• 제목/요약/키워드: Optic microscope

검색결과 48건 처리시간 0.021초

Fomation and Properties of Multiple-Tone Spatial Light Modulator using Garnet Film with In-Plane Magnetization

  • Tsuzuki, A.;Uchida, H.;Takagi, H.;Lim, P.B.;Inoue, M.
    • Journal of Magnetics
    • /
    • 제11권3호
    • /
    • pp.143-146
    • /
    • 2006
  • We attempted to fabricate a new type of magneto optic spatial light modulator (MO-SLM) for multiple-tone modulation by using in-plane magnetization. In the MO-SLM, magnetic property of magneto-optical layer was modified to be suitable for multiple-tone expression by substituting Al in Bi:YIG film. At a driving current to 28 mA in an electrode of the fabricated MO-SLM, changes in brightness of pixels were observed using a polarization microscope.

3극 전계방출 전자총의 정전기 렌즈에 의한 전자빔 거동 (Electron Beam Behaviors by the Electrostatic Lens in Triode Field Emission Gun)

  • 김충수;김동환;박만진;장동영;한동철
    • 한국공작기계학회논문집
    • /
    • 제16권6호
    • /
    • pp.163-167
    • /
    • 2007
  • A field emission electron gun including 3 electrodes including one cathode and two anodes is very important for high resolution electron microscope. To have functions to control the initially-emitted electron beam, two anodes act as an electrostatic lens according to equipotential lines by adjusting the spot size, intensity, and working distance. To verify the action of the electron beam by the electrostatic lens by changing several parameters such as electrode shape, displacement and applied voltage to the electrodes, the two lenses were design and simulated and then their performances were analyzed with angular beam intensity(distribution), electrical optic axis variation and their stability.

전자빔 가공기에서 최적 빔 주사를 위한 제어기의 개발 (Development of Controller for Optimal Beam Scanning in E-Beam Manufacture System)

  • 임선종;이찬홍;강재훈
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 추계학술대회 논문집
    • /
    • pp.154-157
    • /
    • 2005
  • The use of electron-beam(E-Beam) manufacture systems provides a means to alleviate optic exposure equipment's problems. We designed an E-beam manufacture system with SEM function. Optimal beam scanning is one of the most important conditions in the performance of E-beam and SEM. The performance of E-beam manufacture system and images of SEM are a close affinity with each other. Developed E-beam manufacture system consist of the controllers of high voltage, scanning, optic and high voltage generator. In this paper, we analyze the condition of steady beam scanning and describe the development of controller fer optimal beam scanning.

  • PDF

전자빔 가공기의 지능형 원격 빔 조절 기능의 개발 (Development of Intelligent Remote Beam Control Function in E-Beam Manufacturing System)

  • 임선종;유준
    • 한국공작기계학회논문집
    • /
    • 제15권2호
    • /
    • pp.24-29
    • /
    • 2006
  • The use electron-beam(E-beam) manufacturing system provides a means to alleviate optic exposure equipment's problems. We are developing an E-beam manufacturing system with scanning electron microscope(SEM) function. The E-beam manufacturing system consist of high voltage generator, beam blanker, condenser lenses, object lenses, stigmator and stage. The development of E-beam manufacturing system is used on the method of remaking SEM's structure. The functions of SEM are developed. It is important for the test of E-beam performance. In E-beam manufacturing system and SEM, beam focus is important function. In this paper, we propose intelligent remote control function for beam focus in E-beam manufacturing system. The function extends the user's function and gives convenience.

