• Title/Summary/Keyword: Mg-doped

Search Result 343, Processing Time 0.027 seconds

Photoluminescence Properties of Novel $Mg_{2}SnO_{4}:Mn$ Phosphor (새로운 $Mg_{2}SnO_{4}:Mn$ 형광체의 광 발광 특성)

  • Kim, Kyung-Nam;Jung, Ha-Kyun;Park, Hee-Dong;Kim, Do-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.9
    • /
    • pp.817-821
    • /
    • 2001
  • A new $Mg_{2-x}MN_xSnO_4$ phosphor with an inverse spinel structure was synthesized by the solid-state reaction technique. The photoluminescence properties of the $Mg_2SnO_4$:Mn phosphors were investigated under 147nm -vacuum ultraviolet ray excitation. The Mn-doped $Mg_2SnO_4$ phosphor exhibited high emission intensity with the spectrum centered at 500nm wavelength. It was explained that the green emission in $Mg_2SnO_4$:Mn phosphor has originated from energy transfer from $^4T_1$ to $^6A_1$ of $Mn^{2+}$ ion at tetrahedral site of the spinel structure. The $Mn^{2+}$ ion concentration exhibiting the maximum emission intensity under the excitation of 147nm-vacuum ultraviolet ray was 0.25mol%. And the decay time of the phosphor was shorter than 10ms.

  • PDF

Fabrication and superconducting property of $MgB_2$ tape with Al metal powder addition

  • Ko, Jae-Woong;Yoo, Jai-Moo;Chung, Kuk-Chae;Kim, Young-Kuk;Wang, Xiaolin;Dou, Shi Xue;Yoo, Sang-Im;Chung, Woo-Hyun
    • Progress in Superconductivity and Cryogenics
    • /
    • v.9 no.2
    • /
    • pp.15-18
    • /
    • 2007
  • The sub micron sized spherical $MgB_2$ powders were synthesized by spray reaction method. $MgB_2$ tapes with Al addition were fabricated by Powder in Tube (PIT) method. The superconducting property and microstructure of Al doped $MgB_2$ tapes were characterized by X-ray diffraction, optical microscopy and transport measurement under magnetic field. The $J_c$ value of $MgB_2$ tapes was increased with 10 vol. % Al addition. The $J_c$ value of 5,500 A/$cm^2$ and 11,000 A/$cm^2$ at 4.2 K and 5 T were obtained for the $MgB_2$ tape and 10 vol. % of Al added $MgB_2$ tape without heat treatment, respectively. The $J_c$ value of 8,000 A/$cm^2$ and 33,000 A/$cm^2$ at 4.2 K and 5 T were obtained for the $MgB_2$ tape and 10 vol. % of Al added $MgB_2$ tape with heat treatment, respectively. The $J_c$-B curves show enhancement in $J_c$ (B), which suggests that the microstructure and transport properties of $MgB_2$ tapes have been improved with Al addition.

BGR mixture phosphor for white-light-emitting diode of liquid crystal display backlight

  • Lee, Sung-Hoon;Park, Je-Hong;Seo, Kwang-Il;Kim, Jong-Su
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2007.08b
    • /
    • pp.1559-1560
    • /
    • 2007
  • BGR mixture phosphor pumped by 400 nm is developed for white-light-emitting diode of liquid crystal display backlight. White-emitting phosphor is prepared by mixing $Ba_2SiO_4:Eu^{2+}$ and $(Ba,Sr)_3MgSi_2O_8:Eu^{2+},Mn^{2+}$ phosphors.

  • PDF

Diffractive characteristics of the photorefractive gratings in $LiNbO_3$:MgO ($LiNbO_3$:MgO 결정에서 광굴절 격자의 회절 특성)

  • 이재철;장지웅;김준태;신승호
    • Korean Journal of Optics and Photonics
    • /
    • v.10 no.5
    • /
    • pp.391-395
    • /
    • 1999
  • We present the measurement of the diffraction efficiency and response time of the photorefractive grating recorded in $LiNbO_3$ photorefractive crystal doped with 4%-mole MgO. Two laser sources were used in the experiments; frequency-doubled Q-switched Nd:YAG laser ($\lambda$=532 nm) and cw Ar-ion laser ($\lambda$=514.5 nm). The same optical geometry was also used in both experiments in order to maintain the experimental consistency. Using the two-wave mixing scheme in both experiments we measured the maximum diffraction efficiency in the range of beam intensity of 1.6~100 W/ $\textrm{cm}^2$, and the response times for both cases of recording and erasing. Two sets of results obtained from the experiments are compared and analyzed.

  • PDF

Effect of $MnO_2$ Addition on the Electric Properties in Pb($Mg_{1/3}Nb_{2/3}$)$O_3$ Relaxor Ferroelectrics ($MnO_2$ 첨가에 따른 Pb($Mg_{1/3}Nb_{2/3}$)$O_3$계 완화형 강유전체에서의 전기적 물성변화)

  • 박재환
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.7
    • /
    • pp.562-566
    • /
    • 2001
  • The effects of MnO$_2$ addition on the properties in Pb(Mg$_{1}$3/Nb$_{2}$3/)O$_3$ relaxor ferroelectrics were studied in the phase transition temperature range from -4$0^{\circ}C$ to 11$0^{\circ}C$. Specimens were made via solid state processing method. Dielectric properties, piezoelctric properties, electric-field-induced strain were examined to clarify the effect of MnO$_2$ addition in 0.9MN-0.1PT. As the amount of MnO$_2$ increases, the maximum dielectric constant and the dielectric loss decreases. Q$_{m}$ increased by increasing the doping contents of Mn. When 0.5wt% MnO$_2$ was doped, Q$_{m}$ increased from 95 to 480. The electric-filed-induced strain and polarization decreases as the amount of MnO$_2$ increases. From the experimental results, it was suggested that Mn behaves as an ferroelectric domain pinning element.ent.

  • PDF

Enhanced Crystallization Behaviour and Microwave Dielectric Properties of 0.9CaMgSi2O6-0.1MgSiO3 Glass-Ceramics Doped with TiO2

  • Jo, Hyun Jin;Sun, Gui Nam;Kim, Eung Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.2
    • /
    • pp.139-144
    • /
    • 2016
  • The dependence of the microwave dielectric properties of the glass-ceramic composite $0.9CaMgSi_2O_6-0.1MgSiO_3$ on the crystallization behaviour was investigated as functions of the $TiO_2$ content and heat-treatment temperature. The crystallization behaviour of the specimens was evaluated via a combination of the Rietveld and reference-intensity ratio methods. For specimens with a $TiO_2$ content of up to 1 wt.%, a monoclinic diopside phase was formed, whereas a secondary $TiO_2$ phase was formed with further increases in the $TiO_2$ content. The quality factor (Qf) of the specimens was strongly dependent on the degree of crystallization. The highest Qf value was obtained with a $TiO_2$ content of 0.5 wt.%, which was improved by increasing the heat-treatment temperature. The dielectric constant (K) was affected by the size of the crystallites and the $TiO_2$ content. The temperature coefficient of the resonant frequency (TCF) was nearly constant for all of the specimens, regardless of the $TiO_2$ content or heattreatment temperature.