• Title/Summary/Keyword: Layer-by-layer Deposition Method

Search Result 688, Processing Time 0.038 seconds

Comparison between Bi-superconducting Thin Films Fabricated by Co-Deposition and Layer-by-Layer Deposition

  • Yang, Sung-Ho;Park, Yong-Pil
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.9
    • /
    • pp.796-800
    • /
    • 2000
  • Bi$_2$Sr$_2$Ca$_{n}$Cu$_{n+1}$ O$_{y}$(n$\geq$0; BSCCO) thin film is fabricated via two different processes using an ion beam sputtering method i.e. co-deposition and layer-by-layer deposition. A single phase of Bi2212 can be fabricated via the co-deposition process. While it cannot be obtained by the layer-by-layer process. Ultra-low growth rate in our ion beam sputtering system brings out the difference in Bi element adsorption between the two processes and results in only 30% adsorption against total incident Bi amount by layer-by-layer deposition, in contrast to enough Bi adsorption by co-deposition.on.n.

  • PDF

Comparison between BSCCO Thin Films Fabricated by Co-Deposition and Layer-by-Layer Deposition

  • Lee, Hee-Kab;Park, Yong-Pil;Lee, Joon-Ung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.230-234
    • /
    • 2000
  • Bi$_2$Sr$_2$Ca$_{n}$Cu$_{n+1}$ O$_{y}$(n$\geq$0; BSCCO)thin film is fabricated via two different processes using an ion beam sputtering method i.e. co-deposition and layer-by-layer deposition. A single phase of Bi2212 can be fabricated via the co-deposition process. While it cannot be obtained by the layer-by-layer process. Ultra-law growth rate in our ion beam sputtering system brings out the difference in Bi element adsorption between the two processes and results in only 30% adsorption against total incident Bi amount by layer-by-layer deposition, in contrast to enough Bi adsorption by co-deposition.on.n.

  • PDF

Characteristics of Bi-superconducting Thin Films Prepared by Co- and Layer-by-Layer Deposition

  • Yang, Sung-Ho;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.10a
    • /
    • pp.40-44
    • /
    • 2000
  • $Bi_2Sr_2Ca_nCu_{n+1}O_y$($n{\geq}0$; BSCCO)thin film is fabricated via two different processes using an ion beam sputtering method i.e. co-deposition and layer-by-layer deposition. A single phase of Bi2212 can be fabricated via the co-deposition process. While it cannot be obtained by the layer-by-layer process. Ultra-low growth rate in our ion beam sputtering system brings out the difference in Bi element adsorption between the two processes and results in only 30% adsorption against total incident Bi amount by layer-by-layer deposition, in contrast to enough Bi adsorption by co-deposition.

  • PDF

XRD Patterns and Bismuth Sticking Coefficient in $Bi_2Sr_2Ca_nCu_{n+1}O_y(n\geq0)$ Thin Films Fabricated by Ion Beam Sputtering Method

  • Yang, Seung-Ho;Park, Yong-Pil
    • Journal of information and communication convergence engineering
    • /
    • v.4 no.4
    • /
    • pp.158-161
    • /
    • 2006
  • [ $Bi_2Sr_2Ca_nCu_{n+1}O_y(n{\geq}0)$ ] thin film is fabricatedvia two different processes using an ion beam sputtering method i.e. co-deposition and layer-by-layer deposition. A single phase of Bi2212 can be fabricated via the co-deposition process. While it cannot be obtained by the layer-by-layer process. Ultra-low growth rate in our ion beam sputtering system brings out the difference in Bi element adsorption between the two processes and results in only 30% adsorption against total incident Bi amount by layer-by-layer deposition, in contrast to enough Bi adsorption by co-deposition.

Characteristics of $B_2$Sr_2$$Ca_{n-1}$$Cu_n$$O_x$ Superconducting Thin Films Fabricated by Layer-by-Layer Deposition Method (Layer-by-Layer 증착법으로 제작한 $B_2$Sr_2$$Ca_{n-1}$$Cu_n$$O_x$초전도 박막의 특성)

  • 유선종;천민우;박용필
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2003.05a
    • /
    • pp.518-521
    • /
    • 2003
  • Bi$_2$Sr$_2$Ca$_{n-1}$Cu$_{n}$O$_{x}$ superconducting thin films have been fabricated by atomic layer-by-layer deposition using IBS(Ion Beam Sputtering) method. During the deposition, 90 mol% ozone gas of typical pressure of 1~9 $\times$ 10$^{-5}$ Torr are supplied with ultraviolet light irradiation for oxidation. XRD and RHEED investigations reveal out that a buffer layer with some different compositions is formed at the early deposition stage of less than 10 units cell and then Bi-2201 oriented along the c-axis is grown.grown.

