• Title/Summary/Keyword: Nb2O3

Search Result 1,400, Processing Time 0.04 seconds

Effects of Sintering Additives and Atmospheres on the Piezoelectric and Sintering Properties of $Pb_{0.98}Cd_{0.02}Zr_{0.36}Ti_{0.39}Ni_{0.083}Nb_{0.167}O_3$ (소결첨가제와 분위기가 $Pb_{0.98}Cd_{0.02}Zr_{0.36}Ti_{0.39}Ni_{0.083}Nb_{0.167}O_3$의 소결 및 압전 특성에 미치는 영향)

  • 문종하;박진성;박현수
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.11
    • /
    • pp.1260-1266
    • /
    • 1996
  • The effects of SiO2 MnO2 and sintering atmospheres (O2, N2) on the piezoelectric properties and densification behaviors of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 were investigated. The addition of SiO2 to the system enhanced the rate of densification but supressed the rate of grain growth. On the other hand the addition of MnO2 to the system did not nearly affect the rate of densification but increased slightly the rate of grain growth The densification of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 was promoted with increasing the partial pressure of O2. The relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 sintered under O2 atmosphere were higher than under N2 atmosphere. Whereas the mechanical quality factor (Qm) of specimens sintered under O2 atmosphere were lower than under N2 atmosphere. Thus the sintering atmosphere of O2 and N2 in Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 acted as donor and acceptor respectively. As the amount of SiO2 increased the relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 but the mechanical quality factor (Qm) did not nearly change, In the case of the addition of MnO2 to the system the relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 sintered under O2 atmosphere decreased rapidly with increasing the amount of MnO2 but they were unchanged with increasing the amount of MnO2 under N2 sintering atmosphere. Therefore the differences of the relative dielect-ric constant ($\varepsilon$r) and piezoelectric constant (d33) due to sintering atmosphere were diminished as the amount of MnO2 increased.

  • PDF

Influence of PVP on the Thickness of Ferroelectric (Na,K)NbO3 Film by Sol-Gel (솔-젤 법을 통해 제조된 강유전체 (Na,K)NbO3 막의 두께에 미치는 PVP의 영향)

  • Kim, Dae-Gun;Yoo, In-Sang;Kim, Sae-Hoon;Kim, Jin-Ho
    • Korean Journal of Materials Research
    • /
    • v.22 no.12
    • /
    • pp.696-700
    • /
    • 2012
  • (Na, K) $NbO_3$ thick film was successfully achieved using a sol-gel coating process with the addition of polyvinylpyrrolidone (PVP) to a metal alkoxide solution. The transparent coating solution, mixed with Nb:PVP = 1:1 in a molar ration, was synthesized by evaporating the solvent to over 62.5 wt%. Additive PVP increased the viscosity of the solution so that the coating thickness could be enhanced. The thickness of the (Na, K) $NbO_3$ film assisted by PVP was ca. 320 nm at the time of deposition; this value is four times thicker than that of the sample fabricated without PVP. Also, due to PVP binding with the OH groups of the metal alkoxide, the condensation reaction in the film was suppressed. The crystalline size of the (Na, K) $NbO_3$ films assisted by PVP was ca. 15 nm smaller than that of the film fabricated without PVP. After the sintering process at $700^{\circ}C$, the (Na, K) $NbO_3$ films were mainly composed of randomly oriented (Na, K) $NbO_3$ phase of perovskite crystal structure, including a somewhat secondary phase of $K_2Nb_4O_{11}$. However, by adding PVP, the content of the secondary phase became quite smaller than that of the sample without PVP. It was thought that the addition of PVP might have the effect of restraining the loss of potassium and that PVP could hold metalloxane by strong hydrogen bonding before complete decomposition. Therefore, the film thickness of the (Na, K) $NbO_3$ films could be considerably advanced and made more crack-free by the addition of PVP.

Electron Magnetic Resonance Study of Paramagnetic Impurities in LiTaO3 and LiMbO3 Single Crystals (LiTaO3 및 LiMbO3 단결정 내의 상자성 불순물에 관한 전자 자기공명 연구)

  • Yeom, Tae-Ho
    • Journal of the Korean Magnetics Society
    • /
    • v.13 no.5
    • /
    • pp.204-210
    • /
    • 2003
  • Electron magnetic resonance (EMR) of paramagnetic Cr$^{3+}$, Mn$^{2+}$, and Fe$^{3+}$ impurity ions in ferroelectric LiNbO$_3$ and LiTaO$_3$ single crystals has been studied. The actual sites location of paramagnetic impurity ions in the crystals was suggested from the experimental results and zero field splitting parameters calculated by superposition model. It turns out that Cr$^{3+}$ ions in LiNbO$_3$ crystal have two resonance centers and enter both the Li$^{+}$ and Nb$^{5+}$ ions. Mn$^{2+}$ and Fe$^{3+}$ impurity ions in LiNbO$_3$ substitute for Nb$^{5+}$ ions. However, both Cr$^{3+}$ and Fe$^{3+}$ ions in LiTaO$_3$ crystal reside at Li$^{+}$ ions.$ +/ ions.+/ ions.

