• 제목/요약/키워드: MW-CVD diamond film

검색결과 4건 처리시간 0.018초

고주파-마이크로파 2단계 공정에 의한 다이아몬드 막의 성장 (Growth of diamond films by RF-MW two step process)

  • 박상현;우복만;박재윤;이상희;이덕출
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 하계학술대회 논문집 C
    • /
    • pp.1533-1536
    • /
    • 2001
  • To grow the diamond films by using RF-MW two step process, at first, diamond seeds were deposited on silicon substrate by RF plasma CVD, and then a diamond layer grown by MW plasma CVD on the seeds. The grain-size of diamond films deposited by using RF-MW two step process was smaller and denser and also, crystallity of diamond film was better than those of the MW plasma CVD process. The deposited diamond films were analyzed by SEM(scanning electron microscophy), XRD (x-ray diffraction), and Raman spectroscopy.

  • PDF

${CH_4}-{H_2}-{N_2}$ 기체계에서 MW-PACVD를 이용한 결정상 합성 (Synthesis of Crystalline film from ${CH_4}-{H_2}-{N_2}$ gases with MW-PACVD)

  • 김도근;백영준;성태연
    • 한국재료학회지
    • /
    • 제10권9호
    • /
    • pp.648-655
    • /
    • 2000
  • 다이아몬드 합성 조건에서 질소 첨가량은 0%에서 95%까지 변화하였을 때의 합성 거동을 조사하였다. 질소 첨가량이 증가함에 따라 합성된 상은 {100} 성장면으로 이루어진 다이아몬드 막에서 고유의 결정면이 사라지고 나조 크기의 결정들로 이루어진 다이아몬 막으로 변화하였다. 심지어 수소가 없어 메탄과 질소만의 경우에서도 다이아몬드 막 합성이 가능함을 보여주었다. 또한 다이아몬드 구조를 갖는 개별적 입자의 형태는 30%∼80% 질소 첨가범위에서 정팔면체의 결정모양을 가졌고, 이 범위에서 기판온도가 증가함에 따라 육방정 모양의 새로운 결정상을 관찰하였다. 다이아몬드 막의 경우 질소, 첨가량에 무관하게 질소 혼입향은 측정되지 않을 만큼 적었지만, 육방정 결정상은 Si, C 그리고 N으로 이루어진 SiCN화합물임을 확인하였다.

  • PDF

Thermal Properties of Diamond Films Deposited by Chemical Vapor Depositon

  • Chae, Hee-Baik;Baik, Young-Joon
    • The Korean Journal of Ceramics
    • /
    • 제3권1호
    • /
    • pp.29-33
    • /
    • 1997
  • Four diamond films were deposited by the microwave plasma assisted chemical vapor deposition method varying CH4 concentration from 2.5 to 10% in the feeding gases. Thermal conductivity was measured on these free standing films by the steady state method from 80 K to 400K. They showed higher thermal conductivity as the film deposited with lower methane concentration. One exception, 7.79% methane concentration deposited film, was observed to be the highest thermal conductivity. Phonon scattering processes were considered to analyze the thermal conductivity with the full Callaway model. The grain size and the concentration of the extended and the point defects were used as the fitting parameters. Microstructure of diamond films was investigated with the scanning electron microscopy and Raman spectroscopy.

  • PDF

Opto-Electrochemical Sensing Device Based on Long-Period Grating Coated with Boron-Doped Diamond Thin Film

  • Bogdanowicz, Robert;Sobaszek, Michał;Ficek, Mateusz;Gnyba, Marcin;Ryl, Jacek;Siuzdak, Katarzyna;Bock, Wojtek J.;Smietana, Mateusz
    • Journal of the Optical Society of Korea
    • /
    • 제19권6호
    • /
    • pp.705-710
    • /
    • 2015
  • The fabrication process of thin boron-doped nanocrystalline diamond (B-NCD) microelectrodes on fused silica single mode optical fiber cladding has been investigated. The B-NCD films were deposited on the fibers using Microwave Plasma Assisted Chemical Vapor Deposition (MW PA CVD) at glass substrate temperature of 475 ℃. We have obtained homogenous, continuous and polycrystalline surface morphology with high sp3 content in B-NCD films and mean grain size in the range of 100-250 nm. The films deposited on the glass reference samples exhibit high refractive index (n=2.05 at λ=550 nm) and low extinction coefficient. Furthermore, cyclic voltammograms (CV) were recorded to determine the electrochemical window and reaction reversibility at the B-NCD fiber-based electrode. CV measurements in aqueous media consisting of 5 mM K3[Fe(CN)6] in 0.5 M Na2SO4 demonstrated a width of the electrochemical window up to 1.03 V and relatively fast kinetics expressed by a redox peak splitting below 500 mV. Moreover, thanks to high-n B-NCD overlay, the coated fibers can be also used for enhancing the sensitivity of long-period gratings (LPGs) induced in the fiber. The LPG is capable of measuring variations in refractive index of the surrounding liquid by tracing the shift in resonance appearing in the transmitted spectrum. Possible combined CV and LPG-based measurements are discussed in this work.