  • The creep rate is affected by the temperature and in fact. if the temperature above $T_M/2(T_M:melting\;point)$. The aim of the present investigation is to study the relationship of static creep and cyclic creep behavior of pure copper and the formulation of these phenomena with the special attention to the instantaneous strain. strain rate from time and number of cycles have the same inclination Steady state creep rate depend upon maximum stress and can be expressed as linear function according to Power law creep equations Creep rupture time has relation with creep rate. and it make a group represented as the same direct line regardless of max stress, stress ratio and the temperature. Initial strain effect on continuous creep deformation. and have guantitative relationship between elastic and Plastic strain. LMP have similar tendency than OSDP and MHP according to temperature

  • PDF

Long Time Creep Strength and Life Prediction of Steam Turbine Rotor Steel by Initial Strain Method (화력발전용 로터강의 초기 변형률법에 의한 장시간 크리프 수명 및 강도 예측)

  • 오세규;정순억
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.6
    • /
    • pp.1321-1329
    • /
    • 1993
  • Long time creep strength and life prediction of 1% Cr-Mo-V and 12% Cr rotor steel were performed by using round-bar type specimens under static load at 500-600.deg. C TTP (time temperature parameter), MCM (minimum commitment method) and ISM (initial strain method newly devised) as life prediction methods were investigated, and the results could be summarized as follows. (1) The minimum parameter of SEE (standard error) by TTP was proved as LMP (larson-miller parameter), and the minimum parameter of RMS (root mean squares), by data less than 10$^{3}$hrs was MHP (manson-haferd parameter). (2) The parameters of the minimum and the maximum strength values predicted in $10^{5}$hrs creep life of 1% Cr-Mo-V steel by TTP were LMP and MSP, respectively. In case of 12% Cr steel above $550^{\circ}C$ OSDP (orr-sherby-dorn parameter) was minimum and MSP (manson-succop parameter) was maximum, but below $550^{\circ}C$, the inverse phenomena was observed. On the other hand the creep strengths before $10^{3}hrs$ life by MCM were similar to those by TTP, but the strengths after $10^{3}hrs$ life were 10-25% lower than those by TTP. (3) Creep strengths by ISM were maximum 5% lower than those by TTP. Because $10^{5}hrs$ strengths were similar to those of the lower band by TTP, the ISM was safer than the TTP.