Effects of the Addition of $La_2O_3$ on Mechanical Properties and Machinability of $Si_3N_4$ Ball

  • Sang Yang Lee;Sung Ho Kim;Soo Wohn Lee
    • The Korean Journal of Ceramics
    • /
    • 제6권4호
    • /
    • pp.364-369
    • /
    • 2000
  • Silicon nitride with adding La$_2$O$_3$ was sintered by gas pressure sintering (GPS) technique at $1950^{\circ}C$, in $N_2$ gas at 3 MPa, for 2h. Mechanical properties such as hardness, flexural strength, and fracture toughness were determined as a function of the GPS holding time and the contents of La$_2$O$_3$ in silicon nitride. Also machinability of silicon nitride ball with various GPS holding time and amount of La$_2$O$_3$ was evaluated by magnetic fluid grinding (MFG) method. In this study it was found that machinability was influenced significantly with La$_2$O$_3$ contents. However, the different GPS holding time did not affect the machinability very much.

  • PDF

Luminescent Properties of Europium-Doped Lanthanum Silicon Nitride Phosphor

  • Lences, Zoltan;Hrabalova, Monika;Czimerova, Adriana;Sajgalik, Pavol;Zhou, You;Hirao, Kiyoshi
    • 한국세라믹학회지
    • /
    • 제49권4호
    • /
    • pp.325-327
    • /
    • 2012
  • Europium-doped $LaSi_3N_5$ phosphor was synthesized from LaSi/Si/$Si_3N_4/Eu_2O_3$ mixture by nitridation at $1390^{\circ}C$ and additional annealing at $1650^{\circ}C$ for 4 h. The phosphor shows emissions in the green light region with a maximum at 560 nm. With increasing europium content in the general formula $La_{1-z}Eu_zSi_3N_{5-z}O_{1.5z}$ from z = 0.01 to 0.06 there was a maximum emission for z = 0.04 followed by concentration quenching for the highest europium content (z = 0.06).