Removal Characteristics of Heavy Metal by Na-P1 Zeolite Synthesized from Coal Fly Ash

  • Lee Mingyu;Lee Donghwan;Oh Yunghee;Ahn Byoungjoon
    • Environmental Sciences Bulletin of The Korean Environmental Sciences Society
    • /
    • 제1권2호
    • /
    • pp.167-175
    • /
    • 1997
  • This study was conducted for an efficient utilization of waste fly ash obtained from the power plant. Fly ash was used for synthesizing zeolite. Na-P1 zeolite could be easily synthesized from waste fly ash and showed the potential to remove heavy metal ions. The synthetic zeolite showed good adsorption property for heavy metal much better than raw fly ash and natural zeolites. Na-P1 exhibited the high adsorption efficiency with a maximum value of 260 Pb mg/g and strong affinity for $Pb^{2+}$ ion. The metal ion selectivity of Na-P1 was determined in a decreasing order : $Pb^{2+}>Cd^{2+}>Cu^{2+}>Zn^{2+}>Fe^{3+}$.

  • PDF

계화도 간척지에서 석고, 팽화왕겨 및 제올라이트 처리가 토양 중 양이온 함량에 미치는 영향 (Influence of Gypsum, Popped Rice Hulls and Zeolite on Contents of Ca2+, Mg2+, Na+, K+ in Reclaimed Tideland Soils in Kyehwado)

  • 백승화;이상욱;임효빈;김대근;김성조
    • 한국환경농학회지
    • /
    • 제28권1호
    • /
    • pp.25-31
    • /
    • 2009
  • 본 연구는 간척지 토양 중 세사양토에 대하여 입단형성을 위해 가해진 토양개량제가 토양 중 양이온 함량변화에 미치는 영향을 분석하기 위하여 토양개량제로 이수석고 1550 (G1), 3100 (G2), 6200 (G3) kg/10 a, 팽화왕겨 1000 (H1), 2000 (H2), 3000 (H3) kg/10 a, 팽화왕겨 1500 kg/10 a에 zeolite 200 (HZ1), 400 (HZ2), 800 (HZ3) kg/10 a가 되도록 처리량을 달리하여 3년간 연용하고, 버뮤다그래스를 재배한 토양을 60, 90, 120일 경과 후 채취하여 토양개량제 연용이 토양 중 양이온 함량변화에 미치는 결과를 보고한다. 이수석고의 처리는 토양 중 $K^+$, $Na^+$, $Mg^{++}$의 함량을 현저히 감소시키는 것으로 나타났다. $K^+$ 함량은 토양개량제의 종류 및 처리수준과 관계없이 연용기간이 길어질수록 낮아지는 경향이었다. $K^+$ 함량은 연도별의 경우 2004 > 2005 > 2006 순으로 낮았으나 동일연도에서는 이수석고 < 팽화왕겨 < 팽화왕겨+zeolite 순이었으며, 90 DAT에서 잘 나타나고 있었다. $Na^+$ 함량은 토양개량제 연용에 따른 변화는 없었으나 토양개량제의 종류에 의한 함량에서 차이를 보였다. 2006년 120 DAT 처리구에서 이수석고 및 그 처리량에 따라 $Na^+$ 함량이 현저히 감소하는 현상을 볼 수 있었고, 2006년도 토양 중 $Na^+$ 함량은 이수석고 $\ll$ 팽화왕겨 < 팽화왕겨 +zeolite 순이었다. $Mg^{++}$ 함량은 팽화왕겨+zeolite의 경우 년도별 증가형태가 안정적이었고, 시간이 경과할수록 이수석고 < 팽화왕겨 < 정화왕겨+zeolite 순으로 높아지고 있었다. 이수석고 및 그 처리량에 따라 $Mg^{++}$ 함량은 현저히 감소하는 현상을 볼 수 있었고, 팽화왕겨, 팽화왕겨+zeolite 처리구에서는 대조구에 비해 그리고 연용에 따라 감소되는 정도가 적었다. 동일 조건에서의 토양개량제 처리는 이수석고 < 팽화왕겨 < 팽화왕겨+zeolite 순으로 높아지고 있었다 $Ca^{++}$의 경우 이수석고 연용처리는 처리수준이 높을수록 토양 중 $Ca^{++}$이 높아지는 결과가 되었으며, 년도별 변화도 2004 < 2005 < 2006년의 순으로 연용기간이 늘어남에 따라 높아지는 경향이었다. 팽화왕겨, 팽화왕겨+zeolite 연용처리는 대조구에 비해 함량변화가 적었다. 토성이 세 사양토인 간척지의 양이온 중 $K^+$, $Na^+$, $Mg^{++}$ 함량 감소에 효과적인 토양개량제는 이수석고 이었다.

