Effect of machining precision of single ceramic restorations on the marginal and internal fit (단일 도재 수복물의 가공 정밀도가 변연 및 내면 적합도에 미치는 영향)

  • Son, Keunbada;Yu, Beom-Young;Lee, Kyu-Bok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.58 no.4
    • /
    • pp.313-320
    • /
    • 2020
  • Purpose: The purpose of this study was to evaluate the machining precision and the marginal and internal fit of single restorations fabricated with three types of lithium disilicate ceramic blocks and to evaluate the correlation. Materials and methods: Single restorations were designed using a CAD software program. The crown designed model file was extracted from the CAD software program. Three types of lithium disilicate blocks (Rosetta; HASS, IPS e.max CAD; Ivoclar vivadent, VITA Suprinity; VITA) were milled using a milling machine. For the fabrication of the crown scanned model file, the intaglio surface of the restoration was digitized using a contact scanner. Then, using the three-dimensional inspection software (Geomagic control X; 3D Systems), the process of the overlap of the crown designed model and the scanned model and 3-dimensional analysis was conducted. In addition, the marginal and internal fit of the crowns was evaluated by a silicone replication method. The difference among three types of single ceramic crown was analyzed using a Kruskal-Wallis H test, and Spearman correlation analysis was performed to analyze the correlation between machining precision and fitness (α=.05). Results: There was a significant difference in the machining precision and the marginal and internal fit according to the type of ceramic block (P<.001). In addition, the machining precision and the marginal and internal fit were positively correlated (P<.001). Conclusion: The marginal fit of crowns fabricated according to the types of ceramic blocks was within the clinically acceptable range (< 120 ㎛), so it can be regarded as appropriate machining precision applicable to all clinical as aspects in terms of the marginal fit.

In vivo wear determination of novel CAD/CAM ceramic crowns by using 3D alignment

  • Aladag, Akin;Oguz, Didem;Comlekoglu, Muharrem Erhan;Akan, Ender
    • The Journal of Advanced Prosthodontics
    • /
    • v.11 no.2
    • /
    • pp.120-127
    • /
    • 2019
  • PURPOSE. To determine wear amount of single molar crowns, made from four different restoratives, and opposing natural teeth through computerized fabrication techniques using 3D image alignment. MATERIALS AND METHODS. A total of 24 single crowns (N = 24 patients, age range: 18 - 50) were made from lithium disilicate (IPS E-max CAD), lithium silicate and zirconia based (Vita Suprinity CAD), resin matrix ceramic material (Cerasmart, GC), and dual matrix (Vita Enamic CAD) blocks. After digital impressions (Cerec 3D Bluecam, DentsplySirona), the crowns were designed and manufactured (Cerec 3, DentsplySirona). A dualcuring resin cement was used for cementation (Variolink Esthetic DC, Ivoclar). Then, measurement and recording of crowns and the opposing enamel surfaces with the intraoral scanner were made as well as at the third and sixth month follow-ups. All measurements were superimposed with a software (David-Laserscanner, V3.10.4). Volume loss due to wear was calculated from baseline to follow-up periods with Siemens Unigraphics NX 10 software. Statistical analysis was accomplished by Repeated Measures for ANOVA (SPSS 21) at = .05 significance level. RESULTS. After 6 months, insignificant differences of the glass matrix and resin matrix materials for restoration/enamel wear were observed (P>.05). While there were no significant differences between the glass matrix groups (P>.05), significant differences between the resin matrix group materials (P<.05) were obtained. Although Cerasmart and Enamic were both resin matrix based, they exhibited different wear characteristics. CONCLUSION. Glass matrix materials showed less wear both on their own and opposing enamel surfaces than resin matrix ceramic materials.

