PET 필름상 형성한 전자파차폐용 박막과 그 특성 (Formation of Electromagnetic Wave Shielding Thin Film on PET Film Substrate and Their Properties)

  • 임경민;이훈성;배일용;문경만;최철수;이명훈
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2011년도 춘계학술대회 및 Fine pattern PCB 표면 처리 기술 워크샵
    • /
    • pp.205-206
    • /
    • 2011
  • Cu thin films for electromagnetic wave shielding were prepared on PET film and Ni-coated PET film by using Dry and Wet coating method, such as evaporation method, DC sputtering method and copper sulfate($CuSO_4$). After that, Zn thin film and Ni thin film were prepared onto the Cu thin films by using evaporation dry process and Ni electro plating wet process as a finishing treatment, respectively. The result of conductivity test and corrosion resistance test revealed Cu thin films which were formed with bigger grain size and high Cu composition rate have superior properties. Zn thin film by dry evaporation process and Ni thin film by wet electro plating process on Cu thin films were largely contributed to corrosion resistance. However, Ni thin film by wet process made conductivity of all specimen worse, the other hand, Zn thin film by dry process made it better to improve condictivity of specimens just prepared by dry process.

  • PDF

Optimal Sputtering Parameters of Transparent Conducting ITO Films Deposited on PET SUbstates

  • Kim, Hyun-Hoo;Shin, Sung-ho
    • Transactions on Electrical and Electronic Materials
    • /
    • 제1권2호
    • /
    • pp.23-27
    • /
    • 2000
  • Indium in oxide(ITO) films have been deposited on PET and glass substrates by DC reactive magnetron sputtering without post-deposition thermal treatment, The high quality for microstructure, electrical and optical properties of the as-deposited ITO films on unheated substrates is dominated by the sputtering parameters, The influence of the working gas pressure, DC power and oxygen partial pressure has been systematically investigated, The lowest DC power, and oxygen partial pressure has been systematically investigated, The lowest resistivity of ITO films deposited on PET substrates was 6$\times$10$^{-4}$ $\Omega$cm. It has been obtained at a working pressure of 3 mTorr and DC power of 30 W. The sheet resistance and optical transmittance of these film were 22 $\Omega$/square and 84% respectively. The best values of figures of merit for the electrical and optical characteristics such as T/ $R_{sh}$ and $T^{10}$ / $R_{sh}$ are approximately 38.1 and 7.95($\times$10$^{-3}$ $\Omega$$^{-1}$ ), respectively.

  • PDF

FDG PET Findings according to Wandering Patterns of Patients with Drug-naïve Alzheimer's Disease

  • Yang, YoungSoon;Kwak, Yong Tae
    • 대한치매학회지
    • /
    • 제17권3호
    • /
    • pp.90-99
    • /
    • 2018
  • Background and Purpose: To explore anatomic substrate of specific wandering patterns in patients with Alzheimer's disease (AD) by performing positron emission tomography with $^{18}F$ fluorodeoxyglucose positron emission tomography (FDG PET). Methods: Drug-naïve AD patients with wandering (n=80) and without wandering (n=262) were recruited. First, the specific pattern of wandering type was operationally classified according to specific wandering score and clinical assessment. Second, brain FDG PET was performed and fluorodeoxyglucose (FDG) uptake differences of specific brain regions according to wandering patterns were compared to those of non-wanderers. Results: In patients with pacing pattern, FDG PET showed significant lower FDG uptake in both middle cingulum and left putamen cluster compared to non-wanderers. The right precuneus and supplementary motor area in patients with random pattern and left calcarine sulcus, right calcarine sulcus, right middle cingulum, and right post central gyrus in patients with lapping pattern had significantly lower FDG uptake compared to non-wanderers. Conclusions: This study showed that wandering in patients with AD had three distinct patterns. These specific patterns showed significant lower FDG uptake in specific brain areas compared to non-wanderers.

The Flexible Characteristic of Reversible and Robust Nanohair Fastener

  • Park, Seung-Ho;Yoon, Young-Seok;Lee, Dong-Woo;Lee, Dong-Ik;You, Kyoung-Hwan;Pang, Chang-Hyun;Suh, Kahp-Yang
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.432-432
    • /
    • 2011
  • Dry adhesion caused by Nanoscale contact comes up to important scientific issue. Herein, we introduce bendable nanohairy locking fastener system with high shear strength and mechanically flexible backing. The polymeric patches like velcro are composed of an array of straight nanohairs with 100 nm diameter and $1{\mu}m$ height. To fabricate high aspect vertical nanohairs, we used UV molding method with appropriately flexible and rigid polyurethane acrylate material on PET substrate. Two identical nanohairy patches are easily merged and locked each other induced by van der Waals force. Because nanohairs can be arrayed with high density ${\sim}4{\times}10^8/cm^2$, we can obtain high shear adhesion force on flat surface (~22 N/$cm^2$). Furthermore, we can obtian nanohairy locking system with maximum shear adhesion ~48 N/$cm^2$ of curved surface due to flexibility of PET substrate. We confirm the tendency that shear adhesion force increases, as radius of curvature increases.

