• 제목/요약/키워드: NiCr

검색결과 1,884건 처리시간 0.03초

Zn-Pr-Co-Er-M(M=Ni, Mg, Cr)산화물계 바리스터의 전기적, 유전적 특성 (Electrical and Dielectric Characteristics of Zn-Pr-Co-Er-M(M=Ni, Mg, Cr) Oxides-Based Varistors)

  • 남춘우;김명준
    • 한국세라믹학회지
    • /
    • 제41권8호
    • /
    • pp.605-609
    • /
    • 2004
  • 다양한 금속산화물(NiO, MgO, Cr$_2$O$_3$) 첨가에 따른 ZnO 바리스터의 미세구조, 전기적, 유전적 특성을 조사하였다. 평균 결정립 크기는 NiO 첨가로 증가한 반면 Cr$_2$O$_3$ 첨가로 감소하였다 이로 인해 바리스터 전압은Cr$_2$O$_3$ 첨가시 더 높게 나타났다. 바리스터 가운데서 Cr$_2$O$_3$가 첨가된 바리스터가 비직선 지수가 40.5, 누설전류가 2.7 $\mu$A로 가장 우수한 비직선성을 나타내었으며, 유전손실도 0.0589로 비교적 낮게 나타났다.

Effect of Si on Corrosion of Fe-Cr and Fe-Cr-Ni Alloys in wet CO2 Gas

  • Nguyen, T.D.;Zhang, J.;Young, D.J.
    • Corrosion Science and Technology
    • /
    • 제14권3호
    • /
    • pp.127-131
    • /
    • 2015
  • Model alloys Fe-9Cr, Fe-20Cr and Fe-20Cr-20Ni (wt. %) with 0.1 and 0.2 % Si were exposed to $Ar-20CO_2-20H_2O$ gas at $818^{\circ}C$. The undoped alloys formed a thick iron-rich oxide scale. The additions of Si reduced scaling rates of Fe-9Cr to some extent but significantly suppressed the formation of iron oxide scales on Fe-20Cr and Fe-20Cr-20Ni. Carburisation also occurred in all undoped alloys, but not in Si-containing Fe-20Cr and Fe-20Cr-20Ni. Protection against carburisation was a result of the formation of an inner scale layer of silica.

크롬계 이중도금층 제조 및 특성평가 (Fabrication of Chromium-based Double Layered Deposit)

  • 박상언;김동수;김만;장도연;권식철
    • 연구논문집
    • /
    • 통권31호
    • /
    • pp.127-133
    • /
    • 2001
  • In chromium electrodeposition, crack is inevitably accompanied by chromium layer. Behavior of crack formation and crack density were different from the plating conditions such as current density, temperature, waveform of applied current and so on. And cracks have an influence on the corrosion resistance of chromium deposit, because corrosion occurs through the network of cracks between deposit and substrate. Therefore, many researches have been achieved in order to remove the cracks in chromium deposit. Formation of double layers, Cr/Cr and Ni/Cr were investigated to increase corrosion resistance of chromium deposit in this study. As pretreatment prior to outer chromium coating, acid pickling and current control method were examined. Cracks in cross-section of each sample were observed with SEM and CASS(Copper modified acetic acid salt spray) test was performed to evaluate corrosion resistance. It was found that corrosion resistance of Cr/Cr and Ni/Cr double layers were superior to Cr or Ni single layer from the results of CASS test.

  • PDF

아말감과 이종(異種)금속의 거리에 따른 부식에 대한 고찰 (A Study on Corrosion according to Distance between Amalgam and Dissimilar Metals)

