• Title/Summary/Keyword: Laser sealing

Search Result 35, Processing Time 0.032 seconds

Investigation of Glass Substrate Sealing for ECL Application using Laser Welding Technology (레이저 웰딩 기술을 이용한 ECL용 유리 기판 접합에 대한 고찰)

  • Sung, Youl-Moon
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.29 no.12
    • /
    • pp.28-32
    • /
    • 2015
  • In this work, we reported fabrication of sealing the glass substrate using laser treatment at low temperature for electrochemical luminescence (ECL) cell. The laser treatment at temperature is using laser diode. The glass substrate sealing by laser treatment tested at 3-10W, 2-5 mm/s for build and tested. The sealing laser treatment method will allow associate coordination between the two glass substrate was enclosed. The effect of laser treatment to sealing the glass substrate was found to have cracks and air gap at best thickness of about 550-600 im for condition 3 W, 3 mm/s. The surface of sealing was roughness which was not influent to electrodes It can reduce the cracks, crevices and air gaps as well, improves the performance viscosity in butter bus bar electrodes. Therefore, it is more effective viscosity between two FTO glasses substrate.

The Low Temperature Laser Treatment of Sealing Glass Substrate for ECL (ECL용 유리기판의 레이저 저온 실링처리)

  • Choi, Hye-Su;Park, Cha-Soo;Gwak, Dong-Joo;Sung, Youl-Moon
    • Proceedings of the KIEE Conference
    • /
    • 2015.07a
    • /
    • pp.1134-1135
    • /
    • 2015
  • In this paper, we reported fabrication of sealing the glass substrate using laser treatment at low temperature for electrochemical luminescence (ECL) cell. The laser treatment at temperature is using laser diode. The glass substrate sealing by laser treatment tested at 1-5 W, 1-5 mm/s for builted and tested. The sealing laser treatment method will allow associate coordination between the two glass substrate was enclosed. The effect of laser treatment to sealing the glass substrate was found to have cracks and air gap at best thickness of about $845-780{\mu}m$ for condition 5 W, 1-5 mm/s. The surface of sealing was roughness which was not influent to electrodes So, it is more effective viscosity between two glasses substrate.

  • PDF

Laser-Heating Characteristics of CuO-Incorporating Glasses

  • Lee, Jungki;Kim, Jongwoo;Kim, Hyungsun
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.2
    • /
    • pp.119-122
    • /
    • 2015
  • Laser sealing with glass frits appears a promising technology for sealing various electronic devices (e.g., solar cells, displays) due to its several advantages. The purpose of this study is to understand the relationship between the composition of glasses and their laser-heating conditions. To allow glass to be sealed using laser heating, CuO was added to two different glass systems, in different amounts. The optical absorptivity of the glass samples was related directly to their CuO content. The laser-heating temperature and the CuO content exhibited a proportional relationship. Furthermore, the heating temperature increased linearly with the laser power used. From these results, we could determine the appropriate laser-heating conditions and CuO content for sealing electronic devices using laser-sealing technology.

Histologic Evaluation of Blood Vessels Sealed with 1,470-nm Diode Laser: Determination of Adequate Condition for Laser Vessel Sealing

  • Im, Nu-Ri;Moon, Jungho;Choi, Wonshik;Kim, Byoungjae;Lee, Jung Joo;Kim, Heejin;Baek, Seung-Kuk
    • Medical Lasers
    • /
    • v.7 no.1
    • /
    • pp.6-12
    • /
    • 2018
  • Introduction Energy-based devices allow for a more rapid and efficient ligation of blood vessels during operations. In the present study, we evaluated the feasibility of a laser as an alternative energy source for the vessel sealing system and determined the optimal condition of laser for an effective vessel sealing through histologic examination. Materials and Methods The arteries (5 mm diameter) harvested from porcine legs were compressed between two glass-slides to eliminate its luminal space and were irradiated with 1,470-nm diode laser under various sealing conditions, including laser power (5-30 W), irradiation time (5 or 10 seconds), and focus mode (focus or defocus). Subsequently, the irradiated vessels were fixed in 4% formaldehyde and then processed to paraffin block. The paraffinized sample was sectioned and stained with hematoxylin and eosin for histological evaluation. Results The extent of tissue change was positively correlated with duration and power of laser. In defocus mode, the irradiated vessels showed sufficient tissue denaturation for sealing effect without severe tissue destruction. Moreover, among the various conditions of irradiation, laser power between 15 and 20 W, as well as exposure time of 5 seconds were appropriate for sealing the blood vessels. Conclusion Adequate power and irradiation duration of laser can render blood vessels to be sealed effectively, although the higher power of laser may be required to cut the vessels.

