• 제목/요약/키워드: Metal alloy

검색결과 1,893건 처리시간 0.028초

주조티타늄과 기계절삭티타늄 코핑의 변연적합성에 관한 연구 (THE STUDY ABOUT THE MARGINAL FIT OF THE CASTING TITANIUM AND MACHINE-MILLED TITANIUM COPINGS)

  • 오수연;방몽숙;양홍서;박상원;박하옥
    • 대한치과보철학회지
    • /
    • 제44권1호
    • /
    • pp.20-28
    • /
    • 2006
  • Statement of problem: The titanium has advantages of a high biocompatibility, a corrosion resistence, low density, and cheep price, so it is focused as a substituted alloy But it is quite difficult to cast with the tranditional method due to the high melting point, reacivity with element at, elevated temperature. By using the CAD-CAM system for the crown construction, it is possible to reduce the errors while proceeding the wax-up, investing, and casting procedure Purpose: The purposes of this study were to measure the marginal adaptation of the casting titanium coping and machine-milled titanium coping according to the casting methods and the marginal configurations. Material and method: The marginal configurations were used chamfer shoulder, and beveled shoulder. The total 30 copings were used, and these are divided into 6 groups according to the manufacturing method and marginal configuration. The gap between margin of the model and the restoration was measured with 3-dimensional measuring microscope. Results: The following results were obtained; 1. casting gold coping demonstrated the best marginal seal, followed by casting titanium coping finally machine-milled titanium copings. 2. In casting titanium coping, chamfer demonstrated the best marginal seal, followed by shoulder and beveled shoulder. There was no significantly difference in shoulder and beveled shoulder. But all margin form has clinically acceptable 3. In machine-milled titanium copings, chamfer demonstrated the best marginal seal, followed by shoulder and beveled shoulder. Beveled shoulder show large and uneven marginal gap Conclusions: Above result revealed that marginal adaptation of the titanim coping is avail able in the clinical range, it can be used as an alternative metal and it is prefered especially in chamfer or shoulder margin during implant superstructure fabrication. But there should be more research on machine-milled titanium in order to use it in the clinics.

EFFECTS OF SURFACE ROUGHNESS AND MULTILAYER COATING ON THE CORROSION RESISTANCE OF Ti-6Al-4V ALLOY

  • Ko, Yeong-Mu;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2003년도 추계학술발표회초록집
    • /
    • pp.134-135
    • /
    • 2003
  • The dental implant materials required good mechanical properties, such as fatigue strength, combined with a high resistance to corrosion. For increasing fatigue resistance and delaying onset of stress corrosion cracking, shot peening has been used for > 50 years to extend service life of metal components. However, there is no information on the electrochemical behavior of shot peened and hydroxyapatite(HA) coated Ti-6Al-4V alloys. To increase fatigue strength, good corrosion resistance, and biocompatibility, the electrochemical characteristics of Ti/TiN/HA coated and shot peened Ti-6Al-4V alloys by electron beam physical vapor deposition(EB-PVD) have been researched by various electrochemical method in 0.9%NaCl. Ti-6Al-4V alloys were prepared under the condition of hydrogen and vacuum arc furnace. The produced materials were quenched at 1000$^{\circ}C$ under high purity dried Ar atmosphere and were hold at 500$^{\circ}C$ for 2 hrs to achieve the fatigue strength(1140㎫) of materials. Ti-6Al-4V alloys were prepared under the condition of hydrogen and vacuum arc furnace. Shot peening(SP) and sand blasting treatment was carried out for 1, 5, and 10min. On the surface of Ti-6Al-4V alloys using the steel balls of 0.5mm and alumina sand of 40$\mu\textrm{m}$ size. Ti/TiN/HA multilayer coatings were carried out by using electron-beam deposition method(EB-PVD) as shown Fig. 1. Bulk Ti, powder TiN and hydroxyapatite were used as the source of the deposition materials. Electrons were accelerated by high voltage of 4.2kV with 80 - 120mA on the deposition materials at 350$^{\circ}C$ in 2.0 X 10-6 torr vacuum. Ti/TiN/HA multilayer coated surfaces and layers were investigated by SEM and XRD. A saturated calomel electrode as a reference electrode, and high density carbon electrode as a counter electrode, were set according to ASTM GS-87. The potentials were controlled at a scan rate of 100 mV/min. by a potentiostat (EG&G Co.273A) connected to a computer system. Electrochemical tests were used to investigate the electrochemical characteristics of Ti/TiN/HA coated and shot peened materials in 0.9% NaCl solution at 36.5$^{\circ}C$. After each electrochemical measurement, the corrosion surface of each sample was investigated by SEM.