  • 김주원;정은경
    • 치위생과학회지
    • /
    • 제4권3호
    • /
    • pp.103-109
    • /
    • 2004
  • 본 실험은 제조회사 매뉴얼과 통법에 의해서 Amalgam 합금, Ni-Cr alloy의 Crown용 Verabond, Denture용 Talladium $^{TM}alloy$로 각각 24개의 총 72의 시편을 하악 제1대구치근 원심 치관 폭경과 임상에서의 MOD cavity를 고려하여 제작하였고 인공 타액 80ml를 담은 200ml 용 비이커에 시편을 넣어 0mm, 7mm, 40mm 거리에서 7일 후 갈바닉 부식을 측정하였다. 유리금속은 유도 플라즈마 방출 분광기(Inductively Coupled Plasma - Atomic Emission Spectrometer(ICP-AES, JY-50P, VG Elemental Co. France)로 전해액내의 Cu, Ag, Ni, Cr, Sn, Zn, Hg를 정량 분석했으며 그 결과 다음과 같은 결론을 얻었다. 첫째, Cu, Sn, Ag, Hg, Zn은 아말감이 금 합금과 접촉했을 때가 크라운용 Ni-Cr alloy와 덴쳐용 Talladium alloy 보다 아주 많이 유리 했으며 금 합금이 구강조직과 생체 적합성이 가장 좋다지만 아말감과 함께 있을 때 가장 불리 했슴을 알 수 있었다. 둘째, 아말감이 금 합금과 접촉했을 때, 금 합금의 조성에서 Ni, Cr 같은 중금속이 함유되지 않았기 때문인지 전혀 유리되지 않았으나 Sn은 조성에는 없었지만 $227.1{\pm}18.0035{\mu}g/cm^2$나 유리 되었고 Hg도 유리되었는데 이는 아말감 자체의 유리 물질임을 추측할 수 있었다. 셋째, 아말감 합금과 금 합금 사이에서의 0mm, 7mm, 40mm 거리에서는 Cu, Ag는 유의성이 있었으며 Hg는 유의성이 없었다. 이는 금합금은 절대 아말감과 같이 사용해서 안되며 이종 보철물 사이의 거리에 관계없이 사용을 금해야 하는 것으로 사료된다. 넷째, 아말감합금이 Crown용 Ni-Cr 합금과 접촉했을 때 아말감의 Ag이 유리 되지 않았으며 Zn, Ni, Sn, Hg, Cu의 순으로 유리되었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 다섯째, 아말감합금이 Denture용 Talladium alloy 합금과 접촉했을 때 0mm, 7mm, 40mm 거리에서도 유의성이 있었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 여섯째, 인공 타액에서 접촉 시 Amalgam alloy와 Gold, Verabond, Talladium alloy의 Cu, Sn, Ag, Hg, Zn, Ni, Cr의 ICPES 검사 결과 Cu, Hg가 유의성을 있었다. 일곱째, 인공타액에서 아말감합금과 두 비귀금속인 Ni-Cr alloy(crown용), Denture용 Talladium alloy가 접촉한 경우 거리에 따른 Hg, Ni, Cr의 유리 부산물에서 유의성을 확인했다.

  • PDF

모 조선업체 아크 용접 작업자의 공기중 6가 크롬 및 니켈 노출에 관한 연구 (Welder's Exposure to Airborne Hexavalent Chromium and Nickel during Arc Welding in a Shipyard)

  • 신용철;이광용;이나루;오세민;강성규;문영한;이기라
    • 한국산업보건학회지
    • /
    • 제8권2호
    • /
    • pp.209-223
    • /
    • 1998
  • The aim of this study was to evaluate welders' exposure to hexavalent chromium (Cr(VI)) and nickel (Ni) during welding operations in a Korean shipyard. The airborne Cr(VI) and Ni concentrations were measured during metal inert gas (MIG) welding on mild and stainless steel, and manual metal arc (MMA) welding on mild steel. The geometric mean (GM) of Cr(VI) concentrations inside the welding helmet during MIG welding on mild steel were $0.0018mg/m^3$ inside a ship section, and $0.0015-0.0026mg/m^3$ at the welding shops. All of the personal breathing zone air samples were below the American Conference of Governmental Industrial Hygienists (ACGIH) Threshold Limit Value ($TLV^{(R)}$) of $0.01mg/m^3$. Conversely, eighty-eight percent(21 of 24) of the personal breathing zone air samples exceeded the National Institute for Occupational Safety and Health (NIOSH) recommended exposure limit of $0.001mg/m^3$. Ni was not detected on 20 of 23 air samples collected during MIG welding on mild steel. The three Ni samples above the limit of detection ranged from 0.015 to $0.044mg/m^3$. The GM of Cr(VI) concentrations during MMA welding on mild steel were $0.0013mg/m^3$, but Ni was not detected in the air samples during this operation. It is assumed that the airborne Cr(VI) and Ni during mild steel welding were derived from the base metals which contained about 0.03% Cr and 0.03% Ni. The GM of airborne total Cr, Cr(VI) and Ni concentrations during MIG welding on stainless steel were 4.02, 0.13 and $0.86mg/m^3$, respectively, and the levels of Cr(VI) and Ni were above the ACGIH-$TLV^{(R)}$. Cr(VI) comprised about 35.5% of the total chromium(Cr) from MIG welding on mild steel, and about 8.4% of total Cr from MIG welding on stainless steel. The ratios of Cr(VI) to total Cr were significantly different among welding shops. It was concluded that welders were exposed to high levels of Cr(VI) and Ni during welding on stainless steel, and were exposed to low levels of Cr(VI) even during welding on mild steel.

