Evaluation of Mixed-mode Interlaminar Fracture Toughness of Carbon Fabric/Epoxy Composites for Tilting Train Carbody (틸팅차량용 탄소섬유직물/에폭시 복합재의 혼합모우드 층간파괴인성 평가)

  • Yun, Seong-Ho;Heo, Gwang-Su;O, Jin-O;Lee, Sang-Jin;Jeong, Jong-Cheol;Kim, Jeong-Seok
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2005.11a
    • /
    • pp.256-259
    • /
    • 2005
  • Mixed-mode interlaminar fracture toughness of carbon fabric/epoxy composites, which are applicable to tilting train carbody, was evaluated through the MMB (Mixed-mode bending) test. Specimens were made of CF3327 plain woven fabric with epoxy and a starter delamination at one end was made by inserting Teflon film with the thickness of 12.5 μ m. Mixed-mode interlaminar fracture test was conducted for 6 types of specimens with the mode II ratio of 20 ,35, 50, 65, 80, 90%. Also crack propagating behaviors and fractured surfaces were examined through an optical travelling scope and a scanning electron microscope, respectively.

  • PDF

Mixed Mode Interlaminar Fracture Behaviors of Carbon Fabric/Epoxy Composites (탄소섬유직물/에폭시 복합재의 혼합모우드 층간파괴 거동)

  • Yoon, Sung-Ho;Heo, Kwang-Soo;Oh, Jin-Oh
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.35 no.1
    • /
    • pp.58-65
    • /
    • 2007
  • Mixed mode interlaminar fracture behaviors of carbon fabric/epoxy composites were investigated through MMF (Mixed Mode Flexural) test by varying mixed mode ratio ranging from 20% to 90%. Mixed mode interlaminar fracture criteria based on NL point and 5% offset point were also suggested in order to predict mixed mode interlaminar fracture behaviors. Fracture surfaces and crack propagating behaviors were examined through a travelling scope and a scanning electron microscope. According to the results, mixed mode interlaminar fracture behaviors can be predicted by mixed mode interlaminar fracture criterion with m=1.5 and n=0.5 on the basis of NL point or mixed mode interlaminar fracture criterion with m=2 and n=3 on the basis of 5% offset point. Fracture surfaces and crack propagating behaviors are sensitive to mixed mode ratios. MMF test can be successfully applicable in evaluating mixed mode interlaminar fracture toughness of carbon fabric/epoxy composites.

The Effects of the Initial Crack Length and Fiber Orientation on the Interlaminar Delamination of the CFRP/GFRP Hybrid Laminate (초기 균열길이 및 섬유방향이 CFRP/GFRP 하이브리드 적층재의 층간 파괴에 미치는 영향)

  • Kwon, Oh-Heon;Kwon, Woo-Deok;Kang, Ji-Woong
    • Journal of the Korean Society of Safety
    • /
    • v.28 no.1
    • /
    • pp.12-17
    • /
    • 2013
  • Considering the wind power system and the rotor blades which are composed of much technology, the wind power blade would be the most dangerous part because it revolves at high speed and weighs about dozens of tons, if the accident happens. Therefore, the light weight composite materials have been replacing as substitutional materials. The object of this study is to examine the delamination and damage for CFRP/GFRP hybrid composite that is used for strength improvement of a wind power blade. The influence of the initial crack length and fiber orientation for the interlaminar delamination was exposed for the blade safety. Plain woven CFRP instead of GFRP was inserted into the layer of the box spar for improving the strength and blade life. DCB(Double Cantilever Beam) specimen was used for evaluating fracture toughness and damage evaluation of interlaminar delamination. The material used in the experiment is a commercial material known as CF 3327 EPC in plain woven carbon prepreg(Hankuk Carbon Co.) and UD glass fiber prepreg(Hyundai Fiber Co.). From the results, crack growth rate is not so different according to the variation of the initial crack length. Mode I interlamainar fracture toughness of fiber direction $0^{\circ}$ is higher than that of $45^{\circ}$. Interlaminar fracture has an effect on fiber direction and K decreased with lower value according to increasing initial crack length. Also energy release rate fracture toughness was evaluated because CFRP/GFRP hybrid composite with a different thickness is under the mixed mode loading condition. The interlaminar fracture was almost governed by mode I fracture even though the mixed mode.

