• 제목/요약/키워드: Ni-P alloy

검색결과 226건 처리시간 0.024초

NiW 기능성 합금도금을 위한 전해 (Electrolysis for NiW Functional Alloy Plating)

  • 정구진;이철경
    • 한국표면공학회지
    • /
    • 제44권1호
    • /
    • pp.1-6
    • /
    • 2011
  • A NiW functional alloy plating was investigated as variables of metal ion concentration, complexing agent, temperature, pH and applied current density. Even if numerous studies on reaction mechanism of NiW induced codeposition were carried out during couples of decade, it has not been acceptable reaction mechanism. This study was focused on the effect of the plating variables on the alloy composition in the NiW alloy plating. Applied current density could control mainly the alloy composition rather than other plating variables. It has also been confirmed that the functional alloy plating such as layered or gradient plating was possible by controlling applied current density.

압력용기용 Ni-Mo-Cr계 고강도 저합금강의 P, Mn 함량에 따른 템퍼 취화거동 및 입계편석거동 평가 (Evaluation of Temper Embrittlement Effect and Segregation Behaviors on Ni-Mo-Cr High Strength Low Alloy RPV Steels with Changing P and Mn Contents)

  • 박상규;김민철;이봉상;위당문
    • 대한금속재료학회지
    • /
    • 제48권2호
    • /
    • pp.122-132
    • /
    • 2010
  • Higher strength and fracture toughness of reactor pressure vessel steels can be obtained by changing the material specification from that of Mn-Mo-Ni low alloy steel (SA508 Gr.3) to Ni-Mo-Cr low alloy steel (SA508 Gr.4N). However, the operation temperature of the reactor pressure vessel is more than $300^{\circ}C$ and the reactor operates for over 40 years. Therefore, we need to have phase stability in the high temperature range in order to apply the SA508 Gr.4N low alloy steel for a reactor pressure vessel. It is very important to evaluate the temper embrittlement phenomena of SA508 Gr.4N for an RPV application. In this study, we have performed a Charpy impact test and tensile test of SA508 Gr.4N low alloy steel with changing impurity element contents such as Mn and P. And also, the mechanical properties of these low alloy steels after longterm heat treatment ($450^{\circ}C$, 2000hr) are evaluated. Further, evaluation of the temper embrittlement by fracture analysis was carried out. Temper embrittlement occurs in KL4-Ref and KL4-P, which show a decrease of the elongation and a shifting of the transition curve toward high temperature. The reason for the temper embrittlement is the grain boundary segregation of the impurity element P and the alloying element Ni. However, KL4-Ref shows temper embrittlement phenomena despite the same contents of P and Ni compared with SC-KL4. This result may be caused by the Mn contents. In addition, the behavior of embrittlement is not largely affected by the formation of $M_3P$ phosphide or the coarsening of Cr carbides.

마이크로 금형 제작을 위한 니켈-코발트 합금 전주기술개발 (Ni-Co Alloy Electroforming for Micro Mold Fabrication)

  • 신승한;정명기;김영석;한성호;허영무
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 추계학술대회논문집
    • /
    • pp.276-279
    • /
    • 2004
  • The factors affecting Ni-Co alloy electroforming were investigated to determine the optimum bath composition and electroplating parameters, like pH, temperature, and current density, suitable for high speed fabrication of a micro mold with longer lifetime. To obtain alloy deposits having uniform thickness and composition, electroplating parameters were finely tuned with home-made electroforming apparatus. Ni-Co alloy deposits had linearly increased Co with $Co^{2+}$ ion concentration in electroplating bath, and showing $412H_v$ of Victors hardness at $23wt\%$ of Co content. For Ni-Co alloy, sulfonate and diol related organic additives were very effective to alleviate its residual stress and surface roughness. The maximum deposition rate was $106{\mu}m/hr$ at 10ASD and the tensile strength of alloy deposit was 2 times larger than that of Ni only case.