Influences of luting cement shade on the color of various translucent monolithic zirconia and lithium disilicate ceramics for veneer restorations

  • Ghada Alrabeah;Nawaf Alamro;Atif Alghamdi;Ahmed Almslam;Meshari Azaaqi
    • The Journal of Advanced Prosthodontics
    • /
    • v.15 no.5
    • /
    • pp.238-247
    • /
    • 2023
  • PURPOSE. The purpose of this study was to assess the effect of resin cement shade on the color of different novel ultratranslucent monolithic zirconia and lithium disilicate veneer materials. MATERIALS AND METHODS. For a total of 40 specimens, flat cylindrical discs with a 9-mm diameter and 0.5-mm thickness were created using CAD/CAM technology. The specimens were divided into five groups according to their material (n = 8) (e.max, Prettau, Aidite, Shofu and Dima) using A1 shade. Resin discs with the same diameter and shade as the specimens served as tooth-colored substructures. Three shades (neutral, light and warm) of resin cement try-in pastes (Variolink Esthetic LC) were used as the luting cement material. The color of each material group was measured before and after cementation using the three cement shades, and the CIE L*a*b* coordinates were obtained with a spectrophotometer. Values for the translucency parameter (TP) and color change delta E (E) before (baseline) and after cementation of each specimen were determined. To compare differences among the material groups within each shade of cement and among various shades of cement within each material, the data were analyzed using one-way ANOVA and post hoc testing. RESULTS. Color coordinates L*, a* and b* significantly changed after the application of try-in pastes relative to baseline values, with a noticeable decrease in lightness (L*) (P < .05). A significant color change (ΔE) was observed in all tested materials after cementation, with ΔE values exceeding 3.3 (P < .05). Although TP changed after cementation for most materials tested, these changes were not statistically significant (P > .05). Shofu and Dima ceramics showed the lowest TP values, while Aidite and Prettau showed the highest TP values. For e.max, translucency decreased after cementation with neutral and warm shades, and it significantly increased after cementation with a light shade. CONCLUSION. The shade of cement significantly altered the final color of the ceramic veneer material to a level above the threshold at which the clinical perception of color change occurred (> 3.3). The TP was not influenced by the cement shade. The translucency levels of the novel ultratranslucent multilayer monolithic zirconia ceramics Aidite and Prettau were higher than that of the lithium disilicate e.max material.

Biocompatibility study of lithium disilicate and zirconium oxide ceramics for esthetic dental abutments

  • Brunot-Gohin, Celine;Duval, Jean-Luc;Verbeke, Sandra;Belanger, Kayla;Pezron, Isabelle;Kugel, Gerard;Laurent-Maquin, Dominique;Gangloff, Sophie;Egles, Christophe
    • Journal of Periodontal and Implant Science
    • /
    • v.46 no.6
    • /
    • pp.362-371
    • /
    • 2016
  • Purpose: The increasing demand for esthetically pleasing results has contributed to the use of ceramics for dental implant abutments. The aim of this study was to compare the biological response of epithelial tissue cultivated on lithium disilicate ($LS_2$) and zirconium oxide ($ZrO_2$) ceramics. Understanding the relevant physicochemical and mechanical properties of these ceramics will help identify the optimal material for facilitating gingival wound closure. Methods: Both biomaterials were prepared with 2 different surface treatments: raw and polished. Their physicochemical characteristics were analyzed by contact angle measurements, scanning white-light interferometry, and scanning electron microscopy. An organotypic culture was then performed using a chicken epithelium model to simulate peri-implant soft tissue. We measured the contact angle, hydrophobicity, and roughness of the materials as well as the tissue behavior at their surfaces (cell migration and cell adhesion). Results: The best cell migration was observed on $ZrO_2$ ceramic. Cell adhesion was also drastically lower on the polished $ZrO_2$ ceramic than on both the raw and polished $LS_2$. Evaluating various surface topographies of $LS_2$ showed that increasing surface roughness improved cell adhesion, leading to an increase of up to 13%. Conclusions: Our results demonstrate that a biomaterial, here $LS_2$, can be modified using simple surface changes in order to finely modulate soft tissue adhesion. Strong adhesion at the abutment associated with weak migration assists in gingival wound healing. On the same material, polishing can reduce cell adhesion without drastically modifying cell migration. A comparison of $LS_2$ and $ZrO_2$ ceramic showed that $LS_2$ was more conducive to creating varying tissue reactions. Our results can help dental surgeons to choose, especially for esthetic implant abutments, the most appropriate biomaterial as well as the most appropriate surface treatment to use in accordance with specific clinical dental applications.

