• Title/Summary/Keyword: Laser welded tube

Search Result 22, Processing Time 0.032 seconds

OPTIMAL PROCESSING AND SYSTEM MANUFACTURING OF A LASER WELDED TUBE FOR AN AUTOMOBILE BUMPER BEAM

  • Suh, J.;Lee, J.H.;Kang, H.S.;Park, K.T.;Kim, J.S.;Lee, M.Y.;Jung, B.H.
    • International Journal of Automotive Technology
    • /
    • v.7 no.2
    • /
    • pp.209-216
    • /
    • 2006
  • A study has been conducted for an optimal processing and an apparatus for manufacturing a laser welded tube for one-body formed bumper beam. The tube dimensions used in calculation were the thickness of 1.4 mm, the diameter of 105.4 mm and the length of 2000 mm. The tube was formed of a cold rolled high strength steel plate(tensile strength of 600 MPa). The two-roll bending method was the optimal tube forming process in comparison with the UO-bending method, the bending method on the press brake, the multi-step continuous roll-forming method and the 3-roll bending method. Monitoring of the welding quality was conducted and the seam tracking along the butt-joint lengthwise to the tube axis was also examined. The longitudinal butt-joint was welded by using a $CO_2$ laser welding machine equipped with a seam tracker and a plasma sensor. The $CO_2$ laser tube welding machine could be used for precise seam tracking and real-time monitoring of the welding quality. As a result, the developed laser welded tube could be used for a one-body formed automobile bumper beam.

Production of Laser Welded Tube for Automobile Bumper Beam from 60kgf/$\textrm{mm}^2$Grade Steel Sheet (60kgf/$\textrm{mm}^2$급 자동차 범퍼빔용 레이저 용접 튜브 제조기술 및 장치연구)

  • Seo, Jung;Lee, Je-Hoon;Kim, Jong-Soo;Kim, Jung-O;Kang, Hee-Sin;Lee, Moon-Yong;Jung, Byung-Hoon
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.21 no.7
    • /
    • pp.136-144
    • /
    • 2004
  • Optimal process and system to produce the laser welded tube for one body formed bumper beam are studied. The calculated size of tube is a thickness of 1.4mm, diameter of 105.4mm and length of 2000mm. The tube is shaped from a cold rolled high strength steel sheet(tensile strength: 60kgf/$\textrm{mm}^2$ grade). Two roll bending method is the optimal tube shaping process compared to UO-bending, bending on press brake, multi-step continuous roll forming and 3 roll bending methods. Weld quality monitoring and seam tracking along the butt-joint lengthwise to the tube axis are also studied. The longitudinal butt-joint is welded by the $CO_2$ laser welding system equipped with a seam tracker and plasma sensor. The constructed $CO_2$laser tube welding system can be used for the precision seam tracking and the real-time monitoring of weld quality. Finally, the obtained laser welded tube can be used for one-body formed automobile bumper beam.

Minimization of Welding Defect in $CO_2$ Laser Welded Tube

  • Suh Jeong;Kang Hee-Shin;Lee Jae-Hoon;Park Kyoung-Taik;Lee Moon-Yong;Jung Byung-Hun
    • International Journal of Precision Engineering and Manufacturing
    • /
    • v.6 no.3
    • /
    • pp.19-23
    • /
    • 2005
  • To minimize the weld defect in manufacturing of the welded tube by using $CO_2$ laser, the monitoring of the welding quality and the seam tracking along the butt-joint lengthwise to the tube axis are studied. The longitudinal butt-joint is shaped from $60kgf/mm^2$ grade steel sheet by 2 roll bending method, and welded by the $CO_2$ laser welding system equipped with the seam tracker and plasma sensor. The laser welded tube has the thickness of 1.5mm, diameter of 105.4mm and length of 2000mm. The precise positioning of the laser beam on the butt-joint to be assembled is obtained within $200{\mu}m$ by the laser vision sensor. The artificial defects in the butt-joint are well observed by the signal of plasma intensity measured from the plasma sensor of UV wavelength range within 400nm. The developed $CO_2$ laser tube welding system has the function of the precision seam tracking and the real-time monitoring of the welding quality. In conclusion, the laser welded tube can be used for manufacturing of automobile chassis and components after hydro-forming.

A study on manufacturing of laser welded tube from 60kgf/$mm^2$Grade Steel Sheet for one-body forming (60kgf/$mm^2$급 일체화 성형용 레이저 용접 튜브 제조에 관한 연구)

  • Seo, Jung;Lee, Je-Hoon;Kim, Jung-Oh;Kang, Hee-Sin;Lee, Mun-Yong;Jung, Byung-Hoon
    • Proceedings of the KWS Conference
    • /
    • 2003.11a
    • /
    • pp.18-20
    • /
    • 2003
  • Optimal processing and system to produce the laser welded tube for one body formed bumper beam are studied. The calculated size of tube is a thickness of 1.4mm, diameter of 105.4mm and length of 2000mm. The tube is shaped from cool rolled high strength steel sheet(tensile strength: 60kgf/$\textrm{mm}^2$ grade). Two roll bending method is the optimal tube shaping process compared to UO-bending, bending on press brake, multi-step continuous roll forming and 3 roll bending methods. Weld quality monitoring and seam tracking along the butt-joint lengthwise to the tube axis are also studied. The longitudinal butt-joint is welded by the $CO_2$ laser welding system equipped with a seam tracker and plasma sensor. The constructed $CO_2$ laser tube welding system can be used for the precision seam tracking and the real-time monitoring of weld quality. Finally, the obtained laser welded tube can be used for one-body formed automobile bumper beam.

