• Title/Summary/Keyword: Nb3Sn 초전도체

Search Result 10, Processing Time 0.032 seconds

Fabrication technology and application of $Nb_3Sn$ superconductor for high magnetic field (고 자장용 $Nb_3Sn$ 초전도체의 제조기술 및 응용)

  • 오상수;류강식
    • Electrical & Electronic Materials
    • /
    • v.8 no.4
    • /
    • pp.518-525
    • /
    • 1995
  • 본 고에서는 Nb$_{3}$Sn 초전도선재의 대표적인 제조방법 및 원리 그리고 고자장마그네트 설계시 중요한 요소인 Nb$_{3}$Sn의 자장중 초전도특성 및 기계적특성 등에 대하여 고찰하고자 한다. 또한 Nb$_{3}$Sn 초전도선재의 응용분야로서 몇가지 대표적인 예를 들어 현재 세계적으로 활발하게 진행되고 있는 선진국의 고자장 초전도마그네트와 관련된 연구개발동향을 소개하고자 한다.

  • PDF

A Study on Microscopic Deformation Behaviors of $Nb_3Sn$ Superconducting Composite Tape using Acoustic Emission Technique ($Nb_3Sn$ 복합초전도 테이프의 미시적 변형거동 특성평가를 위한 음향방출기법 적용에 관한 연구)

  • 이민래;이준현
    • Composites Research
    • /
    • v.12 no.6
    • /
    • pp.22-30
    • /
    • 1999
  • Since the surface diffusion processed $Nb_3Sn$ superconducting tape has the advantage of having large overall critical current density. it is used for the construction of open type MRI superconducting magnets. However one of the disadvantages of this tape is that $Nb_3Sn$ compound often exhibited multiple cracking due to its intrinsic brittleness when subjected to mechanical loading such as bending and winding during the fabrication process for superconducting coil. This will eventually cause the severe degradation of critical current density. Therefore it is important to understand the microscopic deformation behavior of this kind of superconducting tape under the mechanical loading.In this study, acoustic emission(AE) was used to clarify microscopic deformation behavior at room temperature for $Nb_3Sn$ superconducting tape which was strengthened and stabilized with copper. For this purpose, special attention was paid to AE characteristics including AE event, energy, and amplitude distribution which were associated with microscopic mechanism of deformation of $Nb_3Sn$ superconducting tape under tensile load.

  • PDF

핵융합용 초전도선재의 크롬도금기술

  • Park, Pyeong-Ryeol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.11a
    • /
    • pp.32-32
    • /
    • 2012
  • 화석연료의 남용으로 지구 온난화가 심화되어 환경과 생태계변화가 가속화되고 있고, 급속한 산업의 발달과 인류 삶의 질 향상에 따른 에너지 수요가 급증하고 있는 실정에 있으며, 일본 후쿠시마 원전사태로 원자력 에너지의 위험성으로 지구 인류환경은 심각한 국면을 맞이 하고 있어 대체 에너지의 하나로 핵융합 에너지 필요성이 증대되고 있다. 핵융합 에너지 연구 개발은 우리나라에서 KSTAR가 1997년부터 건설하기 시작하여 지난 2007년에 완공되어 지금 운용 중에 있고, 국제적으로 미국, EU, 러시아, 중국, 한국, 일본 인도가 참여하는 ITER 국제 공동프로젝트가 2004년에 건설을 시작하여 프랑스 카다라쉬에 실증 플란트를 건설 중에 있다. 이러한 핵융합 반응을 위해서는 10e-7이상의 높은 진공과 1억$^{\circ}C$ 이상에서 중수소와 삼중수소가 반응하여 발생하는 플라즈마를 제어 할 필요가 있으며, 초고온의 핵융합 플라즈마를 가두고 가동시키기 위해서는 약 12Tesla이상의 고자장 마그넷이 필요하다. 현재 ITER 실증 플란트에 사용되는 고자장 마그넷은 TF (Toroidal Field)코일과 CS (Central Field)코일에 Nb3Sn 초전도선재가 핵심부품으로 사용되고 있으며 ITER프로젝트에서는 약 850톤의 Nb3Sn 초전도선재가 사용될 전망이다. 그 중에서 일본 25%, EU, 러시아와 한국이 각각 20%, 중국7%, 미국8% 할당되어 참여국 대부분은 초전도선재를 전략적으로 공급하고 있다. 초전도 선재의 크롬도금은 1~2 마이크로미터 이하의 균일하고 얇은 도금 두께와 밀착성이 우수한 품질이 요구된다. 일반적으로 크롬도금은 산업현장에서 컨베이어 벨트 방식으로 장식이나, 내식성 및 내마모성의 특성을 필요로 할 때 사용되고 있으나, 선재에 크롬도금을 릴투릴(Reel to Reel) 방식으로 적용되는 경우는 세계적으로 아주 드물다. 핵융합 마그넷의 CICC(Conduct In Cable Conduit)도체를 만들기 위해서는 초전도선재를 이용, 3(Sc 2+OFC 1)$^*3^*5^*5^*6$형태로 연선과 케이블링을 하게 되며, 초전도 선재를 연선하고 케이블링을 할 때 크롬 도금층이 박리될 가능성이 있어 크롬도금 방법과 프로세스를 특별히 고안할 필요가 있다. ITER핵융합로 마그넷의 TF코일은 높이 14m, 폭 9m 최대자장 12Tesla, 최대전류 68kA, CICC도체 직경이 40mm로서 그 초전도 조관/도체 내부에 0.82mm 직경의 Nb3Sn 초전도 선재가 약 1350가닥으로 연선과 케이블링으로 구성되어 있다. ITER 핵융합 마그넷용 초전도 선재의 크롬도금은 마그넷 권선 후 Nb3Sn 초전도물질을 형성하기 위해서 $650^{\circ}C$에서 500시간 열처리를 실시하며 열처리 시 초전도 선재의 소선들 사이에 발생할 수 있는 소착을 방지하고, 초전도 선재에서 발생하는 AC loss를 감소시키며, Quench시 발생되는 열을 쉽게 확산시킴으로써, 초전도 마그넷의 열적 안정성(Thermal Stability) 향상과 필요에 따라서 소선간 통전울 가능하게 한다. 고려제강의 자회사인 케이에이티는 크롬도금 밀착성이 우수하고 도금두께 0.1마이크로 미터 이내 제어가 가능한 얇고 균일한 도금품질을 개발하여 한국형 핵융합 실험로인 KSTAR에 65톤 전량 공급하였고, 크롬 도금된 무산소동 선재 32톤과 초전도 선재 93톤을 전량 ITER 프로젝트에 공급하고 있으며, 2013년도 상반기에는 공급을 마무리할 예정이다.

