• Title/Summary/Keyword: Metal Foundry

검색결과 227건 처리시간 0.021초

급냉응고법에 의한 금속 섬유제조에 관한 연구 (A Study on the Fabrication of Metal Fiber by Rapid Solidification Process)

  • 백남익;허성강;라형용
    • 한국주조공학회지
    • /
    • 제9권5호
    • /
    • pp.396-402
    • /
    • 1989
  • Metal fibers of Al and stainless steel were fabricated by the PDME method and the Taylor process. Tensile strength of metal fiber produced by both the PDME method and the Taylor process was much higher than that of conventionally solidified materials. Utilizing the PDME method, Al fiber with $100\;{\mu}m$ was fabricated under Ar gas atmosphere, and stainless steel fiber with $50\;{\mu}m$ was fabricated under 0.06 Torr vacuum. Continuous fiber of stainless steel was made by the Taylor process and the surface of this fiber was smother than that fabricated by the PDME method.

  • PDF

탕류 및 응고 해석을 통한 자동차 Gear Housing의 다이캐스팅 주조공정 설계 (Die Casting Process Design of Automobile Gear Housing by Metal Flow and Solidification Simulation)

  • 박진영;김억수;박익민
    • 한국주조공학회지
    • /
    • 제24권6호
    • /
    • pp.347-355
    • /
    • 2004
  • In the die casting process, the flow of liquid metal has significant influence on the quality of casting products and die life. For the optimal process design of automobile gear housing, various analyses were performed in this study by using computer simulation code, MAGMAsoft. The simulation has been focused on the molten metal behaviors during the mold filling and solidification stages for the sound casting products. Also the internal defects were predicted by application of air pressure and feeding criteria.

주철(鑄鐵)의 흑연(黑鉛)구상화에 미치는 Misch Metal Hydride의 첨가효과(添加效果) (Graphite Spheroidization in Cast Iron by Addition of Misch Metal Hydrides)

  • 김관휴;이도재;최답천;박충년
    • 한국주조공학회지
    • /
    • 제8권3호
    • /
    • pp.322-328
    • /
    • 1988
  • 3.9%C-2.0%Si-Fe 조성의 압분체(壓粉體)를 $1350^{\circ}$, Ar가스 분위기에서 50분간 용해한 용탕에 시판(市販) misch metal과 misch metal hydride인 MmH와 $MmH_2$를 각각 여러비율로 첨가(添加)한후 서냉(徐冷)및 급냉(急冷)한 시편의 흑연형상(黑鉛形狀)의 변화로부터 misch metal hydride의 구상화능(球狀化能)과 흑연구상화(黑鉛球狀化) 기구(機構) 로서의 기포설(氣泡說)의 타당성을 고찰한 결과 다음과 같은 결론을 얻었다. 1) Misch metal은 0.5% 이상, 그리고 misch metal hydride는 0.25% 이상 첨가한 때 구상흑연(球狀黑鉛)과 CV 흑연(黑鉛)이 나타났으며, misch metal hydride를 첨가한 때가 misch metal에 비하여 흑연립수(黑鉛粒數)가 더 많았다. 이와같이 misch metal hydride의 첨가량이 misch metal에 비하여 적었음에도 흑연립수(黑鉛粒數)가 더 많은 것을 보면 Mm으로부터 방출되는 다수(多數)의 수소기포(水素氣泡)가 구상흑연(球狀黑鉛)의 정출장소로 되는 것으로 해석되기 때문에 기포설(氣泡說)이 타당하다고 생각된다. 2) Misch metal 과 misch metal hydride의 첨가량(添加量)이 1.0%로 증가되면 두경우 모두 흑연립수(黑鉛粒數)가 감소하였다. 이는 용탕중에 개재된 수소기포(水素氣泡)의 실수율차이에 의한 잔류 수소기포수의 증가율둔화와 첨가량(添加量)의 증가에 따른 잔류 misch metal량의 상대적(相對的) 증가로 인한 다량의 잔류 misch metal이 응고과정에서 수소를 재흡수 용해하여 흑연입수를 결정하는 용탕중의 유효수소기포수(有效水素氣泡數)를 감소시켰기 때문으로 생각된다.

