• 제목/요약/키워드: MIG Arc Welding

검색결과 47건 처리시간 0.021초

박판알루미늄 고속용접용 펄스MIG 용접특성 (The study of variable polarity AC pulse GMA welding system)

  • 김태진;변영복;조기연;조상명;김철우
    • 전력전자학회:학술대회논문집
    • /
    • 전력전자학회 2002년도 전력전자학술대회 논문집
    • /
    • pp.665-668
    • /
    • 2002
  • Joining thin aluminum alloy is difficult using most wilding techniques. Many of problems associated burn-through by the high heat input Common welding techniques are TIG, MIG, and MIG-PULSE welding. The VP-GMAW provides more control of the heat balance in the voiding arc by taking advantage of the different arc characteristics obtained with each of the two polarities. In this paper, we proposed new VP_GMA Welding method by control DSP 320C32, and the characteristic and experiment result-voltage, current, welding bead. penentraion by this method are presented

  • PDF

모 조선업체 아크 용접 작업자의 공기중 6가 크롬 및 니켈 노출에 관한 연구 (Welder's Exposure to Airborne Hexavalent Chromium and Nickel during Arc Welding in a Shipyard)

  • 신용철;이광용;이나루;오세민;강성규;문영한;이기라
    • 한국산업보건학회지
    • /
    • 제8권2호
    • /
    • pp.209-223
    • /
    • 1998
  • The aim of this study was to evaluate welders' exposure to hexavalent chromium (Cr(VI)) and nickel (Ni) during welding operations in a Korean shipyard. The airborne Cr(VI) and Ni concentrations were measured during metal inert gas (MIG) welding on mild and stainless steel, and manual metal arc (MMA) welding on mild steel. The geometric mean (GM) of Cr(VI) concentrations inside the welding helmet during MIG welding on mild steel were $0.0018mg/m^3$ inside a ship section, and $0.0015-0.0026mg/m^3$ at the welding shops. All of the personal breathing zone air samples were below the American Conference of Governmental Industrial Hygienists (ACGIH) Threshold Limit Value ($TLV^{(R)}$) of $0.01mg/m^3$. Conversely, eighty-eight percent(21 of 24) of the personal breathing zone air samples exceeded the National Institute for Occupational Safety and Health (NIOSH) recommended exposure limit of $0.001mg/m^3$. Ni was not detected on 20 of 23 air samples collected during MIG welding on mild steel. The three Ni samples above the limit of detection ranged from 0.015 to $0.044mg/m^3$. The GM of Cr(VI) concentrations during MMA welding on mild steel were $0.0013mg/m^3$, but Ni was not detected in the air samples during this operation. It is assumed that the airborne Cr(VI) and Ni during mild steel welding were derived from the base metals which contained about 0.03% Cr and 0.03% Ni. The GM of airborne total Cr, Cr(VI) and Ni concentrations during MIG welding on stainless steel were 4.02, 0.13 and $0.86mg/m^3$, respectively, and the levels of Cr(VI) and Ni were above the ACGIH-$TLV^{(R)}$. Cr(VI) comprised about 35.5% of the total chromium(Cr) from MIG welding on mild steel, and about 8.4% of total Cr from MIG welding on stainless steel. The ratios of Cr(VI) to total Cr were significantly different among welding shops. It was concluded that welders were exposed to high levels of Cr(VI) and Ni during welding on stainless steel, and were exposed to low levels of Cr(VI) even during welding on mild steel.

  • PDF

Ar/He 보호가스분위기에서 Al 5083 합금의 대전류 MIG 용접특성 (High Current MIG Welding of Al 5083 Alloy under Ar/He Mixed Gas Shielding)

  • 최영배;황인성;강문진;김동철
    • Journal of Welding and Joining
    • /
    • 제32권1호
    • /
    • pp.87-92
    • /
    • 2014
  • Recently, use of thick Al 5083 plate has increased in production of LNG storage tank. In general, multi-pass welding has been used to achieve sufficient penetration in thick plate welding. High current welding which enables high deposition and deep penetration is preferred in thick plate welding because the increase of number of pass increases manufacturing cost and formation of weld defect. In this study, welding characteristics according to various Ar/He shielding gas composition was investigated in high current MIG welding. The bead-on-plate welding and V groove welding were conducted on Al 5083 alloy with a thickness of .25 mm. The effect of shielding gas composition on bead shape was evaluated and proper shielding gas composition was proposed. Also arc stability was examined under selected shielding gas composition. One side-one pass welding experiments were conducted for V groove specimen with a thickness of 25 mm. Mechanical properties and hardness profiles were measured for the V groove specimens.

Control of surface defects on plasma-MIG hybrid welds in cryogenic aluminum alloys

  • Lee, Hee-Keun;Chun, Kwang-San;Park, Sang-Hyeon;Kang, Chung-Yun
    • International Journal of Naval Architecture and Ocean Engineering
    • /
    • 제7권4호
    • /
    • pp.770-783
    • /
    • 2015
  • Lately, high production rate welding processes for Al alloys, which are used as LNG FPSO cargo containment system material, have been developed to overcome the limit of installation and high rework rates. In particular, plasma-metal inert gas (MIG) hybrid (PMH) welding can be used to obtain a higher deposition rate and lower porosity, while facilitating a cleaning effect by preheating and post heating the wire and the base metal. However, an asymmetric undercut and a black-colored deposit are created on the surface of PMH weld in Al alloys. For controlling the surface defect formation, the wire feeding speed and nozzle diameter in the PMH weld was investigated through arc phenomena with high-speed imaging and metallurgical analysis.

