• 제목/요약/키워드: Low-temperature oxidation

검색결과 589건 처리시간 0.026초

LTCC를 소재로 하는 마이크로 리포머의 최적 설계에 관한 연구 ; 일체형 Reformer/PROX 반응기의 설계 및 성능평가 (A Study on the Optimum Design for LTCC Micro-Reformer: Design and performance evalution of monolith fuel reformer/PROX)

  • 정찬화;오정훈;장주희;정명기
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2006년도 추계학술대회 논문집
    • /
    • pp.615-616
    • /
    • 2006
  • A micro-fuel processor system integrating steam reformer and partial oxidation reactor was manufactured using low temperature cofired ceramic (LTCC). A CuO/ZnO/$Al_2O_3$ catalyst and Pt-based catalyst prepared by wet impregnation were used for steam reforming and partial oxidation, respectively. The performance of the LTCC micro-fuel processor was measured at various operating conditions such as the effect of the feed flow rate, the ratio of $H_2O/CH_3OH$, and the operating temperature on the LTCC reformer and CO clean-up system. The catalyst layer was loaded with "Fill and Dry" coating for small volume. The product gas was composed of $70\sim75%$ hydrogen, $20\sim25%$ carbon dioxide, and $1\sim2%$ carbon monoxide at $250\sim300^{\circ}C$, respectively.

  • PDF

산화탄소나노튜브를 이용한 메탄 하이드레이트 형성 (Effect of Oxidation Multi-Walled Carbon Nanotubes for Methane Hydrate Formation)

  • 박성식;김남진
    • 한국태양에너지학회 논문집
    • /
    • 제30권5호
    • /
    • pp.11-16
    • /
    • 2010
  • Methane hydrate is crystalline ice-like compounds which formed methane gas enters within water molecules composed cavity and each other from physically-bond at specially temperature and pressure condition. $1m^3$ of methane hydrate can be decomposed into the maximum of $216m^3$ of methane gas under standard condition. If these characteristics of hydrate are utilized in the opposite sense, natural gas can be fixed into water in the form of a hydrate solid. Therefore the use of hydrate is considered to be a great way to transport and store natural gas in large quantity. However, when methane hydrate is formed artificially, the amount of gas that is consumed is relatively low, due to the slow reaction rate between water and methane gas. Therefore for practical purposes in the application, the present investigation focuses on increasing the amount of gas consumed by adding chemically oxidized OMWCNTs to pure water. The results show that when 0.003 wt% of oxidation multi-walled carbon nanotubes was added to pure water, the amount of gas consumed was almost four times more than that of pure water indicating its effect in hydrate formation and the hydrate formation time decreased at alow subcooling temperature.

디젤입자상물질 여과장치의 배기저감성능 효과 분석 (An Investigation of the Effect of Diesel Particulate Filter for Heavy-duty Diesel Engine on Emission Reduction)

  • 박용희;신대윤
    • 한국환경보건학회지
    • /
    • 제33권1호
    • /
    • pp.36-42
    • /
    • 2007
  • Diesel PM can be controlled using Diesel Particulate Filter, which can effectively reduce the level of soot emissions to ambient background levels. In the Heavy Duty Diesel area, the Continuously Regeneration trap has been widely applied in the retrofit market. As the Special act for the improvement of air quality in the capital area, the retrofit program for DPF to used diesel vehicle has progressed favorably and there are currently over 1,000 of these DPF in use in retrofit applications in korea. These DPF comprise a specially formulated Diesel Oxidation Catalyst upstream of a DPF. The $NO_2$ generated by the DOC is used to combust the carbon collected in the DPF at low temperature. To certificate DPF device that is suitable to domestic circumstances, it is necessary to evaluate exactly the DPF devices according to the regulation of DPF certificate test procedure for retrofit(ministry of environment(MOE) announcement NO. 2005-16). To do so the understand of that regulation like the standard of PM reduction rate is needed. In this study the test procedure including test cycle and BPT test condition was examined and also the test result for specific DPF was analyzed. In every test like field test, PM reduction efficiency test and seoul-10 mode test, no defect could be showed.

TGA를 이용한 가교폴리에틸렌의 방사선 열화 평가 (Evaluation of Radiation Degradation or Crosslinked Polyethylene using TGA)

  • 이청;김기엽;류부형;임기조
    • 한국안전학회지
    • /
    • 제18권2호
    • /
    • pp.50-55
    • /
    • 2003
  • Radiation degradation of crosslinked polyethylene(XLPE) was investigated using thermogravimetric analysis(TGA), The results of TGA were compared with FT-IR, melting temperature, oxidation induction time, and elongation at break on the XLPE exposed by $\gamma$-ray. 5% decomposition temperature of $\gamma$-ray irradiated XLPE showed similar tendencies with the case of elongation at break. Both properties agreed below 1000 KGy, however, did not show any remarkable characteristics above 1000 kGy, these properties can be useful to evaluate the radiation degradation of XLPE for only low irradiated region. Above 1000 kGy, the thermal decomposition activation energy showed decreased, on the contrary, increasing below 1000 kGy. Compared with FT-IR spectrum of irradiated XLPE, it was confirmed that the oxidation reaction was still occurring below 1000 kGy. Radiation degradation of XLPE was dependent upon the irradiation doses, TGA can be a useful tool to evaluate the degradation.