  • PDF

철도 정비창의 폐기물과 혼합된 중금속 오염토 분리에 관한 연구 (A Study on Isolation of Mixed Heavy Metal-Contaminated Soil and the Waste in Railroad Workshop)

  • 손우화;이승호
    • 한국지반환경공학회 논문집
    • /
    • 제13권12호
    • /
    • pp.59-66
    • /
    • 2012
  • 본 연구에서는 철도정비창 부지 내에 폐기물 및 중금속오염 구간에서 채취한 토양을 대상으로 하였다. 그리고 효율적인 정화공정 설계를 위하여 고농도 오염구간, 저농도 오염구간, 폐주물사 함유 시료를 대상으로 입도분포 및 입도 분포 오염농도 분석을 실시하였다. 하지만 폐콘크리트, 폐목재 등의 건설폐기물, 폐주물사, 소각재 등이 부지 전반에 걸쳐 매립되어 있어 일반토양 오염과 다른 양상을 보이고 있었다. 따라서 일반적인 중금속정화기술로는 오염원이 감소하지 않아 혼합된 폐기물 중에 자성을 띠는 성분을 자력선별을 적용하여 실험한 결과 중금속 오염도는 감소하는 것으로 나타났다.

알루미늄 용탕 운반용 고보온성 Ladle 설계 및 평가 (Design and Evaluation of High Insulation Ladle for Carrying Aluminum Molten Metal)

  • 박진영;최석환;윤필환;김억수
    • 한국주조공학회지
    • /
    • 제30권3호
    • /
    • pp.115-120
    • /
    • 2010
  • Recently, an advanced raw material supplying system in diecasting industry that molten metal produced by the raw material supplier can be directly delivered to the diecasting shops was proposed. It was known to have advantages of reducing melting process cost and improving working environment. However, for its successful mass production, the development of high insulation ladle is inevitable. In this study, the optimal mixing ratio of $SiO_2-Al_2O_3$ was investigated and the high insulation ladle with computer simulation result was built in a prototype and evaluated. The prototype which has refractory wall of $SiO_233%-Al_2O_3$ 35%-CaO 33% showed high insulation sufficient for carrying the Al molten metal for 138 minutes. Gas quantity result and SEM-EDS analysis on the melt poured in the ladle also showed extremely low level of 0.028 cc / 100 g and no penetration of Al molten metal into the refractory wall, satisfying the requirements for mass production.

6극 전자석 전자교반 레오캐스팅에 따른 A356의 조직적 / 기계적 영향분석 (Microstructure and Mechanical Property of A356 for Rheocasting Using 6-Pole Electromagnetic Stirring Casting Process)

  • 김백규;노중석;방희재;허민;박진하;전충환
    • 한국주조공학회지
    • /
    • 제40권3호
    • /
    • pp.61-65
    • /
    • 2020
  • Rheo-diecasting with stirring has been used in many material industries. As the 4th Industrial Revolution approaches the world, eco-friendly high-strength and light-weight materials become more important. Casting methods have been studied and used for aluminum-alloy automobile parts. This study carried out the effect analysis of the micro-structure and mechanical properties, such as yield/ultimate tensile strength, elongation, and hardness, of A356 using the 6-pole EMS (electro-magnetic stirring) casting process with a high electromagnetic force. As a result, the hardness and elongation of the A356 after T6 heat-treatment show a significant improvement, respectively, by 20% and 50%.

