용체화처리된 주조용 Mg-8%Al-X%Zn 합금의 부식 거동 (Corrosion Behavior of Solution-Treated Mg-8%Al-X%Zn Casting Alloys)

  • 전중환;황인제
    • 열처리공학회지
    • /
    • 제28권3호
    • /
    • pp.126-133
    • /
    • 2015
  • The aim of this study is to investigate the effect of solution treatment on the corrosion behavior of Mg-8%Al-(0-1)%Zn casting alloys in 1M NaCl aqueous solution. After the solution treatment, all alloys showed single ${\alpha}$-(Mg) phase microstructure by dissolution of ${\beta}(Mg_{17}Al_{12})$ phase into the ${\alpha}$-(Mg) matrix. The $H_2$ evolution volume decreased with an increase in Zn content, which indicates that the addition of Zn plays a beneficial role in decreasing corrosion rate of the Mg-Al-Zn alloy in solution-treated state. The microstructural evaluations on the corrosion products and corroded surfaces after the immersion test in 1 M NaCl solution revealed that the incorporation of more $Al_2O_3$ and ZnO into the corrosion product, by which the penetration of $Cl^-$ ions is impeded, are thought to be responsible for the better corrosion resistance in relation with the Zn addition.

금형 주조한 GZ21 합금과 AZ91 합금의 부식특성 비교 (Comparison of Electrochemical Corrosion Properties of Permanent Mold Casting GZ21 Alloy and AZ91 Alloy)

  • 김대한;김병호;박경철;장인기
    • 한국주조공학회지
    • /
    • 제36권2호
    • /
    • pp.60-66
    • /
    • 2016
  • In this study, comparison of corrosion properties of the Mg-1.5Ge-1Zn (GZ21) alloy and Mg-9Al-1Zn (AZ91) alloy were investigated. The studied alloys were fabricated by permanent mold casting method. And the potentiodynamic test, hydrogen evolution test, immersion test and A.C Impedance test were carried out in a 3.5% NaCl solution with pH7.2 at room temperature to measure the corrosion properties. The microstructure of GZ21 alloy was composed of ${\alpha}-Mg$ and $Mg_2Ge$ phases and AZ91 alloy was composed of ${\alpha}-Mg$ and $Mg_{17}Al_{12}$ phases. From the test results, the corrosion property was improved by adding Ge. It seemed that the corrosion mechanism was changed from galvanic corrosion (AZ91) to filiform corrosion (GZ21).

전자회절실험에 의한 알루미늄 합금 (Al-Cu-Mg)의 미세 S-상 석출입자에 대한 결정구조 연구 (A Study of the Crystal Structure of the Fine S-Phase Precipitate in Al-Cu-Mg Alloy by Electron Diffraction Experiments)

  • 김황수
    • Applied Microscopy
    • /
    • 제35권4호
    • /
    • pp.1-9
    • /
    • 2005
  • 이 논문에서 Al-Cu-Mg 합금의 미세 석출 입자의 S-상 ($Al_2CuMg$) 결정구조에 대해 전자회절실험에 의한 포괄적인 연구 결과가 보고 되어 있다. 이 실험에는 한 S-상 입자를 포함하는 최소 영역의 일정 zone축의 회절패턴(SAED) 관찰과 이에 대응되는 운동학적 이론을 기초로 한 패턴의 시물레이션과의 비교 분석, 그리고 관측된 회절 패턴 필름으로부터 각 Bragg회절 점의 강도의 정량적 데이터 추출과 운동학적 및 동역학적 회절 강도 계산과의 비교 검토의 과정을 포함하고 있다. 이러한 연구의 한 결과 S-상의 결정구조는 일찍이 X-ray 방법으로부터 얻은 PW 모델결정(Perlitz and Westgren, 1943)과 일치함을 보여주고 있고, HREM 방법에 의해 새로이 구한 RaVel (Radmilovic et al., 1999) 모델과는 전혀 맞지않음이 판명되었다.

