PROPERTIES OF PLASMA SPRAYED COATINGS

  • Ding, C.X.;Zhang, Y.F.;Xia, J.Y.
    • 한국진공학회지
    • /
    • 제4권S2호
    • /
    • pp.58-63
    • /
    • 1995
  • Plasma spray has attracted attention as an effective method for obtaining protective coatings. In this paper, the physical, mechanical and thermal properties of coatings are reviewed. The microstructural features of the coatings are described. The relationship between the properties of coatings and their microstructure is also discussed. Plasma sprayed coatings are used to reduce wear and improve thermal protection on a large number of components in various industries. In some cases, the conditions of application are very aggressive and therefore the resulting maintenance costs are expensive. Improved coating materials and appropriate properties of coatings are the most promising ways to solve these problems[1,2]. The optimum coating properties depend on the microstructure of coatings[1-5]. In this paper, some ceramic coatings frequently used in industries were reported. The physical, mechanical and thermal properties of ceramic coatings are reviewed. The microstructure features of coatings are addressed. The relationship between the microstructure of coatings and their properties are discussed.

  • PDF

알루미늄소재의 만용융성형 공정에서 구상화의 크기가 기계적 성질에 미치는 영향 (The Effect of Globule size on the Mechanical Properties in Semi-Solid Forming of Aluminium Alloys)

  • 박상문;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.21-24
    • /
    • 2002
  • One of the factors influences on microstructure of semi-solid product is forging pressure. Generally, the more forging pressure makes the more fine microstructure in semi-solid compression test. The microstructure and mechanical properties were investigated according to the forging pressure. The applied pressure is 110MPa, 140MPa and 170MPa, respectively. Heat treatment conditions also influence to the microstructure and mechanical properties of semi-solid product. T6 heat treatment was performed and the evaluation of microstructure and mechanical properties was investigated according to the aging time in T6 heat treatment.

  • PDF

저변형률속도에서 ARB가공된 무산소동의 미세조직 및 기계적 성질 (Microstructure and Mechanical Properties of Oxygen Free Copper Processed by ARB at Low Strain Rate)

  • 이성희;한승전;임차용
    • 한국재료학회지
    • /
    • 제17권10호
    • /
    • pp.521-525
    • /
    • 2007
  • The microstructure and mechanical properties of an oxygen free copper processed by accumulative roll bonding(ARB) at low strain rate were studied. The copper sheets were highly strained up to an equivalent strain of ${\sim}6.4$ by ARB process at ambient temperature. The strain rate of the copper during the ARB was $2.6sec^{-1}$. The microstructure and mechanical properties of the ARB-processed copper were compared to those of the specimens processed by ARB at relatively high strain rate ($37sec^{-1}$). The microstructure and mechanical properties of the copper with ARB process was very similar to each other despite of some differences in recovery.

Microstructure and Magnetic Properties of Nanocomposite Sm2Fe15Ga2Cx/α-Fe Permanent Magnets

  • Cheng, Zhao-hua
    • Journal of Magnetics
    • /
    • 제8권1호
    • /
    • pp.18-23
    • /
    • 2003
  • In our previous work, microstructure and magnetic properties of two-phase exchange-coupled $Sm_2Fe_{15}Ga_2C_{x}$/$\alpha$-Fe nanocomposites have been investigated by means of x-ray diffraction, transmission electron microscopy and magnetization measurement. It was found the exchange coupling between the magnetically hard phase $Sm_2Fe_{15}Ga_2C_{x}$ and the magnetically soft one ${\alpha}$-Fe results in an enhancement of the remanence. The sizes of crystallites of both phases are, however much larger than the Block domain-wall width of the magnetically hard phase. This microstructure gives rise to a concave demagnetization curve and consequently reduces the maximum energy Product. In order to improve their magnetic properties, a few Percent of Zr, which may be effective to refine the microstructure through rapid quenching, was introduced into the nanocomposites. The addition of Zr was found to improve the magnetic properties significantly, Under optimum heat-treatment conditions, the remanence, coercivity and maximum energy Product increase from 0.65 T, 0.48 T and 50 kJ/$m^{3}$ for the Zr-free sample to 0.72 T, 0.77 T and 71.6 kJ/$m^{3}$ for the 1 at.% Zr-containing one, respectively, The improvements of magnetic properties are due to the refinement of microstructure by the addition of Zr.

Si가 Ti-Si-N 코팅막의 기계적 성밀 및 내산화특성에 미치는 영향 (Effect of Si on Mechanical and Anti-oxidation Properties of Ti-Si-N Coating)

  • 박범희;김정애;이종영;김광호
    • 한국세라믹학회지
    • /
    • 제37권1호
    • /
    • pp.96-101
    • /
    • 2000
  • Comparative studies on microstructure, and mechanical and anti-oxidation properties between TiN and Ti-Si-N films were performed. The Ti-Si-N films were deposited on high-speed steel and silicon wafer substrates by plasma-assisted chemcial vapor deposition(PACVD) technique. The Si addition to TiN film caused to change the microstructure such as grain size refinement, randomly multi-oriented microstructure, and nano-sized codeposition of silicon nitride in the TiN matrix. The Ti-Si-N film, contains Si content of ∼7 at.%, showed the micro-hardness value of ∼3400 HK, which was higher than the pure TiN film whose hardness was ∼1500HK. The Ti-Si(7 at.%)-N film also showed much improved anti-oxidation properties compared with those of the pure TiN film. These properties were also related to the microstructure of Ti-Si(7 at.%)-N film was formed and retarded further oxidation of the nitridelayer. These properties were also related to the microstructure of Ti-Si(7 at.%)-N film which was characterized by nano-sized precipitates of silicon nitride phase in the TiN matrix and randomly oriented grains.