용탕 침투법을 이용한 복합 삽입 금속의 제조 (Fabrication of Composite Filler Metal by Melt Infiltration)

  • 박흥일;김지태;김우열
    • 한국주조공학회지
    • /
    • 제23권5호
    • /
    • pp.244-250
    • /
    • 2003
  • The aim of this study is fabricating of composite filler metal (CFM) by a combination of selective laser sintering (SLS) of stainless steel powders (RapidSteel $2.0^{TM}$ and liquid phase infiltration of Ag-28 wt.%Cu alloy. Porous stainless steel body with inter-connected pore channels was fabricated by SLS, binder decomposing and densification processes. By the direct contact infiltration, the narrow inter-particle channels of the porous body were completely filled with the Ag-28 wt.%Cu alloy infiltrant. During infiltration, the dissolved elements of Fe, Ni and Cr from the porous body were solved into copper solid solution phases, which consist of eutectic structure of composite metal matrix. The S10C/CFM/S10C joints, which have narrow clearance gaps between them up to 10 micrometers, were joined successfully by self-feeding of filler metal from the matrix of CFM. The CFM kept its original thickness and microstructure after brazing. The tensile strength of brazed specimen was higher than 30 kgf/$mm^2$ and showed a typical ductile fracture mode in the CFM.

Cu-Be-Co합금의 물성에 미치는 열처리 조건의 영향 (Effects of Heat-Treatment Conditions on the Properties of Cu-Be-Co Alloy)

  • 정운재;경신호;김기태;김종인
    • 한국주조공학회지
    • /
    • 제14권3호
    • /
    • pp.233-239
    • /
    • 1994
  • The effects of solid solution treatment and aging in the properties of Cu-0.32wt%Be-1.35wt%Co alloy was gravity die casted and forged were investigated in order to examine the optimum heat treatment conditions for production of high conductivity mold material. The optimum properties for mold material were obtained under the conditions which were solid solution treated at $930^{\circ}C$ for 1 hour and aged at $430^{\circ}C$ for 2hours.

  • PDF

리튬 배터리 음극용 SiO2 코어 쉘을 갖춘 나노 다공성 실리콘 입자 제조 (Fabrication of Nano Porous Silicon Particle with SiO2 Core Shell for Lithium Battery Anode)

  • 심보림;김은하;임현민;김원진;김우병
    • 한국재료학회지
    • /
    • 제34권7호
    • /
    • pp.370-376
    • /
    • 2024
  • In this study, we report significant improvements in lithium-ion battery anodes cost and performance, by fabricating nano porous silicon (Si) particles from Si wafer sludge using the metal-assisted chemical etching (MACE) process. To solve the problem of volume expansion of Si during alloying/de-alloying with lithium ions, a layer was formed through nitric acid treatment, and Ag particles were removed at the same time. This layer acts as a core-shell structure that suppresses Si volume expansion. Additionally, the specific surface area of Si increased by controlling the etching time, which corresponds to the volume expansion of Si, showing a synergistic effect with the core-shell. This development not only contributes to the development of high-capacity anode materials, but also highlights the possibility of reducing manufacturing costs by utilizing waste Si wafer sludge. In addition, this method enhances the capacity retention rate of lithium-ion batteries by up to 38 %, marking a significant step forward in performance improvements.

직접가압주조한 Al-5%Ni-5%Mg-(Mm)합금의 조직 및 기계적 성질에 미치는 가압력의 영향 (Effect of Pressure on Microstructures and Mechanical Properties in Al-5%Ni-5%Mg-(Mm) Alloy Manufactured by Direct Squeeze Casting)

  • 우기도;정동석;황인오;김석원
    • 한국주조공학회지
    • /
    • 제21권2호
    • /
    • pp.127-134
    • /
    • 2001
  • Misch metal (rare earth element, Ce, La, Nd, Pr) which has large influence on high-temperature stability and toughness was added to the Al-5%Ni-5%Mg alloy, and squeeze casting was used for Al-5%Ni-5%Mg-(Mm) alloys. The effect of applied pressure and misch metal additions on mechanical properties in Al-5%Ni-5%Mg alloy by direct squeeze casting has been investigated. The applied pressure were 0 MPa(gravity casting), 25, 50 and 75 MPa. Squeeze-cast Al-5%Ni-5%Mg-(Mm) alloys had better mechanical properties than those of non-pressurized cast alloys because of the increased cooling rate by the application of pressure during solidification. By the addition of misch metal in Al-5%Ni-5%Mg alloy, better combination of strength and elongation was obtained. The addition of 0.3%Mm in Al-5%Ni-5%Mg alloy improved the heat resistant property due to the formation of fine eutectic phases.

  • PDF