Decomposition Reaction of Methanol over Ni-Cu/SiO$_2$Catalyst (Ni-Cu/SiO$_2$촉매 상에서의 메탄올 분해 반응)

  • 박지영;문승현;윤형기;박성룡;이상남;정승용
    • Journal of Energy Engineering
    • /
    • v.5 no.1
    • /
    • pp.65-71
    • /
    • 1996
  • Decomposition reaction of methanol was conducted on Ni-Cu/SiO$_2$catalysts with several variables. Variables used in this study are S.V(Space Velocity), partial pressure of methanol, reaction temperature, and composition rate of Ni-Cu. The range of S.V is 10,000-30,000h$\^$-1/, the temperature range is 150-400$^{\circ}C$ and values of Cu/(Ni+Cu) are 0, 0.25, 0.5, 0.75, and 1. Over Ni/SiO$_2$, and Ni-Cu/SiO$_2$, the conversion rate of decomposition reaction of methanol arrived at 100% with increasing of temperature. At this time the selectivity of CO on Ni/SiO$_2$, was suddenly decreased, but on Ni-Cu/SiO$_2$, it was still sustained highly. The main products of reaction were CO and H$_2$, and by-products were CO$_2$ and CH$_4$mainly.

  • PDF

The study of magnetoresistance and magnetic properties in [(CoO/NiO)/NiFe/Cu/NiFe] spin-valve thin films ([(CoO/NiO)/NiFe/Cu/NiFe] spin-valve 박막에서의 자기저항효과와 자기적 특성에 대한 연구)

  • 현준원
    • Electrical & Electronic Materials
    • /
    • v.9 no.10
    • /
    • pp.1060-1065
    • /
    • 1996
  • We have studied the magnetoresistance phenomena on spin valve thin films of antiferromagnetic NiO/CoO. Interlayer coupling oscillates between the antiferrocoupling and ferrocoupling with the variation of Cu thickness. The exchange coupling strength between NiO (antiferromagnetic) and NiFe(ferromagnetic) as a function of NiO texture and interface roughness is investigated by CoO insertion. CoO has significantly higher anisotropy in the (111) plane and interface roughness. It seems that the MR-ratio is increased by CoO inserted films. From the AFM and XRD data, the increase of MR-ratio and exchange field is influenced by the roughness of CoO.

  • PDF

A Study on the Electromagnetic Wave Absorption Properties by the Composition Ratio and Sintering Condition of NiCuZn Ferrite (NiCuZn 페라이트의 조성 및 소결조건에 따른 전자파흡수 특성에 관한 연구)

  • 이영구;박찬규;이문수
    • Journal of the Korea Institute of Information and Communication Engineering
    • /
    • v.5 no.5
    • /
    • pp.994-1000
    • /
    • 2001
  • With the development of electromagnetic communication technology and increased use of electromagnetic wave, the countermeasure of EMI(Electromagnetic Interference) becomes more important socially, and interest for the electromagnetic wave absorber has also increased. In this paper, we have studied characteristics of frequency dependency on complex permittivity and complex permeability according to the changes of composition rate and sintering temperature of NiCuZn ferrite also known as electromagnetic wave absorber and further looked into effect of electromagnetic wave absorption properties. From the measurement where the composition of $Fe_2O_3$ and ZnO of NiCuZn ferrite was fixed at 49 and 34 mol% respectively while composition of NiO and CuO has been varied at each test, we found out that Initial permeability and permittivity were high and the absorbing ability of electromagnetic wave recorded best with $loss tangent(=\mur"/\mur')$ displays more than 1 within the frequency band of 2MHz~9.5MHz when the composition ratio of NiO was ranged around 8.5~9.5 mol% and the sintering temperature was $1080^{\circ}C$.TEX>.

  • PDF

Exchange and Interlayer Coupling in NiO Spin Valve Films (NiO 스핀밸브 박막에서 교환결합과 사잇층 결합에 관한 연구)

  • 박창만;고성호;황도근;이상석;이기암
    • Journal of the Korean Magnetics Society
    • /
    • v.7 no.5
    • /
    • pp.258-264
    • /
    • 1997
  • Exchange and interlayer couplings between a NiFe ferromagnetic layer and an antiferromagnetic NiO layer in NiO/NiFe/Cu/NiFe spin-valve films prepared by rf/dc magnetron sputtering were investigated. The interlayer coupling field ($H_{int}$ decreased with the Cu layer thickness, and the exchange coupling field $(H_{ex}$ saturated to 90 Oe. the magnetitudes of $H_{ex}$ and $H_{int}$ decreased with increasing thickness of the pinned NiFe layer. The increase of $H_{int}$ with the free NiFe layer may be due to the increased magnetization.

