• Title/Summary/Keyword: Low cycle fatigue

Search Result 346, Processing Time 0.027 seconds

A Study on the Cyclic Hardening Property and the Low Cycle Fatigue Behavior of Marine Materials (박용재료(舶用材料)의 반복경화(反復硬化) 및 저(低)싸이클 피로특성(疲勞特性)에 관한 연구)

  • S.M. Cho;K. Horikawa
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.28 no.1
    • /
    • pp.108-116
    • /
    • 1991
  • In the non-linear behavior of many materials, there is difference between the monotonic behavior by static load and the cyclic behavior by cyclic load. In particular, the short fatigue cracks to propagate in elasto-plastic stress concentrations(notches), are governed significantly by the cyclic behavior of materials. Accordingly, it is needed to investigate and compare the monotonic and cyclic behavior of materials. In the pressent study, the stress-strain relations of materials by monotonic and cyclic load tests were examined for 2 kinds of steels(SS41, HT80) and 5 kinds of Al-alloys(A5083-O, A6N01-T5, A7N01-T4, A7016-T6, A7178-T6). And the constants for mechanical properties of the materials were determined by experimental results, Moreover, when a notch was subjected to cyclic load, the effect of cyclic hardening property of materials on the variation of stress-strain amplitude in the notch tip was discussed by the application of Neuber's rule and experiments for a center notched plate.

  • PDF

Research of Diffusion Bonding of Tungsten/Copper and Their Properties under High Heat Flux

  • Li, Jun;Yang, Jianfeng
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.14-14
    • /
    • 2011
  • W (tungsten)-alloys will be the most promising plasma facing armor materials in highly loaded plasma interactive components of the next step fusion reactors due to its high melting point, high sputtering resistance and low deuterium/tritium retention. The bonding technology of tungsten to Cu alloy was one of the key issues. In this paper, W/CuCrZr diffusion bonding has been performed successfully by inserting pure metal interlay. The joint microstructure, interfacial elements migration and phase composition were analyzed by SEM, EDS, XRD, and the joint shear strength and micro-hardness were investigated. The mock-ups were fabricated successfully with diffusion bonding and the cladding technology respectively, and the high heat flux test and thermal fatigue test were carried out under actively cooling condition. When Ni foil was used for the bonding of tungsten to CuCrZr, two reaction layers, Ni4W and Ni(W) layer, appeared between the tungsten and Ni interlayer with the optimized condition. Even though Ni4W is hard and brittle, and the strength of the joint was oppositely increased (217 MPa) due primarily to extremely small thicknesses (2~3 ${\mu}m$). When Ti foil was selected as the interlayer, the Ti foil diffused quickly with Cu and was transformed into liquid phase at $1,000^{\circ}C$. Almost all of the liquid was extruded out of the interface zone under bonding pressure, and an extremely thin residual layer (1~2 ${\mu}m$) of the liquid phase was retained between the tungsten and CuCrZr, which shear strength exceeded 160 MPa. When Ni/Ti/Ni multiple interlayers were used for bonding of tungsten to CuCrZr, a large number of intermetallic compound ($Ni_4W/NiTi_2/NiTi/Ni_3T$) were formed for the interdiffusion among W, Ni and Ti. Therefore, the shear strength of the joint was low and just about 85 MPa. The residual stresses in the clad samples with flat, arc, rectangle and trapezoid interface were estimated by Finite Element Analysis. The simulation results show that the flat clad sample was subjected maximum residual stress at the edge of the interface, which could be cracked at the edge and propagated along the interface. As for the rectangle and trapezoid interface, the residual stresses of the interface were lower than that of the flat interface, and the interface of the arc clad sample have lowest residual stress and all of the residual stress with arc interface were divided into different grooved zones, so the probabilities of cracking and propagation were lower than other interfaces. The residual stresses of the mock-ups under high heat flux of 10 $MW/m^2$ were estimated by Finite Element Analysis. The tungsten of the flat interfaces was subjected to tensile stresses (positive $S_x$), and the CuCrZr was subjected to compressive stresses (negative $S_x$). If the interface have a little microcrack, the tungsten of joint was more liable to propagate than the CuCrZr due to the brittle of the tungsten. However, when the flat interface was substituted by arc interfaces, the periodical residual stresses in the joining region were either released or formed a stress field prohibiting the growth or nucleation of the interfacial cracks. Thermal fatigue tests were performed on the mock-ups of flat and arc interface under the heat flux of 10 $MW/m^2$ with the cooling water velocity of 10 m/s. After thermal cycle experiments, a large number of microcracks appeared at the tungsten substrate due to large radial tensile stress on the flat mock-up. The defects would largely affect the heat transfer capability and the structure reliability of the mock-up. As for the arc mock-up, even though some microcracks were found at the interface of the regions, all microcracks with arc interface were divided into different arc-grooved zones, so the propagation of microcracks is difficult.