Beam-Type Bend Specimen for Interlaminar Fracture Toughness of Laminated Composite under Mixed-Mode Defmrmations (보 형태의 굽힘시편을 이용한 적층복합재료의 혼합모우드 층간파괴인성 평가)

  • 윤성호;홍창선
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.13 no.5
    • /
    • pp.911-920
    • /
    • 1989
  • It this study, beam-type bend specimen is used to evaluate the interlaminar fracture toughness of laminated composite under mixed-mode deformations. The specimen is loaded under three-point bending and hence produced mixed-mode deformations in the vicinity of the crack tip according to the variation of the thickness ratio on delamination plane. Total energy release rate is obtained by elementary beam theory considering the effect of shear deformation. The partitioning of total value into mode-I and mode-II components is also performed. The mixed-mode interlaminar fracture toughness is evaluated by experiments on specimens with several thickness ratios of delamination plane. As the part of delamination plane is thicker, the effect of shear deformation on total energy release rate is increased. Beam-type bend specimen men may be applied to obtain informations on the mixed-mode interlaminar fracture behavior of laminated composites.

A Study on Mixed Mode I/II Interlaminar Fracture Toughness of Carbon Fiber Reinforced Plastic Composites (CFRP 복합재료의 혼합모드 I/II 층간파괴인성치에 관한 연구)

  • Kim, H.J.;Park, M.I.;Kim, J.D.;Koh, S.W.
    • Journal of Power System Engineering
    • /
    • v.4 no.3
    • /
    • pp.48-54
    • /
    • 2000
  • This paper describes the effect of molding pressure, specimen geometries for Mixed Mode I/II interlaminar fracture toughness of carbon fiber reinforced plastic composites by using asymmetrical double cantilever beam(ADCB) specimen. The value of $G_{I/IIC}$ as a function of various molding pressure is almost same at 307, 431, 585 kPa. However it shows the highest value under 307 kPa molding pressure. The effect of $G_{I/IIC}$ due to the change of initial crack length of ADCB specimen was almost negligible in this study. It turns out that the condition for mix mode quasi-static crack growth in ADCB specimen is the ratio of the crack length to that of the specimen, i.e., ${\alpha}/L<0.4$.

  • PDF

A study of mixed-mode interlaminar fracture toughness of graphite/epoxy composite (炭素纖維强化 複合材料의 혼합모우드 層間破壞靭性値에 대한 硏究)

  • 윤성호;홍창선
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.10 no.2
    • /
    • pp.198-207
    • /
    • 1986
  • This study investigates interlaminar fracture characteristics of Graphite/Epoxy composite (HFG Graphite/Epoxy) under mode I (opening mode), mode II (sliding mode) and mixed mode loading conditions. The effects on interlaminar fracture toughness due to different fiber orientations on the crack surface are also investigated. The antisymmetric test fixture proposed by M. Arcan is used for this test. Both critical stress intensity foctors and critical energy release rates were determined and several mixed mode fracture criteria were compared to the experimental data. Also fracture surfaces were investigaed to obtain informations on the fracture behaviors of Graphite/Epoxy composite by means of a scanning electron microscope(SEM).

Prediction of Progressive Interlaminar Fracture in Curved Composite Laminates Under Mode I Loading (모드 I 하중하에서 곡률이 있는 복합재 적층판의 점진적 층간파손 예측)

  • Kang, Seunggu;Shin, Kwangbok;Lee, HyunSoo
    • Proceedings of the Korean Society of Propulsion Engineers Conference
    • /
    • 2017.05a
    • /
    • pp.930-932
    • /
    • 2017
  • In this paper, prediction of progressive interlaminar fracture in curved composite laminates under mode I loading was described. The prediction of progressive interlaminar fracture in curved composite laminates was conducted using cohesive zone model(CZM) in ABAQUS V6.13. Interlaminar fracture toughness used as input parameters in CZM was obtained through mode I, mode II and mixed mode I/II tests. The behaviors of progressive interlaminar fracture for curved composite laminates showed a good agreement between experimental and numerical results.

