Fabrication and Optical Characterization of Glass-ceramics for IR Reflector (적외선 반사체용 결정화유리 제조 및 광학적 특성평가)

  • 박규한;신동욱;변우봉
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.12
    • /
    • pp.1137-1143
    • /
    • 2001
  • In this study, glass-ceramics containing cordierite(2MgO$.$2Al$_2$O$_3$5SiO$_2$) as a major crystalline phase was prepared from MAS (MgO-Al$_2$O$_3$-SiO$_2$) glass system for the application to reflector. Glasses prepared with addition of TiO$_2$as a nucleating agent were crystallized by two-step heat treatment of nucleation and crystal growth. Then nucleation and crystal growth behavior were investigated and the influence of heat treatment schedule on the nature of crystal phases and the diffuse reflectance spectrum was investigated. As a result, cordierite and rutile were precipitated as a major crystalline phases for the glass-ceramics with the nucleation at 750$^{\circ}C$ for 3 hours and then crystallization at 1100$^{\circ}C$ for 5 hours, and this glass-ceramics showed the reflectance over 90% in 570∼2500nm specturm region.

  • PDF

Wear Mechanism of MgO-C Refractory with Thermite Reaction Products of MgO and Al (MgO와 Al의 테르밋 반응생성물이 첨가된 MgO-C계 내화재료의 용손 기구)

  • 최태현;전병세
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.7
    • /
    • pp.832-838
    • /
    • 1996
  • Thermite reaction products of MgO and Al were added to MgO-C refractory to improve the properties of corrosion against the attack of slag, oxidation and mechanical spalling. Corrosion rate of MgO-C-MgAl2O4 spinel refractory at the ratio of 3.3(CaO/SiO2) slag was smaller than that of MgO-C and MgO-C-Al refractory. The excellent corrosion resistance of the MgO-C-MgAl2O4 spinel refractory against the slag attack was appeared by Al and MgAl2O4 spinel with high melting point and corrosion resistance and the high thermal conductivity and low thermal expansion of AIN. Hot M.O.R at 140$0^{\circ}C$ and the resistance of oxidation weight loss at 90$0^{\circ}C$ were 210kg/cm2 and -12% respectively.

  • PDF

A Study on Tungsten Paste for Metallization and Cofiring of an Alumina Green Sheet (Alumina Green Sheet의 동시소성용 텅스텐 페이스트 제조 및 금속 접합에 관한 연구)

  • 박경리
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.3 no.2
    • /
    • pp.39-50
    • /
    • 1996
  • 본 연구에선 주어진 조성의 알루미나 green sheet에 대하여 텅스텐의 입경 및 산화 물의 조성을 변화시키므로써 수축률을 제어하여 camber를최소화하여 결합강도를 최대로 하 는 텅스텐 페스트조성을 찾아내는 것을 목적으로 하였다. 본 실험에서 사용한 텅스텐 분말 의 입경은 0.35$\mu$m, 0.6$\mu$m, 0.72$\mu$m, $1.5\mu$m, 1.9$\mu$m, 3.2$\mu$m이며 frit는 Al2O3, MgO, SiO2 와 Al2O3, CaO, SiO2를 사용하여 각각의 조성에 따라 함량을 변화시키며 실험하였다. 소성 은 154$0^{\circ}C$로 습윤 수소분위기에서 시행하였으며 사용된 알루미나 green sheet의 알루미나 중심 입경은 2.8$\mu$m이었다. 분석은 주사전자 현미경으로 미세구조를 관찰하였고 EPMA Line Profile로 원소 분석을 하였으며 잔류응력을 측정하기 위하여 XRD분석을 하였다. Frit 을 함유하지 않은 경우 텅스텐 분말의 입경이 1.9$\mu$mdlfEo 최대 접합 강도를 나타내었다. Frit을 함유한 경우 Mgo계 frit조성에서는 MgO/Al2O3/SiO3=1/1/1일 때 CaO계 frot 조성에 서는 CaO/Al2O3/SiO2=1/2/1일 때 최대 접합 강도를 나타내었다. Frit 함량을 변화시킨 경우 MgO계는 10wt%함유하였을 때 CaO 계는 5wt%함유하였을 때 최대 접합강도를 나타내었 다. Frit 함량을 변화시킨 경우 MgO계는 10wt%함유하였을 때, CaOr계는 5wt%함유하였을 때 최대 접합강도를 나타내었다.