Additional Study on the Laser Sealing of Dye-Sensitized Solar-Cell-Panels Using V2O5 and TeO2 Containing Glass

  • Cho, Sung-Jin;Lee, Kyoungho
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.2
    • /
    • pp.103-107
    • /
    • 2015
  • The effective glass frit composition used to absorb laser energy and to seal commercial dye-sensitized solar cell panel substrates has been previously developed using $V_2O_5-TeO_2$-based glass with 10 wt% ${\beta}$-eucryptite as a CTE controlling filler. The optimum sealing conditions are provided using a 3 mm beam, a laser power of 40 watt, a scan speed of 300 mm/s, and 200 irradiation cycles. In this study, the feasibility of the developed glass frit is investigated in terms of the sealing strength and chemical durability against the commercial iodide/triiodide electrolyte solution and fluorine-doped tin oxide (FTO) electrode in order to increase the solar cell lifetime. The sealing strength of the laser-sealed $V_2O_5-TeO_2$-based glass frit is $20.5{\pm}1.7MPa$, which is higher than those of thermally sealed glass frit and other reported glass frit. Furthermore, the developed glass frit is chemically stable against electrolyte solutions. The glass frit constituents are not leached out from the glass after soaking in the electrolyte solution for up to three months. During the laser sealing, the glass frit does not react with the FTO electrode; thus, the resistivity of the FTO electrode beneath the laser-sealed area remains the same.

Synthesis of P2O5-V2O5-ZnO Glass Frit for Laser Sealing of OLED by the Addition of Filler (필러 첨가에 의한 OLED의 레이저 실링용 P2O5-V2O5-ZnO 유리프릿의 제조)

  • Bang, Jae-Chul
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.28 no.9
    • /
    • pp.571-576
    • /
    • 2015
  • In this study, we developed a lead-free $P_2O_5-V_2O_5-ZnO$ glass frit for sealing OLED using laser irradiation. The frit satisfied the characteristics required for laser sealing such as low glass transition temperature, low coefficient of thermal expansion (CTE), high water-resistance, and high absorption at the wavelength of the laser beam. Ceramic fillers were added to the glass frit in order to further reduce and match its CTE with that of the commercial glass substrate. The addition of Zirconium Tungsten Phosphate (ZWP) to the frit yielded the most desirable results, reducing the CTE to $45.4{\times}10^{-7}/^{\circ}C$, which is very close to that of the glass substrate ($44.0{\times}10^{-7}/^{\circ}C$). Successful formation of a solid sealing layer was observed by optical and scanning electron microscopy.

Laser Sealing of Dye-Sensitized Solar Cell Panels Using V2O5 and TeO2 Contained Glass (V2O5 및 TeO2 함유 유리를 이용한 염료감응형 태양전지 패널의 레이저 봉착)

  • Cho, Sung Jin;Lee, Kyoung Ho
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.3
    • /
    • pp.170-176
    • /
    • 2014
  • Effective glass frit compositions enabled to absorb laser energy, and to seal a commercial dye-sensitized solar-cell-panel substrate were developed by using $V_2O_5$-based glasses with various amounts of $TeO_2$ substitution. The latter was intended to increase the lifetime of the solar cells. Substitution of $V_2O_5$ by $TeO_2$ provided a strong network structure for the glasses via the formation of tetrahedral pyramids in the glass, and changed the various glass properties, such as glass transition temperature ($T_g$), dilatometric softening point ($T_d$), crystallization temperature, coefficient of thermal expansion (CTE), and glass flowage without any detrimental effect on the laser absorption property of the glasses. The thermal expansion mismatch (${\Delta}{\alpha}$) between the glass frit and the substrate could be controlled within less than ${\pm}5%$ by addition of 10 wt% of ${\beta}$-eucryptite. An 810 nm diode laser was used for the sealing test. The laser sealing test revealed that the VZBT20 glass frit with 10 wt% ${\beta}$-eucryptite was successfully sealed the substrates without interfacial cracks and pores. The optimum sealing conditions were provided by a beam size of 3 mm, laser power of 40 watt, scan speed of 300 mm/s, and 200 irradiation cycles.

