• 제목/요약/키워드: Ni Base Alloys

검색결과 94건 처리시간 0.019초

$LiCl-Li_2O_2$ 용융염계에서 오스테나이트계 합금의 부식거동 (Corrosion Behavior of Austenitic Alloys in the Molten Salts of $LiCl-Li_2O_2$)

  • 오승철;윤기석;임종호;조수행;박성원
    • 한국방사성폐기물학회:학술대회논문집
    • /
    • 한국방사성폐기물학회 2003년도 가을 학술논문집
    • /
    • pp.373-378
    • /
    • 2003
  • $LiCl-Li_2O_2$용융염계에서 용융염 취급장치의 구조재료를 위한 평가의 일환으로 오스테나이트 합금인 Fe-base 및 Ni-base 합금의 부식거동을 분위기온도; 650~$725^{\circ}C$, 부식시간: 24~168h, $Li_2O$농도; 3wt%, 혼합가스농도: Ar-10%$O_2$에서 조사하였다. $LiCl-Li_2O_2$ 용융염계에서 Ni-base 합금이 Fe-base 합금보다 높은 내부식성을 나타내었으며, 또한 Fe-base 합금에서 Fe의 함량이 낮고 Ni의 함량이 높은 경우 부식저항성이 증가하였다. 아울러 Fe-base 합금의 부식생성물은 $Cr_2O_3$, $FeCr_2O_4$ Ni-base 합금에서는 $Cr_2O_3$, $NiFe_2O_4$로 나타났다.

  • PDF

Physico-mechanical properties and prosthodontic applications of Co-Cr dental alloys: a review of the literature

  • Al Jabbari, Youssef S.
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권2호
    • /
    • pp.138-145
    • /
    • 2014
  • Cobalt-Chromium (Co-Cr) alloys are classified as predominantly base-metal alloys and are widely known for their biomedical applications in the orthopedic and dental fields. In dentistry, Co-Cr alloys are commonly used for the fabrication of metallic frameworks of removable partial dentures and recently have been used as metallic substructures for the fabrication of porcelain-fused-to-metal restorations and implant frameworks. The increased worldwide interest in utilizing Co-Cr alloys for dental applications is related to their low cost and adequate physico-mechanical properties. Additionally, among base-metal alloys, Co-Cr alloys are used more frequently in many countries to replace Nickel-Chromium (Ni-Cr) alloys. This is mainly due to the increased concern regarding the toxic effects of Ni on the human body when alloys containing Ni are exposed to the oral cavity. This review article describes dental applications, metallurgical characterization, and physico-mechanical properties of Co-Cr alloys and also addresses their clinical and laboratory behavior in relation to those properties.

ROLE OF GRAIN BOUNDARY CARBIDES IN CRACKING BEHAVIOR OF Ni BASE ALLOYS

  • Hwang, Seong Sik;Lim, Yun Soo;Kim, Sung Woo;Kim, Dong Jin;Kim, Hong Pyo
    • Nuclear Engineering and Technology
    • /
    • 제45권1호
    • /
    • pp.73-80
    • /
    • 2013
  • The primary water stress corrosion cracking (PWSCC) of Alloy 600 in a PWR has been reported in the control rod drive mechanism (CRDM), pressurizer instrumentation, and the pressurizer heater sleeves. Recently, two cases of boric acid precipitation that indicated leaking of the primary cooling water were reported on the bottom head surface of steam generators (SG) in Korea. The PWSCC resistance of Ni base alloys which have intergranular carbides is higher than those which have intragranular carbides. Conversely, in oxidized acidic solutions like sodium sulfate or sodium tetrathionate solutions, the Ni base alloys with a lot of carbides at the grain boundaries and shows less stress corrosion cracking (SCC) resistance. The role of grain boundary carbides in SCC behavior of Ni base alloys was evaluated and effect of intergranular carbides on the SCC susceptibility were reviewed from the literature.