  • PDF

열팽창계수차에 기인된 잔류응력을 이용한 세라믹 캠 팔로우어의 크라우닝 제어 (Control of Crowning Using Residual Stress induced by the Difference of Tehermal Expansion Between Ceramic and Carbon Steel in Ceramic Cam Follower)

  • 최영민;이재도;노광수
    • 한국재료학회지
    • /
    • 제10권10호
    • /
    • pp.703-708
    • /
    • 2000
  • 최근에 상용차용 디젤 엔진의 성능 향상을 목적으로 엔진 설계가 급격히 변화되면서 캠 팔로우어(cam follower)와 캠(cam) 사이에 작용하는 접동면 하중의 증가로 접동면에서의 마모가 중요한 문제가 되고 있다. 본 연구에서는 기존의 주절체 및 소결합금 캠 팔로우어에 비해 내마모성이 우수한 세라믹 캠 팔로우어를 개발하였다. 잔류 응력을 완화시켜주는 중간층을 사용하지 않고 질화규소($Si_3N_4$) 팁과 중탄소강을 활성납재를 사용하여 직접 접합후 냉각시키는 과정에서 두 모재의 열팽창계수차에 의한 크라우닝(crowning, R) 이 형성되도록 하였다. 접합에 사용한 중탄소강은 열팽창시 이력(hysteresis) 거동을 나타내었으며, $A_{c1}$ 변태점인 $723^{\circ}C$ 이하에서 접합할 경우 원하는 크라우닝이 형성되었다. 접합온도가 $723^{\circ}C$ 이상이 되면 크라우닝 (R) 값이 온도에 따라 지수함수적으로 증가하였으며 이는 중탄소강의 상변태에 의한 열팽창.수축의 이력 특성으로 설명되어질 수 있었다. 규격에 맞는 크라우닝이 형성되는 최적 접합 온도는 $700~720^{\circ}C$의 범위였다. 질화규소와 중탄소강의 직접 접합방법으로 접합과 동시에 크라우닝을 형성시키고 제어함으로써 난가공재인 세라믹을 곡면 가공하지 않고도 적당한 곡률을 갖는 저가의 세라믹 캠 팔로우어를 제조할 수 있었다.

  • PDF

원주(原州) 법천리출토(法泉里出土) 금동식리(金銅飾履)에 대한 연구(硏究) (A Study on Gilded Ornamental Shoes Excavated from Beopcheon-ri, Wonju)

  • 권혁남;유혜선
    • 박물관보존과학
    • /
    • 제3권
    • /
    • pp.65-69
    • /
    • 2001
  • 백제문화의 중요한 자료가 되고 있는 원주 법천리 고분군 중 1호분과 4호분에서 금동식리편이 발굴되었다. 특히 이 식리에는 스파이크가 존재하여 백제의 식리 제작과 금동 기술에 대한 정보를 제공할 수 있다. 본 연구는 이곳에서 출토된 식리편을 분석하여 식리의 제작 방법, 당시 사용된 동의 특성 등을 조사하였다. 스파이크는 투과X-선과 현미경 등을 통해 관찰해 본 결과 하나의 몸체로 제작되어 머리 부분을 두드려 금동판에 부착하였다. 이 금동판은 대부분 구리로 되어 있으며 재결정에 의한 쌍정이 나타나고 있고, 비금속개재물의 EDS 분석 결과 납을 함유하고 있다. 또한 금동판이 두 개로 되어있다는 증거가 나타나지 않아 장식용으로 리벳을 사용한 것으로 보인다. 금동판의 도금은 금도금층의 두께가 불균일하고 내부가 비어 있으며 EDS 분석에서 수은이 검출되는 것으로 보아 아말감법에 의한 도금을 하였다.