High Temperature Deformation Behavior of Al-Zn-Mg-Based New Alloy Using a Dynamic Material Model

  • Jang, Bong Jung;Park, Hyun Soon;Kim, Mok-Soon
    • Metals and materials international
    • /
    • 제24권6호
    • /
    • pp.1249-1255
    • /
    • 2018
  • High temperature compression tests for newly developed Al-Zn-Mg alloy were carried out to investigate its hot deformation behavior and obtain deformation processing maps. In the compression tests, cylindrical specimens were deformed at high temperatures ($300-500^{\circ}C$) and strain rates of 0.001-1/s. Using the true stress-true strain curves obtained from the compression tests, processing maps were constructed by evaluating the power dissipation efficiency map and flow instability map. The processing map can be divided into three areas according to the microstructures of the deformed specimens: instability area with flow localization, instability area with mixed grains, and stable area with homogeneous grains resulting from continuous dynamic recrystallization (CDRX). The results suggest that the optimal processing conditions for the Al-Zn-Mg alloy are $450^{\circ}C$ and a strain rate of 0.001/s, having a stable area with homogeneous grains resulting from CDRX.

알카리 수용액에서 Mg-Al 합금의 양극산화시 전류밀도와 양극산화 시간의 효과 (Effects of Time and Current Density in Anodizing of Mg-Al Alloy in Alkaline Solution)

  • 장석기;김성종;김정일
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제29권1호
    • /
    • pp.107-115
    • /
    • 2005
  • The effects on the formation of anodic oxide films on Mg-Al alloy (AZ91) in 1M-NaOH solution was investigated using parameters of current density and time during anodizing The general tendency has been confirmed that the increase of anodizing time improves the corrosion resistance. It is considered that the formation of anodic oxide film was increased by increasing the applied current and the anodizing time to generate active dissolution reaction In anodizing at constant current density. passivity potentials shifted to noble direction with increasing current densities. It was confirmed that oxygen quantify in anodic oxide films increased with anodizing time. The compact films above 4 $mA/cm^2$ were formed with the shape of an island in grooves at early stage and then grew with combination of the islands

자동차 경량 부품 제조를 위한 Al-Cu-Mg 분말 합금의 소결 및 열처리 특성 (Sintering and Heat Treatment Characteristics of Al-Cu-Mg Powder Metallurgy Alloy for Lightweight Automotive Parts)

  • 안병민
    • 한국생산제조학회지
    • /
    • 제23권2호
    • /
    • pp.152-156
    • /
    • 2014
  • Lightweight materials such as aluminum and magnesium have recently received much attention in the automotive industries because of environmental and fuel-efficiency concerns. Using the powder metallurgy (PM) process for these materials creates significant opportunities for the cost-effective manufacture of lightweight automotive parts. In the present study, an Al-Cu-Mg alloy was fabricated using conventional PM processes. Primarily, the effects of the alloying elements on the sintering characteristics and mechanical behavior after heat treatment were investigated. A microstructural analysis was performed using an optical microscope and a scanning electron microscope to investigate the behavior of liquid phase sintering, including the formation of precipitates. The dependence of the mechanical behavior on the alloying elements was evaluated based on the transverse rupture strength.

Mg, Zn, Si 성분이 7xxx 계 알루미늄 합금의 압출성에 미치는 영향 (The Effect of Mg, Zn, Si wt(%) on the Extrudability of 7xxx Al Alloy)

  • 함현욱;김병민;조훈;조형호
    • 한국정밀공학회지
    • /
    • 제16권11호
    • /
    • pp.148-157
    • /
    • 1999
  • The objective of this study is to investigate the effect of three main chemical compositions(Mg, Zn, Si) on extrudability of 7xxx Al alloy with high tensile strength. A few Al alloys based on 7xxx alloys were metal mold cast with various weight*%) of Mg 0.3-1.2%, Zn 5.0-8.0% and Si 0.4-0.7%, to envestigate the effects of extrudability, as well as mechanical properties. To measure the extrudability of cast billets, maximum extrusion pressure and surface temperature at die exit before tearing occurs were obtained by experiment and simulation of thermo-viscoplastic F.E.M. Also the yield and tensile strength of extruded products were tested.