($NH_4^\;^+-N$ 흡착제(吸着劑)로서의 천연(天然) Zeolite의 이용(利用) (Utilization of Natural Zeolite for $NH_4^\;^+-N$ Adsorbent)

  • 김상수;허남호;최정
    • 한국환경농학회지
    • /
    • 제10권1호
    • /
    • pp.27-31
    • /
    • 1991
  • 국내산 천연(天然) zeolite의 $NH_4^\;+-N$ 제거제(除去劑)로서의 이용가능성(利用可能性)을 검정하기 위해 천연(天然) zeolite에 의한 $NH_4^\;^+-N$의 흡착능(吸着能)을 조사하였다. zeolite의 주구성점토광물(主構成粘土鑛物)은 clinoptilolite와 mordenite였다. Zeolite에 의한 $NH_4\;^+$의 흡착반응은 4시간 후에는 흡착평형(吸着平衡)에 도달하였다. $NH_4\;^+$ 흡착량은 zeolite의 입경(粒徑)에 의해 영향을 크게 받지 않았다. 치환성 양(陽)이온에 따른 $NH_4\;^+$ 흡착량은 Na-> Ca> K-zeolite의 순(順)이었다. 반응용액(反應溶液)의 pH가 높을수록 또 동일량(同一量)의 용액에 대한 시료량이 증가할수록 $NH_4\;^+-N$흡착량은 증가하였다. Zeolite에 의한 $NH_4\;^+$흡착등온곡선은 Langmuir 식(式)에 적용(適用)되었다.

  • PDF

종결정 코팅층이 다공성 ${\alpha}$-알루미나 지지체 표면에 성장되는 NaA 제올라이트 분리층의 미세구조에 미치는 영향 (Effect of Seed Coating Layer on the Microstructure of NaA Zeolite Separation Layer Grown on ${\alpha}$-alumina Support)

  • 김민지;;한문희;조철희
    • 멤브레인
    • /
    • 제24권5호
    • /
    • pp.375-385
    • /
    • 2014
  • 본 연구에서는 종결정 코팅층이 NaA 제올라이트 분리막 형성에 미치는 영향에 대하여 고찰하였다. NaA 제올라이트 분리막은 평균입경 100 nm 종결정을 다공성 ${\alpha}$-알루미나 표면에 진공여과 코팅하고 $100^{\circ}C$에서 24시간 수열처리하여 합성되었다. 이때 지지체 표면에 분포된 종결정 양을 조절한 후 형성된 NaA 제올라이트 분리층의 두께와 결정입 크기 등 미세구조에 미치는 영향에 대하여 고찰하였다. 종결정 코팅 양은 지지체를 통과한 종결정 수용액의 여과 양을 조절하여 제어하였다. 종결정을 단일층으로 코팅한 후 합성하였을 경우, 코팅 양이 증가함에 따라 분리층 단면에서의 두께와 균일도는 증가하였으며, 표면에서의 결정입 크기는 감소하면서 균일도는 증가하였다. 반면, 종결정을 다층으로 코팅한 후 합성하였을 경우, 균일한 분리층을 형성하였지만 단일층으로 코팅된 경우에 비하여 불균일하였으며 두꺼운 분리층이 형성되었다. 균일하고 초박형의 결함이 없는 제올라이트 분리층을 형성하기 위해서는 종결정을 균일하고 단일층으로 코팅하여야 함을 알 수 있었다. 본 연구로부터 종결정의 코팅 상태가 이차성장에 의한 NaA 제올라이트 분리층의 미세구조를 결정하는 중요한 인자임을 확인할 수 있었다.

