전자빔 용접된 고장력 알루미늄 합금 용접부의 고온균열 발생 및 특성에 관한 연구

  • 김성욱;김경민;윤의박;이창희
    • 한국레이저가공학회지
    • /
    • 제4권1호
    • /
    • pp.39-48
    • /
    • 2001
  • This study was performed to evaluate basic characteristics of electron beam weldability for high strength aluminum alloys. The aluminum alloys used were A5083 and A6N01, and A7N01. The principal welding process parameters, such as accelerating voltage, beam current, welding speed and chamber pressure were investigated. The dimension and microstructure of welds were evaluated with OLM, and SEM (EDAX). In addition, weldability variation(cracking) due to process parameters was also evaluated. The degree of cracking in the EB fusion zone appears to be affected mainly by aspect ratio, such that as aspect ratio increases the cracking tendency also increases. The alloying element itself may also affect the hot cracking resistance, but its role is considered to be indirect effect such that the relatively higher vaporization pressure elements of Zn and Mg give deeper weld penetration and thus results in greater cracking tendency.

  • PDF

열분석 방법에 의한 급냉응고 Al-Li-Zr 합금의 시효거동 연구 (Study on the Aging Behaviors of a Rapidly Solidified Al-Li-Zr Alloy by Differential Scanning Calorimetry)

  • 홍영준;강정윤;김인배;이상래
    • 한국재료학회지
    • /
    • 제5권4호
    • /
    • pp.405-411
    • /
    • 1995
  • 급냉응고된 Al-3.51wt%Li-0.34wt%Zr 합금의 시효거동을 시차주사열량계(DSC)에 의한 열분석 방법으로 조사하였다. DSC에 의한 비열측정 결과 $\delta$’의 석출에 의한 발열반응과 $\delta$, $\beta$ 및 복합석출상의 석출에 의한 발열반응을 확인하였으며 $\delta$’ 및 $\delta$의 재고용에 의한 2개의 흡열반응을 확인하였다. 7$0^{\circ}C$ 저온시효시 $\delta$’의 석출에 의한 발열반응 이전에 흡열반응이 나타났으며 이것은 $\delta$’ 석출 이전에 $\delta$’ 전구생성물이 형성되었음을 의미한다. DSC 곡선상에 나타난 발열과 흡열곡선을 해석하여 얻은 $\delta$’상 석출과 재고용의 활성화에너지값은 각각 83KJ/mol과 98KJ/mol로서 Al-Li 2원계 및 Al-Li-Mg에 비해 높은 값을 나타내엇으며, 시효에 의한 강화가 일어나 DSC에 의한 비열변화 조사결과 나타난 $\delta$’상 석출 완료 시효조건점 (21$0^{\circ}C$, 1시간)에서 최고경도값(Hv 160)을 나타내었다.

  • PDF

HIGH STRENGTH ALUMINIUM ALLOYS PROCESSED BY SPRAY/CODEPOSITION

  • Juarez-Islas, Julio Alberto
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 1992년도 추계학술발표강연 및 논문개요집
    • /
    • pp.14-14
    • /
    • 1992
  • During the past five years a very successful effort has been made to improve existing and develop new aluminium alloys. The progress achieved has been possible because of the development of new production methods, such as powder metallurgy and spray/deposition. These methods make use of rapid solidification process which alloys compositions other than those achieved by conventional ingot metallurgy. The ingot metallurgy of the 2000 and 7000 series used thus far, as well as the age hardening Al-Li alloys, show several disadvantages caused by the production process. Such problems are primarily coarse intermetallic constituent phases, coarse grains and macrosegregation, resulting in low fracture toughness. The present contribution reports results of an experimental investigation performed on a modern high strength spay deposited aluminium alloy of the Al-Zn-Mg-Cu (7075 and the modified 7150X) type. Results are given in terms of its microstructural characterization by using X-ray diffractomertry and transmission electron microscopic. The mechanical propierties of those alloys in the as-extruded and extruded+aged condition were evaluated by using microhardness Vickers, tensile test and fracture toughness measurements.

  • PDF

EFFECT OF INTERMETALLIC COMPOUND ON MECHANICAL PROPERTIES OF Al-Cu DISSIMILAR BRAZING JOINT

  • Koyama, Ken;Shinozaki, Kenji;Ikeda, Kenji;Kuroki, Hidenori
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.555-560
    • /
    • 2002
  • Brazing of Al to Cu using AI-Si-Mg-Bi brazing alloy has been carried out in the vacuum furnace. In the bonded interlayer, there were two kinds of intermetallic compounds. One of these intermetallic compounds was e phase and the other was b phase. The growth of b phase was controlled by diffusion Al into Cu. Deformation behavior of Al-Cu brazing joint was brittle without deformation of the base metal. Shear strength of the joint was only about 20MPa. The shear specimen broken in the intermetallic compound, which was mainly e phase. Shear strength did not depend on the bonding temperature.

  • PDF

Perpendicular Magnetization of FePt Alloy Films Epitaxially Grown on Si(100)

  • Ahn, Jae-Young;Lee, Nyun-Jong;Kim, Tae-Hee
    • Journal of Magnetics
    • /
    • 제14권4호
    • /
    • pp.144-146
    • /
    • 2009
  • This study examined the structure and perpendicular magnetization of FePt films grown on Pt/Fe/MgO(100) buffered Si(100) substrates by molecular beam epitaxy. The [Fe(0.17nm)/Pt(0.2nm)]$_N$ multilayers were prepared at room temperature to form a $L1_0$-FePt phase after vacuum annealing. Perpendicular magnetic anisotropy (PMA) was observed in the films after at least 15 repetitions (N = 15) of Fe/Pt deposition and annealing at $300{^{\circ}C}$ for 1 hour. Careful structural analysis of the films was carried out by x-ray diffraction and high-resolution transmission electron microscopy. These results will assist in the development of the low temperature $L1_0$- FePt deposition process, which will be essential for future extremely high density magnetic recording media.