Environmental Effect on Corrosion Behaviour of Zr-2.5Nb Alloy (Zr-2.5Nb 합금의 부식거동에 미치는 부식 매질 효과)

  • Ju, Gi-Nam;Gwon, Sang-Cheol;Kim, Yeong-Seok
    • Korean Journal of Materials Research
    • /
    • v.8 no.1
    • /
    • pp.3-9
    • /
    • 1998
  • 40$0^{\circ}C$ H$_{2}$O, D$_{2}$O및 $O_{2}$분위기에서 Zr-2.5Nb합금의 부식거동을 분석하였다. Martensitic $\alpha$'-Zr상이나 $\alpha$-Zr과 $\beta$-Zr상의 Zr-2.5Nb합금인 경우, 부식분위기에 매우 민감하여, $O_{2}$속에서 가장 큰 부식속도를 보였다. 반면, $\alpha$-Zr나 $\beta$-Zr상의 경우, 부식 매질에 따른 별다른 차이없이 높은 부식저항성을 보였다. 이러한 Zr-2.5Nb 합금의 미세조직 및 부식 매질에 따른 부식거동변화는 Zr-2.5Nb 합금의 음극 지배 부식반응의 관점으로 해석되었으며, 이들 결과를 이용하여 CANDU 형및 RBMK 형 Zr-2.5Nb 압력관의 가동조건 차이를 설명할 수 있었다. Zr-2.5Nb 합금의 모든 조직에서 주로 단사정 ZrO$_{2}$산화물이 형성되었으며, 산화물내 정방정 ZrO$_{2}$비율은 산화물 두께가 증가함에 따라 감소하였다.

  • PDF

Effect of Sintering Temperature on the Dielectric Property of Lead Magnesium Niobate-Lead Titanate Ceramics

  • Hwang, Hak-In;Jung, Jong-Man;Park, Joon-Shik
    • The Korean Journal of Ceramics
    • /
    • v.4 no.4
    • /
    • pp.286-291
    • /
    • 1998
  • Dielectric properties of $Pb(Mg_{1/3}Nb_{2/3})O_{3}-PbTiO_{3}$, ceramics prepared by the columbite precursor method have been investigated as a function of the sintering temperature in the range of 1000∼$1250^{\circ}C$. The $Pb(Mg_{1/3}Nb_{2/3})O_{3}-PbTiO_{3}$ ceramics show typical relaxor ferroelectric behavior. As the sintering temperature increased, the dielectric constant increased and the phase transition temperature shifted to lower temperature. The TCK(temperature coefficient of dielectric constant) and VRK (variation rate of dielectric constant) increased with increasing sintering temperature. The $Pb(Mg_{1/3}Nb_{2/3})O_{3}-PbTiO_{3}$ compositions sintered at $1250^{\circ}C$ appear to be suitable for ferroelectric bolometer.

  • PDF

Preparation of Pb(Fe1/2Nb1/2)O3 Powders by Supercritical Fluid Method (초임계 유체법을 이용한 Pb(Fe1/2Nb1/2)O3분말 제조)

  • 임대영;김병규;최근목;홍석형;김태훈
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.6
    • /
    • pp.566-569
    • /
    • 2002
  • In general, Pb-based complex perovskite powders have not been directly prepared because pyrochlore that is secondary phase appears. In this study, we tried to prepare Pb(Fe$_{1}$2/Nb$_{1}$2/)O$_3$ which was used to the electronic multicomponent by supercitical fluid method in order to fabricate very active powder not through pyrochlore.

COMPOSITIONAL DEPENDENCE OF $128^{\circ}$ Y CUT $LiNbO_3$ CRYSTALS ON SAW CHRACTERISTICS ($128^{\circ}$ Y Cut $LiNbO_3$단결정의 조성비 변화에 따른 SAW특성변화)

  • 이상학;한재용;조순형;윤의박
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.2 no.1
    • /
    • pp.30-36
    • /
    • 1992
  • In order to measure the characteristics of Surface Acousitc Wave(SA W) with compositions of $LiNbO_3$ single crystal, $128^{\circ}$ Y cut wafer was fabricated from $LiNbO_3$ single crystals with the composition range of 47-50 $Li_2O$mol%. Delay lines were formed on the $128^{\circ}$ Y cut wafer using photolithography technique. Delay time was measured by pulse-echo overlap method. The compositional dependence of SAW characteristics, SAW velocity, electro-mechanical coupling coefficient$(K_s^2)$ and temperature coefficient of delay time(TCD), were investigated.