Pervaporation Separation of Water from Aqueous TFEA Solution by NaY Zeolite Membrane

  • Jeon, Hyun-Soo;Ahn, Hyo-Seong;Lee, Young-Jin;Song, In-Ho;Lee, Hyer-Yeon;Lee, Yong-Taek;Park, In-Jun;Lee, Soo-Bok
    • Korean Membrane Journal
    • /
    • 제8권1호
    • /
    • pp.31-35
    • /
    • 2006
  • Pervaporation of water/2,2,2-trifluoroethanol (TFEA) mixtures was performed using a NaY zeolite membrane which was prepared by a hydrothermal synthesis. Pervaporation with a zeolite membrane is one of the economic separation technologies for liquid mixtures including organic/water solutions. The effects of a TFEA feed concentration and a temperature were studied on the permeation flux and the separation factor. Not only the water flux increased significantly with the increase of the operating temperature, but also the TFEA flux through the NaY zeolite membrane rapidly increased with the increase of the temperature at the feed concentration below 0.8 mole fraction of TFEA.

Synthesis and Permeation Characteristics of Zeolite Membranes

  • Kita, Hidetoshi
    • 한국막학회:학술대회논문집
    • /
    • 한국막학회 1997년도 추계 총회 및 학술발표회
    • /
    • pp.5-8
    • /
    • 1997
  • Introduction : Membranes made from inorganic materials are generally superior to organo-polymeric materials in thermal and mechanical stability, and chemical resistance. Among inorganic materials zeolite is a promising candidate for a high performance membrane because of the unique characteristics of zeolite crystals such as molecular sieving, ion exchange, selective adsorption and catalysis. Although there are many recent reportsl on the preparation of zeolitc membranes and the gas permeation through the membranes, only a limited number of publications deal with pervaporation studies. Recently, we have reported a high pervaporation performance of NaA zeolite membrane for the separation of water/organic liquid mixtures. and of NaY zeolite menlbrane for the separation of methanol/MTBE. Here, preparation of zeolite (LTA, ZSM-5 and FAU) membranes and their permeation properties are discussed.

  • PDF

($NH_3$ 가스 제거를 위한 천연 지오라이트의 이용 (Utilization of Natural Zeolite for Removal of $NH_3$ Gas)

  • 이동훈;최정;박명섭
    • 한국환경농학회지
    • /
    • 제16권4호
    • /
    • pp.327-332
    • /
    • 1997
  • 천연 zeolite를 이용하여 악취성분의 하나인 $NH^3$ gas를 제거하기 위해서 $NH_3$ gas를 zeolite column에 통과시켜 그 제거율을 조사하였다. Zeolite column에서 $NH_3$ gas의 유속이 느릴수록 column 통과농도가 낮게 나타났다. 천연 zeolite에 흡수된 수분함량은 전체적으로 $NH_3$ gas의 흡착에 영향을 주며, 동일량의 천연 zeolite를 column에 나누어 설치하는 방법에 따라서는 통과농도에 거의 영향이 없으나, 첨가량이 많으면 통과농도가 감소하였다. 천연 zeolite에 포화된 치환성양이온은 $NH_3$ gas의 제거율에 영향을 주며, 그 결과는 K->Natural->Na->Ca-zeolite순으로 나타났다. 따라서, $NH_3$ gas의 제거율을 높이기 위해서는 column통과유속, 천연 zeolite의 함수량 및 포화 양이온도 고려되어야 한다.

  • PDF

한국산 천연 제올라이트로부터 제올라이트 NaX로의 전환 (Transformation of Korean Natural Zeolite to Faujasite NaX)

  • 박윤희;하백현
    • 공업화학
    • /
    • 제5권1호
    • /
    • pp.24-29
    • /
    • 1994
  • 모더나이트와 크리노프티로라이트가 혼재되어 있는 한국산 천연 제올라니트(경북 구룡포산)로부터 제올라이트 X를 합성하였다. 원료를 열처리한 결과 크리노프티로라이트는 없어지고 모더나이트만 남았다. 2N-8N의 염산으로 알루미늄을 추출하거나 혹은 열처리한 국산 천연 제올라이트에 NaCl과 $NaAlO_2$ 및 NaOH를 첨가한 혼합용액을 $95^{\circ}C$에서 12~36시간 동안 반응시켜 제올라이트 X를 얻었다. 염산으로 전처리한 시료 25g을 3.5g NaCl, 8g $NaAlO_2$와 6N NaOH 50ml의 혼합용액으로 $95^{\circ}C$에서 24시간 반응시킨 것이 제올라이트 NaX의 최대수율을 나타내었다.