  • PDF

PET 기판 위해 $SiO_2$ 버퍼층 도입에 따른 IT 박막의 접착 및 전기적.광학적 특성 연구 (A Study on Adhesion and Electro-optical Properties of ITO Films deposited on Flexible PET Substrates with $SiO_2$ Buffer Layer)

  • 강자연;김동원;윤환준;박광희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.316-316
    • /
    • 2008
  • Using an evaporation method, $SiO_2$ was deposited as a buffer layer between a flexible PET substrate and a ITO film deposited by DC magnetron sputtering and electro-optical properties were investigated with thickness variance of $SiO_2$ layers. After coating a $SiO_2$ layer and a ITO film, the ITO/$SiO_2$/PET was heated up to $200^{\circ}C$ and the resistivity and the transmittance were measured by hall effect measurement system and UV/VIS/NIR spectroscopy. As a result of depositing a $SiO_2$ buffer layer, the resistivity increased and the transmittance and adhesion property were enhanced than ITO films with no buffer layers and the resistivity was lowered as $SiO_2$ thickness increased from 50 $\AA$ to 100 $\AA$. It was found that the transmittance was independent of annealing temperature variance in $150^{\circ}C{\sim}200^{\circ}C$ and the resistivity decreased as the temperature increased and especially decreasing rate of the resistivity was higher as the buffer layer thickness was thinner. So under optimized depositing of $SiO_2$ buffer layers and post-annealing of ITO/$SiO_2$/PET, ITO films with enhanced adhesion, electro-optical properties can obtained.

  • PDF

ITO층의 두께에 따른 ITO/PET sheet의 변형거동 및 균열 형성 거동 (Influence of ITO Thickness on the Deformation and Cracking Behaviors of ITO/PET Sheets)

  • 김진열;홍순익
    • 한국재료학회지
    • /
    • 제19권1호
    • /
    • pp.1-6
    • /
    • 2009
  • In this study, the stress-strain response and the cracking behaviors of ITO film on a PET substrate are investigated. The cracking behaviors of ITO thin films deposited on a thermoplastic semi-crystalline polymer developed for flexible display applications was investigated by means of tensile experiments equipped with an electrical measurement apparatus and an in-situ optical microscope. Electrical resistance increased gradually in the elastic-to-plastic transition region of the stress strain curves and cracks formed. Numerous cracks were found in this region, and the increase of the resistance was linked to the cracking of ITO thin films. Upon loading, the initial cracks perpendicular to the tensile axis were observed at about 1% of the total strain. They propagated to the entire sample width as the strain increased. The spacing between the horizontal cracks is thought to be determined by the fracture strength and the thickness of the ITO film as well as by the interfacial strength between the ITO and PET. The effect of the strain rate on the cracking behavior was also investigated. The crack density increased as the strain increased. The spacing between the horizontal cracks (perpendicular to the stress axis) increased as the strain rate decreased. The increase of the crack density as the strain rate decreased can be attributed to the higher fraction of the plastic strain to the total strain at a given total strain. The higher critical strain for the onset of the increase in the resistance and the crack initiation of the ITO/PET with a thinner ITO film (300 ohms/sq.) suggests a higher strength of the thinner ITO film.

유기물 기판 위에 증착된 ZnO:Al 투명전도막의 전기적 특성에 미치는 기판 바이어스 전압의 효과 (Effect of Substrate Bias Voltage on the Electrical Properties of ZnO:Al Transparent Conducting Film Deposited on Organic Substrate)

  • 곽동주
    • 조명전기설비학회논문지
    • /
    • 제23권1호
    • /
    • pp.78-84
    • /
    • 2009
  • 본 연구에서는 ZnO:Al 박막의 필름형 염료감응 태양전지의 투명전도막으로의 웅용 가능성을 연구하기 위하여 PET 기판 위에 r. f. 마그네트론 스퍼터링법으로 ZnO:Al 박막을 증착하였으며, ZnO:Al 박막의 전기적 그리고 광학적 특성의 향상을 위하여 기판 바이어스 전압을 인가하였다. 그 결과, 정(+)의 기판 바이어스 전압은 플라즈마 중의 전자를 기판의 스퍼터 원자에 충돌하게 함으로써 박막에 부가적인 에너지를 공급하게 되어 박막의 결정성장 및 전기적 특성을 향상시키고 있음을 알 수 있었다. 그러나 +30[V] 이상의 과도한 기판 바이어스 전압을 인가한 경우, 박막의 전기적 특성은 나빠졌으며, 특히 부(-)의 바이어스 전압을 인가한 경우 결정 성장이 나타나지 알아, 전기적 특성의 향상을 위한 기판 바이어스 전압의 효과가 매우 제한적으로 작용되고 있음을 알 수 있었다. 본 연구에서는 +30(V)의 기판 바이어스 조건하에서 $1.8{\times}10^{-3}[{\Omega}-cm]$의 체적 저항율 및 87.77(%)의 광 투과율을 얻을 수 있었다.

고형오구 입자크기가 고형오구의 세척성에 미치는 영향 (The Effect of Particle Size on the Detergency of Particulate Soil)

  • 문미화;강인숙
    • 한국의류학회지
    • /
    • 제34권4호
    • /
    • pp.653-662
    • /
    • 2010
  • This study investigates the effect of particle size on the detergency of particulate soil using an $\alpha-Fe_2O_3$ particle as the model. Monodispersed spherical $\alpha-Fe_2O_3$ particles were prepared by the hydrothermal aging of an acidic $FeCl_3$ and HCl solution. The $\xi$-potential of PET fiber was measured by the streaming potential method. The potential energy of interaction between the particle and fiber was calculated using the heterocoagulation theory for a sphere-plate model. The $\xi$-potential of PET fiber and potential energy of interaction between particles and fiber increased with a decreasing particle size in a DBS solution. However, in the nonionic surfactant solution, the $\xi$-potential signs of PET fiber and $\alpha-Fe_2O_3$ particles were (-) and (+), respectively; there was no repulsive power between the particles and substrate. The adhesion of particles to the fabric increased with increasing particle size in the anionic surfactant solution and their removal from the fabric increased with a decreasing particle size. The adhesion of particles to the fabric and their removal from the fabric was biphasic with a maximum and minimum at 0.1% concentration of the surfactant solution. In the nonionic surfactant solution the adhesion of particles to fabric and their removal from the fabric were greater than the ones in the anionic surfactant DBS solution.