  • PDF

Weld Quality Monitoring and Seam Tracking in Making of Welded Tube using $CO_2$ Laser ($CO_2$ 레이저를 이용한 용접튜브 제조공정에서의 용접선 추적 및 용접품질 모니터링)

  • Suh, Jeong;Lee, Jae-Hoon;Kim, Jeng-O;Kang, Hee-Shin;Lee, Moon-Yong;Jung, Byung-Hun
    • Journal of Welding and Joining
    • /
    • v.21 no.7
    • /
    • pp.34-41
    • /
    • 2003
  • Weld quality monitoring and seam tracking along the butt-joint lengthwise to the tube axis are studied. The material of tube is 60kg/$\textrm{mm}^2$ grade steel sheet, and the longitudinal butt-joint is shaped by 2 roll bending machine. The tube with a thickness of 1.5mm, diameter of 105.4mm and length of 2000mm is successfully obtained by the $CO_2$ laser welding system equipped with a seam tracker and plasma sensor. Experimental results show that the developed welding system can be used for the precision seam tracking and the real-time monitoring of weld quality, and the laser welded tube can be used for car body md component after tubular hydroforming.

Welding Characteristics of Inconel Plate Using Pulsed Nd : YAG Laser Beam (펄스형 Nd:YAG 레이저빔을 이용한 인코넬 판재의 용접 특성)

  • 변진귀;박광수;한원진;심상한
    • Laser Solutions
    • /
    • v.3 no.1
    • /
    • pp.12-20
    • /
    • 2000
  • The nuclear steam generators are subjected to corrosion environmental condition during operation that can result in stress corrosion in the tube wall. If any tube wall degradation is recognized, the tube must be repaired by plugging or sleeving. For the sleeving repair, Nd : YAG laser welded sleeving technology is one of the most promising when considering radioactive working conditions in the nuclear power plant. In this paper, the laser welding characteristics of steam generator tube and sleeve materials are investigated. The effects of average laser power, laser energy, welding speed, pulse duration and frequency are evaluated. Based on these results, Nd : YAG laser welded sleeving repair was applied to the degraded steam generator tubes in real environment.

  • PDF

Shear Strength of lnconel Tube Welded with Pulsed Nd:YAG Laser (펄스형 Nd:YAG레이저로 용접된 Inconel Tube의 전단강도)

  • Chang, W.;Kim, J. D.;Chung, J. M.;Kim, C. J.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1995.10a
    • /
    • pp.125-128
    • /
    • 1995
  • The remote sleeve repair-welding technology using the pulsed Nd:YAG laser for increasing the lifetime of the steam generator tube in the nuclear power plant has been developed. The laser welding has many advantages on deep penetration depth and narrow heat affect zone(HAZ). The inconel 600 tube and inconel 690 sleeve used high temperature and high pressure service have been welded as round lap welds. It is found that the relation between the connection width and welding parameters. It is found that the shear strength in proportion to the connection width by conducting tensile-shear tests.

  • PDF

Development of magnesium tube manufacturing technology with strip cast and warm rolled AZ31 sheet. (마그네슘 압연판재를 이용한 용접 튜브 제조 기술 개발)

  • Lee, Mok-Young;Han, Soo-Sik;Chang, Woong-Seong;Lee, Heung-Gyu
    • Proceedings of the KWS Conference
    • /
    • 2010.05a
    • /
    • pp.96-96
    • /
    • 2010
  • Magnesium alloy is being used for structural material since it has high specific strength. Tubular shape was effective way for enhanced structural design. To manufacture the tube, it is necessary to weld the butted joint of both tubular formed sides. But the magnesium alloy was hardly welded with conventional welding processes. The laser welding was effective way to joint magnesium alloys because it had high weld strength and productivity compare with other welding processes. In this study, magnesium alloy sheets was formed at elevated temperature to tubular shape and welded with laser. Consequently, the magnesium alloy tube was making successful with warm forming and laser welding and bicycle frame was making with it.

  • PDF

Welding of Inconel Tube with Pulsed Nd:YAG Laser (펄스형 Nd:YAG 레이저 빔에 의한 Inconel Tube의 용접)

  • Kim, J.D.;Chang, W.;Chung, J.M.;Kim, C.J.
    • Journal of Welding and Joining
    • /
    • v.17 no.1
    • /
    • pp.82-87
    • /
    • 1999
  • The basic remote sleeve repair-welding technology by the pulsed Nd:YAG laser for increasing the lifetime of the steam generator tube in a nuclear power plant has been developed. The relationship between the connection width and welding parameters have been investigated for the fundamental research to apply the sleeve-repair-welding technique to the nuclear industry. The Inconel 600 tube and Inconel 690 sleeve used for high temperature and high pressure service were welded as round lap welding by Nd:YAG laser. It was observed that the tensile shear strength, 340MPa of the welded specimen is equivalent to about 60% of that of the base metal (Inconel 600), 550MPa. The difference between the hardness of the base metal and that of the laser welds was about 10%. Ductile fracture was partly occurred in the weld but the cracking has not been observed. In spite of absence of the crack, the strength of welds was not sufficient in terms of the tensile shear strength.

  • PDF