• Title/Summary/Keyword: Nano lubricant

Search Result 41, Processing Time 0.228 seconds

Fe계 합금 분말 소결품(SMF9060)의 마모 특성 연구 (A Study on Tribological Characteristics of Powder Sintered Fe-base Alloy (SMF9060))

  • 김상윤;김대욱;박영민;신동철;김태규
    • 열처리공학회지
    • /
    • 제27권2호
    • /
    • pp.65-71
    • /
    • 2014
  • SMF9060 material is a Fe-based powder sintered alloy that is used for several automobile components such as Synchronize Hub, oil pump and transmission. These components are required excellent wear resistance and durability. In this study, we have performed a dry wear test at the ambient air and Ar gas conditions in the room temperature, and a lubricant wear test at the room temperature and engine oil temperature of $100^{\circ}C$. The amount of wear volume and coefficient friction are measured by a Profilometer and a Ball on disk type wear tester. The wear volume in Ar gas condition was a little higher than that in the ambient air condition. However the wear volume in the lubricant wear condition was much lower than in the dry wear condition. XRD analysis of the debris in Ar gas condition showed that the oxide film was not formed.

R-22 냉매 분위기하에서 스크롤 압축기 스러스트 베어링의 윤활특성 평가 (Performance Evaluation of Thrust Slide-Bearing of Scroll Compressors under R-22 Environment)

  • 조상원;김홍석;이재근;이형국;이병철;박진성
    • 대한설비공학회:학술대회논문집
    • /
    • 대한설비공학회 2006년도 하계학술발표대회 논문집
    • /
    • pp.590-595
    • /
    • 2006
  • This paper presents the friction and anti-wear characteristics of nano-oil with a mixture of a refrigerant oil and carbon nano-particles in the thrust slide-bearing of scroll compressors. Frictional loss in the thrust slide-bearing occupies a large part of total mechanical loss in scroll compressors. The characteristics of friction and anti-wear using nano-oil are evaluated using the thrust bearing tester for measuring friction surface temperature and the coefficient of friction at the thrust slide-bearing as a function of normal loads up to 4,000 N and orbiting speed up to 3,200 rpm. It is found that the coefficient of friction increases with decreasing orbiting speed and normal force. The friction coefficient of carbon nano-oil is 0.015, while that of pure oil is 0.023 under the conditions of refrigerant gas R-22 at the pressure of 5 bars. It is believed that carbon nano-particles can be coated on the friction surfaces and the interaction of nano-particles between surfaces can be improved the lubrication in the friction surfaces. Carbon nano-oil enhances the characteristics of the anti-wear and friction at the thrust slide-bearing of scroll compressors.

  • PDF

나노 사이즈 탄소입자의 마찰마모 특성에 관한 연구 (A Study on Friction and Wear Characteristics of Nano-size Carbon)

  • 정광우;최정규;문성용;정근우
    • Tribology and Lubricants
    • /
    • 제24권5호
    • /
    • pp.264-268
    • /
    • 2008
  • A large number of additives have been used with the efforts of improving the performance of lubricants used along with the development of internal combustion engine. In this study, nano-sized graphite was used as liquid-lubricant additive. In order to disperse graphite into oil, we esterified the nano-carbon manufactured by our company with various types of alcohol. After measuring the anti-wear in accordance with the types of alcohol and added concentration, it has been found that its anti-wear/friction decrease has been improved in case of adding 0.1% of the sample composed with C12/14 mixed alcohol & hexadecanol.

나노입자를 적용한 냉장고 압축기용 오일의 윤활특성 평가 (Performance Evaluation of Nano-Lubricants at Refrigeration Oil)

  • 이광호;황유진;권래언;이재근;김석로;방선욱
    • 대한설비공학회:학술대회논문집
    • /
    • 대한설비공학회 2008년도 하계학술발표대회 논문집
    • /
    • pp.184-188
    • /
    • 2008
  • It has been recognized that friction coefficient decreased with decreasing viscosity of oil in lubrication. In general, the more viscosity decreases, the more wear rate increases due to decrease load carrying capacity. It has been proposed that nano particles in oil decrease friction coefficient and wear rate. The purpose of this study is to apply oil of lower viscosity that mix with nano particles at the compressor used in a refrigerator to decrease friction coefficient keeping Load carrying capacity. Mineral oil of 8 cSt were used and mixed with nano particle. Friction coefficient was evaluated by a disk-on-disk tester. As a result, friction coefficient of nano oil decreased by 90% in comparison with raw oil. These results lead us to the conclusion that nano oil is new plan to raise efficiency of the compressor.

