• Title/Summary/Keyword: Magnetic Force(자력)

Search Result 97, Processing Time 0.029 seconds

Magnetic properties of $\textrm{SiO}_2$/CoNiCr/Cr thin films ($\textrm{SiO}_2$/CoNiCr/Cr 합금 박막의 자기적 성질)

  • Kim, Taek-Su;Kim, Jong-O;Seo, Gyeong-Su
    • Korean Journal of Materials Research
    • /
    • v.7 no.1
    • /
    • pp.69-75
    • /
    • 1997
  • Thin films of $Si0_2(1000{\AA})/CoNiCr(400{\AA})/Cr$ were fabricated as a function of Cr thickness by KF magnetron sputtering. The saturation magnetization, coercive force and squareness with annealing temperature for these films were investigated. The values of saturation magnetization of $SiO_2/CoNiCr/Cr$ thin films decreased as the thickness of Cr underlayer increased, whereas coercive force increased as the thickness of Cr underlayer increased. The value of Ms was 600 emu/cc and the maximum value of Hc was 550 Oe. Especially, the value of saturation magnetization was rapidly decreased $SiO_2/CoNiCr/Cr(1700{\AA})$ thin films as the annealing temperature increased And the coercive force increased as the annealing temperature increased When annealing temperature was $650^{\circ}C$, the Ms was reduced to 90 % of the as-deposited film. And the Hc was showed maximum 1600 Oe. It was thought that Cr diffusion into CoNiCr layer reduced the magnetic moment of CoKiCr layer. In addition. Hc might he increased due to grain growth perpendicular to the film plane.

  • PDF

Analysis of distributed MMF on tooth for induction motor using Magnetic Equivalent Circuit (자기등가회로법에 의한 유도전동기의 치기자력 분포해석)

  • Jeong, Jong-Ho;Lee, Eun-Woong;Lim, Su-Saeng;Kim, Jun-Ho
    • Proceedings of the KIEE Conference
    • /
    • 2001.07b
    • /
    • pp.638-640
    • /
    • 2001
  • In this paper, system equation of the magnetic equivalent circuit of the induction motor be consist of the magnetomotive force transformation matrix and the flux transformation matrix. The system equation is fed by three phase sinusoidal current and get to magnetomotive force on the teeth. This study confirmed the time and spatial distribution of the magnetomotive force on the teeth created by the winding.

  • PDF

Magnetic levitation force and trapped magnetic field of top-seeded melt-processed YBCO superconductors with multiseeding (다중 종자결정성장법으로 제조한 YBCO 초전도체의 자기 부상력과 포획자력)

  • Kim, Chan-Joong;Jee, Young-A;Kim, Ho-Jin;Joo, Jin-Ho;Han, Young-Hee;Kim, Sang-Jun;Hong, Gye-Won
    • 한국초전도학회:학술대회논문집
    • /
    • v.9
    • /
    • pp.358-362
    • /
    • 1999
  • Magnetic levitation forces and trapped magnetic fields of top-seeded melt growth-processed YBCO superconductors with multiseeding were studied. The number of seeds was varied from one to six. The surface magnetic field of the prepared YBCO samples was dependent on the number of the seeds. The trapped magnetic field of the top surface decreased with increasing the number of the seed. Particularly, it drastically decreased at the YBCO grain boundary, probably due to the weak rink nature of the boundary. The magnetic levitation force also decreased with increasing the number of the seeds, similar to the variation of the surface magnetic field.

  • PDF

Effects of heat treatment and Co addition on the magnetic properties of FeCoBSi thin film (FeCoSiB 자성박막의 자기적 특성에 미치는 Co 및 열처리의 영향)

  • 신현수;양성훈;장태석;박종완
    • Journal of the Korean Vacuum Society
    • /
    • v.9 no.4
    • /
    • pp.389-393
    • /
    • 2000
  • Effects of Co addition and heat treatment on the magnetic properties of Fe-Si-B thin films were investigated. The compositions of metalloids, i.e, B and Si, in the alloys were kept 10 at.% each. Heat treatments were carried out in the temperature range from 100 to $300^{\circ}C$ for up to 60 min. Amorphous thin films of FeCoSiB were deposited on the water-cooled substrates by dc magnetron sputtering. The composition of thin films was controlled by placing proper number of pellets of alloying elements and analyzed by ICP, resulting in $Fe_{80-X}Co_ XB_{10}Si_{10}$ (X=8~18 at.%). Saturation magnetization of the alloys increased as Co concentration increased up to 10 at.% and then decreased with further increase of Co concentration. However, coercive force of the films decreased with the increase of Co concentration. Furthermore, the coercive force was also reduced by the annealing due to the residual stress relief.

