Manufacture of Medium Density Fiberboard from Exploded MDF Waste (폐 MDF 폭쇄 섬유로부터의 MDF제조)

  • Lee Hwa-Hyoung;Seo In-Su;Cho Youn-Min;Park Han-Sang
    • Journal of the Korea Furniture Society
    • /
    • v.16 no.1
    • /
    • pp.9-16
    • /
    • 2005
  • This study was carried out to displace traditional virgin wood fiber by exploded MDF-waste fiber for the manufacture of medium density fiberboard. MDF waste was exploded in condition of $215^{\circ}C,20$ minutes. The higher the mixing ratio of exploded MDF-waste fiber, the lower the MOR and IB of MDF. There was no difference of formaldehyde emission by desiccator method between virgin wood fiber and exploded MDF-waste fiber. Adding $25^{\circ}C$ of exploded MDF-waste fiber met the KS of MDF 15 type.

  • PDF

Dimensional Change of Melamine Sheet Laminated MDF Flooring by Heating (멜라민시트 적층 MDF 마루판재의 가열에 의한 치수변화)

  • Min, Ill-Hong;Kim, Eui-Sik;Han, Gyu-Seong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.24 no.4
    • /
    • pp.32-39
    • /
    • 1996
  • The overall purpose of this study was to investigate the dimensional changes of melamine sheet laminated medium density fiberboard(MDF) floorings by sub-heating system(Ondol). This study was also conducted to improve the properties of melamine sheet laminated MDF floorings. The effects of density, resin content, manufacturing speed of MDF and types of melamine sheet on dimensional and weight changes of floorings were investigated. The results were as followings. 1. Dimensional and weight change of melamine sheet laminated MDF flooring by heating decreased with decreasing the density of MDF. 2. Dimensional and weight change of melamine sheet laminated MDF flooring by heating decreased with increasing the resin content of MDF. 3. Dimensional and weight change of melamine sheet laminated MDF flooring by heating decreased with decreasing the manufacturing speed of MDF. 4. Dimensional change of melamine sheet laminated MDF flooring in width direction by heating was doubled than that in machine direction. 5. Dimensional change and curling of high pressure melamine laminate(HPM) laminated MDF flooring by heating was less than those of low pressure melamine laminate(LPL) flooring. 6. Weight loss of melamine sheet laminated MDF flooring by heating has linear relationship with shrinkage.

  • PDF

Finger Jointing of MDF by High-frequency Plate Heating (고주파 평면가열에 의한 중밀도섬유판(MDF)의 핑거접합)

  • So, Won-Tek
    • Journal of the Korea Furniture Society
    • /
    • v.17 no.2
    • /
    • pp.25-34
    • /
    • 2006
  • This experiment was carried out to investigate the high-frequency gluing characteristics of poly vinyl acetate emulsion adhesive(PVAc) on MDF edge-glued boards. The edge-glued boards were glued lengthwise with butt, scarf, or finger joint. The wastes of MDF boards were reused as board materials. The obtained results are summarized as follows; the bending strength of edge-glued MDF increased slightly with the HF heating time, but the economically desirable heating time was 6 minutes. The bending and tensile strength of edge-glued MDF were high with scarf, finger and butt joint, in order. The strength of finger jointed MDF showed 80% of scarf jointed MDF. The effects of location of finger joints on the bending strength of edge-glued MDF were larger than those of the numbers of finger joints. The bending strength of edge-glued MDF with one joint on the middle position showed 40% decrease in comparison with non-jointed MDF.

  • PDF

Surface Properties of Fancy Veneer Overlaid Medium Density Fiberboard by Coating (도장처리에 의한 무늬단판 오버레이 MDF의 표면물성)

  • Kim, Jong-In;Park, Jong-Young;Doh, Geum-Hyun;Joung, Doo-Jin;Park, Sang-Bum
    • Journal of the Korea Furniture Society
    • /
    • v.18 no.1
    • /
    • pp.13-19
    • /
    • 2007
  • The influences of coating on oak veneer overlaid Medium Density Fiberboard (MDF) were evaluated. The hardness of 9mm-MDF by hardness test were increased about 28% with coating on MDF and the more increased hardness of 31% with oak veneer overlaid MDF. The hardness of veneer overlaid MDF increased with increment of the veneer thickness and that of overlaid MDF showed the higher hardness compared to non-overlaid MDF. The optimum moisture content in terms of the hardness of panels MDF was in the range of 7% to 10% and the hardness was decreased with increasing of the moisture content. Any cracks were not overlaid coated on the MDF but the cracks were observed on the overlaid MDF after Soak under Vacuum Dry 10-cycle. The thicker veneer-overlaid MDF showed more cracks.

