Comparative Study of Properties of Dental Zirconia According to Microwave Sintering Method (마이크로웨이브 소결방법에 따른 치과용 지르코니아의 물리적 특성)

  • Kim, Tae-Suk;Yu, Chin-Ho;Kim, Gi-Chul;Park, Won-Uk;Seo, Jung-Il;Hwang, Kyu-Hong
    • Journal of Technologic Dentistry
    • /
    • v.34 no.1
    • /
    • pp.11-21
    • /
    • 2012
  • Purpose: Densification and mechanical properties of dental zirconia ceramics were evaluated by different sintering methods. Materials and Methods: Y-TZP zirconia block(Kavo $Everest^{(R)}$ ZS blank, Kavo dental GmbH, Bismarckring, Germany) was used in this study. Sintering were performed in heat sintering furnace and microwave sintering furnace, and then experimented and analyzed on a change in densification according to the sintering time, a change in densification according to thickness, flexural strength and micro-structure in zirconia specimens. Results: Microwave sintering was very effective in considerable mechanical properties such as flexural strength and bulk density was drastically increased than conventional electric heating method. It is also shown that microwave sintering time was faster and more economical than common method to be present in qualities which equal or exceed. Conclusion: It will be important to seek the accurate sintering condition of dental zirconia by microwave sintering method and the continuous research is necessary for the study of relationship between sintering methods and mechanical properties.

Domain formation and expansion during periodic poling of congruent $LiNbO_3$ using external field (조화용융조성 $LiNbO_3$의 주기적 분극 반전 동안 도메인 생성 및 이동에 관한 연구)

  • Kwon, S.W.;Yang, W.S.;Lee, H.M.;Kim, W.K.;Lee, H.Y.;Yoon, D.H.;Song, Y.S.
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.16 no.2
    • /
    • pp.53-58
    • /
    • 2006
  • When external field was applied to congruent $LiNbO_3$, it was investgated for domain formation and expansion of $LiNbO_3$. The domain wall velocities of 0.5 mm thickness $LiNbO_3$ were 28.70, 16.02 and $5.75{\mu}m/sec$ under poling field of 23.5, 22.0 and 21.0 kV/mm, respectively. As $1 M{\Omega}$ resistor was used in domain inversion system, harmonic domain inversion was not achieved by rapid domain expansion. And 50% duty cycle periodically poled $LiNbO_3$ have been fabricated by charge control using $10 M{\Omega}$ resistor.

Improved Uniformity of GaAs/AlGaAs DBR Using the Digital Alloy AlGaAs Layer (디지털 합금 AlGaAs층을 이용하여 제작된 GaAs/AlGaAs DBR의 균일도 향상)

  • Cho, N.K.;Song, J.D.;Choi, W.J.;Lee, J.I.;Jeon, Heon-Su
    • Journal of the Korean Vacuum Society
    • /
    • v.15 no.3
    • /
    • pp.280-286
    • /
    • 2006
  • A distributed Bragg reflector (DBR) for the application of $1.3{\mu}m$ vertical cavity surface emitting laser (VCSEL) has grown by digital-alloy AlGaAs layer using the molecular beam epitaxy (MBE) method. The measured reflection spectra of the digital-alloy AlGaAs/GaAs DBR have uniformity in 0.35% over the 1/4 of 3-inch wafer. Furthermore, the TEM image showed that the composition and the thickness of the digital-alloy AlGaAs layer in AlGaAs/GaAs DBR was not affected by the temperature distribution over the wafer whole surface. Therefore, the digital-alloy AlGaAs/GaAs DBR can be used to get higher yield of VCSEL with the active medium of InAs quantum dots whose gain is inhomogeneously broadened.

Mechanical Properties of Synthesized Nano Laminating $Ti_3SiC_2$ by Reaction Press Sintering (반응 가압 소결 방법으로 합성된 nano laminating $Ti_3SiC_2$의 기계적 특성)

  • 황성식;박상환;김찬묵
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.396-400
    • /
    • 2003
  • A new synthesis process for nano laminating Ti$_3$SiC$_2$ has been developed using TiCx (x=0.67) and Si powder as starting materials by a reaction hot pressing. Bulk Ti$_3$SiC$_2$ was fabricated using a green body consisting of TiCx and Si by a hot pressing under the pressures of 25 MPa at 1420-1550 $^{\circ}C$ for 90 min. The synthesized Ti$_3$SiC$_2$ was consisting of only TiCx and Ti$_3$SiC$_2$. The relative density of sintered bulk Ti$_3$SiC$_2$ was increased as the hot pressing temperature was increased, which was mainly due to the increase in TiCx contents in synthesized Ti$_3$SiC$_2$. The synthesized Ti$_3$SiC$_2$ bulk was consisted of nano sized lamella structure of 20-100 nm in thickness. It was found that TiCx particles in Ti$_3$SiC$_2$ would increase the 3-point bending strength of synthesized Ti$_3$SiC$_2$ bulk. The maximum 3-P. bending strength of synthesized Ti$_3$SiC$_2$ bulk was more than 800 MPa. The Vickers hardness of synthesized Ti$_3$SiC$_2$bulk was as low as 5 Gpa, which was decreased with the indentation load. The quasi-plastic deformation behaviors were observed around indentation mark on Ti$_3$SiC$_2$.