마찰교반용접 툴 변화에 따른 마그네슘 합금 압출 판재 마찰교반용접부 기계적 물성 평가 (Evaluation of Mechanical Properties of Extruded Magnesium Alloy Joints by Friction Stir Welding : Effect of Welding Tool Geometry)

  • 선승주;김정석;이우근;임재용
    • 한국산학기술학회논문지
    • /
    • 제17권10호
    • /
    • pp.280-288
    • /
    • 2016
  • 본 연구의 목적은 마찰교반용접을 마그네슘 합금에 응용하기에 앞서 형상이 다른 두 종류의 용접 툴을 마찰교반용접 시험에 적용 및 비교하여 마그네슘 합금 마찰교반용접에 더 적합한 용접 툴을 제안하였다. 용접 툴의 효과를 알아보기 위해서 용접조건 변수 중 이송속도는 200mm/min으로 고정하였고 회전속도를 400, 600, 800rpm으로 변화시키면서 용접부의 거동과 용접 툴 변화에 따른 효과를 평가 및 관찰하였다. 기계적 물성 평가를 위해 인장시험과 경도시험을 수행하였으며, 용접부 내 거동 및 결함의 유무를 확인하기 위하여 용접부에 수직인 방향의 횡단면을 광학현미경을 통해 관찰하였다. 용접 툴에 관계없이 회전속도가 400rpm일 때 결함이 관찰되었으며, 회전속도가 증가할수록 결함이 감소하는 경향을 보였다. 최종적으로 회전속도 800rpm에서 결함이 없는 용접부를 얻었다. 용접 툴 변화에 따른 기계적 물성 평가 결과 C type 용접 툴을 적용한 경우 보다 우수한 결과가 나타났다. 기계적 물성이 가장 우수한 용접조건은 회전속도 800rpm, 이송속도 200mm/min 이었고, 이때 용접부의 인장강도, 항복강도 그리고 연신율은 모재 대비 90.0%, 69.1%, 83.2% 수준으로 각각 나타났다.

Evaluations of Si based ternary anode materials by using RF/DC magnetron sputtering for lithium ion batteries

  • 황창묵;박종완
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2010년도 제39회 하계학술대회 초록집
    • /
    • pp.302-303
    • /
    • 2010
  • Generally, the high energy lithium ion batteries depend intimately on the high capacity of electrode materials. For anode materials, the capacity of commercial graphite is unlike to increase much further due to its lower theoretical capacity of 372 mAhg-1. To improve upon graphite-based negative electrode materials for Li-ion rechargeable batteries, alternative anode materials with higher capacity are needed. Therefore, some metal anodes with high theoretic capacity, such as Si, Sn, Ge, Al, and Sb have been studied extensively. This work focuses on ternary Si-M1-M2 composite system, where M1 is Ge that alloys with Li, which has good cyclability and high specific capacity and M2 is Mo that does not alloy with Li. The Si shows the highest gravimetric capacity (up to 4000mAhg-1 for Li21Si5). Although Si is the most promising of the next generation anodes, it undergoes a large volume change during lithium insertion and extraction. It results in pulverization of the Si and loss of electrical contact between the Si and the current collector during the lithiation and delithiation. Thus, its capacity fades rapidly during cycling. Si thin film is more resistant to fracture than bulk Si because the film is firmly attached to the substrate. Thus, Si film could achieve good cycleability as well as high capacity. To improve the cycle performance of Si, Suzuki et al. prepared two components active (Si)-active(Sn, like Ge) elements film by vacuum deposition, where Sn particles dispersed homogeneously in the Si matrix. This film showed excellent rate capability than pure Si thin film. In this work, second element, Ge shows also high capacity (about 2500mAhg-1 for Li21Ge5) and has good cyclability although it undergoes a large volume change likewise Si. But only Ge does not use the anode due to its costs. Therefore, the electrode should be consisted of moderately Ge contents. Third element, Mo is an element that does not alloys with Li such as Co, Cr, Fe, Mn, Ni, V, Zr. In our previous research work, we have fabricated Si-Mo (active-inactive elements) composite negative electrodes by using RF/DC magnetron sputtering method. The electrodes showed excellent cycle characteristics. The Mo-silicide (inert matrix) dispersed homogeneously in the Si matrix and prevents the active material from aggregating. However, the thicker film than $3\;{\mu}m$ with high Mo contents showed poor cycling performance, which was attributed to the internal stress related to thickness. In order to deal with the large volume expansion of Si anode, great efforts were paid on material design. One of the effective ways is to find suitably three-elements (Si-Ge-Mo) contents. In this study, the Si based composites of 45~65 Si at.% and 23~43 Ge at.%, and 12~32 Mo at.% are evaluated the electrochemical characteristics and cycle performances as an anode. Results from six different compositions of Si-Ge-Mo are presented compared to only the Si and Ge negative electrodes.