  • PDF

Analysis of Bi-Superconducting Thin Films Fabricated by Using the Layer by Layer Deposition and Evaporation Deposition Method

  • Yang, Seung-Ho;Cheon, Min-Woo;Lee, Ho-Shik;Park, Yong-Pil
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2007.06a
    • /
    • pp.517-520
    • /
    • 2007
  • The BSCCO thin film fabricated by using the layer by layer deposition method was compared with the BSCCO thin film fabricated by using the evaporation method. Reevaporation in the form of Bi atoms or $Bi_2O_3$molecules easily bring out the deficiency of Bi atoms in thin film due to the long sputtering time of the layer by layer deposition. On the other hand, the respective atom numbers corresponding to BSCCO phase is concurrently supplied on the film surface in the evaporation deposition process and leads to BSCCO phase formation. Also, it is cofirmed that by optimizing the deposition condition, each single phase of the Bi2201 phase and the Bi2212 phase can be fabricated, the sticking coefficient of Bi element is clearly related to the changing of substrate temperature and the formation of the Bi2212 phase.

  • PDF

Epitaxial Growth of BSCCO Films by IBS Method (IBS법에 의한 BSCCO 박막의 에피택셜 성장)

  • 양승호;박용필
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2002.05a
    • /
    • pp.627-630
    • /
    • 2002
  • Bi$_2$Sr$_2$CuOx(Bi-2201) thin films were fabricated by atomic layer-by-layer deposition using an ion bean sputtering method. 10 wt% and 90 wt% ozone mired with oxygen were used with ultraviolet light irradiation to assist oxidation. XRD and RHEED investigations revealed that a buffer layer is formed at the early stage of deposition (less than 10 unit cell), and then c-axis oriented Bi-2201 grows on top of it.

  • PDF

Epitaxy Growth of the Thin Films Fabricated by Layer by Layer Method (Layer by Layer 법으로 제작한 박막의 에피택셜 성장)

  • Kim, Tae-Gon;Cheon, Min-Woo;Yang, Sung-Ho;Park, Yong-Pil;Park, No-Bong;Lee, Hee-Kab
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.529-530
    • /
    • 2006
  • $Bi_2Sr_2CuO_x$ thin films have been fabricated by atomic layer-by-layer deposition using the ion beam sputtering method. During the deposition, 10 and 90 wt%-ozone/oxygen mixture gas of typical pressure of $1{\sim}9{\times}10^{-5}\;Torr$ are supplied with ultraviolet light irradiation for oxidation. XRD and RHEED investigations reveal out that a buffer layer with some different compositions is formed at the early deposition stage of less than 10 units cell and then Bi-2201 oriented along the c-axis is grown.

  • PDF

Sticking Characteristics in BiSrCaCuO Thin Film Fabricated by Layer-by-Layer Sputtering Method (순차 스퍼터법으로 제작한 BiSrCaCuO 박막의 부착 특성)

  • Cheon, Min-Woo;Park, Yong-Pil;Kim, Jeong-Ho
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.05d
    • /
    • pp.45-48
    • /
    • 2003
  • BiSrCaCuO thin films were fabricated by atomic layer-by-layer deposition using an ion beam sputtering method. 10 wt% and 90 wt% ozone mixed with oxygen were used with ultraviolet light irradiation to assist oxidation. At early stages of the atomic layer by layer deposition, two dimensional epitaxial growth which covers the substrate surface would be suppressed by the stress and strain caused by the lattice misfit, then three dimensional growth takes place. Since Cu element is the most difficult to oxidize, only Sr and Bi react with each other predominantly, and forms a buffer layer on the substrate in an amorphous-like structure, which is changed to $SrBi_2O_4$ by in-situ anneal.

  • PDF

Fabrication of Bi-superconducting Thin Films by Layer-by-layer Sputtering Method (순차 스퍼터법에 의한 Bi-초전도 박막의 제작)

  • 심상흥;양승호;박용필
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.613-616
    • /
    • 2001
  • Bi$_2$Sr$_2$CuO$_{x}$ thin films have been fabricated by atomic layer-by-layer deposition using ion beam sputtering(IBS) method. During the deposition, 10 and 90 wt%-ozone/oxygen mixture gas of typical pressure of 1~9$\times$10$^{-5}$ Torr are supplied with ultraviolet light irradiation for oxidation. XRD and RHEED investigations reveal out that a buffer layer with some different compositions is formed at the early deposition stage of less than 10 units cell and then Bi-2201 oriented along the c-axis is grown.n.

  • PDF