  • PDF

Change in Chemical Compositions of Leachate and Medium Density Fiberboard from a Laboratory-scale Simulated Landfill

  • Lee, Min;Prewitt, Lynn;Mun, Sung Phil
    • Journal of the Korean Wood Science and Technology
    • /
    • v.44 no.2
    • /
    • pp.231-240
    • /
    • 2016
  • The change in chemical compositions of leachate and medium density fiberboard (MDF) from a laboratory-scale simulated landfill which constructed in a plastic container containing alternating layers of soil and MDF was investigated to evaluate decomposing of MDF in soil. Four treatments were conducted: 1) MDF in soil, 2) MDF only, 3) cured UF resin in soil, and 4) soil only. Molecular weight (MW) distribution of compounds in leachate from soil only treatment did not change over time. In UF resin in soil treatment, the MW distribution shifted to a lower MW distribution over time, while the peak shifted to the left indicated changing to higher MW distribution in leachate from treatment 1 and 2 contained MDF. Higher percent nitrogen in leachate was observed in MDF containing treatments due to the UF resin in the MDF. The percent carbon slightly increased in MDF only while that greatly decreased in MDF in soil treatment maybe due to bacterial activity. The percent of extractable materials from the MDF decreased greatly on day 35 compare to day 0, and subsequently did not change much on day 77. In contrast, percent holocellulose and lignin did not change much over time. No structural change of the wood fiber in MDF occurs during the study. Water-soluble materials from MDF in soil contributed the change in chemical composition of leachate.

Long-term Prospect of MDF Production and Supply Plan of Domestic Softwood Log in Korea (국내 MDF생산 장기전망과 국산 침엽수원목 공급방안)

  • Park, Yong Bae;Kim, Chul Sang;Jung, Byung Heon
    • Journal of Korean Society of Forest Science
    • /
    • v.97 no.1
    • /
    • pp.45-52
    • /
    • 2008
  • The objectives of this study are to explain a supply plan of domestic softwood log by long-term prospect of MDF production to stably promote industry of MDF. For it, we developed the long supply function as Ordinary Least Squares Method. Between 2005 and 2050, it was estimated that quantity of domestic production of MDF increased from 1,653 thousand $m^3$ to 2,041 thousand $m^3$. In 2050, quantities of domestic softwood log used by raw materials to product MDF of 2,041 thousand $m^3$ were estimated to be used about 1,355 thousand $m^3$. Exampling Pinus rigida used presently by raw materials to product MDF, cutting area of it is estimated to be 10,828 ha per year. And larch is cutted about 9,160 ha per year. This study estimated annual softwood log cutting amount and total afforestation area at 2050 year by 3 scenarios which are 35%, 45% and 55% about use of domestic softwood log for MDF production. If we do a criterion of cutting area, we advantage to plant larch. But the species of trees are use and growth property. We think that the afforestation policy must be performed on the base of those to supply raw materials of MDF. Although government plans hardwood afforestation policy after cutting Pinus rigida, it needs to support and manage certainly afforestation area of softwoods to need to supply raw materials of MDF to stably promote industry of MDF.

The Effect of Final Moisture Content of Mat on the Physical and Mechanical Properties of UF-bonded MDF (매트의 최종함수율이 요소수지 제조 MDF의 물리·기계적 성질에 미치는 영향)