Thixoforming을 위한 재가열용 유도코일 설계의 최적화 (Optimization of Induction Coil Design for Reheating in Thixoforming Process)

  • 김남석
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 춘계학술대회논문집
    • /
    • pp.165-168
    • /
    • 1999
  • The coil design of induction heating systems and their optimization are of paramount importance for semi-solid processing(SSP) The authors of this paper present the coil design and optimization of a 60 Hz induction heating system for ALTHIX 86S (Al-6%_Si-3%Cu-0.3%Mg) alloy. An objective function on the basis of the optimization process for the coil design is proposed by introducing an optimization technique. Finally the results of the optimal coil design are also applied to the induction heating process to obtain a fine globular microstructure. The proposed new objective function based on the computational techniques would contribute to obtaining the thixoformed components with good mechanical properties and reducing lead time.

  • PDF

마그네슘 합금의 크리이프 거동에 표면처리가 미치는 영향 (The Effect of Surface Treatment on Creep Behaviors of Mg Alloy)

  • 강대민;안정오;강민철
    • 소성∙가공
    • /
    • 제18권4호
    • /
    • pp.347-353
    • /
    • 2009
  • The apparent activation energy, the applied stress exponent, and rupture life have been measured from creep experiments over the range of $200^{\circ}C$ to $220^{\circ}C$ and the applied stress range of 64MPa to 94MPa. The materials were used AZ31 magnesium alloys treated by plasma electrolytic oxidation of $20{\mu}m$ and $40{\mu}m$ at surface to investigate the its influence on creep behavior, and creep tests were carried out under constant applied stress and temperature. The experimental results showed that the dipper the thickness of surface treatment the higher the activation energy and stress exponent. And the higher temperature and applied stress, the lower stress exponent and activation energy, respectively. Also the dipper the thickness of surface treatment the longer creep rupture time.

CV흑연주철(黑鉛鑄鐵)의 응고특성(凝固特性)에 관한 연구(硏究) (A Study on the Solidification Characteristics of CV Graphite Cast Iron)

  • 김철진;김수영;이계완
    • 한국주조공학회지
    • /
    • 제5권3호
    • /
    • pp.5-12
    • /
    • 1985
  • Many researchers have studied the eutectic solidification of CV Graphite Cast Iron qualitatively. However quantative studies have not been done. The type of eutectic solidification of CV Graphite Cast Iron treated with CG Alloy (Fe-Si-Mg-5Ti-Ca-Ce) was studied quantitatively through M.D.E. value (Mushy Degree of Eutectic Solidification) = $t_2/t_1)$, where $t_1$ is the difference of the eutectic solidification starting time between surface and center part of the casting sample, and $t_2$ is the time of eutectic solidification of the center part. Following results were obtained. (1) The M.D.E. value of CV graphite cast iron lies between that of spheroidal graphite and that of flake graphite cast iron but is closer to that of Flake graphite cast iron. (2) The M.D.E. value of CV graphite cast iron depends upon CV ratio. (3) The time required for eutectic solidification increases as graphite form is changed from Flake, CV. to spheroidal graphite. (4) The M.D.E. value increases as cooling rate increases.

  • PDF

DC 스퍼터법에 의해 제작한 Zn계 합금박막의 나노조직구조와 전기화학적 특성 평가 (Nano Structure of Zn Alloy Thin Films Prepared by DC Sputtering Method and Their Electrochemical Characteristics Evaluation)

  • 배일용;김연원;문경만;김기준;이명훈
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.226-226
    • /
    • 2009
  • 일반적으로 알루미늄이나 아연 등과 같은 이온화 경향이 큰 금속들은 그 자체의 활성적인 특성으로 인해 강재와 같은 이온화 경향이 낮은 금속재의 표면에 도금 또는 코팅함으로서 사용 환경 중 자체 내식성 보유와 더불어 손상 결함시 희생양극적인 역할 등의 잇점으로 많이 사용되고 있다. 본 연구에서는 DC 스퍼터링법에 의해 표면조직이 치밀한 여러 가지의 Zn-Mg 합금박막을 제작하였다. 이들 박막은 종래의 Zn도금에 비해 부식환경 중 장기간 갈바닉쌍을 형성하여 모재 금속에 대한 보호막 기능을 우수하게 하는 것으로 나타났다.

  • PDF

마그네슘합금 상의 크로메이트 대체를 위한 전기화학적 아연코팅 (An alternative electrochemical zinc coating to chromate treatment of Mg alloy substrate)

  • 김형찬;김영석;한성호;이상준;전동술;최헌수
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.132-132
    • /
    • 2009
  • 마그네슘 합금은 비강도, 전동감쇠능 등 여러 장점으로 인하여 모바일 제품, 자동차 항공기 등 여러 영역에서 사용되고 있다. 하지만 내부식성 문제로 인하여 사용이 제한되고 있는 실정이다. 마그네슘 합금의 표면 처리는 기존에 전해 및 무전해 도금, 양극산화, 화성처리 등의 방법의 있으나 일반적으로 화성처리인 3가 크로데이트 후 도장 공정이 내식성 증가를 위해 적용되고 있다. 본 연구에서는 전기화학적인 방법으로 3가 크로메이트를 대체할 수 있는 친환경적이고 경제적인 아연 코팅을 마그네슘합금(AZ91) 소재에 생성시켰다. 표면특성 및 전기화학적인 분석은 SEM, EDX, XRD, potentiostat/galvanostat을 이용하였다.