AL5083 합금에 대한 Plasma-GMA 용접에서 분산분석을 이용한 공정변수의 특성 평가 (Weldability Evaluation in Plasma-GMA Hybrid Welding for Al-5083 Using Analysis of Variance)

  • 정진수;이종중;이희근;박영환
    • Journal of Welding and Joining
    • /
    • 제32권1호
    • /
    • pp.28-33
    • /
    • 2014
  • In this paper, I-butt welding with 6mm thickness using Plasma-GMA welding was carried out. And weld characteristics of the Al-5083 aluminium alloy for Plasma-GMA hybrid welding was evaluated. The orthogonal experimental design was used to investigate the influence of plasma-MIG welding parameters such as plasma current, wire feeding rate, MIG-welding voltage and welding speed on the weld bead geometry and tensile strength using the ANOVA(Analysis of Variation). Then we conducted evaluation of contribution for process parameters. ANOVA results show that bead dimensions are affected by wire feeding speed, welding voltage and welding speed and tensile strength is mainly affected by welding speed and plasma arc current. Tensile strength was decreased by rise in plasma welding current because GMA welding current was decreased by plasma arc.

MIG 용접 시 외부 전자기력이 미치는 영향에 관한 연구 (A Study on the Effect of External Electromagnetic force in MIG Welding)

  • 김재성;김용;류덕희;이보영
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 추계학술발표대회 개요집
    • /
    • pp.171-173
    • /
    • 2004
  • Electromagnetic force is one of the most important factor that effect on metal transfer mode, short-circuit rate, spatter generation rate and mechanical properties of weld metal etc. Also, shielding gas and welding current have influence on metal transfer mode in GMAW. In this paper, different ways for external electromagnetic forces are applied by attaching cylindrically rounded conducting wire solenoid on touch tip holding. With the applied electromagnetic field, the arc transfer mode changes from normal mode to rotating mode and spatter generation decreased in electromagnetic fields(N-pole). In MIG welding, the influences of electromagnetic force on the spatter generation showed different tendency as in the $CO_2$ welding. It is possible reasons were discussed.

  • PDF

하이브리드 용접과 레이저 용접에 의한 세립강 용접부의 미세조직변화에 관한 연구 (Microstructure Evolution of UFG Steel Weld by Hybrid and Laser Welding)

  • 동현우;이목영;안용식
    • 동력기계공학회지
    • /
    • 제14권3호
    • /
    • pp.58-63
    • /
    • 2010
  • A laser beam welding and an electric arc welding were combined, and the positive points of each welding method are drawn such as high speed, low thermal load, deep penetration, and high productivity. The fiber laser-MIG conjugated welding. namely the hybrid welding has been studied mainly for the automation industry of a pipeline welding. In this study, the MIG welding was combined with a fiber laser welding to make up the hybrid welding. The weld shapes, microstructures and mechanical properties for weld zones after the hybrid welding or only fiber laser welding were investigated on the 700 MPa grade Ultra Fine Grained(UFG) high strength steel. The amount of acicular ferrite in weld metals and HAZ(heat affected zone) was observed larger after hybrid welding compared with after only laser welding. The Vickers hardness of the top area of the fusion zone after fiber laser welding was higher compared with after hybrid welding.

회주철 프레스 금형에 대한 경화육성 자동 MIG 용접시 균열 및 기공방지 기법의 개발 (The development of prevention technique for crack and porosity occured during hardening overlay auto MIG welding for press die of gray cast iron)

  • 유광선;황재련;김덕환;김병훈;황지선;조상명
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.114-116
    • /
    • 2005
  • There are some problems when weld gray cast iron which is used well in automobile industry with auto MIG welding. the problems are followed like this 1) Occurrence of porosity and hardening organization. 2) Occurrence of crack due to lower elongation of gray cast iron when restraint stress works on. 3) Occurrence of porosity and unstable bead shape due to unstable arc under low current MIG welding.. especially there is a restraint on chemical composition of weld metal because the weldment demands more than 570Hv hardness. so it is hard to use Fe-Ni wire to prevent cracks occured on weldment and new welding method is needed to resolve that problems. This study shows how to prevent porosity and cracks occurring when weld gray cast iron trimming die and shows a new welding method for press die of gray cast iron

  • PDF

MIG-WELDING OF MAGNESIUM ALLOYS WITH PARTICULAR CONSIDERATION OF DROP DETACHMENT

  • Wohlfahrt, H.;Rethmeier, M.;Wiesner, S.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.94-100
    • /
    • 2002
  • During the last years, great progress has been made in the fields of welding power sources and filler materials for the MIG-welding of magnesium alloys. This advice resulted in a better welding process, md, therefore, in highly improved welding results. Furthermore the gap between short-circuiting- and spray-arc-trunsfer could be closed by the triggered short-circuiting- and the short-circuiting-arc with pulse overlay. A crucial contribution to the welding process is the energy input into the filler material. Many problems result from the physical properties of magnesium, for instance its narrow interval between melting point 600$^{\circ}C$ and vaporization point 1100$^{\circ}C$. The energy input into the filler material has to be regulated in such a way that the wire will melt but not vaporize. For th is reason, special characteristics of power sources hue been examined and optimized with the help of high-speed-photographs of the welding process with particular consideration of the drop detachment. An important improvement of the weld seam profile has been achieved by using filler material of only 1.2 mm in diameter. The experiments hue been made with 2.5 mm thick extruded profiles of AZ31 and AZ6l. The results of tensile testing showed strength values of 80 to 100% of the base metal. B ending angles up to 60$^{\circ}$ have been reached. The fatigue strength under reversed bending of the examined magnesium alloys after welding reaches 50% of the strength of the base metal. When the seam reinforcement is ground of the fatigue strength can be raised up to 75% of the base metal.

  • PDF