• 제목/요약/키워드: NR/EPDM blend

검색결과 9건 처리시간 0.016초

Effect of Precured EPDM on the Property of Magneto-rheological Elastomer Based on NR/EPDM Blend

  • Na, Bokgyun;Chung, Kyungho
    • Elastomers and Composites
    • /
    • 제53권2호
    • /
    • pp.67-74
    • /
    • 2018
  • Magneto-rheological elastomers (MREs) are smart materials in which the inherent stiffness and damping properties can be changed by the influence of an external magnetic field. The magneto-rheological (MR) effect depends on the orientation characteristics of the dispersed magneto-responsible particles (MRPs) in the matrix. In this study, natural rubber (NR) and ethylene propylene diene rubber (EPDM) were blended and used as a matrix of an MRE. EPDM was pre-cured before blending with NR. The Mooney viscosity, curing characteristics, and mechanical properties were analyzed with various pre-curing conditions of EPDM and the NR/EPDM blend. The results show that excellent mechanical properties of the NR/EPDM blend-based MRE were obtained when the pre-curing time of EPDM was 60 min. The aging property of the NR-based MRE was improved by the introduction of pre-cured EPDM. Also, the anisotropic MRE showed a higher MR effect than that of the isotropic MRE.

EPDM과 각종(各種) Polymer의 Blend에 의(依)한 성능변화(性能變化) 및 그 응용(應用)에 관(關)한 연구(硏究)(제6보(第6報)) EPDM과 Natural Rubber 및 Butadiene-Styrene Rubber의 Blend에 대(對)하여 (Studies on the Physical Properties and Application of EPDM-Polymer Blends. Part 6. Physical Properties for EPDM-NR-SBR Blends)

  • 김준수
    • Elastomers and Composites
    • /
    • 제7권2호
    • /
    • pp.183-192
    • /
    • 1972
  • As a series of tile studies of EPDM-Polymer blends, tile experiment are concentrated to the investigation of the physical properties of tile EPDM-NR-SBR blends. The results are shown as follows: 1. In blending, tensile strength decreased with increase in EPDM contents, especially the ratio of EPDM/NR-SBR is 75/25. 2. Elongation and tear strength were much influenced by blending, especially the ratio of EPDM/NR-SBR is 50/50. 3. Ozone resistance is much improved after blending. It was effective more than tile ratio of EPDM/NR-SBR is 25/75. 4. Aging resistance is much improved after blending. It was effective more than the ratio of EPDM/NR-SBR is 50/50. 5. Hardness increased with increase in EPDM contents and on the other hand, abrasion resistance decreased.

  • PDF

EPDM/NR 블랜드의 물성에 관한 연구 (The Study on the Properties of EPDM/NR Blends)

  • 고진환;박성수
    • Elastomers and Composites
    • /
    • 제29권2호
    • /
    • pp.121-130
    • /
    • 1994
  • The physical properties of rubber blend between natural rubber(NR) and ethylene propylene diene terpolymer(EPDM) were investigated as a study of EPDM composite materials. For EPDM/NR blends, the effects of ethylene and diene contents in EPDM, blend ratio, dicumyl peroxide(DCP) curing system on the physical properties, interfacial adhesion force and dynamic crack growth etc. were studied. EPDM/NR blends loaded with carbon black were prepared by mechanical mixing and cured by plate heating cure press. Crosslinking density was measured by swelling method with toluene. The physical properties of all blends were measured with Instron, fatigue to failure(FTF), Demattia flex cracking tester(DMFC), scanning electron microscopy (SEM), etc. As the ethylene and diene contents in EPDM increased, the physical properties, such as dynamic crack growth, adhesion to other component were increased too. Interfacial adhesion force of EPDM/NR blends to dissimilar layer was improved by the use of optimum peroxide curing system.

  • PDF

Fatigue Crack Growth Behavior of NR/EPDM Blend

  • Chung, Woo-Won;Chang, Young-Wook
    • Macromolecular Research
    • /
    • 제9권6호
    • /
    • pp.319-326
    • /
    • 2001
  • Fatigue crack growth (FCG) behavior of natural rubber/ethylene-propylene-diene rubber (NR/EPDM) blend vulcanizates under dynamic tearing condition was investigated by using a fracture mechanics approach. It appeared that variation of crack growth rate with blend compositions was dependent on the level of imposed tearing energy G. At low tearing energy region, the FCG rates of the blend were lower as the EPDM content was increased, while at high tearing energy region, the trend was reversed. Over the measured range of tearing energy G, all blend compositions showed the lower crack growth rates compared to the average of properties of component elastomers. When the blends were thermally aged, the fatigue resistance of the blends was deteriorated in proportion to the concentration of EPDM phase. Fatigue crack growth behavior of the blends was supposed to be associated with the inhomogeneities of the crosslink structure of the blends arising from cure incompatibility of the EPDM and NR when they are sulphur cured.

  • PDF

EPDM과 각종(各種) Polymer의 Blend에 의(依)한 성능변화(性能變化) 및 그 응용(應用)에 관(關)한 연구(硏究)(제1보(第1報)) EPDM과 Natural Rubber의 Blend에 대(對)하여 (Studies on the Physical Properties and Application of EPDM-Polymer Blends. Part 1. Physical Properties for EPDM-NR Blends)

  • 김준수
    • Elastomers and Composites
    • /
    • 제6권2호
    • /
    • pp.65-72
    • /
    • 1971
  • The purpose of this study is to establish an effective way to utilize the application of EPDM-Polymer blends. First of all, the physical properties for EPDM/NR blends and compounding agents were studied. The results are shown as follows: 1. In blending, tensile strength and tear strength decreased with increase in EPDM contents. It was not effective more than the ratio of EPDM/NR is 50/50. 2. Elongation is influenced by blending, especially the ratio of EPDM/NR is 50/50. 3. It was found that both the resistance for ozone and aging were much improved after blending.

