality with the increase of concentrations. (7) The correlation coefficients between per cent sterile eggs and larval mortality for the experimental plots of 0.125, 0.25 and $0.5\%$ treatments showed r=+0.83 and +0.85, respectively, and it seemed to be close correlation between the lethal effects on the embryonic and post-embryonic developments. (8) Since the $SC_{50}$ of the sterile eggs was $0.133\%$ and $SC_{50}$ of the larval mortality was $0.565\%$, it was considered that tile lethal factors expressed more in the egg stages than the larval stages. (9) The ratio of female to male in the $F_l$ adults showed 100 : 125, 100 : 108 and 100 : 124 for the plots of 0.125, 0.25 and $0.5\%$ treatments, respectively. And it n·as considered that the sex ratio distortions might occur with the higher concentrations. (10) When the F, males originated 1.on the eggs had been laid by p, in the period of 16-18 days after treatment, were crossed to normal females $(BC_1)$ and made sib matings $(F_2)$, the per cent sterile eggs of the $BC_1$ generation were 13.88 and $33.04\%$ , and were 31.01 and $38.73\%$ for the $F_2$generation with the plots of 0.0625 and $0.125\%$ treatment, respectively. And these seemed to be a results of the $F_1$ individuals are carrying some chromosomal aberrations (11) The larval mortality was the highest in the $F_2$ plot and followed the female backcross plot, and the least in the male backcrosses. (12) The proportions of 1st and 2nd instar larvae among the larval development at tile 17th day after oviposition were 10.98, 27.26, 32.98 and $15.73\%$ in the normal female $\times$ normal male, $F_1$ female$\times$normal male, normal $female \;\times F_1$ male and $female \;\times F_1$ male plots, respectively. It was considered that the larval development might be delayed by the treatment in the 2nd generation. (13) Per cent larval mortality and sterile eggs were greater in the $F_2$ sib mating plots $(F_3)$ than both of $F_2$ backcrosses. Therefore, it seemed that some of the recessive lethal mutations might affect in the further generations. (14) The sterility, induced by the treatment of chemosterilant, hempa, was considered as the result of the dominant lethal mutations due to chromosomal aberrations such as translocation and/or deletion. The effects of these lethal factors seemed to be inherited tip to 3rd generation after treatment.

  • PDF