  • PDF

석탄 비산재로 합성한 Na-A형 제올라이트에 의한 구리와 아연 이온의 동역학적 흡착 특성 (Adsorption Kinetics of Cupper and Zinc Ion with Na-A Zeolite Synthesized by Coal Fly Ash)

  • 이창한
    • 한국환경과학회지
    • /
    • 제20권12호
    • /
    • pp.1607-1615
    • /
    • 2011
  • The adsorption performance of cupper and zinc ions($Cu^{2+}$ and $Zn^{2+}$) in aqueous solution was investigated by an adsorption process on reagent grade Na-A zeolite(Z-WK) and Na-A zeolite (Z-C1) prepared from coal fly ash. Z-C1 was synthesized by a fusion method with coal fly ash from a thermal power plant. Batch adsorption experiment with Z-C1 was employed to study the kinetics and equilibrium parameters such as initial metal ions concentration and adsorption time of the solution on the adsorption process. Adsorption rate of metal ions occurred rapidly and adsorption equilibrium reached at less than 120 minutes. The kinetics data of $Cu^{2+}$ and $Zn^{2+}$ ions were well fitted by a pseudo-second-order kinetics model more than a pseudo-first-order kinetics model. The equilibrium data were well fitted by a Langmuir model and this result showed $Cu^{2+}$ and $Zn^{2+}$ adsorption on Z-C1 would be occupied by a monolayer adsorption. The maximum adsorption capacity($q_{max}$) by the Langmuir model was determined as $Cu^{2+}$ 99.8 mg/g and $Zn^{2+}$ 108.3 mg/g, respectively. It appeared that the synthetic zeolite, Z-C1, has potential application as absorbents in metal ion recovery and mining wastewater.

Zeolite X의 양이온에 따른 암모니아 흡착 성능 연구 (Ammonia Adsorption Capacity of Zeolite X with Different Cations)

  • 박준우;서영주;류승형;김신동
    • 공업화학
    • /
    • 제28권3호
    • /
    • pp.355-359
    • /
    • 2017
  • Si/Al 몰비율이 1.08~1.20를 가진 제올라이트 X를 수열합성반응을 이용하여 제조한 후, $Mg^{2+}$ 또는 $Cu^{2+}$을 지닌 금속질산염용액으로 이온교환을 하여 이온 교환된 제올라이트 X를 준비하였다. 모든 준비된 제올라이트 X 시료들에 대해 XRD, SEM, EDS를 이용하여 제올라이트의 결정 구조 변화를 확인하였으며, 암모니아 승온 탈착법($NH_3$-TPD)을 통해 시료의 암모니아 흡착능력에 대한 분석을 진행하였다. XRD 결과, 준비된 제올라이트 X는 양이온성분에 상관없이 Faujasite (FAU) 결정상을 유지하였지만, $Mg^{2+}$$Cu^{2+}$로 이온교환된 제올라이트 X에 대한 결정화도는 감소되었다. EDS분석결과, 이온 교환된 제올라이트 X시료들 안에 각각의 양이온이 분포되어 있는 것을 확인할 수 있었다. $NH_3$-TPD 분석결과 $Mg^{2+}$-와 $Cu^{2+}$-제올라이트 X의 암모니아 흡착능은 각각 1.76 mmol/g과 2.35 mmol/g이었으나, $Na^+$-제올라이트 X의 암모니아 흡착능은 3.52 mmol/g ($NH_3/catalyst$)으로 확인되었다. 향후 암모니아를 제거하기 위한 흡착제로서 $Na^+$-제올라이트 X가 활용될 가능성이 높다고 사료된다.