  • PDF

용사피막의 마찰.마모 특성 평가에 관한 연구 (A Study on the Evaluation of the Friction and Wear Properties of the Sprayed Coating Layer)

  • 김영식;김윤해;김종호;최영국;강태영
    • Journal of Welding and Joining
    • /
    • 제14권3호
    • /
    • pp.66-74
    • /
    • 1996
  • In this study, friction and wear properties of flame sprayed specimens and hard Cr plating specimens were tested, and their properties were compared each other in dry and lubrication condition. Ni-Cr powder and steel powder were used as the spray powder and sprayed on the steel(S45C) substrate by flame sprayed method. Each wear surface was observed with SEM after friction and wear test. The friction coefficient of the as-forged steel specimens was the highest among surface treatment specimens, and the other specimens appeared in order as follows ; hard Cr-plating specimens, Ni-Cr powder sprayed specimens, steel powder sprayed specimens. Comparing the wear volumes in dry condition, as forged steel specimens appeared the greatest wear volume, and the other specimens appeared wear volume in order as follows ; Ni-Cr powder sprayed specimens, steel powder sprayed specimens, hard Cr plating specimens. In friction and wear test, the hard Cr plating specimens were worn by the abrasive phenomenon, involving the cracks. The wear volume of steel powder sprayed specimens was lower than that of Ni-Cr powder sprayed specimens. Comparing the tensile strength of both sprayed coating layers, the steel powder sprayed coating layer was better than Ni-Cr powder sprayed coating layer.

  • PDF

금합금과 Ni-Cr 합금의 납착부 인장강도 (TENSILE BOND STRENGTH OF SOLDER JOINT BETWEEN GOLD ALLOY AND NICKEL-CHROMIUM ALLOY)

  • 정준호;최현미;최정호;안승근;송광엽;박찬운
    • 대한치과보철학회지
    • /
    • 제34권1호
    • /
    • pp.143-150
    • /
    • 1996
  • The purpose of this study was to evaluate the tensile strength of solder joint between gold alloy and nickel-chromium alloy. The specimens were made with type III gold alloys and Ni-Cr-Be alloy and Degular Lot 2 solder. Eighteen paired specimens were made, and subdivided into three groups. Group I specimens were gold alloy-gold alloy combination, Group II specimens were gold alloy-Ni-Cr alloy combination, Group III specimens were Ni-Cr alloy-Ni-Cr alloy combination. Solder block were made with solder investment(Degussa A,G, Germany) and stored in room temperature for 24 hours. To reduce the formation of metallic oxide and increase wetting properties, flux was used before preheating and soldering procedure. The specimens were preheated at $650^{\circ}C$ and flux were applied again and gas-oxygen torch was used to solder the specimen. All soldered specimens were subjected to a tensile force in the Instron universal testing machine : the crosshead speed was 1 mm/mim. Tensile strength values of three soldered joint groups were 1. Gold alloy-Gold alloy solder joint : $$48.8kg/mm^2$$ 2. Gold alloy-Ni-Cr alloy solder joint : $$30.9kg/mm^2$$ 3. Ni-Cr alloy-Ni-Cr alloy solder joint : $$31.8kg/mm^2$$ The microscopic examination of fracture site showed cohesive and combination fracture modes in gold alloy specimens, but showed all adhesive fracture modes in Ni-Cr alloy containing specimens.