  • PDF

A STUDY ON THE RESISTANCE OF WEAR AND CYTOTOXICITY OF THE TITANIUM SURFACE AFTER FILM DEPOSITIONS (박막증착시 티타늄 표면의 마손저항도와 세포독성에 관한 연구)

  • Kim Hyung-Woo;Kim Chang-Whe;Kim Yung-Soo
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.39 no.1
    • /
    • pp.84-95
    • /
    • 2001
  • Titanium is widely used in dentistry for its low density, high strength, fatigue resistance, corrosion resistance, and biocompatibility. But it has a tendency of surface damage under circumstance of friction and impact for its low hardness of the surface. Coating is one of methods fir increasing surface hardness. Its effect is to improve surface physical characteristics without change of titanium. Diamond-like carbon and titanium nitride are known for its high hardness of the surface. So that this study was aimed at the wear test and the cytotoxicity test of the commercially pure titanium and Ti-6Al-4V alloy which were deposited by diamond-like carbon film or titanium nitride film to acertain improvement of the surface hardness and the biocompatibility. A disk (25mm diameter, 2mm thickness) was made of commercially pure titanium and Ti-6Al-4V alloy and these substrates were deposited by diamond-like carbon film or titanium nitride film. Diamond-like carbon film was deposited by the method of radiofrequency plasma assisted chemical vapor deposition and titanium nitride film was deposited by the method of reactive arc ion plating. Then these substrates were tested about wear characteristics by the pin-on-disk type wear tester in which ruby ball was used as a wear causer under the load of 32N, The fracture cycles were measured by rotating the substrates until their films were fractured. The wear volume was measured after 150 cycles and 3,000 cycles using surface profiler. The cytotoxicity test was peformed by the method of the MTT assay. The results were as follows : 1. In the results of the wear volume test, commercially pure titanium and titanium alloy which were coated by diamond-like carbon film or titanium nitride aim had higher resistance against wear than the substrates which were not coated by any films (P<0.05). 2. In the results of the fracture cycle test and the wear volume test, diamond-like carbon film had higher resistance against wear than titanium nitride film (P<0.05). 3. In both coatings of diamond-like carbon aim and titanium nitride film, Ti-6Al-4V alloy had higher resistance against wear than commercially pure titanium (P<0.05) 4. In the results of the cytotoxicity test, diamond-like carbon film and titanium nitride film had little cytotoxicity as like commercially pure titanium or Ti-6Al-4V alloy (P>0.05).

  • PDF

Clinical Observation on Recombinant Human Endostatin Combined with Chemotherapy for Advanced Gastrointestinal Cancer

  • Gao, Shao-Rong;Li, Lu-Ming;Xia, Hai-Ping;Wang, Guang-Ming;Xu, Hong-Yan;Wang, Ai-Rong
    • Asian Pacific Journal of Cancer Prevention
    • /
    • v.16 no.9
    • /
    • pp.4037-4040
    • /
    • 2015
  • Objective: To explore the clinical efficacy and toxic and side effects of recombinant human endostatin (rhendostatin/endostar) combined with chemotherapy in the treatment of advanced gastric cancer. Materials and Methods: A total of 70 patients with advanced gastrointestinal adenocarcioma confirmed by histopathology and/or cytological examination were divided into group A (37 patients) and group B (33 patients). Patients in group A were given intravenous drip of 15 mg endostar added into 500 mL normal saline, once every other day until the cessation of chemotherapy or patients' maximal tolerance to chemotherapy. Patients in group B received chemotherapy alone. Two groups selected the same chemotherapy regimens. FOLFIRI scheme: 90-min intravenous drip of $180mg/m^2$ irinotecan, intravenous drip of $200mg/m^2$ calcium folinate (CF) and $400mg/m^2$ 5-fluorouracil (5-Fu) on d1, and continuous intravenous pumping of 2 $400mg/m^2$ 5-Fu for 46 h. FOLFOX4 scheme: intravenous injection of $85mg/m^2$ oxaliplatin (L-OHP), $200mg/m^2$ calcium folinate (CF) and $400mg/m^2$ 5-FU on d1 for 2 h, and then continuous intravenous pumping of 2 $400mg/m^2$ 5-Fu for 46 h. XELOX scheme: oral administration of 1 $500mg/m^2$ xeloda (or tegafur 50~60 mg) in twice during d1~14 and intravenous drip of $135mg/m^2$ L-OHP on d1 for 2 h. The modified FOLFOX scheme: intravenous injection of $135mg/m^2$ L-OHP on d1 for 2 h, $200mg/m^2$ CF and 1.0 g tegafur during d1~5. Whereas, control Group B received chemotherapy regimens which were same as Group A, but no addition of endostar. Before chemotherapy, patients were given intravenous injection of 8 mg ondansetron, intramuscular injection of 10 mg metoclopramide and 20 mg diphenhydramine for prevention of vomiting, protection of liver and stomach as well as symptomatic supportive treatment. One cycle was 21 d, 4~6 cycles in total. The efficacy was evaluated every 2 cycles. Results: 32 patients in Group A could be evaluated, and the response rate (RR) and disease control rate (DCR) were 59.38% and 78.13%, respectively. 31 patients in Groups could be evaluated, and the RR and DCR were 32.26% and 54.84%, respectively. The differences between 2 groups were significant. The toxic effects include myelosuppression, gastrointestinal reaction, fatigue, cardiotoxicity and peripheral neurotoxicity. Conclusions: Preliminary observations show that endostar (once every other day) combined with chemotherapy is effective in the treatment of advanced gastrointestinal cancer, with low toxic effects, good tolerance, deserving further study.