태양 선택흡수막의 특성 분석 (Property Analysis of Solar Selective Coatings)

  • 이길동
    • 한국태양에너지학회 논문집
    • /
    • 제33권4호
    • /
    • pp.31-38
    • /
    • 2013
  • The chemical composition of the black Cr solar selective coatings electrodeposited were investigated for property analysis by using a XPS(X-ray photoelectron spectroscopy) before and after annealing in air at $300^{\circ}C{\sim}500^{\circ}C$ for 120 hours. Black Cr selective coating exposed by solar radiation for 5 months was compared with annealed sample. In addition, The Cu solar selective coatings were prepared by thermal oxidation method for low temperature application. The samples obtained were characterized by using the optical reflectance measurements by using a spectrometer. Optical properties of oxidized Cu solar coatings were solar absorptance $({\alpha}){\simeq}0.62$ and thermal emittance $({\epsilon}){\simeq}0.41(100^{\circ}C)$. In the as-prepared Cr black selective coating, the surface of the coating was found to have Cr hydroxide and Cr. The Cr hydroxide of the major component was converted to $Cr_2O_3$ or $CrO_3$ form after annealing at $500^{\circ}C$ with the desorption of water molecules. The black Cr selective coating was degraded significantly at temperature of $500^{\circ}C$. The main optical degradation modes of this coating were diffusion of Cu substrate materials.

저압 침탄에 의한 Ti-6Al-4V 합금의 표면 특성 개선 (Improvement of Surface Properties of Ti-6A1-4V Alloy by Low Pressure Carburizing)

  • 김지훈;박종덕;김성완
    • 열처리공학회지
    • /
    • 제16권4호
    • /
    • pp.191-196
    • /
    • 2003
  • For improvement of the wear performance of Ti alloy, vacuum-carburizing technique was tried for the first time using propane atmosphere. During the low pressure carburizing carbide was formed at the surface and carbon transfer was occurred from the carbide to the matrix. It was found that: (i) surface hardness increased with the reduction of operating pressure and time; (ii) optimum hardness distribution could be obtained with the proper choice of temperature and carbon flux control; and, (iii) case depth was largely influenced not by time but by temperature. The two steps process was recommended for obtaining thick case depth and high surface hardness of Ti alloy. For the low oxygen partial pressure, it was necessary to introduce additional CO gas to the atmosphere.Grain boundary oxidation and non-uniformity could be prevented.

저장조건(貯藏條件)이 들깨유(油) 및 참깨유(油)의 산패도(酸敗度)에 미치는 영향(影響) (Effects of Storage Conditions on Rancidity of Perilla and Sesame Seed Oils)

  • 김혜경;이양자;이기열
    • Journal of Nutrition and Health
    • /
    • 제12권1호
    • /
    • pp.51-58
    • /
    • 1979
  • It is a general trend everywhere that the uses of vegetable oils are increasing due to the fact that they are effective in curing and preventing symptoms of high blood pressure and various heart failure conditions. At the same time the concept that oxidative rancidity is caused by the oxidation of unsaturated fatty acid moieties whose subsequent decomposition gives rise to various undesirable, sometimes toxic compounds is now well accepted. Linolenic acid (C, 18:3) is one of highly unsaturated and readily oxidizable fatty acid. The content of this essential polyunsaturated fatty acid in perilla seed oil (PSO) was found to be as high as 48% while only 1.5% in sesame seed oil (SSO). In this experiment the oxidative stability of PSO was compared with that of SSO. The experimental test group were as follows: A) Stored at different temperatures, namely $4^{\circ}C,\;30^{\circ}C,$ and $60^{\circ}C,$ B) Stored at room temperature $(20{\pm}5^{\circ}C)$ ; a. protected from sunlight and air, b. exposed to air without sunlight c. exposed to sunlight but protected front air, d. completely exposed to both air and sunlight. The following results were obtained; 1) It was found to be most stable against oxidation to store both PSO and SSO under the low temperature $(4^{\circ}C)$ condition. According to P.V. measurements it was found to be safe to keep both oils up to $30^{\circ}C$ for at least 8 weeks. When exposed to air, sunlight and high temperature $(60^{\circ}C)$, P.V. of PSO reached there peak values, which were much higher than those of SSO. This explains much of its instability as compared to SSO against oxidation. 2) The effect of high temperature $(60^{\circ}C)$ on A.V. was found to be more striking than those of all the other storage conditions. The condition of refrigeration was most effective in keeping A.V. low for both oils as was the case in P.V. 3) For both oils, I.V. decreased throughout the experimental period (8 weeks). The range of decrement was larger for PSO than SSO. 4) There was no significant change in the compositions of fatty acids of SSO caused by various experimental storage conditions. But for PSO the compositions of stearic, oleic and linoleic acid were decreased, whereas linolenic acid was increased proportionally.