  • PDF

치과주조용 비귀금속 합금의 금속 용출 수준 (Concentration of elemental ions released from non-precious dental casting alloys)

  • 사공준;박수철
    • 대한치과기공학회지
    • /
    • 제35권1호
    • /
    • pp.1-17
    • /
    • 2013
  • Purpose: This study was to assess the extents of the release of metals from the non-precious alloys used for dental casting by measuring the differences in the extents of the release of metals by types of alloys, pH level and elapsed time. Methods: Uniform-sized specimens(10 each) were prepared according to the Medical Device Standard of the Korea Food and Drug Administration(2010) and International Standard Organization(ISO22674, 2006), using four types of alloys(one type of Ni-Cr and one type of Co-Cr used for fixed prosthesis, and one type of Ni-Cr and one type of Co-Cr used for removable prosthesis). A total of 12 metal-release tests were performed at one-day, three-day, and two-week intervals, for up to 20 weeks. The metal ions were quantified using an Inductively Coupled Plasma-Atomic Emission Spectrometer. Results: The results showed that the extent of corrosion was higher in the ascending order of Jdium-$100^{(R)}$, Bellabond-$Plus^{(R)}$, Starloy-$C^{(R)}$, and Biosil-$F^{(R)}$. The lower the pH and the longer the elapsed time were, the greater the increase in metal corrosion. At pH 2.4, the release of Ni from Jdium-$100^{(R)}$, a Ni-Cr alloy, was up to 15 times greater than the release of Co from the Co-Cr alloy from two weeks over time, indicating that the Ni-Cr alloy is more susceptible to corrosion than the Co-Cr alloy. Conclusion: It is recommended that Co-Cr alloy, which is highly resistant to corrosion, be used for making dental prosthesis with a non-precious alloy for dental casting, and that non-precious alloy prosthesis be designed in such a way as to minimize the area of its oral exposure. For patients with non-precious alloy prostheses, a test of the presence or absence of periodontal tissue inflammation or allergic reaction around the prosthesis should be performed via regular examination, and education on the good management of the prosthesis is needed.

Ni-Tl-P합금피막을 이용한 수처리장치용 정전류소자의 개발 (Development of constant current device for using in the water treatment controller with Ni-Tl-P alloy deposits)

  • 류일광
    • 환경위생공학
    • /
    • 제18권3호통권49호
    • /
    • pp.35-42
    • /
    • 2003
  • The electric resistance and constant current were investigated on the nickel-thallium-phosphorus alloy deposits by electroless-plating. The Ni-Tl-P alloy deposits were achieved with a bath using sodium hypophosphit as the reducing agent and sodium citrate as the comlexing agent. The basic plating solution is composed of 0.1M NiSO$_4$, 0.005${\sim}$0.0IM Tl$_2$S0$_4$, 0.1${\sim}$O.2M sodium hypophosphite and 0.02${\sim}$O.IM sodium citrate and the plating condition were pH 5${\sim}$6, temperrature 80$_4$90${\circ}$C. The results obtained are summarized as follows: 1) The crystal structure of deposit was amorphous structure as deposited state, became microcrystallized centering on Ni(111) plane by heat treatment at 200${\circ}$C, and grew as polycrystalline Ni, Ni$_3$P, Ni$_5$p$_2$,Tl, etc. by heat treatment higher than 350${\circ}$C. The grain size of plated deposits was grown up to 28.3~42.0nm by heat treatment for 1hour at 500${\circ}$C. 2) The electrical resistivity showed a comparatively high value of 192.5$_4$208.3 ${\mu}$${\Omega}$Cm and its thermal stability was great with resistivity value less than 0.22% in the thermal surroundings of 200${\circ}$C. 3) Ni-Tl-P alloy deposit showed such good constant current-making-effect in the variation of electric voltage, heat treatment temperature, and the composition of the deposit that it can be put to practical use as the matter of constant current device.

