• 제목/요약/키워드: Linepipe

검색결과 26건 처리시간 0.022초

API X70 및 X80급 라인파이프강의 준정적 및 동적 비틀림 변형 거동 (Quasi-Static and Dynamic Torsional Deformation Behavior of API X70 and X80 Linepipe Steels)

  • 김용진;김양곤;신상용;이성학
    • 대한금속재료학회지
    • /
    • 제48권1호
    • /
    • pp.8-18
    • /
    • 2010
  • This study aimed at investigating quasi-static and dynamic torsional deformation behavior of three API X70 and X80 linepipe steels. Quasi-static and dynamic torsional tests were conducted on these steels. having different grain sizes and volume fractions of acicular ferrite and polygonal ferrite, using a torsional Kolsky bar. The test data were then compared via microstructures and adiabatic shear band formation,. The dynamic torsional test results indicated that the steels rolled in the single phase region had higher maximum shear stress than the steel rolled in the two phase region, because the microstructures of the steel rolled in the single phase region were composed mainly of acicular ferrites. In the X80 steel rolled in the single phase region, the increased dynamic torsional properties could be explained by a decrease in the overall effective grain size due to the presence of acicular ferrite having smaller effective grain size. The possibility of adiabatic shear band formation was analyzed from the energy required for void initiation and variation in effective grain size.

ERW 용접 전후 API X70 라인파이프강의 미세조직과 기계적 특성 변화 (Effect of Electrical Resistance Welding on Microstructure and Mechanical Properties of API X70 Linepipe Steel)

  • 오동규;최예원;신승혁;정한길;곽진섭;황병철
    • 열처리공학회지
    • /
    • 제35권4호
    • /
    • pp.185-192
    • /
    • 2022
  • Variations in the microstructure and mechanical properties of API X70 steel processed by piping, electrical resistance welding (ERW), and post seam annealing (PSA) are investigated in this study. In the welding zone, some elongated pearlites are formed and grains coarsening occurs due to extra heat caused by the ERW and PSA processes. After the piping, the base metal shows continuous yielding behavior and a decrease in yield and impact strengths because mobile dislocation and back stress are introduced during the piping process. On the other hand, the ERW and PSA processes additionally decreased the impact strength of welding zone at room and low temperatures because some elongated pearlites easily act as crack initiation site and coarse ferrite grains facilitate crack propagation. As a result, the fracture surface of the welding zone specimen tested at low temperature revealed mostly cleavage fracture unlike the base metal specimen.

철강 압연제품의 제조기술 및 응용 (Manufacturing Technologies and Applications of Steel Strip Products)

  • 권오준
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.10-21
    • /
    • 1999
  • Recent progress in manufacture of hot and cold rolled steel strip products and their applications were reviewed. The main trend in the technological development has been to meet the customers' requests for quality improvement and cost reduction. The weight reduction to reduce the fuel consumption is the main issue in the automotive industry and, therefore, various steels have been developed to improve formability as well as strength. The steels include super-EDDQ steels, bainitic steels, TRIP steels, etc. In the oil industry, efforts have been focused to improve strength together with either low temperature toughness or HIC/SSCC resistance. The packaging industry is also a highly competitive market, and steel and canmaking companies have worked cooperatively to develop cost-effective canmaking processes as well as high performance steels. This type of cooperation has also been found important in other industries such as the appliance and electronic industries for the benefits of both steelmakers and customers.

  • PDF

라인파이프용 고강도 열연강판의 기계적 성질 (Mechanical Properties of High Strength Hot Strips For Line Pipe Application)

  • 김문수;김준성;강기봉;노광섭
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.383-389
    • /
    • 1999
  • The purpose of this study was to investigate the effects of alloying and rolling condition on the mechanical properties and to develop high strength line pipe steels with good toughness. Tests were carried out by the laboratory experiments followed by mill trials and mass production. It was found that a small addition of microalloying elements, such as Nb, V with Mo or Ti remarkably increased the strength and toughness of hot strips. The optimum condition of thermomechanical rolling on low carbon microalloyed steel improved the toughness through the formation of a fine and uniform microstructure. Based on this mill trials following the fundamental research, the production technology of line pipe steels, grade X70∼X100 with high toughness, has been established. These grade steels exhibit excellent low temperature toughness (vTs= under -80$^{\circ}C$) and sufficient strength in both the base metal and the ERW seam weld position, respectively.

  • PDF

Effect of $H_2S$ Partial Pressure and pH of Test Solution on Hydrogen Induced Cracking of High Strength Low Alloy Steels

  • Kim, Wan Keun;Koh, Seong Ung;Kim, Kyoo Young;Yang, Boo Young;Jung, Hwan Kyo
    • Corrosion Science and Technology
    • /
    • 제4권6호
    • /
    • pp.236-241
    • /
    • 2005
  • Hydrogen induced cracking (HIC) is one of the hydrogen degradation phenomena of linepipe steels caused by $H_2S$ gas in the crude oil or natural gas. However, NACE TM0284-96 standard HIC test method is hard to satisfy the steel requirements for sour service application since it uses more severe environmental conditions than actual conditions. Therefore, in order to use steels effectively, it is required to evaluate HIC resistance of steels in the practical range of environmental severity. In this study, HIC resistance of two high strength low alloy (HSLA) steels being used as line pipe steels was evaluated in various test solutions with different $H_2S$ pressures and pH values. The results showed that the key parameter affecting crack area ratio (CAR) is $H_2S$ partial pressure of test solution when the pH value of test solution is not over 4. Hydrogen diffusivity was not a constant value, but it was rather affected by the hydrogen ion concentration (pH value) in the solution.

X65 및 X70강 가스배관의 DWTT 및 파괴인성평가 (Estimation of fracture toughness of X65 and X70 steels by DWTT)

  • 조예원;송영호;김정민;김우식;박준식
    • 한국가스학회지
    • /
    • 제16권3호
    • /
    • pp.54-64
    • /
    • 2012
  • 실 배관을 평가하는 DWTT (Drop Weight Tearing Test)의 파괴인성 값은 실 배관의 파괴인성 값 및 연성취성천이 온도를 예측할 수 있는 실험방법이므로, 최근 DWTT의 값에 대한 중요성이 증가되고 있다. 본 연구에서는 API X70과 API X65 라인파이프강의 DWTT 후의 온도에 따른 연성파면율, 역파면율, 흡수에너지와 온도 $-60^{\circ}C$~상온)와의 관계를 비교분석 하고자 하였다. X65과 X70의 값에서 마찬가지로 연성파면율 및 흡수에너지는 온도가 낮아질수록 함께 낮아지는 경향을 보였으며, X70의 경우에는 $-40^{\circ}C$ 까지 연성파괴를 보이는 반면, X65는 $-30^{\circ}C$ 까지 연성파괴를 보였다.