  • PDF

금속결합층의 조성이 $\textrm{ZrO}_2$-$\textrm{CeO}_2$-$\textrm{Y}_2\textrm{O}_3$ 단열층의 내구성에 미치는 영향 (Effect of Composition of Bond Coating on the Durability of the Plasma Sprayed $\textrm{ZrO}_2$-$\textrm{CeO}_2$-$\textrm{Y}_2\textrm{O}_3$ Thermal Barrier Coating)

  • 김혜성;김병희;서동수
    • 한국재료학회지
    • /
    • 제9권1호
    • /
    • pp.73-80
    • /
    • 1999
  • The effect of alloy compositions of the bond coating on the plasma sprayed-thermal barrier coatings was investigated. The performance of the coating composed of Rene80/NiCrAl/ZrO$_2$-CeO$_2$-Y$_2$O$_3$ and Rene80/CoNiCrAlY/ZrO$_2$-CeO$_2$-Y$_2$O$_3$was evaluated by isothermal and thermal cyclic test in an ambient atmosphere at 115$0^{\circ}C$. The failure of Rene80/NiCrAl/ZrO$_2$-CeO$_2$-Y$_2$O$_3$ coatings was occurred at the bond coating/ceramic coating interface while Rene80/CoNiCrAlY/ZrO$_2$-CeO$_2$-Y$_2$O$_3$ coating was failed at the substrate/bond coating interface after thermal cyclic test. The lifetime of Rene80/NiCrAl/ZrO$_2$-CeO$_2$-Y$_2$O$_3$coatings was longer than Rene80/CoNiCrAlY/ZrO$_2$-CeO$_2$-Y$_2$O$_3$coating. The oxidation rate of the NiCrAl bond coating examined by TGA was lower than CoNiCrAlY bond coatings. In summary, these results suggest that Rene80/CoNiCrAlY/ZrO$_2$-CeO$_2$-Y$_2$O$_3$system as thermal barrier coating be not suitable considering the durability of the coating layer for high temperature oxidation and thermal stress.

  • PDF

Fe-17%Mn 합금의 진동감쇠능 및 내식성에 미치는 Cr, Ni 첨가의 영향 (Effects of Cr and Ni on Damping Capacity and Corrosion Resistance of Fe-17%Mn Alloy)

  • 김정철;한동운;백진현;김태훈;백승한;이영국
    • 한국주조공학회지
    • /
    • 제25권2호
    • /
    • pp.73-79
    • /
    • 2005
  • Effects of Cr and Ni addition on damping capacity, mechanical property, and corrosion resistance of Fe-17%Mn martensitic alloy have been studied. Martensite start temperature($M_{S}$) of the alloy decreases linearly with increasing Cr and Ni contents up to 15%. The damping capacity decreases gradually from 27 to 22% in specific damping capacity(SDC) with increasing Cr and Ni contents from zero to 10%, and decreases rapidly with further Cr and Ni content in Fe-17%Mn alloy. The tensile strength of the alloy maintains a level of 60 $kgf/mm^{2}$ regardless of Cr content with an elongation of 20 to 25%. But, in case of Fe-17%Mn-x%Ni alloy, the tensile strength decreased rapidly with the Ni content of above 10% because of austenite morphology. Immersion test in 5% NaCl solution leads to the result that the corrosion resistance of the alloy becomes excellent above 10% Cr. From the above results, it is concluded that the optimum Cr content to improve the mechanical property and corrosion resistance of the alloy in 5%NaCl solution with a lesser decrease in damping capacity is about 10%. In the case of 5% $H_{2}SO_{4}$ condition, the Fe-17%Mn-10%Ni is an optimum alloy.

다단연소사이클 엔진 적용을 위한 Ni-Cr 코팅에 관한 연구 (Study on Ni-Cr Electro Plating Process for Staged Combustion Cycle Engine)

  • 배병현;황양진;이규환;이병호;한영민;김영준;노용오;조황래;현성윤;방정석
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2017년도 제48회 춘계학술대회논문집
    • /
    • pp.857-863
    • /
    • 2017
  • 본 논문은 다단연소사이클 엔진의 연소실 내벽을 고온, 고압의 환경으로부터 보호하기 위한 열차폐 코팅 공정 개발에 관한 내용이다. 기존 연소기 내벽에는 열차폐 특성이 우수한 Zr 기반의 세라믹용사코팅을 적용했지만, 세라믹의 특성상 연소실 내벽(금속)과 열팽창계수 차이로 인해 박리가 발생할 수 있다. 때문에 로켓 선진국에서는 열차폐 효과를 다소 희생 하더라도 밀착력 향상을 위하여 금속계 코팅인 Ni-Cr 도금을 적용하고 있다. 본 연구에서는 연소기에 적용 가능한 상향 순환식 유동셀을 적용한 도금조를 개발했으며, 반복적인 공정 개선을 통해 도금 두께 $100{\mu}m$이상, ${\pm}10%$의 두께 균일도를 만족하는 Ni, Cr 도금 공정조건을 확립했다.

  • PDF