  • Lee, Hwa-Hyoung;Maloney, Thomas M.
    • Journal of the Korean Wood Science and Technology
    • /
    • v.23 no.4
    • /
    • pp.85-90
    • /
    • 1995
  • 목질보드 제조에 있어 매트의 최종함수율은 에너지가 필요한 목질 엘리먼트의 초기 건조공정이나 열압싸이클공정, 목질보드의 균질정합성, 목질재료의 물리 기계적 성질 및 치수안정에 지대한 영향을 주기 때문에 대단히 중요하다. 지금까지 PB에 대한 최종매트의 함수율에 대한 연구는 많이 보고되어 있으나 요소수지로 제조되는 MDF에 대한 연구보고는 없으며 미국과 한국을 위시한 각국이 MDF의 최종함수율을 PB에 준하여 8~11%로 조정하여 MDF를 제조하고 있다. 따라서 본 연구는 미국산 침엽수 혼합수종으로부터 제조된 가압 해섬섬유와 요소수지로 제조된 MDF의 물리 기계적 성질에 관련된 적정 최종매트 함수율을 규명하고자 실시하여 다음과 같은 결론을 얻었다. 1. 혼합 침엽수 원료로부터 제조된 요소수지제조 MDF의 적정 최종 매트 함수율은 13% 부근으로서 현재 MDF공장에서 적용되고 있는 8~11%보다 높았다. 2 평판이 시작되는 최종매트 함수율은 15.4%였다.

  • PDF

Manufacture of high density Fiberboard from disintergrated and beaten MDF Waste (폐MDF의 해리와 고해처리를 통한 고밀도 Fiber Board제조)

  • Lee, Hwa-Hyoung;Seo, In-Su;Cho, Youn-Min;Park, Han-Sang
    • Journal of the Korea Furniture Society
    • /
    • v.17 no.1
    • /
    • pp.63-71
    • /
    • 2006
  • This study was carried out to resplace traditional virgin wood fiber by recycled MDF-waste fiber for the manufacture of high density fiberboard. For the recycling, MDF waste was disintegrated for 10 minutes and beaten for 15 minutes. There was no difference in formaldehyde emission by desiccator method between virgin wood fiber and disintergrated and beaten MDF-waste fiber. Fiberboard which was maded from 100% of disintergrated and beaten MDF-waste fiber showed similar physical and mechanical properties to those of virgin fiber. The yield of recycled fiber from MDF waste was 85%.

  • PDF

Evaluation of Material Properties of Acetylated Medium Density Fiberboard (MDF) (아세틸화 처리 중밀도 섬유판(MDF)의 재질 평가)

  • LEE, Jong Shin;KIM, Soung Joon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.48 no.3
    • /
    • pp.393-404
    • /
    • 2020
  • This study examined the material properties of MDF manufactured using acetylated pinus radiata fibers against moisture and compared the properties with the fiberboard quality standards of KS F 3200. Since acetylated MDF shows very low moisture content, water absorption and thickness swelling than the quality standards, it is expected to have an excellent dimensional stability. The bending strength in wetting condition of the acetylated MDF reached approximately 70% of the bending strength in dry condition, making it suitable for the quality standards. The internal bond of the acetylated MDF in the wetting condition was higher than the minimum internal bond of the quality standards in the dry condition, showing a good water resistance. Since the water droplet contact angle of the acetylated MDF is larger than that of untreated MDF, it is determined that it contributes in improving the water resistance due to the low wettability.

A Study on the Flame Retardant Performance of MDF Wood According to Flame Retardant Treatment Method (방염처리 방법에 따른 MDF 목재의 방염성능에 관한 연구)

  • Cha, Jung-Min;Hyun, Seong-Ho;Kim, In-Beom;Yoon, Myung-O
    • Fire Science and Engineering
    • /
    • v.25 no.6
    • /
    • pp.146-155
    • /
    • 2011
  • In the study, test was carried out to compare the flame retardant performance for the specimen of MDF wood to which field flame retardant treatment (post processing flame retardant) is applied, which is coated with flame retardant film of 5 companies, locally distributed, and MDF wood (nontreated, flame retardant film non-coated) to which aqueous or oil-based fire-retardant paint is applied. As a result of combustion test of MDF wood which was coated with flame retardant film of 5 companies, 2 products showed suitable values in 4 criteria, but other 3 products showed 10~40 % disqualification rate. In regard of characteristics of fire-retardant paint, oil-based fire-retardant paint is better than aqueous fire-retardant paint in flame retardant performance criteria, but MDF wood to which oilbase fire-retardant paint was applied was shown to have higher toxicity index grade than MDF wood to which aqueous fire-retardant paint was applied relatively.