  • PDF

Effect of Temperature on Interlaminar Fracture Toughness of Filament-Wound Carbon/Epoxy Composites (필라멘트 와인딩된 카본/에폭시 복합재의 층간파괴인성에 미치는 온도 영향)

  • Im, JaeMoon;Shin, KwangBok;Hwang, Taekyung
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.39 no.5
    • /
    • pp.491-497
    • /
    • 2015
  • This paper reports an experimental study for evaluating the effect of temperature on the mode I, mode II and mixed-mode interlaminar fracture toughness of adhesive joints with a curved cross-section of filament-wound dome-separated composite pressure vessel. Mode I and mixed-mode interlaminar fracture toughness were evaluated using DCB specimens, while mode II interlaminar fracture toughness was determined using ENF specimens. $[{\pm}10^{\circ}]_6$, $[{\pm}27^{\circ}]_6$ and ($[{\pm}10^{\circ}]_3/FM73/[{\pm}27^{\circ}]_3$) winding specimens with the curved cross-section were considered. In-situ temperature environments were simulated with a range of $-30^{\circ}C-60^{\circ}C$ using an environmental chamber and furnace. Experimental results on the effect of temperature indicate that interlaminar fracture toughness tends to be high at low temperature and is degraded with increase in temperature. For specimen types, it was found that interlaminar fracture toughness of $[{\pm}10^{\circ}]_3/FM73/[{\pm}27^{\circ}]_3$ winding specimens considered as adhesive joints of dome and helical part was higher than other specimens.

Analysis of a Composite Double Cantilever Beam with Stitched Reinforcements Under Mixed Mode Loading : Formulation (I)

  • Jang Insik;Sankar Bhavani V.
    • Journal of Mechanical Science and Technology
    • /
    • v.19 no.2
    • /
    • pp.567-577
    • /
    • 2005
  • Several methods for improving the interlaminar strength and fracture toughness of composite materials are developed. Through-the-thickness stitching is considered one of the most common ways to prevent delamination. Stitching significantly increases the Mode I fracture toughness and moderately improves the Mode II fracture toughness. An analytical model has been developed for simulating the behavior of stitched double cantilever beam specimen under various loading conditions. For z-directional load and moment about the y-axis the numerical solutions are compared with the exact solutions. The derived formulation shows good accuracy when the relative error of displacement and rotation between numerical and exact solution were calculated. Thus we can use the present model with confidence in analyzing other problems involving stitched beams.

Progressive Failure Analysis of Adhesive Joints of Filament-Wound Composite Pressure Vessel (필라멘트 와인딩 복합재 압력용기의 접착 체결부에 대한 점진적 파손 해석)

  • Kim, Junhwan;Shin, Kwangbok;Hwang, Taekyung
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.38 no.11
    • /
    • pp.1265-1272
    • /
    • 2014
  • This study performed the progressive failure analysis of adhesive joints of a composite pressure vessel with a separated dome by using a cohesive zone model. In order to determine the input parameters of a cohesive element for numerical analysis, the interlaminar fracture toughness values in modes I and II and in the mixed mode for the adhesive joints of the composite pressure vessel were obtained by a material test. All specimens were manufactured by the filament winding method. A mechanical test was performed on adhesively bonded double-lap joints to determine the shear strength of the adhesive joints and verify the reliability of the cohesive zone model for progressive failure analysis. The test results showed that the shear strength of the adhesive joints was 32MPa; the experiment and analysis results had an error of about 4.4%, indicating their relatively good agreement. The progressive failure analysis of a composite pressure vessel with an adhesively bonded dome performed using the cohesive zone model showed that only 5.8% of the total adhesive length was debonded and this debonded length did not affect the structural integrity of the vessel.