  • PDF

Al-5%Mg계 주조합금의 물성 및 시효경화특성에 미치는 합금원소의 영향 (Effects of Alloying Elements on the Properties and Aging Hardening of Al-5%Mg Based Casting Alloys)

  • 김정민;박준식;조재익;김현길
    • 한국주조공학회지
    • /
    • 제30권1호
    • /
    • pp.29-33
    • /
    • 2010
  • The microstructure of Al-5%Mg based alloy mainly consists of aluminum matrix with a small amount of AlMn phase. The addition of Sc or Zn to the base alloy significantly improved the as-cast tensile strength, while the addition of Fe deteriorated both strength and ductility. Although the Al-5%Mg based alloy was not heat-treatable, aging hardening could be observed in the case that Sc or Zn was added to the base alloy. TEM analysis showed that very fine AlSc or AlMgZn precipitates were formed after T6 heat treatment, resulting in enhanced strength. The corrosion resistance measured as corrosion potential was found to decrease a little by adding Zn, whereas other alloying elements were not clearly influential.

($AlSi_7Mg$알루미늄 합금의 초정 구형화에 대한 주조조건의 영향 (Effect of the Casting Conditions on the Globulization of Primary Al of $AlSi_7Mg$ Alloy)

  • 한요섭;이호인;이재철
    • 한국주조공학회지
    • /
    • 제23권1호
    • /
    • pp.40-46
    • /
    • 2003
  • Semisolid forming requires alloys with non-dendritic microstructure of the thixotropy. Recently, low pouring temperture method without stirring, i.e. liquidus casting has been found out new fabrication method of the semisolid metals. Effects of melt superheat and mold conditions on the globulization of primary Al of $AlSi_7Mg$ alloy were investigated in gravity casting process without stirring. The microstructures of primary Al as function of melt superheat and mold temperature show globular, rosette and dendritic shapes. The conditions for globular microstructure of primary Al were low melt superheat < 35 K and low mold temperature < 500 K. The thermal conditions for globular microstructure of primary Al were undercooled melt at early solidification stages and slow cooling < 0.6 K/s. It was found that the initial microstructure was maintained throughout the solidification and the globules of primary Al can be obtained by high nucleation of fine and spherical nuclei due to enhanced undercooling of melt.

펄스 YAG 레이저 용접시 유기하는 플라즈마의 스펙트럼선 동정과 발광특성 (Spectral Line Identification and Emission Characteristics of the Laser-Induced Plasma in Pulsed Nd:YAG Laser Welding)

  • 김종도
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제23권3호
    • /
    • pp.360-368
    • /
    • 1999
  • The paper describes spectroscopic characteristics of plasma induced in the pulsed YAG laser welding of alloys containing a large amount of volatile elements. The authors have conducted the spectroscopic analyses of laser induced Al-Mg alloys plasma in the air and argon atmosphere. In the air environment the identified spectra were atomic lines of Al, Mg, Cr, Mn, Cu, Fe and Zn and singly ionized Mg lines as well as the intense molecular spectra of ALO and MgO formed by chemi-cal reactions of evaporated Al and Mg atoms from the pool surface with oxygen in the air. In argon atmosphere MgO and AlO spectra vanished but AlH spectrum was detected. the hydrogen source was presumable hydrogen dissolved in the base metals water absorbed on the surface oxide layer or $H_2$ and $H_2O$ in the shielding gas. The resonant lines of Al and Mg were strongly self-absorbed in particular self-absorption of the Mg line was predominant. These results show that the laser induced plasma was made of metallic vapor with relatively low temperature and high density.