Cyclic Seismic Performance of RBS Weak-Axis Welded Moment Connections (RBS 약축 용접모멘트접합부의 내진성능 평가)

  • Lee, Cheol Ho;Jung, Jong Hyun;Kim, Sung Yong
    • Journal of Korean Society of Steel Construction
    • /
    • v.27 no.6
    • /
    • pp.513-523
    • /
    • 2015
  • In steel moment frames constructed of H-shapes, strong-axis moment connections should be used for maximum structural efficiency if possible. And most of cyclic seismic testing, domestic and international, has been conducted for strong-axis moment connections and cyclic test data for weak-axis connections is quite limited. However, when perpendicular moment frames meet, weak-axis moment connections are also needed at the intersecting locations. Especially, both strong- and weak-axis moment connections have been frequently used in domestic practice. In this study, cyclic seismic performance of RBS (reduced beam section) weak-axis welded moment connections was experimentally investigated. Test specimens, designed according to the procedure proposed by Gilton and Uang (2002), performed well and developed an excellent plastic rotation capacity of 0.03 rad or higher, although a simplified sizing procedure for attaching the beam web to the shear plate in the form of C-shaped fillet weld was used. The test results of this study showed that the sharp corner of C-shaped fillet weld tends to be the origin of crack propagation due to stress concentration there and needs to be trimmed for the better weld shape. Different from strong-axis moment connections, due to the presence of weld access hole, a kind of CJP butt joint is formed between the beam flange and the horizontal continuity plate in weak-axis moment connections. When weld access hole is large, this butt joint can experience cyclic local buckling and subsequent low cycle fatigue fracture as observed in this testing program. Thus the size of web access hole at the butt joint should be minimized if possible. The recommended seismic detailing such as stickout, trimming, and thicker continuity plate for construction tolerance should be followed for design and fabrication of weak-axis welded moment connections.

Cyclic Seismic Testing of Cruciform Concrete-Filled U-Shape Steel Beam-to-H Column Composite Connections (콘크리트채움 U형합성보-H형강기둥 십자형 합성접합부의 내진성능)

  • Park, Chang-Hee;Lee, Cheol-Ho;Park, Hong-Gun;Hwang, Hyeon-Jong;Lee, Chang-Nam;Kim, Hyoung-Seop;Kim, Sung-Bae
    • Journal of Korean Society of Steel Construction
    • /
    • v.23 no.4
    • /
    • pp.503-514
    • /
    • 2011
  • In this research, the seismic connection details for two concrete-filled U-shape steel beam-to-H columns were proposed and cyclically tested under a full-scale cruciform configuration. The key connecting components included the U-shape steel section (450 and 550 mm deep for specimens A and B, respectively), a concrete floor slab with a ribbed deck (165 mm deep for both specimens), welded couplers and rebars for negative moment transfer, and shear studs for full composite action and strengthening plates. Considering the unique constructional nature of the proposed connection, the critical limit states, such as the weld fracture, anchorage failure of the welded coupler, local buckling, concrete crushing, and rebar buckling, were carefully addressed in the specimen design. The test results showed that the connection details and design methods proposed in this study can well control the critical limit states mentioned above. Especially, the proposed connection according to the strengthening strategy successfully pushed the plastic hinge to the tip of the strengthened zone, as intended in the design, and was very effective in protecting the more vulnerable beam-to-column welded joint. The maximum story drift capacities of 6.0 and 6.8% radians were achieved in specimens A and B, respectively, thus far exceeding the minimumlimit of 4% radians required of special moment frames. Low-cycle fatigue fracture across the beam bottom flange at a 6% drift level was the final failure mode of specimen A. Specimen B failed through the fracture of the top splice plate of the bolted splice at a very high drift ratio of 8.0% radian.