광섬유 공초점 간섭 현미경과 위상 변위법을 결합한 표면 검색 (Surface profiling by the phase shifting method in fiber-optical confocal scanning interference microscopes)

  • 김대찬;이승걸
    • 한국광학회지
    • /
    • 제10권3호
    • /
    • pp.201-207
    • /
    • 1999
  • 단일모드 광섬유와 결합기를 이용하여 간결한 구조의 광섬유 공초점 간섭 현미경을 구성하였으며, 위상 변위법을 응용한 표면 검색 방법을 제안하여 통신용의 반도체 레이저와 같이 비교적 긴 파장의 광원과, 낮은 NA의 대물렌즈를 사용하더라도 정밀한 시료 표면 검색이 가능함을 보였다. 이때 시료 표면의 높낮이는 시료로부터 반사된 빛의 위상으로부터 결정되며, 종래의 공초점 현미경에 비하여 주사시간을 크게 단축할 수 있었다. 끝으로 종래의 방법에 비해 제안된 방법은 시료의 반사율 변화에 덜 민감함을 확인할 수 있었다.

  • PDF

도룡뇽(Hynobius leechi)의 시각계 발생 (Development of Visual System in Korean Salamander(Hynobius leechi))

  • 정선우;윤춘식;김덕훈
    • 한국안광학회지
    • /
    • 제3권1호
    • /
    • pp.9-13
    • /
    • 1998
  • 한국산 도룡농 Hynobius leechi의 시각계발생을 형태학적으로 연구하였다. 수정란을 채집하여 멸균된 생리식염수에서 발생시키고 5-30mm길이의 유생을 크기별로 하였다. 표본은 paraffin에 포매하고 절편하여 광학현미경하에서 관찰하였다. 5mm유생에서, 안배에 의해 유도된 수정체의 원기는 감각외 배엽과 결함되어 있었다. 12mm유생은 수정체가 구형으로 되고 색소상피가 뚜렷해지나 망막층의 분화는 일어나지 않았다. 14-16mm유생은 망막층의 분화가 뚜렷해지며 수정체의 중심부섬유의 핵이 붕괴되었다. 20mm유생의 안배의 외연부는 얇아져서 홍채와 모양체를 형성하였다. 30mm유생에서는 맥락막이 두터워지고 연골이 안구의 외곽에서도 나타났다. 광수용세포층의 외절은 점차로 길게 성장하고 안구신경은 연골을 지나 뇌의 복측에 연결된다.

  • PDF

저유전율을 가지는 D-Glass Fiber의 제조 및 특성 (Fabrication and Properties of D-Glass Fiber with Low Dielectric Constant)

  • 정보라;이지선;이미재;임태영;이영진;전대우;신동욱;김진호
    • 한국재료학회지
    • /
    • 제28권4호
    • /
    • pp.254-259
    • /
    • 2018
  • General D-glass(Dielectric glass) fibers are adaptable to PCBs(Printed circuit boards) because they have a low dielectric constant of about 3.5~4.5. However, very few papers have appeared on the physical characteristics of D-glass fibers. D-glass fibers were fabricated via continuous spinning process using bulk D-glass. In order to fabricate the D-glass, raw materials were put into a Pt crucible, melted at $1650^{\circ}C$ for 2 hrs, and then annealed at $521{\pm}10^{\circ}C$ for 2 hrs. We obtained transparent clear glass. The transmittance and adaptable temperature for spinning of the bulk marble glass were characterized using a UV-visible spectrometer and a viscometer. Continuous spinning was carried out using direct melting spinning equipment as a function of the fiberizing temperature in the range of $1368^{\circ}C$ to $1460^{\circ}C$, while the winder speed was between 100 rpm and 200 rpm. We investigated the physical properties of the D-glass fibers. The average diameters of the glass fibers were measured by optical microscope and FE-SEM. The average diameters of the D-glass fibers were 21.36 um at 100 rpm and 34.06 um at 200 rpm. The mechanical properties of the fibers were confirmed using a UTM(Universal materials testing machine). The average tensile strengths of the D-glass fibers were 467.03 MPa at 100 rpm and 522.60 MPa at 200 rpm.