  • PDF

Evaluation of 1Cr-1Mo-0.25V Steel Degradation Using Magnetic Barkhausen Noise (Barkhausen noise를 이용한 1Cr-1Mo-0.25V강의 열화도 평가)

  • Lee, Jong-Min;Ahn, Bong-Young;Nahm, Seung-Hoon;Lee, Seung-Seok;Lee, Ouk-Sub;Nam, Young-Hyun
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.7
    • /
    • pp.1262-1269
    • /
    • 2002
  • It is inevitable to evaluate the life of turbine rotor because the operating periods of power plants need to be extended. For the test, seven kinds of specimens with different degradation levels were prepared by the isothermal heat treatment at $630^{\circ}C$. Magnetic methods utilizing Barkhausen noise coercive force($BN_c$) were applied to detect the degradation caused by thermal aging. Magnetic property of material is related with domain dynamics and that is affected by the microstructure of material. Therefore $BN_c$ is very sensitive to the microstructure change of the material. With the increase of degradation, $BN_c$ was decreased and this phenomenon is considered due to precipitations and grain size. The result was compared with Vickers hardness($H_v$) and coercive force($H_c$) to detect the relative variation, and was related with $H_v$ and YS to estimate the change of the mechanical properties with the degradation.

Removal of Impurities by Magnetic Separation from Waste Fluidized Cracking Catalyst for Its Reuse (폐FCC 촉매의 재활용 과정에서 자력 선별법에 의한 불순물 제거 연구)

  • Ban Bong-Chan;Lee Jin-Suk;Kim Dong-Su
    • Resources Recycling
    • /
    • v.12 no.1
    • /
    • pp.55-64
    • /
    • 2003
  • Presently, the reuse of waste FCC catalysts, which generated from the refining process of crack oil, after the removal of con-taminated metallic impurities have not been attempted domestically yet because the separation technology f3r the impurities from waste catalysts has not been established. As a basic study far the reusable portion from the waste FCC catalysts and treatment of metallic impurities are assured, there will be invoked an significant contribution not only in the recycling of abandoned wastes up to date but also in the treatment efficiency of wastes and extraction of economical benefits from them. The magnetic separation of impurities such as Fe, Ni, and V, from waste FCC catalyst has been attempted with or without its pre-oxidation at high temperature for the purpose of its reuse. The results showed that the separability of impurities by magnetic force was high far non-preoxidized catalysts compared with preoxidized ones, and employment of screen-type matrix showed a higher separation efficiency than ball-type matrix. The separability increased with the strength of magnetic field, and the method of ball matrix has separation efficiency of maximum 51.10%. The amount of metallic impurities was in the decreasing order of V, Ni, and Fe depending upon ICP analysis.

Evaluation of 1Cr-1Mo-0.25V Steel Degradation Using Magnetic Barkhausen Noise (Magnetic Barkhausen Noise를 이용한 1Cr-1Mo-0.25V강의 열화도 평가)

  • Lee, J.M.;Ahn, B.Y.;Nam, Y.H.;Nahm, S.H.;Lee, S.S.;Lee, O.S.
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.250-255
    • /
    • 2001
  • It is inevitable to evaluate the life of turbine rotor because the operating periods of power plants need to be extended. The magnetic methods utilizing Magnetic Barkhausen noise curve were applied to detect the degradation caused by thermal aging. The Magnetic property of material depends on the domain dynamics and it is affected by the microstructure of material. Therefore the magnetic property is very sensitive to the microstructure change of the material. It is, thus, very useful to detect the state of degradation of varying materials. The test specimen made of 1Cr-1Mo-0.25V steel was used widely for turbine rotor material, and seven kinds of specimens with different degradation levels were prepared by the isothermal heat treatment at $630^{\circ}C$. With the increase of degradation, BHN was decreased. The result was compared with coercive force and vickers hardness.