Preparation and Characterization of Glass-ceramics in MgO-${Al_2}{O_3}$-$SiO_2$ Glass (MgO-${Al_2}{O_3}$-$SiO_2$계 결정화유리의 제조 및 물성평가)

  • 손성범;최세영
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.6
    • /
    • pp.604-611
    • /
    • 2000
  • Glass-ceramics containing a cordierite (2MgO-2Al2O3-5SiO2) as a main crystal phase was prepared from MgO-Al2O3-SiO2 system glass through a controlled 2-step heat treatment for the application to magnetic memory disk substrate for higher storage capacity. Parent glasses prepared with addition of CeO2 as a fulx and TiO2 as a nucleating agent were crystallized by a 2-step heat treatment i.e. nucleation and crystal grwoth. Then the maximum nucleation and crystal growth rates were investigated and several properties such as bending strength, surface hardness and surface roughness were also studied for heat treated glass. As a result, only a $\alpha$-cordierite was precipitated as a main crystal phase for all heat treatment conditions and the maximum nucleation and crystal growth rates were 2.4$\times$109/㎣.hr at 80$0^{\circ}C$ and 0.3${\mu}{\textrm}{m}$/hr at 915$^{\circ}C$ respectively. After being nucleated at 80$0^{\circ}C$ for 5 hours and then crystallized at 915$^{\circ}C$ for 1 hour, the heat treated glass had a crystal volume fraction of 17.6% and crystal size fo 0.3${\mu}{\textrm}{m}$, and showed the optimum properties for the application to magnetic memory disk substrates as follows. ; Bending strength of 192 MPa, Vidkers hardness of 642.1kgf/$\textrm{mm}^2$, and surface roughness of 27$\AA$.

  • PDF

Geochemical Dispersion and Enrichment of Fluvial Sediments Depending on the Particla Size Distribution (입도분포에 따른 하상퇴적물의 지구화학적 분산 및 부화)

  • 이현구
    • Economic and Environmental Geology
    • /
    • v.32 no.3
    • /
    • pp.247-260
    • /
    • 1999
  • Geochermical characteristics of the fluvial sediments deprnding on particle size distribution size were investigated in the respect of majir, minor and rare eath element chemisitry. Ratios of $Al_{2}O_{3}/Na_{2}O$ and $K_{2}O/Na_{2}O$ of the sediments show the homogeneous valus, and partly positive correlation with $SiO_{2}/Al_{2}O_{3}$, respecively. Characteristics of minor element ratios (V/Ni, Cr/V, Ni/Co and Zr/Hf)are within the lower and narrow range. Thesesuggested that sediment sources may be acidic to intermediate granitic rock, and may be explained by simple weathering and sedimentation. With increasing SiO2 contents, concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, CaO and MgO decreased, but those of $K_{2}O$ and $Na_{2}O$ increased, Concentrations of Ba, Be, Cs, Cu, Li, Ni, Sr, V and Zr show comparatively normal negative and some positive trends. Compared with the mean composition of granite, concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, MnO, CaO and MgO in the sediments of the study area were highly enriced. Among some minor and rare earth elements, concentrations of As, Cd, Cu, and V were enriched, but those of Be, Ce, Rb, Sc, Sr and Zn were depleted when compared with average composition of granite. By decreasing of particle size fractions, SiO2, Rb and Sr conterts decreased, but concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, CaO, MgO, $TiO_{2}$, MgO, $P_{2}O_{5}$, Be, Cu, Hf, Pb, V and Zr increased. From the correlations between particle size fractions and element concenreations, some elements of $Fe_{2}O_{3}$, CaO, MgO, $P_{2}O_{5}$, Cu, Ni, Zn and Zr showed typical trends in the secondary contramination sediments. These trends are typically shown under 100 mesh fractions. It indicates that the fraction of minus 100 mesh is the optimum size fraction for geochemical and environmental survey.

  • PDF

The Oxide Coating Effects on the Magnetic Properties of Amorphous Alloys

  • 배영제;Jang, Ho G.;Chae, Hee K.
    • Bulletin of the Korean Chemical Society
    • /
    • v.17 no.7
    • /
    • pp.621-625
    • /
    • 1996
  • A variety of metal oxides were coated by sol-gel process from their metal alkoxides on the ribbons of Co-based and Fe-based amorphous alloys, and the effects of surface oxide coating on the magnetic properties of the alloy are investigated. The core loss is found to be reduced significantly by the oxide coating, the loss reduction becoming more prominent at higher frequencies. The shape of the hystersis loop is also dependent upon the kind of the coated metal oxide. The coatings of MgO, SiO2, MgO·SiO2 and MgO·Al2O3 induce tensile stress into the Fe-based ribbon whereas those of BaO, Al2O3, CaO·Al2O3, SrO·Al2O3 and BaO·Al2O3 induce compressive stress. These results may be explained by the modification of domain structures via magnetoelastic interactions with the shrinkage stress induced by the sol-gel coating.