에너지 전자상태 계산으로 도출된 이론값을 이용한 니켈 합금 설계 (Design of Nickel Alloys Using the Theoretical Values Calculated from the Electronic State Energies)

  • 백민숙;강법성;백경철;김병일;윤동주
    • 한국재료학회지
    • /
    • 제25권11호
    • /
    • pp.642-646
    • /
    • 2015
  • Super alloys, which can be divided into three categories, i.e. Ni-base, Co-base, and Fe-base alloys, are widely used for high temperature applications. Since superalloys contain many alloying elements and precipitates, their chemistry and processing parameters need to be carefully designed. In this study, we designed a new Ni alloy to prevent corrosion due to water vapor and gases at high temperatures. The new alloy was designed using the theoretical value of the resulting energy electronic state calculation($DV-X{\alpha}$ method). The components that were finally used were Cr, Mo, and Ti, with Ni as a base. For these alloys, elements were selected in order to compare their values with that of the average theoretical basis for an Inconel 625 alloy. Finally, two kinds of Ni alloy were designed: Ni-28Cr-4Mo-2Ti and Ni-20Cr-10Mo-1Ti.

Ni-Cr-Fe 및 Ni-Fe-Cr-Mo계 합금의 용접부 균열특성에 관한 연구 Part II : 열영향부의 액화균열 (A Study on the Cracking Behavior in the Welds of Ni-Cr-Fe and Ni-Fe-Cr-Mo Alloys)

  • 김희봉;이창희
    • Journal of Welding and Joining
    • /
    • 제15권5호
    • /
    • pp.46-55
    • /
    • 1997
  • This study has evaluated the liquation cracking behavior in the heat affected zone of several Ni base superalloys (Incoloy 825, Inconel 718 and Inconel 600). 304 and 310S austenitic stainless steels were also included for comparison. In addition, the mechanism of liquation cracking in the HAZ was postulated based on the extensive microstructural examinations with SEM, EDAX and TEM. The liquation cracking resistance of Ni base alloys was found to be far inferior to that of austenitic stainless steels. The liquation cracking of Incoloy 825 and Inconel 718 was believed to be closely related with the Laves-austenite(Ti rich in 825 and Nb rich in 718) and MC-austenitic eutectic phases formed along the grain boundaries by constitutional liquation and incipient melting under rapid welding thermal contraction. Further, liquation cracking resistance of the HAZ was dependent not only upon the type and amount of low melting phases but also on the grain size.

  • PDF

고온 리튬용융염에서 Ni 200 및 Ni-base 합금의 부식거동 (Corrosion Behavior of Ni 200 and Ni-base Alloys in Hot Lithium Molten salt)

  • 조수행;임종호;윤기석;박성원
    • 한국재료학회지
    • /
    • 제14권4호
    • /
    • pp.251-259
    • /
    • 2004
  • In the development of the advanced spent fuel management process based on the molten salt technology, it is essential to choose the optimum material for the process equipment handling molten salt. Corrosion behavior of Ni 200 and Ni-base alloys in molten salt of LiCl-$Li_2$O under oxidation atmosphere was investigated in the temperature range of $650~800^{\circ}C$ for 24~312 hrs. The order of corrosion rate was Ni 200 > Inconel 690 > Inconel 601 > Inconel 600. Inconel 600 alloy showed the highest corrosion resistance among the examined alloys, but Ni 200 exhibited the highest corrosion rate. Corrosion products of Inconel 600 and Inconel 601 were $Cr_2$$O_3$ and $NiFe_2$$O_4$. In case of Inconel 690, a single layer of $CrO_2$$O_3$ was formed in the early stage of corrosion and an outer layer of $NiFe_2$O$_4$ and inner layer of $Cr_2$$O_3$ were formed with increase of corrosion time. Inconel 600 showed local corrosion behavior and Inconel 601, 690 showed uniform corrosion behavior.

Precipitation Behavior of ${\gamma}"$ in Severely Plastic Deformed Ni-base Alloys

  • Kim, Il-Ho;Kwun, S.I.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.962-963
    • /
    • 2006
  • The precipitation behaviors of ${\gamma}"(Ni_3Nb)$ in four Ni-base alloys were investigated. The four alloys were forged Ni20Cr20Fe5Nb alloy, mechanically alloyed Ni20Cr20Fe5Nb alloy, IN 718 alloy and ECAPed(equal channel angular pressing) IN 718 alloy. Aging treatment was employed at either $600^{\circ}C$ or $720^{\circ}C$ for 20 hrs. The TEM observation and hardness test were performed to identify the formation of ${\gamma}"$. The precipitation of ${\gamma}"$ was noticed after aging at $600^{\circ}C$ for 20 hrs in the mechanically alloyed Ni20Cr20Fe5Nb alloy and ECAPed IN 718 alloy, while it was observed after aging at $720^{\circ}C$ for 20 hrs in the forged Ni20Cr20Fe5Nb alloy and IN 718 alloy before ECAP. The lower aging temperature for ${\gamma}"$ precipitation in the mechanically alloyed Ni20Cr20Fe5Nb alloy and ECAPed IN 718 alloy than in the forged Ni20Cr20Fe5Nb alloy and IN 718 alloy before ECAP appeared to be due to the severe plastic deformation which occurred during mechanical alloying or ECAP.