How adjustment could affect internal and marginal adaptation of CAD/CAM crowns made with different materials

  • Hasanzade, Mahya;Moharrami, Mohammad;Alikhasi, Marzieh
    • The Journal of Advanced Prosthodontics
    • /
    • v.12 no.6
    • /
    • pp.344-350
    • /
    • 2020
  • PURPOSE. Recently introduced hybrid and reinforced glass ceramic computer-aided design/computer-aided manufacturing (CAD/CAM) materials have been used for full-coverage restorations. However; the effect of adjustment and type of materials on internal and marginal adaptation are unknown. This study aimed to evaluate and compare the marginal and internal adaptations of crowns made of three different CAD/CAM materials before and after adjustment. MATERIALS AND METHODS. One acrylic resin maxillary first molar was prepared and served as the master die. Thirty-six restorations were fabricated using CAD/CAM system (CEREC Omnicam, MCXL) with three materials including lithium disilicate (IPS e.max CAD), zirconia-reinforced lithium silicate (Suprinity), and hybrid ceramic (Enamic). Internal and marginal adaptations were evaluated with the reference point matching technique before and after adjustment. The data were analyzed using mixed ANOVA considering α=.05 as the significance level. RESULTS. The effect of adjustment and its interaction with the restoration material were significant for marginal, absolute marginal, and occlusal discrepancies (P<.05). Before adjustment, Suprinity had lower marginal discrepancies than IPS e.max CAD (P=.18) and Enamic (P=.021); though no significant differences existed after adjustment. CONCLUSION. Within the limitations of this study, crowns fabricated from IPS e.max CAD and Suprinity resulted in slightly better adaptation compared with Enamic crowns before adjustment. However, marginal, axial, and occlusal discrepancies were similar among all materials after the adjustment.

Shear bond strength of resin cement to an acid etched and a laser irradiated ceramic surface

  • Kursoglu, Pinar;Karagoz Motro, Pelin Fatma;Yurdaguven, Haktan
    • The Journal of Advanced Prosthodontics
    • /
    • v.5 no.2
    • /
    • pp.98-103
    • /
    • 2013
  • PURPOSE. To evaluate the effects of hydrofluoric acid etching and Er,Cr:YSGG laser irradiation on the shear bond strength of resin cement to lithium disilicate ceramic. MATERIALS AND METHODS. Fifty-five ceramic blocks ($5mm{\times}5mm{\times}2mm$) were fabricated and embedded in acrylic resin. Their surfaces were finished with 1000-grit silicon carbide paper. The blocks were assigned to five groups: 1) 9.5% hydrofluoric-acid etching for 60 s; 2-4), 1.5-, 2.5-, and 6-W Er,Cr:YSGG laser applications for 60 seconds, respectively; and 5) no treatment (control). One specimen from each group was examined using scanning electron microscopy. Ceramic primer (Rely X ceramic primer) and adhesive (Adper Single Bond) were applied to the ceramic surfaces, followed by resin cement to bond the composite cylinders, and light curing. Bonded specimens were stored in distilled water at $37^{\circ}C$ for 24 hours. Shear bond strengths were determined by a universal testing machine at 1 mm/min crosshead speed. Data were analyzed using Kruskal-Wallis and Mann-Whitney U-tests (${\alpha}$=0.05). RESULTS. Adhesion was significantly stronger in Group 2 ($3.88{\pm}1.94$ MPa) and Group 3 ($3.65{\pm}1.87$ MPa) than in Control group ($1.95{\pm}1.06$ MPa), in which bonding values were lowest (P<.01). No significant difference was observed between Group 4 ($3.59{\pm}1.19$ MPa) and Control group. Shear bond strength was highest in Group 1 ($8.42{\pm}1.86$ MPa; P<.01). CONCLUSION. Er,Cr:YSGG laser irradiation at 1.5 and 2.5 W increased shear bond strengths between ceramic and resin cement compared with untreated ceramic surfaces. Irradiation at 6 W may not be an efficient ceramic surface treatment technique.