  • PDF

폐 피복관 처리를 위한 염소계-불소계 혼합용융염 내 지르코늄 전해정련공정에서 삼불화알루미늄의 효과 연구 (Effect of AlF3 on Zr Electrorefining Process in Chloride-Fluoride Mixed Salts for the Treatment of Cladding Hull Wastes)

  • 이창화;강덕윤;이성재;이종현
    • 방사성폐기물학회지
    • /
    • 제17권2호
    • /
    • pp.127-137
    • /
    • 2019
  • 삼불화알루미늄($AlF_3$)이 포함된 염화물-불화물 혼합 용융염에서 ZIRLO 튜브를 이용한 지르코늄 전해정련공정을 실증하였다. 순환 전압전류실험 결과, $AlF_3$의 농도가 증가함에 따라 금속환원의 개시 전위가 일정하게 증가하고 지르코늄-알루미늄 합금형성과 관련된 추가적인 peak의 크기가 점차 증가하는 것으로 나타났다. 전류조절 전착법과 달리, -1.2 V의 일정전위에서 수행한 지르코늄 전해정련에서 방사형 판 구조의 지르코늄 성장이 염의 상단 표면에서 확연하게 나타났으며, 전착물 지름의 크기는 $AlF_3$의 농도에 따라 점차 증가하는 것으로 나타났다. 주사전자현미경(SEM)과 에너지 분산 X선 분광기(EDX)와 X선 광전자 분광기(XPS)를 이용하여 판 구조의 지르코늄 전착물을 분석한 결과, 극미량의 알루미늄이 지르코늄-알루미늄 합금 형태로 존재하며, 전착물의 상단과 하단 간에 서로 다른 화학성분구조를 갖는 것으로 나타났다. $AlF_3$의 첨가는 전착물 내 잔류염 양을 줄이고, 지르코늄 회수를 위한 전류효율을 향상시키는 데 효과적인 것으로 나타났다.

타이타늄 표면 코팅 처리에 따른 타이타늄도재관의 파절강도 비교 (A COMPARISON OF FRACTURE STRENGTHS OF PORCELAIN-FUSED-TO-TITANIUM CROWN AMONG TITANIUM SURFACE COATING TREATMENTS)