  • PDF

나노 다이아몬드 입자를 첨가한 엔진 오일의 알루미늄 6061 합금에 대한 마모 특성 (Wear Characteristics of Lubricant with Nano-diamond Particles on Al-6061 Aluminum Alloy)

  • 황성완
    • 한국기계가공학회지
    • /
    • 제20권12호
    • /
    • pp.16-23
    • /
    • 2021
  • Pin-to-disc wear testing experiments were conducted to investigate the wear characteristics of commercial oil (5W-40) with nano-diamond particles. The upper specimen was a SUJ-2 high-carbon chromium steel ball with a diameter of 4 mm, and the lower specimen was made of the Al-6061 alloy. The applied load was 5 N, and the sliding speed was 0.25 m/s. The wear tests were conducted at a sliding distance of 500 m. The friction coefficients and wear rates of the Al-6061 specimens were tested using commercial oil with different nano-diamond concentrations ranging from 0 to 0.02 wt.%. The addition of nano-diamond particles to commercial oil reduced both the wear rate and coefficient of friction of the Al-6061 alloy. The use of nano-diamond particles as a solid additive in oil lubricants was found to improve the tribological behavior of the Al-6061 alloy. For the Al-6061 alloy, the optimal concentration was found to be 0.005 wt.% in view of the friction coefficient and wear rate. Further investigation is needed to determine the optimal concentration of nano-diamond particles for various loadings, sliding speeds, oil temperatures, and sliding distances.

군용 수중 운동물체의 성능강화를 위한 초소수성 나노 패터닝 기술 (Superhydrophobic Nano Patterning Techniques for Enhanced Performance of Naval Underwater Vessels)

  • 홍순국;이기영
    • 한국해양공학회지
    • /
    • 제27권2호
    • /
    • pp.114-120
    • /
    • 2013
  • A superhydrophobic surface means that the contact angle between the solid surface and a water droplet is more than $150^{\circ}$. Materials with a superhydrophobic surface have a self-cleaning function because of the Lotus effect, in which water is not absorbed by the material but rolls off of it. If such a Lotus effect can be applied to the surface of underwater vessels, submarines, torpedos, and so on, enhanced vessels can be made based on this lubricant effect reducing the friction coefficient for the liquid. Because polymer composites can be easily applied in various nanotechniques, they are more advantageous than conventional materials like iron in terms of a superhydrophobic surface. Furthermore, a superhydrophobic surface bring enhanced anticorrosion and ecotechnology because no paint is needed on underwater vessels.

나노다이아몬드가 분산된 엔진오일의 마찰공학 특성 (Tribology Properties of Nanodiamond Dispersed Engine Oil)

  • 전수형;엄영랑;이창규
    • 한국분말재료학회지
    • /
    • 제18권5호
    • /
    • pp.417-422
    • /
    • 2011
  • Hydrophobic nanodiamond (ND) were dispersed in engine oil (Helix Oil, Shell co.) as an additives to improve tribology properties. In this study, nanodiamond prepared by an explosive method was used. Tribology properties of both pure Helix oil and engine oil containing ND additive were evaluated. The rotating disks were made of Gray Cast Iron (240 Hv) and SKD11 (710 Hv). Surface topographies of the disks' wear tracks and friction coefficient were compared. The results show that nanodiamond-dispersed lubricants are capable of reducing these metals' wear loss. The friction coefficient is strongly affected to the hardness of wear track.

