  • In according with concrete structural design standard, it is common designing flexure reinforcement concrete to induce tension failure. So reinforcing ratio is limited to inducing tension failure. And maximum reinforcing ratio is regulated to protecting concrete compression strength caused by over reinforced building. Minimum reinforcing ratio is also limited in designing standard to protecting brittle failure as extremely using less reinforcing bar. But in minimum reinforcing ratio it is extremely conservative or it is sometimes impossible to induce stable tension-failure because they are depending on yield failure and experienced method and concrete designing standard strength. Therefore the purpose of the present paper is to evaluate the flexural behavior of minimum steel ratio of reinforced concrete of beams and to propose the guide-line of equation of minimum steel ratio by performing static flexural test of 16 beams according to size effect, number of steel, yielding stress of steel, and concrete compressive strength which are presumed effective variables. From experimental results, the equation of minimum steel ratio was newly proposed considered size effect.

전단경간비와 주인장철근비가 철근콘크리트 보의 최소전단철근비에 미치는 영향 (Effects of Shear Span-to-depth Ratio and Tensile Longitudinal Reinforcement Ratio on Minimum Shear Reinforcement Ratio of RC Beams)

  • 이정윤;김욱연;김상우;이범식
    • 콘크리트학회논문집
    • /
    • 제16권6호
    • /
    • pp.795-803
    • /
    • 2004
  • 현행 구조설계기준식에서는 취성적으로 파괴하는 최소전단보강철근 파괴를 방지하기 위하여 철근콘크리트 보에 최소전단보강철근을 배근하도록 규정하고 있다. 최소전단철근비는 콘크리트의 압축강도와 함께 주인장철근비와 전단경간비에 영향을 받는다. 이 연구에서는 주인장철근비와 전단경간비가 철근콘크리트 보의 최소전단철근비에 미치는 영향을 파악하기 위하여 14개의 철근콘크리트 보를 실험하였다. 실험에 의하면 전단 여유율은 주인장철근비가 증가할수록 증가하였고, 전단경간비가 증가할수록 감소하였다. 실험 결과는 ACI 318-02 기준식과 선행 연구의 제안식과 비교되었다.

동해방지를 위한 초기재령 콘크리트의 최소 양생 시간 예측 (Minimum Curing Time Prediction of Early Age Concrete to Prevent Frost Damage)

  • 배수원;이성태;김진근
    • 콘크리트학회논문집
    • /
    • 제19권1호
    • /
    • pp.27-37
    • /
    • 2007
  • 이 연구의 목적은 초기재령 콘크리트가 동해를 입을 경우가 예상될 때, 동해저항성을 확보하는데 필요한 최소 양생 시간의 예측법을 제안하는 것이다. 먼저, 실험을 통하여 동해시점이 지연될수록, w/c가 낮을수록, 그리고 1종 시멘트보다 3종 시멘트를 사용한 콘크리트가 동해에 의한 압축강도 감소율이 낮으며 동해는 얼음결정의 형성과 성장을 통해 발생됨을 확인하였다. 초기재령 콘크리트가 동해를 입었을 경우, 콘크리트 내에 존재하는 모세공극의 자유수가 얼음으로 상변화를 일으키면서 압축강도의 감소를 유발하므로 동해저항성은 모세공극의 포화도에 따라 결정된다. 따라서, 모세공극의 임계포화도 개념을 근거로 초기동해의 방지를 위한 최소양생시간의 예측법을 제안하였다.

슬래브가 있는 넓은 보-기둥 접합부의 전단거동 (Shear Behavior of Wide Beam-Column Joints with Slab)

  • 안종문;최종인;신성우;이범식;박성식;양지수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.157-162
    • /
    • 2003
  • An experimental investigation was conducted to study the behavior of high-strength RC wide beam-column joints with slab subjected to reversed cyclic loads under constant axial load. Six half scale interior wide beam-column assemblies representing a portion of a frame subjected to simulated seismic loading were tested, including three specimens without slab and three specimens with slab. The primary variables were compressive strength of concrete($f_ck$=285, 460kgf/$cm^2$), the ratio of the column-to-beam flexural capacity($M_r$=$\Sigma M_c / \Sigma M_b$ ; 0.77 -2.26), extended length of the column concrete($l_d$ ; 0, 12.5, 30cm), ratio of the column-to-beam width(b/H ; 1.54, 1.67). Test results are shown that (1) the behavior of specimen using high-strength concrete satisfied for required minimum ductile capacity according to increase the compressive strength, (2) the current design code and practice for interior joints(type 2) are apply to the wide beam-high strength concrete column.