전기선폭발법에 의한 Cu-Ni-P 합금 나노 분말 제조 (Cu-Ni-P Alloy Nano Powders Prepared by Electrical Wire Explosion)

  • 김원백;박제신;서창열;이재천;김정환;오용준
    • 한국분말재료학회지
    • /
    • 제14권2호
    • /
    • pp.108-115
    • /
    • 2007
  • Cu-Ni-P alloy nano powders were fabricated by the electrical explosion of electroless Ni plated Cu wires. The effect of applied voltage on the explosion was examined by applying pulse voltage of 6 and 28 kV, The estimated overheating factor, K, were 1.3 for 6 kV and 2.2 for 28 kV. The powders produced with pulse voltage of 6 kV were composed of Cu-rich solid solution, Ni-rich solid solution, and $Ni_3P$ phase. While, those produced with 28 kV were complete Cu-Ni-P solid solution and small amount of $Ni_3P$ phase. The initial P content of 6.5 at.% was reduced to 2-3 at.% during explosion due to its high vapour pressure.

Cu-Ni-Si-P 합금의 기계적 및 전기적 성질에 미치는 첨가원소의 영향 (The Influence of Alloying Elements Addition on the Electrical and Mechanical Properties of Cu-Ni-Si-P Alloy)

  • 김승호;염영진;박동환
    • 열처리공학회지
    • /
    • 제27권1호
    • /
    • pp.1-9
    • /
    • 2014
  • For connector material applications, the influence alloying elements of Mn, Cr, Fe, and Ti and cold rolling reduction on the mechanical property, electrical conductivity and bendiability of Cu-Ni-Si-P alloy was investigated. The hot rolled plates were solution treated at $980^{\circ}C$ for 1.5 h, quenched into water, cold rolled by 10% and 30% reduction in thickness, and then aged at $440{\sim}500^{\circ}C$ for 3, 4, 5 times. respectively. Cu-Ni-Si-P-x alloys cold rolled by 10 reduction before heat treatment have a good bendability compare to cold rolled by 30 reduction. Cu-3.4Ni-0.8Si-0.03P-0.1Ti shows the peak strength value of 759 MPa, an electrical conductivity of 39%IACS, an elongation of 10% and a hardness of 256 Hv aged at $440^{\circ}C$ for 6 hrs. Thus it is suitable for lead frame and connector.

아말감과 이종(異種)금속의 거리에 따른 부식에 대한 고찰 (A Study on Corrosion according to Distance between Amalgam and Dissimilar Metals)