  • 김지혜;박상원;방몽숙;양홍서;박하옥;임현필;오계정;김현승;이광민;이경구
    • 대한치과보철학회지
    • /
    • 제45권2호
    • /
    • pp.203-215
    • /
    • 2007
  • Statement of problem: Titanium and its alloy, with their excellent bio-compatibility and above average resistance to corrosion, have been widely used in the field of dentistry. However, the excessive oxidization of titanium which occurs during the process of firing on porcelain makes the bonding of titanium and porcelain more difficult than that of the conventional metal-porcelain bonding. To solve this problem related to titanium-porcelain bonding, several methods which modify the surfaces, coat the surfaces of titanium with various pure metals and ceramics, to enable the porcelain adhesive by limiting the diffusion of oxygen and forming the adhesive oxides surfaces, have been investigated. Purpose: The purpose of this study was to know whether the titanium-porcelain bonding strength could be enhanced by treating the titanium surface with gold and TiN followed by fabrication of clinically applicable porcelain-fused-to-titanium crown Material and method: The porcelain-fused-to-titanium crown was fabricated after sandblasting the surface of the casting titanium coping with $Al_2O_3$ and treating the surface with gold and TiN coating followed by condensation and firing of ultra-low fusing porcelain. To compare with porcelain-fused-to-titanium crowns, porcelain-fused-to-gold crowns were fabricated and used as control groups. The bonding strengths of porcelain-fused-to-gold crowns and porcelain-fused-totitanium crowns were set for comparison when the porcelain was fractured on purpose to get the experimental value of fracture strength. Then, the surface were examined by SEM and each fracturing pattern were compared with each other Result:Those results are as follows. 1. The highest value of fracture strength of porcelain-fused-to-titanium crowns was in the order of group with gold coating, group with TiN coating, group with $Al_2O_3$ sandblasting. No statistically significant difference was found among the three (P>.05). 2. The porcelain-fused-to-gold crowns showed the highest value in bonding strength. The bonding strength of crowns porcelain-fused-to-titanium crowns of rest groups showed bonding strength reaching only 85%-94% of that of PFG, though simple comparision seemed unacceptable due to the difference in materials used. 3. The fracturing patterns between metal and porcelain showed mixed type of failure behavior including cohesive failure and adhesive failure as a similar patterns by examination with the naked eye and SEM. But porcelain-fused-to-gold crowns showed high incidence of adhesive failure and porcelain-fused-to-titanium crowns showed high incidence of cohesive failure. Conclusion: Above results proved that when fabricating porcelain-fused-to-titanium crowns, treating casting titanium surface with gold or TiN was able to enhance the bonding strength between titanium and porcelain. Mean value of masticatory force was found to showed clinically acceptable values in porcelain bonding strength in all three groups. However, more experimental studies and evaluations should be done in order to get better porcelain bonding strength and various surface coating methods that can be applied on titanium surface with ease.

타이타늄의 표면개질에 따른 도재 결합 특성 (THE BOND CHARACTERISTICS OF PORCELAIN FUSED BY TITANIUM SURFACE MODIFICATION)

  • 최택휴;박상원;방몽숙;양홍서;박하옥;임현필;오계정;김현승;이광민;이경구
    • 대한치과보철학회지
    • /
    • 제45권2호
    • /
    • pp.169-181
    • /
    • 2007
  • Statement of problem: Titanium is well known as a proper metal for the dental restorations, because it has an excellent biocompatibility, resistance to corrosion, and mechanical property. However, adhesion between titanium and dental porcelains is related to the diffusion of oxygen to the reaction layers formed on cast-titanium surfaces during porcelain firing and those oxidized layers make the adhesion difficult to be formed. Many studies using mechanical, chemical and physical methods to enhance the titanium-ceramic adhesion have been actively performed. Purpose: This study meant to comparatively analyse the adhesion characteristics depending on different titanium surface coatings after coating the casts and wrought titanium surfaces with Au and TiN. Material and method: In this study, the titanium specimens (CP-Ti, Grade 2, Kobe still Co. Japan) were categorized into cast and wrought titanium. The wrought titanium was cast by using the MgO-based investment(Selevest CB, Selec). The cast and wrought titanium were treated with Au coating($ParaOne^{(R)}$., Gold Ion Sputter, Model PS-1200) and TiN coating(ATEC system, Korea) and the ultra low fusing dental porcelain was fused and fired onto the samples. Biaxial flection test was done on the fired samples and the porcelain was separated. The adhesion characteristics of porcelain and titanium after firing and the specimen surfaces before and after the porcelain fracture test were observed with SEM. The atomic percent of Si on all sample surfaces was comparatively analysed by EDS. In addition, the constituents of specimen surface layers after the porcelain fracture and the formed compound were evaluated by X-ray diffraction diagnosis. Result: The results of this study were obtained as follows : 1. The surface characteristics of cast and wrought titanium after surface treatment(Au, TiN, $Al_2O_3$ sandblasting) were similar and each cast and wrought titanium showed similar bonding characteristics. 2. Before and after the biaxial flection test, the highest atomic weight change of Si component was found in $Al_2O_3$ sandblasted wrought titanium(28.6at.% $\rightarrow$ 8.3at.%). On the other hand, the least change was seen in Au-Pd-In alloy(24.5at.% $\rightarrow$ 9.1at.%). 3. Much amount of Si components was uniformly distributed in Au and TiN coated titanium, but less amount of Si's was unevenly dispersed on Al2O3 sandblasting surfaces. 4. In X-ray diffraction diagnosis after porcelain debonding, we could see $Au_2Ti$ compound and TiN coating layers on Au and TiN coated surfaces and $TiO_2$, typical oxide of titanium, on all titanium surfaces. 5. Debonding of porcelain on cast and wrought titanium surface after the biaxial flection is considered as a result of adhesion deterioration between coating layers and titanium surfaces. We found that there are both adhesive failure and cohesive failure at the same time. Conclusion: These results showed that the titanium-ceramic adhesion could be improved by coating cast and wrought titanium surfaces with Au and TiN when making porcelain fused to metal crowns. In order to use porcelain fused to titanium clinically, it is considered that coating technique to enhance the bonding strength between coating kKlayers and titanium surfaces should be developed first.