  • PDF

RC 보의 강도증진에 따른 최소전단철근 규준의 적합성 평가에 관한 연구 (Assessment of Code Requirments on Minimum Shear Reinforcement in High-Strength RC Beams)

  • 윤영수;원종필;장일영
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1996년도 봄 학술발표회 논문집
    • /
    • pp.289-294
    • /
    • 1996
  • This paper persents the assessment of the minimum shear reinforcement requirements in normal, medium and high-strength reinforced concrete beams. Twelve shear tests were conducted on full-scale beam specimens having design concrete compressive strengths of 35, 70 and 100 MPa. Different amounts of minimum shear reinfrocement were investigated, including the amounts required by Korean Concrete Standard (KCI88), JCI86, ACI89 (revised 1992) and CSA94 standard. The performance of the different amounts of shear reinforcement are discussed in terms of the shear capacity, the ductility and the crack control at service load levels. An assessment of code provisions for minimum shear reinforcememt, and the prediction and comparison of the ultimate shear capacity are also presented.

  • PDF

Mechanical and durability properties of marine concrete using fly ash and silpozz

  • Jena, T.;Panda, K.C.
    • Advances in concrete construction
    • /
    • 제6권1호
    • /
    • pp.47-68
    • /
    • 2018
  • This article reports the utilization of fly ash (FA) waste product from industry and silpozz which is an agro-waste from agriculture as an environmental friendly material in construction industry. The evaluation of strength and durability study was observed using FA and silpozz as a partial replacement of Ordinary Portland Cement (OPC). The studied parameters are compressive strength, flexural strength, split tensile strength and bond strength as well as the durability study involves the acid soluble chloride (ASC), water soluble chloride (WSC), water absorption and sorptivity. Scanning electron microscopy (SEM) and XRD of selected samples are also done. It reveals from the test results that the deterioration factor (DF) in compressive strength is 4% at 365 days. The DF of split tensile strength and flexural strength is 0.96% and 0.6% at 90 days respectively. The minimum slip is 1mm and 1.1mm after 28 days of testing bond strength for NWC and SWC sample respectively. The percentage decrease in bond strength is 10.35% for 28 days SWC samples. The pre-cast blended concrete samples performed better to chloride diffusion. Modulus of elasticity of SWC samples are also studied.The water absorption and sorptivity tests are conducted after 28 days of curing.

전단보강이 된 철근콘크리트보의 전단강도에 관한 실험적 연구 (An Experimental Study on the Shear Strength of R.C Beam with Web reinforcement)

  • 이근광;홍기섭;신영수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1993년도 가을 학술발표회 논문집
    • /
    • pp.184-189
    • /
    • 1993
  • This is an experimental investigation the shear behavior of reinforced concrete with stirrup of which stress ranges 0.0㎏/㎠ to 7.0㎏/㎠. Five rectangular beams which concrete strengths are 287㎏/㎠ and 380㎏/㎠, a/d=3, and main steel ratio equal to 1.96% was tested. Those were designed to fail in shear. The shear cracking load and failure load were measured and compared with ACI's equation and Zutty's proposed equation. The results are following : ACI equation and Zutty's equation are consertive. As the concrete compressive strength increased, reserved shear strength of beams with minimum web reinforcement decreases. According to increase of web reinforcement , the rate of increases of shear strength is decreased. The failure modes of specimen with minimum web reinforcement are shear compression failure which is reached after diagonal shear cracking.