FRACTURE STRENGTH AND MARGINAL FIT OF IN-CERAM, COPY-MILLED IN-CERAM, AND IPS EMPRESS 2 ALL-CERAMIC BRIDGES

  • Hwang Jung-Won;Yang Jae-Ho;Lee Sun-Hyung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.39 no.6
    • /
    • pp.641-658
    • /
    • 2001
  • All-ceramic restorations have become an attractive alternative to porcelain-fused-to-metal crowns. In-Ceram, and more recently IPS Empress 2 were introduced as a new all-ceramic system for single crowns and 3-unit fixed partial dentures. But their strength and marginal fit are still an important issue. This study evaluated the fracture resistance and marginal fit of three systems of 3 unit all-ceramic bridge fabricated on prepared maxillary anterior resin teeth in vitro. The 3 all-ceramic bridge systems were: (1) a glass-infiltrated, sintered alumina system (In-Ceram) fabricated conventionally, (2) the same system with copy-milled alumina cores (copy-milled In-Ceram), (3) a heat pressed, lithium disilicate reinforced glass-ceramic system (IPS Empress 2). Ten bridges of each system with standardized design of framework were fabricated. All specimens of each system were compressed at $55^{\circ}$ at the palatal surface of pontic until catastrophic fracture occurred. Another seven bridges of each system were fabricated with standard method. All of the bridge-die complexes were embedded in epoxy resin and sectioned buccolingually and mesiodistally. The absolute marginal discrepancy was measured with stereomicroscope at ${\times}50$ power. The following results were obtained: 1. There was no significant difference in the fracture strength among the 3 systems studied. 2. The Weibull modulus of copy-milled In-Ceram was higher than that of In-Ceram and IPS Empress 2 bridges. 3. Copy-milled In-Ceram($112{\mu}m$) exhibited significantly greater marginal discrepancy than In Ceram ($97{\mu}m$), and IPS Empress 2 ($94{\mu}m$) at P=0.05. 4. The lingual surfaces of the ceramic crowns showed smaller marginal discrepancies than mesial and distal points. There was no significant difference between teeth (incisor, canine) at P=0.05. 5. All-ceramic bridges of three systems appeared to exhibit sufficient initial strength and accept able marginal fit values to allow clinical application.

  • PDF

Ceramic color differences of dental Ni-Cr alloy by compositional change (치과용 Ni-Cr 합금의 조성에 따른 세라믹의 색차 분석)

  • Kim, Sa-Im;Kim, Tae-Yeon;Kim, Se-Ha;Kang, Jeong-Gyu;Lee, Jung-Hwan
    • Journal of Technologic Dentistry
    • /
    • v.43 no.4
    • /
    • pp.168-174
    • /
    • 2021
  • Purpose: This study was conducted to investigate alloys spectrophotometrically including yttrium of nickel-chromium (Ni-Cr) alloys, which are used as substitutes for the regulation of beryllium and provide helpful improvements in Ni-Cr alloys. Methods: Four groups of specimens (ZN, ZY, SN and EM) were prepared for analysis. Color parameters were measured with a spectrophotometer, and color difference (∆E*) was calculated. The t-test and one-way analysis of variance test were used to determine significant difference, and the Tukey test was used to identify where the differences were. To measure the spectroscopic reflectivity, the spectroscopic reflectance was measured and converted into CIE L*, a*, b* color system. Results: The ∆E* value of each metal ceramic group after opaque firing of Ni-Cr alloy with and without yttrium was <2, and the total group color difference (∆E*) was below 1 in the dentin ceramic all experimental group. However, the a* and b* values of the metal ceramic groups were higher than that in the lithium disilicate all ceramic group, and the chroma was higher than the natural tooth. The brightness of all experimental groups was similar to that of the shade guide sample. Conclusion: Yttrium added to Ni-Cr alloys showed similar CIE L*, a*, b* values to Ni-Cr alloys that did not contain yttrium, indicating that yttrium had no effect on color in metallic ceramic systems.

