• Title/Summary/Keyword: Mesh Fabric

Search Result 52, Processing Time 0.019 seconds

Stealth, electromagnetic interception, and electrical properties of aluminum sputtered clothing materials - Focusing on the density change - (알루미늄 스퍼터링 처리 의류소재의 스텔스 특성과 전자파 차단 및 전기적 특성에 관한 연구 - 밀도 변화를 중심으로 -)

  • Han, Hye Ree
    • The Research Journal of the Costume Culture
    • /
    • v.30 no.4
    • /
    • pp.579-593
    • /
    • 2022
  • This study examines the surface characteristics, electrical conductivity, electromagnetic wave blocking characteristics, infrared (IR) transmittance, stealth function, thermal characteristics, and moisture characteristics of IR thermal imaging cameras. Nylon film (NFi), nylon fabric (NFa), and 5 types of nylon mesh were selected as the base materials for aluminum sputtering, and aluminum sputtering was performed to study IR thermal imaging, color difference, temperature change, and so on, and the relationship with infrared transmittance was assessed. The electrical conductivity was measured and the aluminum-sputtered nylon film demonstrated 25.6kΩ of surface resistance and high electrical conductivity. In addition, the electromagnetic wave shielding characteristics of the sputtering-treated nylon film samples were noticeably increased as a result of aluminum sputtering treatment as measured by the electromagnetic wave blocking characteristics. When NFi and NFa samples with single-sided sputtering were placed on the human body (sputtering layer faced the outside air) and imaged using IR thermographic cameras, the sputtering layer displayed a color similar to the surroundings, showing a stealth effect. Moreover, the tighter the sample density, the better the stealth function. According to the L, a, b measurements, when the sputtering layer of NFi and NFa samples faced the outside air, the value of a was generally high, thereby demonstrating a concealing effect, and the △E value was also high at 124.2 and 93.9, revealing a significant difference between the treated and untreated samples. This research may be applicable to various fields, such as the military wear, conductive sensors, electromagnetic wave shielding film, and others.

Resorbability and histological reaction of bioabsorbable membranes (수종의 흡수성 차단막의 생체 분해도와 조직학적 반응)

  • Suk, Hun-Joo;Kwon, Suk-Hoon;Kim, Chang-Sung;Choi, Seong-Ho;Jeon, Dong-Won;Kim, Chong-Kwan
    • Journal of Periodontal and Implant Science
    • /
    • v.32 no.4
    • /
    • pp.781-800
    • /
    • 2002
  • The major goals of periodontal therapy are the functional regeneration of periodontal supporting structures already destructed by periodontal disease. There have been many efforts to develop materials and therapeutic methods to promote periodontal wound healing. With the development of non-resorbable membrane, GTR has proved to be the representive technique of periodontal regeneration. However, due to various clinical problems of non-resorbable membrane, resorbable membrane was developed and it showed to be clinically effective. The newly developed Para-Dioxanone membrane has a characteristic of non-woven fabric structures which is different from the generally used membranes with structure of mesh form. In addition, Chitosan membrane has been developed to apply its adventage maximally in GTR. Although a number of different types of membranes had been clinically used, researches on absorption rate of membranes were inadequate and limited to subjective opinions. However, since long term period of resorption and space maintenance are required in implant or ridge augmentation, accurate verification of resorption rate is clinically important. In this study, we had implanted Resolut(R), Biomesh(R), Para-Dioxanone membrane and Chitosan membrane (Size : 4mm ${\times}$ 4mm) on dorsal side of Sprague Dawley rat, and sacrified them after 4 weeks, 8 weeks, 12 weeks respectively. Histologic observation was carried out, and the following results were obtained by calculating the objective resorption rate. 1. In case of Resolut(R), external resorption took place initially, followed by internal resorption. Surface area are 5.76${\pm}$2.37$mm^2$, 4.90${\pm}$l.06$mm^2$, 4.90${\pm}$0.98$mm^2$ at 4 weeks, 8 weeks, 12 weeks respectively, and invasion rate of connective tissue to membrane are 31.6${\pm}$4.5%, 52.8${\pm}$9.4%, 56.4${\pm}$5.1% respectively. 2. Biomesh(R) showed a pattern of folding, relatively slow resorption rate with small size of membrane. Surface area are 3.62${\pm}$0.82$mm^2$, 3.63${\pm}$0.76$mm^2$, 4.07${\pm}$1.14$mm^2$ at 4 weeks, 8 weeks, 12 weeks respectively, and invasion rate of connective tissue to membrane are 26.1${\pm}$5.8%, 30.9${\pm}$3.4%, 29.2${\pm}$3.6%, respectively. 3. Para-Dioxanone membrane was surrounded by fibrous conncetive tissue externally, and resorption took place internally and externally. Surface area are 5.96${\pm}$1.05$mm^2$, 4.77${\pm}$10.76$mm^2$, 3.86${\pm}$0.84$mm^2$ at 4 weeks, 8 weeks, 12 weeks respectively, and invasion rate of connective tissue to membrane are 30.7${\pm}$5.1%, 53.3${\pm}$4.4%, 69.5${\pm}$3.1%, respectively. 4. Each fiber of Chitosan membrane was surrounded by connective tissue and showed external resorption pattern. It showed little invasion of inflammatory cells and excellent biocompatability. The resorption rate was relatively slow. Surface area are 6.01${\pm}$2.01$mm^2$, 5.49${\pm}$1.3$mm^2$, 5.06${\pm}$1.38$mm^2$ at 4 weeks, 8 weeks, 12 weeks respectively, and invasion rate of connective tissue to membrane are 31.3${\pm}$3.6%, 38.4${\pm}$3.80%, 39.7${\pm}$5.6%, respectively. Consequently, Para-Dioxanone membrane and Chitosan membrane are found to be clinically effective for their excellent tissue reaction and biocompatibility. Futhermore, the advantage of bone regenerating ability as well as the relatively long resorption period of Chitosan membrane, it might be widely used in implant or ridge augmentation.