  • PDF

탄소섬유시트의 전단부착강도에 관한 연구 (Adhesive Shear Strength of Carbon Fiber Sheet)

  • 김윤철
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제12권1호
    • /
    • pp.109-116
    • /
    • 2008
  • 탄소섬유시트의 부착성능을 조사하는 방법으로써 중앙을 절단한 보 공시체를 이용한 휨 거동 형식의 시험기를 개발하여, 콘크리트의 압축강도를 변수로 정적 재하 실험을 실시하였다. 탄소섬유시트의 파단의 결과를 이용하여 이 시험기의 검증과 함께 전단부착강도의 산출식을 도출하려고 노력 하였다. 그 결과, 첫 번째로 새로운 형식의 시험기에 의한 부착강도시험의 타당성이 증명되었다. 두 번째는 CFS 표면 변형률의 결과로부터 구해진 전단부착강도는 2종류의 경향이 있음이 발견되었다. 그 데이터 중에서 비교적 안정성이 높은 전단부착강도의 평균치는 3.41MPa, 하한치는 2.11MPa이었다. 이번 실험에서는 콘크리트의 강도가 전단부착강도에 미치는 특별한 영향을 볼 수 없었다.

MMA 모르터 복합체의 강도특성 및 부재설계 (I) (Member design and strength characteristics of the MMA mortar composites (I))

  • 지효선
    • 복합신소재구조학회 논문집
    • /
    • 제6권3호
    • /
    • pp.41-49
    • /
    • 2015
  • The repair of manhole raise has been caused much construction times and disruption of traffic flow, serious environmental pollution from crushed construction wastes, and budget waste due to the repeated repair construction works. In order to overcome such problems, we have developed the new manhole repairing composite structures by using a glass fiber-reinforced polymer (GFRP) pipe, which can raise manhole to the regular height of the overlayed road pavement with rapid construction and minimum traffic jams. This environmental-friendly technology is method completed by the methyl methacrylate monomer (MMA) double wide flanged GFRP pipe composite structures in order to raise manhole to the regular height. In this paper, two kinds of the compressive strength tests of MMA mortar composites were conducted and evaluated by a general compressive strength test, and compressive strength test after freezing-thawing resistance test. It was found that this MMA mortar composites will be used for the application of the double wide flanged GFRP pipe composite structures.

Correlation study on microstructure and mechanical properties of rice husk ash-Sodium aluminate geopolymer pastes

  • Singh, N. Shyamananda;Thokchom, Suresh;Debbarma, Rama
    • Advances in concrete construction
    • /
    • 제11권1호
    • /
    • pp.73-80
    • /
    • 2021
  • Rice Husk Ash (RHA) geopolymer paste activated by sodium aluminate were characterized by X-ray diffractogram (XRD), scanning electron microscope (SEM), energy dispersion X-Ray analysis (EDAX)and fourier transform infrared spectroscopy (FTIR). Five series of RHA geopolymer specimens were prepared by varying the Si/Al ratio as 1.5, 2.0, 2.5, 3.0 and 3.5. The paper focuses on the correlation of microstructure with hardened state parameters like bulk density, apparent porosity, sorptivity, water absorption and compressive strength. XRD analysis peaks indicates quartz, cristobalite and gibbsite for raw RHA and new peaks corresponding to Zeolite A in geopolymer specimens. In general, SEM micrographs show interconnected pores and loosely packed geopolymer matrix except for specimens made with Si/Al of 2.0 which exhibited comparatively better matrix. Incorporation of Al from sodium aluminate were confirmed with the stretching and bending vibration of Si-O-Si and O-Si-O observations from the FTIR analysis of geopolymer specimen. The dense microstructure of SA2.0 correlate into better performance in terms of 28 days maximum compressive strength of 16.96 MPa and minimum for porosity, absorption and sorptivity among the specimens. However, due to the higher water demand to make the paste workable, the value of porosity, absorption and sorptivity were reportedly higher as compared with other geopolymer systems. Correlation regression equations were proposed to validate the interrelation between physical parameters and mechanical strength. RHA geopolymer shows comparatively lower compressive strength as compared to Fly ash geopolymer.