Wear behaviors of HVOF spray coating of Co-alloy T800

  • Cho, Tong-Yul;Yoon, Jae-Hong;Kim, Kil-Su;Park, Bong-Kyu;Youn, Suk-Jo;Back, Nam-Ki;Chun, Hui-Gon
    • 한국결정성장학회지
    • /
    • 제16권3호
    • /
    • pp.121-126
    • /
    • 2006
  • HVOF thermal spray coating of Co-alloy T800 is progressively replacing the classical hard coatings such as chrome plating because of the very toxic $Cr^{6+}$ ion known as carcinogen causing lung cancer. For the study of the possibility of replacing of chrome plating, the wear properties of HVOF Co-alloy T800 coatings are investigated using the reciprocating sliding tester both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C)$. The possibility as durability improvement coating is studied for the application to the high speed spindles vulnerable to frictional heat and wear. Wear mechanisms at the reciprocating sliding wear test are studied for the application to the systems similar to the sliding test such as high speed spindles. Wear debris and frictional coefficients of T800 coatings both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C)$ are drastically reduced compared to those of non-coated surface of parent substrate Inconel 718. This study shows that the coating is recommendable for the durability improvement coatings on the surfaces vulnerable to frictional heat. The sliding surfaces are weared by the mixed mechanisms such as oxidative wear, abrasion by the sliding ball slurry erosion by the mixture of solid particles and small drops of the melts and semi-melts of the attrited particles cavitation by the relative motions among the coating, sliding ball, the melts and semi-melts. and corrosive wear. The oxide particles and the melts and semi-melts play roles as solid and liquid lubricant reducing the wear and friction coefficient.

A Study on the Friction and Wear Properties of Tribaloy 800 Coating by HVOF Thermal Spraying

  • Cho, Tong-Yul;Yoon, Jae-Hong;Kim, Kil-Su;Youn, Suk-Jo;Song, Ki-Oh;Back, Nam-Ki;Chun, Hui-Gon;Hwang, Soon-Young
    • 한국표면공학회지
    • /
    • 제39권5호
    • /
    • pp.240-244
    • /
    • 2006
  • Tribaloy 800 (T800) powder is coated on the Inconel 718 substrate by the optimal High Velocity Oxy-Fuel (HVOF) thermal spray coating process developed by this laboratory. For the study of the possibility of replacing of the widely used classical chrome plating, friction, wear properties and sliding wear mechanism of coatings are investigated using reciprocating sliding tester both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C). Both at room temperature and at $538^{\circ}C$, friction coefficients and wear debris of coatings are drastically reduced compared to those of non-coated surface of Inconel 718 substrate. Friction coefficients and wear traces of both coated and non-coated surfaces are drastically reduced at higher temperature of $538^{\circ}C$ compared with those at room temperature. At high temperature, the brittle oxides such as $CoO,\;Co_3O_4,\;MoO_2,\;MoO_3$ are formed rapidly on the sliding surfaces, and the brittle oxide phases are easily attrited by reciprocating slides at high temperature through complicated mixed wear mechanisms. The sliding surfaces are worn by the mixed mechanisms such as oxidative wear, abrasion, slurry erosion. The brittle oxide particles and melts and partial-melts play roles as solid and liquid lubricant reducing friction coefficient and wear. These show that the coating is highly recommendable for the durability improvement coating on the surfaces vulnerable to frictional heat and wear.

Nano-Wear and Friction of Magnetic Recording Hard Disk by Contact Start/Stop Test

  • Kim, Woo Seok;Hwang, Pyung;Kim, Jang-Kyo
    • KSTLE International Journal
    • /
    • 제1권1호
    • /
    • pp.12-20
    • /
    • 2000
  • Nano-wear and friction of carbon overcoated laser-textured and mechanically-textured computer hard disk were characterised after contact start/stop (CSS) wear test. Various analytical and mechanical testing techniques were employed to study the changes in topography, roughness, chemical elements, mechanical properties and friction characteristics of the coating arising from the contact start/stop wear test These techniques include: the atomic force microscopy (AFM), the continuous nano-indentation test, the nano-scratch test, the time-of-flight secondary ion mass spectroscopy (TOF-SIMS) and the auger electron spectroscopy (AES). It was shown that the surface roughness of the laser-textured (LT) bump and mechanically textured (MT) Bone was reduced approximately am and 7nm, respectively, after the CSS wear test. The elastic modulus and hardness values increased after the CSS test, indicating straining hardening of the top coating layer, A critical load was also identified fer adhesion failure between the magnetic layer and the Ni-P layer, The TOF-SIMS analysis also revealed some reduction in the intensity of C and $C_2$$F_59$, confirming the wear of lubricant elements on the coating surface.

  • PDF