Laser Processing Technology in Semiconductor and Display Industry (반도체 및 디스플레이 산업에서의 레이저 가공 기술)

  • Cho, Kwang-Woo;Park, Hong-Jin
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.27 no.6
    • /
    • pp.32-38
    • /
    • 2010
  • Laser material processing technology is adopted in several industry as alternative process which could overcome weakness and problems of present adopted process, especially semiconductor and display industry. In semiconductor industry, laser photo lithography is doing at front-end level, and cutting, drilling, and marking technology for both wafer and EMC mold package is adopted. Laser cleaning and de-flashing are new rising technology. There are 3 kinds of main display industry which use laser technology - TFT LCD, AMOLED, Touch screen. Laser glass cutting, laser marking, laser direct patterning, laser annealing, laser repairing, laser frit sealing are major application in display industry.

Experimental Studies of Force Control for Crack Sealing Robot

  • Jeon, Poong-Woo;Cho, Hyun-Taek;Jung, Seul
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 2003.10a
    • /
    • pp.1077-1081
    • /
    • 2003
  • In this paper, experimental studies of force tracking control for the crack sealing robot are presented. Crack sealing robot is built to detect, track and seal the crack on the pavement. Before sealing, crack must be detected by a laser sensor and a camera sensor, then cleaned for a better sealing job. In order to maintain contact with the ground force control is required to brush all dirt in the crack out for preparing sealing cracks with tars. Impedance control algorithm is presented to regulate a specified desired force. Experimental studies of the proposed force control algorithm are conducted under unknown environment stiffness and location. Performances of force control algorithm are stable and excellent.

  • PDF

THE EFFECTS OF ND:YAG LASER AND IRRIGANTS ON CANAL SEALING ABILITY (근관치료시 Nd:YAG Laser 사용과 세척액에 따른 치근단 폐쇄효과의 비교)

  • Kim, Jin-Woon;Lee, Hee-Ju;Hur, Bock
    • Restorative Dentistry and Endodontics
    • /
    • v.26 no.4
    • /
    • pp.307-315
    • /
    • 2001
  • The application of Nd:YAG laser and irrigants to the root surface can change its surface configurations. The purpose of this study was to investigate the effects of Nd:YAG laser and irrigants on the apical seal of obturated canals. In this study, 66 single rooted teeth were randomly assigned to 4 group of 14 teeth each. 8 teeth were served us positive and negative controls. The teeth were divided into 6 groups as follows. Group A: Nd:YAG laser, 5% NaOCl + Rc-prep Group B: Nd:YAG laser, Saline Group C: 5% NaOCl + Rc-prep Group D: Saline Group E: Positive control Group F: Negative control 66 teeth were instrumented using Maillefer ProFile$^{\circledR}$ (Orifice Shapers, .04 taper, .06 taper Dentsply, Switzerland). Two of each group were selected at random, and the canal wall surfaces were examined under a SEM. 12 teeth of each group were obturated using by lateral condensation technique. Specimens were immersed in india ink for 7days, decalcified by 10% nitric acid, dehydrated by 75. 80. 85, 90, 95 and 100% alcohol in order cleared by methyl salicylate and then measured of dye penetration with stereomicroscope($\times$15 magnification) and Image Pro plus. The data were analyzed statistically by one-way ANOVA test and Duncan's Multiple Range test. The results were as follows : 1. The mean leakage was 0.128$\pm$0.376 for group A, 0.237$\pm$0.325 for group B, 0.397$\pm$0.468 for group C, 0.586$\pm$0.402 for group D, and there were statistically significant differences between group A and group D, group B and group D. (p<0.05). 2. Group A had better sealing ability than Group C, but there was statistically no significant differences. (p>0.05). 3. Group B had better sealing ability than Group D and there was statistically significant difference. (p<0.05). 4 Group A had better sealing ability than Group B, but there was statistically no significant difference. (p>0.05). 5. Group C had better sealing ability than Group D, but there was statistically no significant difference. (p>0.05). 6. As a result of observation under SEM, Smear layers were removed in Group A, B. but Smear layers were partially removed and smear plugs were remained in Group C, Smear layers were not removed in Group D. To be specially, Melting of smear layer were showed in Group C. 7. These results suggests that the laser has a potential in reducing the apical microleakage of obturated canals.

  • PDF