슬래그 재활용 원료를 이용한 유리섬유 제조 및 특성 (Properties and Fabrication of Glass Fiber using Recycled Slag Materials)

  • 이지선;김선욱;라용호;임태영;이영진;전대우;김진호
    • 한국재료학회지
    • /
    • 제28권12호
    • /
    • pp.763-768
    • /
    • 2018
  • In this study, glass fibers are fabricated via a continuous spinning process using manganese slag, steel slag, and silica stone. To fabricate the glass fibers, raw materials are put into an alumina crucible, melted at $1550^{\circ}C$ for 2 hrs, and then annealed at $600^{\circ}C$ for 2 hrs. We obtain a black colored glass. We identify the non-crystalline nature of the glass using an XRD(x-ray diffractometer) graph. An adaptable temperature for spinning of the bulk marble glass is characterized using a high temperature viscometer. Spinning is carried out using direct melting spinning equipment as a function of the fiberizing temperature in the range of $1109^{\circ}C$ to $1166^{\circ}C$, while the winder speed is in the range of 100rpm to 250rpm. We investigate the various properties of glass fibers. The average diameters of the glass fibers are measured by optical microscope and FE-SEM. The average diameter of the glass fibers is $73{\mu}m$ at 100rpm, $65{\mu}m$ at 150rpm, $55{\mu}m$ at 200rpm, and $45{\mu}m$ at 250rpm. The mechanical properties of the fibers are confirmed using a UTM(Universal materials testing machine). The average tensile strength of the glass fibers is 21MPa at 100rpm, 31MPa at 150rpm, 34MPa at 200rpm, and 45MPa at 250rpm.

Thermal and Electro-Optic Properties of a Side Chain Liquid Crystalline Polysilozanes cotaining a Low Molecuar Weight LIquid Crystal

  • Lee, Tae-Jeong;Kim, Eun-Yeong;Huh, Jae-Ho;Wang, Young-Soo;Kim, Han-Do
    • 한국섬유공학회:학술대회논문집
    • /
    • 한국섬유공학회 1997년도 추계총회 및 학술발표회 논문집
    • /
    • pp.32-35
    • /
    • 1997
  • Aggregation states ans electro-optic properties of a binary mixture by mixing a side chain type liquid crystalline polymer(LCP) and a low molecular weight liquid crystal(LMLC) have been studied. Side chain liquid crystalline polysiloxanes were synthesized from allyl bromide, p-hydroxy benzoic acid, p-cyanophenol, p-methoxyphenol and polysiloxanes. Low molecular weight liquid crystals were synthesized from allyl bromide, p-hydroxy benzoic acid and 4-cyano 4'-hydroxy biphenyl. And then, their properties were compared with blended liquid crystals. The thermal properties of the blended liquid crystals were evaluated using differential scanning calorimetry. The phase behavior of blended sample with temperature were also observed polarized microscope with hot stage. Thus, it seemed to us that a study of LC polysiloxanes with LMLC would be useful, especially in view of the fact that, systematic investigations have been carried out on the effects of changes in LCP/LMLC binary system on the properties of this relatively new type of liquid crystal.

  • PDF

외부전계 인가에 의한 조화용융조성 LiNbO3 결정의 주기적 분극반전 (Congruent LiNbO3 Crystal Periodically Poled by Applying External Field)

  • 권순우;양우석;이형만;김우경;이한영;윤대호;송요승
    • 한국세라믹학회지
    • /
    • 제42권11호
    • /
    • pp.749-752
    • /
    • 2005
  • When an electric field higher than a characteristic coercive field is applied to a ferroelectric such as $LiNbO_3$, the orientation of the spontaneous polarization is reversed, which causes the reversal of the sign of odd-rank tensor properties such as electro-optic and nonlinear optic coefficients. A fabrication process of insulator and periodic external field assisted poling of a z-cut $LiNbO_3$ have been optimized for a periodic $180^{\circ}$ phase inversion along z-axis. The poling jig and the poling control system, fully controlled by a computer, for high quality and reproducible PPLN fabrication have been devised. Periodically polarization reversed PPLN was adjusted based on the fabricated thickness of insulator. The poling structure of PPLN was observed under a microscope after etching PPLN samples by an etching solution ($HF:HNO_3$ = 1 : 2) for about 15 min.