A STUDY ON THE BOND STRENGTH OF RESIN CEMENTS TO EMPRESS 2 CERAMIC (Empress 2 도재와 레진시멘트의 결합강도에 관한 연구)

  • Kim Jeong-Suk;Hwang Hee-Seong;Jeong Chang-Mo;Jeon Young-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.39 no.2
    • /
    • pp.184-196
    • /
    • 2001
  • The objective of this study was to investigate the influence of resin cements and ceramic etching on shear bond strength of Empress 2 ceramic and observe the change of microstructure of ceramic according to etching time. Sixty-six square ceramic specimens($6{\times}6{\times}1.5mm$) were prepared. 6 specimens were etched with different etching times(0, 10, 20, 30, 40 and 60 seconds) and observed by means of a scanning electron microscope(SEM). Other sixty specimens were divided into 6 groups with 10 specimens in each group. 3 groups were etched with 4% hydrofluoric acid and each groups was bonded with 3 resin cements(Variolink II, Super-Bond C&B, Panavia F). Each specimen was subjected to a shear load in an Instron at a cross-head speed of 0.5mm/min and was observed with SEM after mechanical testing to establish modes of failure. The results were as follows : 1. Within etched groups, Variolink II and Super-Bond C&B exhibited significantly greater bonding strengths than Panavia F(p<0.05) 2. Bond strength of etching groups had three to five times greater than that of no-etching groups. 3. All of no-etching groups showed adhesive failure and etching groups mostly showed mixed failure. And, 20-second etching specimen showed the most distinct lithium disilicate crystal. so it is considered that 20-second etching is optimal time for bonding.

  • PDF

Shear bond strength in bilayer metal-heat pressed glass ceramic structure (열가압 방식의 금속-유리도재 이중 구조물의 전단결합강도에 대한 연구)

  • Lee, Kyungeun;Park, Jin-Young;Kim, Ji-Hwan;Kim, Woong-Chul
    • Journal of Technologic Dentistry
    • /
    • v.39 no.2
    • /
    • pp.101-107
    • /
    • 2017
  • Purpose: The purpose of this study was to compare the shear bond strength of the metal-heat pressed glass ceramic bilayer structure. Methods: Metal framework specimens were prepared and surface is spreaded opaque(IPS InLine system opaque, IvoclarVivadent, Liechtenstein). There were 10 specimens for each bilayer dental ceramic group. The first group was porcelain fused metal, Press on metal IPS Inline press group, and press on metal HASS prototype group. Specimens measured for the shear bond strength on Schwickerath test by Instron universal testing machine(Instron3345, Instron Corp., USA). Mean average bond strength values of each specimen group were analyzed using a one-way ANOVA analysis of variance Saphiro-wilk's test. Statistical analysis were performed using IBM SPSS 23.0(IBM Co., Armonk, USA) Results: $RMS{\pm}SD$ The highest mean average HASS POM showed a bond strength value ($47.55{\pm}12.80Mpa$). The lowest mean average values Porcelain fused metal ($33.30{\pm}2.00Mpa$). Independent t-test was conduct to analysis the significant difference (p<0.05) (Table 3). Conclusion: Three kinds of Metal/ glass bilayer dental ceramics bond strength were clinical acceptability. Especially, as lithium disilicate containing represents higher bond strength.