  • 김주원;정은경
    • 치위생과학회지
    • /
    • 제4권3호
    • /
    • pp.103-109
    • /
    • 2004
  • 본 실험은 제조회사 매뉴얼과 통법에 의해서 Amalgam 합금, Ni-Cr alloy의 Crown용 Verabond, Denture용 Talladium $^{TM}alloy$로 각각 24개의 총 72의 시편을 하악 제1대구치근 원심 치관 폭경과 임상에서의 MOD cavity를 고려하여 제작하였고 인공 타액 80ml를 담은 200ml 용 비이커에 시편을 넣어 0mm, 7mm, 40mm 거리에서 7일 후 갈바닉 부식을 측정하였다. 유리금속은 유도 플라즈마 방출 분광기(Inductively Coupled Plasma - Atomic Emission Spectrometer(ICP-AES, JY-50P, VG Elemental Co. France)로 전해액내의 Cu, Ag, Ni, Cr, Sn, Zn, Hg를 정량 분석했으며 그 결과 다음과 같은 결론을 얻었다. 첫째, Cu, Sn, Ag, Hg, Zn은 아말감이 금 합금과 접촉했을 때가 크라운용 Ni-Cr alloy와 덴쳐용 Talladium alloy 보다 아주 많이 유리 했으며 금 합금이 구강조직과 생체 적합성이 가장 좋다지만 아말감과 함께 있을 때 가장 불리 했슴을 알 수 있었다. 둘째, 아말감이 금 합금과 접촉했을 때, 금 합금의 조성에서 Ni, Cr 같은 중금속이 함유되지 않았기 때문인지 전혀 유리되지 않았으나 Sn은 조성에는 없었지만 $227.1{\pm}18.0035{\mu}g/cm^2$나 유리 되었고 Hg도 유리되었는데 이는 아말감 자체의 유리 물질임을 추측할 수 있었다. 셋째, 아말감 합금과 금 합금 사이에서의 0mm, 7mm, 40mm 거리에서는 Cu, Ag는 유의성이 있었으며 Hg는 유의성이 없었다. 이는 금합금은 절대 아말감과 같이 사용해서 안되며 이종 보철물 사이의 거리에 관계없이 사용을 금해야 하는 것으로 사료된다. 넷째, 아말감합금이 Crown용 Ni-Cr 합금과 접촉했을 때 아말감의 Ag이 유리 되지 않았으며 Zn, Ni, Sn, Hg, Cu의 순으로 유리되었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 다섯째, 아말감합금이 Denture용 Talladium alloy 합금과 접촉했을 때 0mm, 7mm, 40mm 거리에서도 유의성이 있었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 여섯째, 인공 타액에서 접촉 시 Amalgam alloy와 Gold, Verabond, Talladium alloy의 Cu, Sn, Ag, Hg, Zn, Ni, Cr의 ICPES 검사 결과 Cu, Hg가 유의성을 있었다. 일곱째, 인공타액에서 아말감합금과 두 비귀금속인 Ni-Cr alloy(crown용), Denture용 Talladium alloy가 접촉한 경우 거리에 따른 Hg, Ni, Cr의 유리 부산물에서 유의성을 확인했다.

  • PDF

Electronic Structures and Physical Properties of the Ordered and Disordered $Ni_2$MnGa Alloy Films

  • Kim, K. W.;Lee, N. N.;Y. Y. Kudryavtsev;Lee, Y. P.
    • 한국진공학회지
    • /
    • 제12권S1호
    • /
    • pp.104-106
    • /
    • 2003
  • In this study, the electronic structures and physical properties of Ni$_2$MnGa alloy films and their dependence on the order-disorder structural transitions were investigated. The results show that the ordered films behave nearly the same as the bulk $Ni_2$MnGa alloy, including the martensitic transformation at 200 K. Unexpectedly, the disordering in $Ni_2$MnGa alloy films does not lead to any appreciable magnetic ordering down to 4 K. An annealing of the disordered films restores the ordered structure with an almost full recovery of the magnetic and the transport properties of the ordered $Ni_2$MnGa alloy films. A possible explanation of the disappearance of magnetic moment in the disordered film is given by using the ab initio first-principles electronic-structure calculations.

열처리조건에 따른 Cu-Ni-Si-Sn-Fe-P 석출경화형 동합금계의 물성변화 특성 (Mechanical and Physical Property Changes of Cu-Ni-Si-Sn-Fe-P Copper Alloy System According to the Heat Treatment Conditions)

  • 김승호;염영진
    • 열처리공학회지
    • /
    • 제26권5호
    • /
    • pp.225-232
    • /
    • 2013
  • The influence of aging treatment, addition elements and rolling reduction ratio on the microstructure, mechanical, electrical and bendability properties of Cu-Ni-Si-P-x (x = Fe, Sn, Zn) alloys for connector material application was investigated. SEM/EDS analysis exhibited that Ni2-Si precipitates with a size of 20~100 nm were distributed in grains. Fe, Sn, Zn elemnets in Cu-Ni-Si-P alloy imporved the mechanical strength but it was not favor in increasing of electrical conductivity. As higher final rolling reduction ratio, the strength and electrical conductivity is increased after aging treatment, but it indicated excellent bendability. Especially, Cu-2Ni-0.4Si-0.5Sn-0.1Fe-0.03P alloy show the tensile strength value of 700MPa and the electrical conductivity was observed to reach a maximum of 40%IACS. It is optimal for lead frame and connector.