  • PDF

EPDM과 각종(各種) Polymer의 Blend에 의(依)한 성능변화(性能變化) 및 그 응용(應用)에 관(關)한 연구(硏究) (제2보(第2報)) EPDM과 Butadiene-Styrene Rubber의 Blend에 대(對)하여 (Studies on the Physical Properties and Application of EPDM-Polymer Blends. Part 2. Physical Properties for EPDM-SBR Blends)

  • 김준수
    • Elastomers and Composites
    • /
    • 제6권2호
    • /
    • pp.73-79
    • /
    • 1971
  • As a series of the studies of EPDM-Polymer blends, the experiments are concentrated to the investigation of the physical properties of the EPDM-SBR blends. The results are shown as follows: 1. Tensile strength decreased with increase in EPDM contents and the decreasing value was good results than NR blending. 2. It was found that the aging were much improved after blending and experiments data was good results than NR blending.

  • PDF

불포화 고무와 포화 고무의 공가류 및 내오존성 (Covulcanization and Ozone resistance for Unsaturated and Saturated Rubbers)

  • 임원우;정일택;한민현
    • 접착 및 계면
    • /
    • 제2권4호
    • /
    • pp.32-38
    • /
    • 2001
  • 본 실험에서는 공가류와 내오존성을 동시에 만족하는 고무 조성비의 영향에 대하여 검토하였다. 사용한 시편은 NR, SBR, BR, IIR 및 EPDM을 다양한 비율로 블렌딩 한 고무 조성물(시편 A), NR/BR/SBR로 구성된 불포화 고무 조성물(시편B)와 NR/IIR/EPDM로 구성된 포화 고무 조성물(시편C)이다. 시편A와 시편B, 시편A와 시편C를 각각 공가류시켜 PAD 접착 시편을 제작하여 박리강도를 측정하였다. 또한 시편A에 대해서 내오존성을 평가하였다. 시편 A의 불포화 고무 조성중(NR/BR Blend)에 BR보다 NR의 비율이 높을수록 시편B와 시편C와의 접착 강도가 높았고, 또다른 불포화 고무 조성(NR/SBR)에서는 NR보다 SBR 함량이 높을수록 접착 강도는 높았다. 또한 시편A의 조성중에서 NR/BR/IIR/EPDM 조성물 보다 NR/SBR/IIR/EPDM 조성물이 접착성이 우수하였다. 고무 조성중 불포화 고무가 많을수록 접착 강도는 우수하였으나, 내오존성은 다소 열세였다. 불포화 고무와 포화 고무의 비율이 60/40 정도 일 때 접착 강도와 내오존성이 모두 양호하였다.

  • PDF

Pyrolysis-Gas Chromatography를 이용한 가황 고무의 열분석에 관한 연구(II) (NBR, CR 및 EPDM 가황체) (Studies on analysis of Rubber Vulcanizates by Pyrolysis-Gas Chromatography (II) (NBR, CR, and EPDM Vulcanizates))

  • 허동섭;김종석;김경자;안병국;서수교
    • Elastomers and Composites
    • /
    • 제22권4호
    • /
    • pp.314-323
    • /
    • 1987
  • A blend ratio of rubber vulcanzates comprising NBR, CR, EPDM, NR, BR, and SBR alone or blended is determind through a P.G.C. It is found that a characteristic peak of elastomer is proportional to the content of each elastomer when they are pyrolysed. It is also classified to the different AN content in NBR vulcanizates, identification of sulfur-modified and non-sulfur bearing CR polymers, and the content of ethylene, propylene monomer and the third monomer in EPDM vulcanizetes.

  • PDF

신개발 유두컵 라이너용 고무조성물의 물리적 특성 조사 (Study on the Physical Properties of New Developed Teat Cup Liner Compounds)

  • 이정치
    • 한국임상수의학회지
    • /
    • 제24권2호
    • /
    • pp.201-207
    • /
    • 2007
  • The teat cup liner compounds with improved physical property were developed using tri-polymer blend of natural rubber(NR), ethylene propylene diene monomer rubber(EPDM) and butyl rubber, and the changes of the physical properties of compounds were measured under various conditions such as standard, thermal, alkaline detergent and acid solutions aging conditions. The hardness of the new teat cup liner compound 1 was 50 and that of the compound 2 was 51 under standard condition. The tensile strength and elongation of the new compound 1 were $154kgf/cm^2$ and 675% under the standard condition, respectively. Also, those of the new compound 2 were 180 kgf/cm and 634% under the same condition. Their hardness were increased about $2{\sim}6%$ and the tensile strength and elongation were decreased about 10% under the $25^{\circ}C$ water and detergent solutions. Even though the new teat cup liner compounds exhibited so much decreased tensile properties under the $105^{\circ}C$ thermal aged condition, they sustained more stable aged physical properties including tensile strength and elongation than those of imported teat cup liner materials. Consequently, the new teat cup liner compounds would give prolonged lift cycle if they are used as a teat cup liner product.