  • PDF

Occurrence and Chemical Composition of Ti-bearing Minerals from Samgwang Au-ag Deposit, Republic of Korea (삼광 금-은 광상에서 산출되는 함 티타늄 광물들의 산상 및 화학조성)

  • Yoo, Bong Chul
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.33 no.3
    • /
    • pp.195-214
    • /
    • 2020
  • The Samgwang Au-Ag deposit has been one of the largest deposits in Korea. The deposit consists of eight lens-shaped quartz veins which filled fractures along fault zones in Precambrian metasedimentary rock, which feature suggest that it is an orogenic-type deposit. The Ti-bearing minerals occur in wallrock (titanite, ilmenite and rutile) and laminated quartz vein (rutile). They occur minerals including biotite, muscovite, chlorite, white mica, monazite, zircon, apatite in wallrock and white mica, chlorite, arsenopyrite in laminated quartz vein. Chemical composition of titanite has maximum vaules of 3.94 wt.% (Al2O3), 0.49 wt.% (FeO), 0.52 wt.% (Nb2O5), 0.46 wt.% (Y2O3) and 0.43 wt.% (V2O5). Titanite with 0.06~0.14 (Fe/Al ratio) and 0.06~0.15 (XAl (=Al/Al+Fe3++Ti)) corresponds with metamorphic origin and low-Al variety. Chemical composition of ilmenite has maximum values of 0.07 wt.% (ZrO2), 0.12 wt.% (HfO2), 0.26 wt.% (Nb2O5), 0.04 wt.% (Sb2O5), 0.13 wt.% (Ta2O5), 2.62 wt.% (As2O5), 0.29 wt.% (V2O5), 0.12 wt.% (Al2O3) and 1.59 wt.% (ZnO). Chemical composition of rutile in wallrock and laminated quartz vein has maximum values of 0.35 wt.%, 0.65 wt.% (HfO2), 2.52 wt.%, 0.19 wt.% (WO3), 1.28 wt.%, 1.71 wt.% (Nb2O3), 0.03 wt.%, 0.07 wt.% (Sb2O3), 0.28 wt.%, 0.21 wt.% (As2O5), 0.68 wt.%, 0.70 wt.% (V2O3), 0.48 wt.%, 0.59 wt.% (Cr2O3), 0.70 wt.%, 1.90 wt.% (Al2O3) and 4.76 wt.%, 3.17 wt.% (FeO), respectively. Rutile in laminated quartz vein is higher contents (HfO2, Nb2O3, As2O5, Cr2O3, Al2O3 and FeO) and lower content (WO3) than rutile in wallrock. The substitutions of rutile in wallrock and laminated quatz vein are as followed : rutile in wallrock [(Fe3+, Al3+, Cr3+) + Hf4+ + (W5+, As5+, Nb5+) ⟵⟶ 2Ti4+ + V4+, 2Fe2+ + (Al3+, Cr3+) + Hf4+ + (W5+, As5+, Nb5+) ⟵⟶ 2Ti4+ + 2V4+], rutile in laminated quartz vein [(Fe3+, Al3+) + As5+ ⟵⟶ Ti4+ + V4+, (Fe3+, Al3+) + As5+ ⟵⟶ Ti4+ + Hf4+, 4(Fe3+, Al3+) ⟵⟶ Ti4+ + (W5+, Nb5+) + Cr3+], respectively. Based on these data, titanite, ilmenite and rutile in wallrock were formed by resolution and reconcentration of cations (W5+, Nb5+, As5+, Hf4+, V4+, Cr3+, Al3+, Fe3+, Fe2+) in minerals of wallrock during regional metamorphism. And then rutile in laminated quartz vein was formed by reconcentration of cations (Nb5+, As5+, Hf4+, Cr3+, Al3+, Fe3+, Fe2+) in alteration minerals (white mica, chlorite) and Ti-bearing minerals reaction between hydrothermal fluid originated during ductile shear and Ti-bearing minerals (titanite, ilmenite and rutile) in wallrock.

Crystal Growth and their photorefractive properties for optical memo (광메모리 단결정의 성장과 그 특성)

  • 유영문
    • Broadcasting and Media Magazine
    • /
    • v.6 no.1
    • /
    • pp.78-87
    • /
    • 2001
  • Seven kinds of most representative photorefractive crystals expected to contribute to the realization of the volume holographic storage were reviewed The growth conditions and problems for highly homogeneous optical qualities of the following crystals depending on the growth methods were discussed;(1) $LiNbO_3$ and $Bi_2SiO_{20}$ by Czochralski method (2) $Bi_{12}TiO_{20}$, $KNbO_3$ and $BaTiO_3$ by top seeded solution growth and (3) $(Sr_{1-x}Ba_{x})Nb_{2}O_{6}$ and $(K_{1-y}Na_y)_{2A-2}(Sr_{1-x}Ba_x)_{2-A}Nb_2O_6$ by Stepanov method, And then the figure of merits for the estimation of phororefractive materials on performances, such as $Q_1$, $Q_2$ and sensitivity, were discussed.

  • PDF