방사선 치료에서 3D 프린터로 제작된 금속 필라멘트의 투과율에 관한 유용성 평가 (Evaluation of the Usefulness of the Transmittance of Metal Filaments Fabricated by 3D Printers in Radiation Therapy)

  • 권경태;장희민;윤명성
    • 한국방사선학회논문지
    • /
    • 제15권7호
    • /
    • pp.965-973
    • /
    • 2021
  • 방사선 치료는 고에너지 X선을 최소 20 Gy에서 80 Gy까지 다양하게 조사되기 때문에 종양이 위치하는 국소부위에 고선량을 투여하며 일부 정상조직의 여러 부작용이 예상 된다. 현재 임상에서는 정상조직의 차폐를 위한 노력으로 대표적인 재료인 납을 사용하고 있지만 납은 인체에 유해한 중금속으로 분류되고 있으며 다량의 피부접촉은 중독을 유발할 수 있다. 따라서 본 연구는 FDM(Fused Deposition Modeling)방식의 3차원 프린터의 재료 Tungsten, Brass, Copper을 이용하여 납의 한계점을 보완 할 수 있는 측정시트를 제작하고 투과성능을 알아보고자 한다. 3D 프린터를 이용해 Tungsten 혼합 필라멘트 투과측정 시트 크기는 70 × 70 mm, 두께는 1, 2, 4 mm로 제작하였으며 제작한 측정시트의 투과성능을 확인하기 위해 선형가속기 (TrueBeam STx, S/N: 1187)에서 발생된 6, 15 MV을 Water Phantom과 Ion chamber (FC-65G), elcetrometer (PTW UNIDOSE)을 사용하여 SSD 100 cm, 물 속 5 cm에서 100 MU를 조사하여 측정하고 투과성능을 평가하였다. 각 소재의 측정시트를 1 mm씩 증가시킨 결과 6 MV에서는 Tungsten 시트의 경우 3.8~3.9 cm일때의 시트는 기존 납의 차폐체 두께 6.5 cm 보다 얇으며, 15 MV에서는 Tungsten 시트의 경우 4.5~4.6 cm일 때 시트는 기존 납의 차폐체 두께 7 cm 보다 얇으며 동등한 성능을 확인할 수 있었다. 본 연구를 통하여 Tungsten 합금 필라멘트을 이용하여 제작한 투과측정 시트는 고에너지 영역에서의 투과 차폐 가능성을 확인하였으며. 대체품으로써의 사용가능성 또한 우수함을 확인하였다, 향후 3D 프린팅 기술로 차폐제 제작을 위한 기초자료로 제공할 수 있을 것으로 사료 된다.