  • PDF

Low Firing Temperature Nano-glass for Multilayer Chip Inductors (칩인덕터용 저온소성 Nano-glass 연구)

  • An, Sung-Yong;Wi, Sung-Kwon
    • Journal of the Korean Magnetics Society
    • /
    • v.18 no.1
    • /
    • pp.43-47
    • /
    • 2008
  • [ $ZnO-Bi_2O_3-Al_2O_3-B_2O_3-SiO_2$ ] nano-glass has been prepared by sol-gel method. The mean particle size was 60.3 nm with narrow size distribution. The nano-galss has been used as a sintering aid for the densification of the NiZnCu ferrites. The ferrite was sintered with nano-glass sintering aids at $840{\sim}900^{\circ}C$, 2 h and the initial permeability, quality factor, density, and saturation magnetization were also measured. The initial permeability of 0.5 wt% nano-glass added toroidal sample for NiZnCu ferrites sintered at $900^{\circ}C$ was 193.3 at 1 MHz. The initial permeability and saturation magnetization were increased with increasing annealing temperature. As a result, $ZnO-Bi_2O_3-Al_2O_3-B_2O_3-SiO_2$ nano-glass systems were found to be useful as sintering aids for multilayer chip inductors.

Magneto resistance in NiO/NiFe/Cu/NiFe spin-valve Sandwiches (NiO/NiFe/Cu/NiFe 스핀-밸브 샌드위치의 자기저항 특성)

  • 김재욱
    • Electrical & Electronic Materials
    • /
    • v.10 no.10
    • /
    • pp.1016-1021
    • /
    • 1997
  • Magneto resistance properties in spin-valve sandwiches with various thickness of nanmagnetic layer in contact with the ferromagnetic NiFe film were investigated. The NiFe layer in contact with the NiO film was pinned by strongly exchange-biased coupling and the free NiFe layer at the film surface induced a sharp change in the magnetoresistance at -5~15Oe due to small coercivity. The NiO/NiFe/Cu/NiFe film showed a magnetoresistance ratio in the range of 2.3~2.9% and a field sensitivity above 2.2%/Oe with various of nonmagnetic layer. The NiO/NiFe/Cu/NiFe film of the field sensitivity above 2.2%/Oe suggests stang possibility of magnetic sensor matter.

  • PDF

Synthesis of Cobalt(II), Nickel(II) and Copper(II) Complexes with Tetradentate Schiff Base Ligand of o-BSDT $H_2$ and Electrochemical properties in DMSO (네자리 Schiff Base 리간드의 Cobalt(II), Nickel(II) 및 Copper(II) 착물의 합성과 DMSO용액에서 전기화학적 성질)

  • Ki-Hyung Chjo;Jong-Soon Kim
    • Journal of the Korean Chemical Society
    • /
    • v.31 no.6
    • /
    • pp.509-519
    • /
    • 1987
  • The tetradentate Schiff base ligand, 3,4-bis(salicylidene diimine) toluene, have been prepared by the reaction of salicylaldehyde with 3,4-diaminotoluene by Duff method. The Schiff base ligand reacts with Ni(II), Co(II), and Cu(II) ions to form new complexes, [Ni(o-BSDT)${\cdot}(H_2O)_2$], [Co(o-BSDT)${\cdot}(H_2O)$], and [Cu(o-BSDT)]. It seems that Ni(II) and Ni(II) complexes are hexacoordinated with the Schiff base ligand and two molecules of water, while the Cu(II) complexes are tetracoordinated with the Schiff base. The mole ratio of tetradentate Schiff base ligand to metals was found to be 1 : 1. The redox chemistry of these complexes was investigated by polarography and cyclic voltammetry with glassy carbon electrode in DMSO with 0.1M TEAP${\cdot}$[Ni(o-BSDT)${\cdot}(H_2O)_2$] hav EC reaction mechanisms which undergo a irreversible electron transfer followed by a fast chemical reaction. [Co(o-BSDT)${\cdot}(H_2O)_2$] undergoes a reduction of Co(II) to Co(I) and a oxidation of Co(II) to Co(III), and [Cu(o-BSDT)] undergoes a reduction of Cu(II) to Cu(I).

  • PDF