  • PDF

Hybrid Rubber Mount by Using Magnetic Force (자력을 이용한 하이브리드 고무 마운트)

  • Ahn, Young Kong;Kim, Dong-Woo
    • Transactions of the Korean Society for Noise and Vibration Engineering
    • /
    • v.24 no.3
    • /
    • pp.236-246
    • /
    • 2014
  • This paper presents a hybrid rubber mount with magnet to isolate effectively the vibration in vehicle, forklift, and so on. The hybrid mount does not have any controller of the magnetic force. Dynamic stiffness of the mount is reduced by only magnetic suction according to the applied magnetic field and damping coefficient increased. Performance of conventional rubber mount with using electromagnet has been investigated by MTS Tester. The governing equation of the hybrid mount was derived and verified by comparison with experimental and theoretical results. The equation can be used practically and usefully in the design of the mount and analysis of the mounting system. The hybrid mount provides excellent performance in vibration isolation and its structure is very simpler than active with controller and a semi-active mount with a functional fluid. Furthermore, production cost of the mount using permanent magnets is very lower than that of the active mount with electromagnets. Therefore, commercial potential of the mount is very high.

Frequency Dependance of Inductance of FeCoB Amorphous Magnetic Films (FeCoB계 아몰퍼스 자성박막의 인덕턴스의 주파수 의존성)

  • 신용진;소대화;김현욱;서강수;임재근
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.5
    • /
    • pp.413-417
    • /
    • 1998
  • In this paper, we investigate frequency dependance of inductance of FeCoB amorphous magnetic films. $(Fe_{1-x}Co_x)_{79}Si_2B_{19}$ was used as the basic composition of amorphous magnetic film having near zero magnetostriction. The amorphous magnetic films were fabricated with x=0.94 and x=0.95 by using sputtering method at high frequency. The films were anneald under non-magnetic field and near crystallization temperatures(30min at $280^{\circ}C$, 30min and 1hr at $400^{\circ}C$, respectively). As the results of the experiments with the fabricated films, the lowest coercive force was 0.084[Oe] at 400[W] of the input power and the crystallization temperature was $360^{\circ}C$ . In the case 30min at 40$0^{\circ}C$ the inductance value in the low frequency with x=0.95 was higher by 488% than that with x=0.94. The quality factor Q was below 0.7 for all samples. We obtained the highest quality value at 400[KHz] with 30min at $280^{\circ}C$ and x=0.94. The value was about 0.62. Also, the quality factor value was about 0.35 at 1[MHz] with 30min at $280^{\circ}C$ and x=0.95.

  • PDF

Performance Evaluation of Hydraulic and Magnetic Clamp Crane for Transporting Curved Steel Plate for Shipbuilding, with Permanent Magnet Applied (영구자석을 적용한 선박용 곡면 철판 이송용 유압식 마그네틱 클램프 이송장치의 성능평가에 대한 고찰)

  • Moon, Byung Young;Lee, Sung Bum;Lee, Ki Yeol
    • Journal of Ocean Engineering and Technology
    • /
    • v.29 no.4
    • /
    • pp.322-330
    • /
    • 2015
  • As a new technical approach, a hydraulic and magnetic clamp device was developed to realize a magnetic clamp crane system by simultaneously actuating eight individual hydraulic cylinders. In this approach, an Sr-type of ferritic permanent magnet (SrO· 6Fe2O3), rather than the previous electromagnet, was utilized for the purpose of lifting and transporting the large curved steel plates used for manufacturing ships. This study had the goal of developing and manufacturing a hydraulic, magnetic clamp prototype composed of three main parts, including the base frame, cylinder joint, and magnet joint, in order to safely transport curved steel plates. Furthermore, this research included a performance evaluation of the manufactured prototype and acquired the purposed quantity value in the performance test. The most significant item, the magnetic adhesive force (G), was evaluated in a performance test, which utilized a ferritic permanent magnet (Sr type) with 3700~4000 G of residual induction (Br) and 2640/2770 Oe of coercive force (Hc). In particular, relevant items such as the hoist tension (kN), transportation time (s), and applied load (Kgf) on the hydraulic cylinders were also evaluated in order to determine the optimum values.