  • PDF

Development of ITER TF Cable-in-Conduit Conductors and Their Characteristics (ITER TF 초전도 도체 개발과 특성)

  • Kim, Hyoung-Chan;Oh, Dong-Keun;Park, Su-Hyeon;Kim, Kee-Man;Bruzzone, P.
    • Progress in Superconductivity
    • /
    • v.10 no.2
    • /
    • pp.108-115
    • /
    • 2009
  • As a participant taking part in the ITER TF conductor R&D program, we developed two toroidal field conductors with variations of conduit thickness resulting in the different void fraction of the conductors. The estimated void fractions of the conductors are 31% and 33%. In this paper we present the details of the TF conductor development and performance test results of them carried out by the measurement of current sharing temperature under cyclic loading. Regarding the conductor development, the internal-Sn-processed $Nb_3Sn$ strand characteristics, strand cabling, twist pitch and characteristics of the conduit materials are presented. For the understanding of the conductor design and performance, the conductor test results are presented and the effect of the conductor design parameters such as void fraction and twist pitch is discussed based on the results.

  • PDF

Properties of Butt Joint in $Nb_{3}$Sn Conductors with change of Surface Pressure (접촉 면압에 따른 $Nb_{3}$Sn 도체의 Butt 접합부 특성)

  • 이호진;김기백;김기만
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2002.02a
    • /
    • pp.253-255
    • /
    • 2002
  • Since a butt Joint is smaller than a lap type joint, it is expected to have smaller AC losses. The butt joint is produced by the diffusion bonding of the contacting surface under pressured and heated condition. It is important to find robust joining conditions, because butt joint has small contact area and has the shape by which the quality of bonding is hard to be checked. In this research, the loading pressure is considered as the joining parameter to find optimum joining condition. The DC resistance of the joint may be changed by the surface pressure during joining process, because the superconducting strands near the contact surface are failed by large plastic deformation. The range from 10 MPa to 18 MPa is expected optimum surface pressure in the conditions of 1 hour heating time and $750^{\circ}C$ temperature in the vacuum furnace.

  • PDF

The analysis of bending processes in $Nb_{3}$Sn Cable-in-Conduit Conductors ($Nb_{3}$Sn 도관 케이블 도체의 굽힘변형 해석)

  • 남현일;이호진;박재학
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2002.02a
    • /
    • pp.259-262
    • /
    • 2002
  • Cable-in-Conduit Conductors (CICC) have been used for fabrication of nuclear fusion magnets. Bending process is included in fabrication of superconducting magnet such as termination of conductors. Because of plastic deformation by bending process, there can be a large residual stress and change of shape in bent conductors. Void volume fraction in conductors is also changed by bending process. In this study, Commercial code was used to analyze the bending process at various bending curvature radius. The calculated residual stress of conductors bent at less than about 40cm curvature radius exceeded the allowable stress.