  • PDF

CORROSION BEHAVIOR OF NI-BASE ALLOYS IN SUPERCRITICAL WATER

  • Zhang, Qiang;Tang, Rui;Li, Cong;Luo, Xin;Long, Chongsheng;Yin, Kaiju
    • Nuclear Engineering and Technology
    • /
    • 제41권1호
    • /
    • pp.107-112
    • /
    • 2009
  • Corrosion of nickel-base alloys (Hastelloy C-276, Inconel 625, and Inconel X-750) in $500^{\circ}C$, 25MPa supercritical water (with 10 wppb oxygen) was investigated to evaluate the suitability of these alloys for use in supercritical water reactors. Oxide scales formed on the samples were characterized by gravimetry, scanning electron microscopy/energy dispersive spectroscopy, X-ray diffraction, and X-ray photoelectron spectroscopy. The results indicate that, during the 1000h exposure, a dense spinel oxide layer, mainly consisting of a fine Cr-rich inner layer ($NiCr_{2}O_{4}$) underneath a coarse Fe-rich outer layer ($NiFe_{2}O_{4}$), developed on each alloy. Besides general corrosion, nodular corrosion occurred on alloy 625 possibly resulting from local attack of ${\gamma}$" clusters in the matrix. The mass gains for all alloys were small, while alloy X -750 exhibited the highest oxidation rate, probably due to the absence of Mo.

용출법을 이용한 치과용 base metal alloy의 세포독성에 관한 실험적 연구 (An Experimental Study on The Cytotoxicity of Dental Base Metal Alleys by Extraction Method)

  • 윤민의;진태호;동진근
    • 대한치과보철학회지
    • /
    • 제27권2호
    • /
    • pp.123-130
    • /
    • 1989
  • In order to investigate the biocompatibility of base metal alloys in dental prosthesis, the 3 types of Ni-Cr alloys and the 3 types of Co-Cr alloys were collected and each alloy was extracted in the culture medium. L-cells derived from the subcutaneous tissue of mouse and extracted medium were cultivated. The relative growth rate of L-cells in the tissue culture was calculated with N-R assay. The obtained results were as follows: 1. In the case of the Co-Cr alloys tested, its cytotoxicity proved weak. 2. In the case of the Ni-Cr alloys tested, there was no significant degree of cytotoxicity, especially 25% Victory was proved noncytotoxicity.

  • PDF

실험 계획법 및 열역학 계산법을 이용한 초고온가스로용 니켈계 초합금 설계 방법론 (Methodology of Ni-base Superalloy Development for VHTR using Design of Experiments and Thermodynamic Calculation)

  • 김성우;김동진
    • Corrosion Science and Technology
    • /
    • 제12권3호
    • /
    • pp.132-141
    • /
    • 2013
  • This work is concerning a methodology of Ni-base superalloy development for a very high temperature gas-cooled reactor(VHTR) using design of experiments(DOE) and thermodynamic calculations. Total 32 sets of the Ni-base superalloys with various chemical compositions were formulated based on a fractional factorial design of DOE, and the thermodynamic stability of topologically close-packed(TCP) phases of those alloys was calculated by using the THERMO-CALC software. From the statistical evaluation of the effect of the chemical composition on the formation of TCP phase up to a temperature of 950 oC, which should be suppressed for prolonged service life when it used as the structural components of VHTR, 16 sets were selected for further calculation of the mechanical properties. Considering the yield and ultimate tensile strengths of the selected alloys estimated by using the JMATPRO software, the optimized chemical composition of the alloys for VHTR application, especially intermediate heat exchanger, was proposed for a succeeding experimental study.