  • PDF

$Cr_{2}O_{3}$이 첨가된 PNN-PZT 압전세라믹스에서의 미세구조 및 특성 (Microstructure and Properties of $Cr_{2}O_{3}$additive ternary PZT Ceramics)

  • 박정호;김철수;김성곤;이상렬
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.972-975
    • /
    • 2001
  • The effect of Cr$_2$O$_3$(0 to 0.5 wt%) doping on the microstructure and electrical properties of ternary Pb(Zr,Ti)O$_3$-Pb(Ni,Nb)O$_3$piezoelectric ceramic has been investigated. Abnormal grain growth (grain size 3.3 to 11.2 $\mu$m) and densification are found. Minor additives of $\leq$0.1 wt% improve the mechanical coupling factor, but with more additives of $\geq$0.2 wt% electrical properties deteriorate. Thus, these phenomna can be ascribed mainly to anomalous developed microstructure. The large grains were composed of a core region that is free of Cr and a surrounding shell region rich in Cr. The interfaces between the core and the shell were composed of misfit dislocations. The mechanical properties of the specimens were strongly influenced by this microstructural change. The microstrutural and compositonal evolution of the specimens containing different amounts of Cr$_2$O$_3$were monitored. Electrical properties were measured and related to the variations in the microstructure.

  • PDF

티타늄 합금(Ti-6Al-4V)의 조직변화에 따른 기계적 특성 평가 (The Evaluation of Mechanical properties on the Changes of Microstructure for Titanium Alloy (Ti-6Al-4V))

  • 권재도;배용탁;최성종
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.135-140
    • /
    • 2000
  • The characteristics of mechanical behavior were estimated for Ti-6Al-4V alloy with four kinds of microstructure prepared with heat treatments. For this study, impact test, tensile test and fatigue crack growth test were performed, and then compared mechanical properties on the four microstructures. Furthermore, for quantitative evaluation, fractal dimensions of crack pass were obtained using the box counting method. The main results obtained are summarized as follows. (1) The microstructures exhibited equiaxed microstructure, bimodal-microstructure and lamellar microstructure by heat treatment. (2) The impact absorbed energy and elongation is superior in the bimodal-microstructure, and the hardness and tensile strength are superior in the lamellar microstructure. (3) The fatigue crack growth rate is similar to all microstructures in the low ${\Delta}K$ region. The fatigue crack growth rate of equiaxed microstructure is fastest, and that of lamellar microstructure is lowest in the high ${\Delta}K$ region. (4) The fractal dimension D of lamellar microstructure is higher then that of the equiaxed microstructure and bimodal microstructure.

  • PDF

EFFECT OF MICROSTRUCTURE ON MECHANICAL PROPERTIES IN FRICTION STIR WELDED CAST A356 ALUMINUM ALLOY

  • Sato, Yutaka S.;Kaneko, Takayasu;Urata, Mitsunori;Kokawa, Hiroyuki
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.493-498
    • /
    • 2002
  • Friction stir welding (FSW) is a relatively new solid-state joining process which can homogenize the heterogeneous microstructure by intensely plastic deformation arising from the rotation of the welding tool. The present study applied the FSW to an A356 aluminum (AI) alloy with the as-cast heterogeneous microstructure in the T6 temper condition, and examined an effect of microstructure on mechanical properties in the weld. The base material consisted of Al matrix with a high density of strengthening precipitates, large eutectic silicon and a lot of porosities. The FSW led to fragment of the eutectic silicon, extinction of the porosities and dissolution of the strengthening precipitates in the Al alloy. The dissolution of strengthening precipitates reduced the hardness of the weld around the weld center and the transverse ultimate tensile strength of the weld. Longitudinal tensile specimen containing only the stir zone showed the roughly same strength as the base material and a much larger elongation. Moreover, Charpy impact tests indicated that the stir zone had remarkably the higher absorbed energy than the base material. The higher mechanical properties of the stir zone were attributed to a homogenization of the as-cast heterogeneous microstructure by FSW.

  • PDF

성형미세구조가 질화알루미늄의 소결 및 물성에 미치는 영향 (Effect of Green Microstructure on the Sintering and Properties of Aluminum Nitride)

  • 이해원;전형우;송휴섭
    • 한국세라믹학회지
    • /
    • 제32권2호
    • /
    • pp.209-216
    • /
    • 1995
  • In order to investigate the effect o green microstructure on the sintering behavior and properties of AlN ceramics, samples were prepared by slip casting and dry pressing. The slip cast samples had high green density, fine pore size and narrow pore size distribution. They showed much higher sinterability and more homogeneous sintered microstructure compared to the dry pressed samples. Both increased thermal conductivity and flexural strength for samples prepared by slip casting could be attributed to the improved microstructural homogeneity with isolated second phase(s).