  • PDF

Theoretical study on the stability and mechanical property of conductor for superconducting power cable (초전도 송전 케이블용 도체의 안정성 및 기계적특성에 대한 이론적 검토)

  • Oh, S.S.;Oh, B.H.;Ha, D.W.;Cho, J.W.;Kown, Y.K.;Ryu, K.S.;NamKung, D.;Jang, J.K.
    • Proceedings of the KIEE Conference
    • /
    • 1995.07a
    • /
    • pp.147-149
    • /
    • 1995
  • The stabilization of the conductor in superconducting power cable is very important from the view point of protection. In this study, critical thicknesses of superconducting layer of $Nb_{3}Sn$ conductor and stabilizer Cu have been estimated under the adiabatic condition. The bending stress of $Nb_{3}Sn$/SUS composite superconducting tape on the curvature radius was also evaluated.

  • PDF

Magnetic $T_c$ Measurements of Composite Superconductors for a Standard Method (복합초전도체의 자기적 임계온도 측정의 표준화연구)

  • Lee K. W;Kim M. S;Kim D. H;Lee S. G
    • Progress in Superconductivity
    • /
    • v.6 no.1
    • /
    • pp.24-31
    • /
    • 2004
  • Magnetic $T_{c}$ of composite superconductors has been studied for providing a standard method. Various magnetization-temperature curves of NbTi, $Nb_3$Sn and Bi-2223 wires were measured using a SQUID magnetometer. Magnetization-temperature curve of zero-field-cooled procedure showed larger values than fie Id-cooled procedure. To obtain higher resolution near the onset temperature, we employed a two-field-direction method which measures a magnetization-temperature curve of a specimen first in positive and then negative fields. Analytical comparison of the magnetic $T_{c}$, with the resistive T$_{c}$ was accomplished for three specimens. The magnetic $T_{c}$/ mettled showed more detailed information on superconducting state of a specimen than the resistive$T_{c}$/ method. We have also studied the field dependence of the magnetic $T_{c}$ from 5 Oe to 120 Oe, however, no significant difference on field strength was found in our three specimensns

  • PDF

Numerical analysis about current non-uniformity in superconducting CICC (cable-in-conduit conductor) joint (초전도 관내연선도체 접합부에서의 전류 불균일에 대한 수치적 분석)

  • Lee, Sang-Il;Jeong, Sang-Kwon;Choi, Sung-Min;Park, Kap-Rai
    • Progress in Superconductivity and Cryogenics
    • /
    • v.9 no.3
    • /
    • pp.41-45
    • /
    • 2007
  • This paper presents transport current non-uniformity in a joint for superconducting multistage cable-in-conduit conductor (CICC) and relaxation in the CICC. The joint is considered to have a current loop linked to an external magnetic field so that it becomes an emf voltage source. It is numerically analyzed using an electrical transmission line model. The inductive current in a resistive joint is compared to that of a non-resistive joint when the ramping field is applied vertically to the joints. Regarding the parameter values of the model. a full scale $Nb_3Sn$ CICC and a strand-to-strand (STS) joint for the toroidal field magnet of the KSTAR (Korea Superconducting Tokamak Advanced Research) device are referenced to. It is found that the resistive joint prevents the current from rising too much and enhances decaying the current when the ramping stops. The 'flattop' current is found to be proportional to the ramp rate of the field (dB/dt). The relaxation length, which is defined as the length within which the maximum induced current falls by 1/e. is found to saturate within 0.27m.

The Trapped Field Characteristics of YBCO Superconductor Composite in Terms of Applied Magnetic Field (인가 자기장에 의한 YBCO 초전도체 복합체의 포획 자기장 특성)

  • Lee, M.S.;Jang, G.E.;Choi, Y.S.;Jun, B.H.;Han, Y.H.;Park, B.J.
    • Progress in Superconductivity
    • /
    • v.12 no.1
    • /
    • pp.12-16
    • /
    • 2010
  • We have measured the trapped field of YBCO bulk with different configuration by applying the magnetic field of $Nb_3Sn$ superconducting magnet. Initially the circular type of YBCO bulk superconductor was prepared and then hole, parallel to the c-axis and located at the center of bulk was mechanically drilled. The YBCO bulk with hole was filled with resin. Typical size of hole in YBCO bulk was 10 mm in diameter. Trapped field characteristics were compared with different specimen conditions. Our preliminary result indicates the increment rate of trapped field, 0.232 kG, measured on the YBCO without hole was much higher than that, 0.011 kG, measured on YBCO with hole.