Surface Reaction Products of CP- Ti and Ti-25wt%Pd Castings Used for Dental Application (치과용 티타늄 및 Ti-25wt%Pd 주조체의 표면반응생성물)

  • 정준영;문수;이진형
    • Journal of Biomedical Engineering Research
    • /
    • v.25 no.5
    • /
    • pp.383-389
    • /
    • 2004
  • A commercially pure Ti(CP-Ti) and Ti-25wt%Pd alloy for dental applications were cast into a phosphate-bonded Al$_2$ $O_3$/ $SiO_2$ investment mold and the surface of the casting specimens were investigated by means of SEM/EDS, XRD and XPS. The addition of 25wt%Pd in CP-Ti showed a moderate mold reaction owing to the considerable lowering of melting point. XRD analysis of the investment after burn-out treatment revealed that it consisted essentially of $SiO_2$, Al$_2$ $O_3$, P$_2$O$\_$5/, Mg$_3$(P $O_4$)$_2$, AlP $O_4$, Mg$_2$ $SiO_4$, MgAl$_2$ $O_4$ The mold reaction products were Ti$\_$5/Si$_3$ and Ti $O_2$ in case of CP-Ti casting and Ti $O_2$ and SiO$\_$x/ in case of Ti-25wt% Pd casting.

High Temperature Corrosion Characteristics of Al-Si-Mg Alloy in O2 and H2S/H2 Environments (Al-Si-Mg 합금의 산소 및 황화수소 환경에서의 고온부식 특성)

  • Lee, Yeong-Hwan;Son, Young-Jin;Lee, Byung-Woo
    • Journal of Power System Engineering
    • /
    • v.21 no.2
    • /
    • pp.14-19
    • /
    • 2017
  • The corrosion characteristics of Al-Si-Mg alloy were investigated in $O_2$ and $H_2S/H_2$ environments at high temperature. The weight gain and the reaction rate constant of the Al-Si-Mg alloy were measured in the oxygen and hydrogen sulfide environments at 773K. The weight gain of Al-Si-Mg alloy was showed parabolic increase in the oxygen and hydrogen sulfide environments. The reaction rate constants were confirmed to be $1.45{\times}10^{-4}mg^2cm^{-4}sec^{-2}$ in the oxygen environment and $6.19{\times}10^{-4}mg^2cm^{-4}sec^{-2}$ in the hydrogen sulfide environment respectively. As a result of XPS analysis on the specimen surface, $Al_2O_3$ and MgO compounds were detected in oxygen environment and $Al_2(SO_4)_3$ sulfate was detected in the hydrogen sulfide environment. Corrosion rate of Al-Si-Mg alloy was about 4.3 times faster in hydrogen sulfide environment than oxygen environment.

A Study on the Transparent Glass-Ceramics on the MgO-$Al_2O_3$-$SiO_2$ System (투명 결정화유리에 관한 연구 MgO-$Al_2O_3$-$SiO_2$계에 대하여)

  • 박용완;김형준
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.5
    • /
    • pp.406-414
    • /
    • 1991
  • The composition of base glass was selected as MgO 8, Al2O3 24, SiO2 68 in weight percent. TiO2 and ZrO2 were added to the base glass to investigate their effects as nucleating agents. In the case of ZrO2 addition, the optimum temperature for nucleation, which was related to the precipitation of tetragonal ZrO2, was 80$0^{\circ}C$. The optimum growth condition for the crystal was 87$0^{\circ}C$ for 8 hrs, and the major crystal phases precipitated in the samples were $\beta$-quartz ss. and mullite. The light transmissivity turned out to be around 80 per cent. On the other hand, when the TiO2 was added, it was difficult to determine the nucleating temperature, because the samples turned easily into translucency during the heat treatment. Therefore, it was almost impossible to retain transparency in the samples. The light transmissivity was below 30 per cent.

  • PDF

Synthesis and Characterization of Cordierite Glass-Ceramics for Low Firing Temperature Substrate: (I) Crystallization and Shrinkage Behavior of $MgO-Al_2O_3-SiO_2$ Glass Powders (저온소결 세라믹 기판용 Cordierite계 결정화유리의 합성 및 특성조사에 관한 연구: (I) $MgO-Al_2O_3-SiO_2$계 유리분말의 결정화 및 수축거동)

  • 이근헌;김병호;임대순
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.6
    • /
    • pp.451-458
    • /
    • 1992
  • Dense glass-ceramics for low firing temperature substrate were prepared by addition of CeO2 flux to the glass of MgO-Al2O3-SiO2 system. Glass powders were fabricated by melting at 150$0^{\circ}C$ and ball milling. Glass powder compacts were sintered at 800~100$0^{\circ}C$ for 3h. The crystallization and the shrinkage behaviors of glass powder compacts were analyzed by XRD, DTA and TMA. The shrinkage of glass powder compact increased with increasing the amount of CeO2. Because the softening temperature decreased and the crystallization temperature increased with increasing the amount of CeO2. Apparently, addition of CeO2 prevented formation of $\mu$-cordierite phase from the glass-ceramics and improved formation of $\alpha$-cordierite phase. Therefore crystallization properties were enhanced.

  • PDF