  • PDF

Al-Ce 산화물에 담지된 CuO 촉매상에서 저온 CO산화반응 (Low Temperature CO Oxidation over CuO Catalyst Supported on Al-Ce Oxide Support)

  • 박정현;윤현기;신채호
    • Korean Chemical Engineering Research
    • /
    • 제55권2호
    • /
    • pp.156-162
    • /
    • 2017
  • CuO의 함량이 반응활성에 미치는 영향을 조사하기 위하여 CuO(x)/0.3Al-0.7Ce (x = 2~20 wt%) 촉매를 함침법으로 제조하고 저온 CO 산화반응을 수행하였다. CuO(10)/0.3Al-0.7Ce 촉매가 반응물 중 수분의 존재 유무에 관계없이 가장 우수한 반응활성을 나타내었다. 수분의 존재는 활성점에 CO와의 경쟁흡착으로 활성점이 감소하여 50% CO 전환율 온도인 $T_{50%}$가 약 $50^{\circ}C$ 고온으로 이동되어 관찰되었다. $N_2O$-적정실험으로 구한 구리 표면적과 CO-펄스 실험으로 계산된 격자산소의 양은 CuO의 함량 증가에 따라 증가하였고, CuO(10)/0.3Al-0.7Ce 촉매에서 최대화되었다. 이러한 특성 분석결과는 사용된 촉매의 CO 산화반응에 대한 $T_{50%}$의 경향과 잘 일치하였다. 위의 특성분석 결과로부터, CuO(x)/0.3Al-0.7Ce 촉매의 CO 산화반응에 대한 반응성은 구리 표면적과 격자산소의 양과 밀접하게 관련된다고 결론지을 수 있다.

분쇄 방법 및 하소온도에 따른 Doner-doped BaTiO3의 전기적 특성 (Electrical Properties of Donor-doped BaTiO3 Ceramics by Attrition Milling and Calcination Temperature)

  • 이정철;명성재;전명표;조정호;김병익;신동욱
    • 한국전기전자재료학회논문지
    • /
    • 제21권3호
    • /
    • pp.217-221
    • /
    • 2008
  • In this study, We have been investigated the effect of calcination temperature and high-energy ball-milling of powder influences the $BaTiO_3$-based PTCR(Positive Temperature coefficient Resistance) characteristics and microstructure. The mixed powder was obtained from $BaCO_3$, $TiO_2$, $CeO_2$ ball-milled in attrition mill. The mixed powder was calcine from 1000 $^{\circ}C$ to 1200 $^{\circ}C$ in air and then it was sintered in reduction- re-oxidation atmosphere. As a result, The room-temperature electrical resistivity decreased and increased with increasing calcination temperature. specially, Attrition milled powder could have low room-temperature resistivity and high PTC jump order at 1100 $^{\circ}C$. attrition milling had lower room-temperature resistivity than ball milling. Particle size decreased by Attrition milling of powder influences in calcination temperature and room-temperature resistivity.

운전조건에 따른 O3/UV, TiO2/UV 및 O3/TiO2/UV 시스템의 BTEX 증기처리에 관한 비교 연구 (A Comparative Study on Degradation of BTEX Vapor by O3/UV, TiO2/UV, and O3/TiO2/UV System with Operating Conditions)

  • 김경진;박옥현
    • 한국대기환경학회지
    • /
    • 제24권1호
    • /
    • pp.91-99
    • /
    • 2008
  • A multilayer tower-type photoreactor, in which $TiO_2$-coated glass-tubes were installed, was used to measure the vapor-phase BTEX removal efficiencies by ozone oxidation ($O_3$/UV), photocatalytic oxidation ($TiO_2$/UV) and the combination of ozone and photocatalytic oxidation ($O_3/TiO_2$/UV) process, respectively. The experiments were conducted under various relative humidities, temperatures, ozone concentrations, gas flow rates and BTEX concentrations. As a result, the BTEX removal efficiency and the oxidation rate by $O_3/TiO_2$/UV system were highest, compared to $O_3$/UV and $TiO_2$/UV system. The $O_3/TiO_2$/UV system accelerated the low oxidation rate of low-concentration organic compounds and removed organic compounds to a large extent in a fixed volume of reactor in a short time. Therefore, $O_3/TiO_2$/UV system as a superimposed oxidation technology was developed to efficiently and economically treat refractory VOCs. Also, this study demonstrated feasibility of a technology to scale up a photoreactor from lab-scale to pilot-scale, which uses (i) a separated light-source chamber and a light distribution system, (ii) catalyst fixing to glass-tube media, and (iii) unit connection in series and/or parallel. The experimental results from $O_3/TiO_2$/UV system showed that (i) the highest BTEX removal efficiencies were obtained under relative humidity ranging from 50 to 55% and temperature ranging from 40 to $50^{\circ}C$, and (ii) the removal efficiencies linearly increased with ozone dosage and decreased with gas flow rate. When applying Langmuir-Hinshelwood model to $TiO_2$/UV and $O_3/TiO_2$/UV system, reaction rate constant for $O_3/TiO_2$/UV system was larger than that for $TiO_2$/UV system, however, it was found that adsorption constant for $O_3/TiO_2$/UV system was smaller than that for $TiO_2$/UV system due to competitive adsorption between organics and ozone.