  • PDF

Preparation of ZnO Thin Film by Electrophoretic Deposition(EPD)

  • Jun, Byung-Sei
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.1
    • /
    • pp.78-83
    • /
    • 2012
  • The electrophoretic deposition(EPD) of ZnO nano-sized colloids is investigated by changing the colloid number concentration, applied force, and deposition time. The change of the colloid size in a suspension was examined by the different colloid number concentrations (N = $3.98{\times}10^{15}$, N = $3.98{\times}10^{14}$, and N = $3.98{\times}10^{13}$) with an increase of the deposition time and applied forces. Deposition behavior was investigated by changing the applied fields (from DC 5 V to 50 V) and the deposition time (5 min to 25 min). The surface microstructures of the as-deposited films were investigated by SEM. The dried films were sintered from $850^{\circ}C$ to $1,050^{\circ}C$ for 2 h and then the microstructures were also explored by SEM. The agglomeration rate was enhanced by increasing the colloid number concentration of colloids. Colloid number concentration in a suspension must be rapidly decreased at higher values of the electric field. ZnO nano-sized colloids had the highest zeta potential value of over -28 mV in methanol. A homogeneous microstructure was obtained at colloid number concentration of N = $3.98{\times}10^{13}$, applied DC field of 5 V/cm and 15 min of deposition time at an electrode distance of 1.5 cm. Under these conditions, the deposited films were sintered at $850^{\circ}C$ and $1,050^{\circ}C$ for 2 h. The results show a typical pore-free surface morphology of a uniform thickness of 400 nm under these experimental conditions.

Fabrication of a Nano-Wire Grid Polarizer for Brightness Enhancement in TFT-LCD Display (TFT-LCD용 휘도 성능을 향상시키는 나노 와이어 그리드 편광 필름의 제작)

  • Huh, Jong-Wook;Nam, Su-Yong
    • Journal of the Korean Graphic Arts Communication Society
    • /
    • v.29 no.3
    • /
    • pp.105-124
    • /
    • 2011
  • TFT-LCD consists of LCD panel on the top, circuit unit on the side and BLU on the bottom. The recent development issues of BLU-dependent TFT-LCD have been power consumption minimization, slimmerization and size maximization. As a result of this trend, LED is adopted as BLU instead of CCFL to increase brightness and to reduce thickness. In liquid crystal displays, the light efficiency is below 10% due to the loss of light in the path from a light source to an LCD panel and presence of absorptive polarizer. This low efficiency results in low brightness and high power consumption. One way to circumvent this situation is to use a reflective polarizer between backlight units and LCD panels. Since a nano-wire grid polarizer has been known as a reflective polarizer, an idea was proposed that it can be used for the enhancement of the brightness of LCD. The use of reflective polarizing film is increasing as edge type LED TV and 3D TV markets are growing. This study has been carried out to fabrication of the nano-wire grid polarizer(NWGP) and investigated the brightness enhancement of LCD through polarization recycling by placing a NWGP between an c and a backlight unit. NWGPs with a pitch of 200nm were fabricated using laser interference lithography and aluminum sputtering and wet etching. And The NWGP fabrication process was using by the UV imprinting and was applied to plastic PET film. In this case, the brightness of an LCD with NWGPs was 1.21 times higher than that without NWGPs due to polarization recycling.

Congruent LiNbO3 Crystal Periodically Poled by Applying External Field (외부전계 인가에 의한 조화용융조성 LiNbO3 결정의 주기적 분극반전)

  • Kwon, Soon-Woo;Yang, Woo-Seok;Lee, Hyung-Man;Kim, Woo-Kyung;Lee, Han-Young;Yoon, Dae-Ho;Song, Yo-Seung
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.11 s.282
    • /
    • pp.749-752
    • /
    • 2005
  • When an electric field higher than a characteristic coercive field is applied to a ferroelectric such as $LiNbO_3$, the orientation of the spontaneous polarization is reversed, which causes the reversal of the sign of odd-rank tensor properties such as electro-optic and nonlinear optic coefficients. A fabrication process of insulator and periodic external field assisted poling of a z-cut $LiNbO_3$ have been optimized for a periodic $180^{\circ}$ phase inversion along z-axis. The poling jig and the poling control system, fully controlled by a computer, for high quality and reproducible PPLN fabrication have been devised. Periodically polarization reversed PPLN was adjusted based on the fabricated thickness of insulator. The poling structure of PPLN was observed under a microscope after etching PPLN samples by an etching solution ($HF:HNO_3$ = 1 : 2) for about 15 min.

Magnetism of Nanocomposite Quartz Powder by use of MCR Method

  • Soh, Deawha;Lim, Byoungjae;Soh, Hyunjun;Mofa, N.N.;Ketegenov, T.A.;Mansurov, Z.A.
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2004.05a
    • /
    • pp.113-116
    • /
    • 2004
  • The materials showing high structure dispersion with functional properties were developed on the quartz base and those were obtained by mechano-chemical reaction technology. Depending on the processing conditions and subsequent applications the materials produced by mechano-chemical reaction show concurrently magnetic, dielectric and electrical properties. The obtained magnetic-electrical powders classified by aggregate complex of their features as segnetomagnetics, containing a dielectric material as a carrying nucleus, particularly the quartz on that surface one or more layers of different compounds were synthesized having thickness up to 10~50 nm showing magnetic, electrical properties and others. The similarity of the structure of surface layers of quartz particles subjected to mechano-chemical processing and nano-structure cluspol (clusters in a polymer matrics) material was also confirmed by the fact that the characteristics of ferromagnetic quartz of insulating nano-composite powder were changed with time, after its preparing process was completed. The magnetic permeability of the sample was decreasing within first two months down by 15~20 %. Then, the magnetic characteristics were almost stabilized steadily and continuously. The observed changes were related with defective structure of the particles, elastic stress relief, and changes of electron density and magnetic moment in deformation zones. This process of stabilization of the investigated properties could be intensified by the thermal annealing heat treatment in short time period of the nano-composite quartz powders at the temperature ranges of 100~15$0^{\circ}C$.

  • PDF