다양한 표면처리에 따른 리튬이온 이차전지용 파우치 필름을 위한 접착성에 관한 연구 (Study of Adhesion according to Various Surface Treatments for Lithium Ion Secondary Battery Pouch Film)

  • 김도현;배성우;조정민;유민숙;김동수
    • 한국정밀공학회지
    • /
    • 제33권3호
    • /
    • pp.231-234
    • /
    • 2016
  • Pouch film is manufactured by laminating aluminum foil, polyamide film and polypropylene film with an adhesive or extrusion resin. However, a surface treatment is required for the aluminum because bonding does not occur easily between the aluminum foil and the polymer film. Thus, for this study, surface treatment experiments were performed in order to confirm the effect on adhesion strength. First, a variety of surface treatment solutions were coated on aluminum foil, and contact angle and surface morphology analysis was carried out for the surface-treated aluminum. For lamination of the surface-treated aluminum foil with polyamide film, a polyurethane base adhesive was prepared for the adhesive strength test specimens. The adhesive strength between the aluminum foil and the polyamide film of the resulting specimens was measured (UTM). With such an experiment, it was possible to evaluate the effect on adhesive strength of the various surface treatments.

LTCC 기판을 이용한 PZT 압력 센서의 제작 및 특성 연구

  • 허원영;황현석;이태용;이경천;송준태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 춘계학술대회 논문집
    • /
    • pp.13-13
    • /
    • 2010
  • Piezoelectric sensors are extensively used to measure force because of their high sensitivity and low cost. however, the development of device with reduced size but with improved sensitivity is highly important. Low-temperature co-fired ceramic (LTCC) is one of promising materials for this application than a silicon substrate because it has very good electrical and mechanical properties as well as possibility of making various three dimensional (3D) structures. In this work, piezoelectric pressure sensors based on hybrid LTCC technology were presented. The LTCC diaphragms with thickness of $400\;{\mu}m$ were fabricated by laminating 12 green tapes which consist of alumina and glass particle in an organic binder. The piezoelectric sensing layer consists of PZT thin film deposited by RF magnetron sputtering method on between top and bottom Au electrodes. The PZT films deposited on LTCC diaphragms were successfully grown and were analyzed by using X-ray diffraction method (XRD) and field emission scanning electron microscope (FESEM).

  • PDF

3차원 LTCC 기판을 이용한 PZT 압력센서의 주파수 응답 특성 (Frequency response characteristics of PZT pressure sensor using three dimensional LTCC substrates)

  • 허원영;이경천;황현석;이태용;송준태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.204-204
    • /
    • 2010
  • A development of device with reduced size and improved sensitivity is highly impotant Pb(Zr,Ti)$O_3$ thin films are widely used both to make actuator and sensor due to their high sensitivity and low cost. In this study, the feasibility of a piezoelectric presssure sensors based on hybrid low-temperaute co-fired ceramic (LTCC) technology were presented. The LTCC diaphragms with thickness of $400\;{\mu}m$ were fabricated by laminating 4 green tapes which consist of alumina and glass particle in an organic binder. PZT thin films were successfully prepared on between top and bottom Au electrode with LTCC substrates using RF magnetron sputtering. In addition, The frequency response characteristics of the sensor under varing pressure has been analysed. by Network Analyser (HP-8722D). A frequency shift range has been obseved from 1.7GHz to 1.8GHz with a good linearity for applied pressure from 0 psi up to 25 psi.

  • PDF

LTCC 기판위에 성장시킨 PZT 박막의 열처리시 $O_2$가 미치는 영향 (Effects of annealing under oxygen atmosphere of PZT thin films on LTCC substrates)

  • 이경천;허원영;황현석;이태용;이종덕;송준태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.205-205
    • /
    • 2010
  • Recently, low temperature co-fired ceramic (LTCC) technology is widely used in sensors, actuators and microsystem fields because of its very good electrical and mechanical properties, high stability as well as possibility of making 3D micro structures. In this study, we investigated the effects of on $O_2$ annealing treatment on the electrical properties of Pb(ZrTi)$O_3$ (PZT) thin films deposited on LTCC substrate. The LTCC substrates with thickness of $400\;{\mu}m$ were fabricated by laminating 4 green tapes which consist of alumina and glass particle in an organic binder. The PZT thin films were deposited on Au / LTCC substrates by RF magnetron sputtering method. The change of the crystallization of the films were investigated under various atmosphere. The structural variation of the films were analyzed by using X-Ray diffraction (XRD) and field emission scanning electron microscopy (FESEM) and secondary ion mass spectrometry (SIMS).

  • PDF

인발성형 공정을 통한 이종재료 복합소재 프레임 개발 및 내구성 평가 (Development and Durability Evaluation of a Bimaterial Composite Frame by Pultrusion Process)

  • 이학성;강신재
    • 한국생산제조학회지
    • /
    • 제23권2호
    • /
    • pp.145-151
    • /
    • 2014
  • Recently, the growing demand for weight reduction and improved structure durabilityfor commercial vehicles has led to active research into the development and application of suitablecomposite materials. This studysuggests abimaterial composite frame produced by apultrusion process to replace steel frames. We focused on the development of a composite frameconsisting of two types of materialsby mixing anorthotropic material with anisotropic material. The inside layer consisted of an aluminum pipe, and the outside layer was composed of a glass fiber pipe. To determine the strength and failure mechanisms of the composite material, tensile tests, shear tests, and three-point bending tests were conducted, followed by fatigue tests. After static testing, the fatigue tests were conducted at a load frequency of 5 Hz, a stress ratio (R) of 0.1, and an endurance limit of $10^6$ for the S-N curve. The resultsshowed that the failure modes were related to both the core design and the laminating conditions.

서부경남의 소목장 연구 I - 대한민국 명장 김병수의 교육과정 - (A study on A Cabinet Maker in Western Gyeongnam Porvince in Korea - A Curriculrum of Byeung-Soo Kim, A Master in Korea -)

  • 김민경;변희섭;김철환;문선옥
    • 한국가구학회지
    • /
    • 제26권4호
    • /
    • pp.409-420
    • /
    • 2015
  • This study intends to explore a teaching philosophy of a Master, a joiner, a cabinet maker, Byeung-Soo Kim who has devoted his entire life on creating and making traditional Korean wood furniture since the elementary school. His teaching method is to make his learners skillful by learning how to make traditional Korean furniture with the traditional technique or joint handmade. They are able to create the furniture in passing through some levels such as a beginning, a middle, a high, and a special class for three years. Each level suggests that the students should study its own joints from laminating, dado, butt, dovetail, mitered, mortise-and-tenon, rabbet, tongue-and-groove and so on. The teaching method is very unique as the technique different and difficult to fine it from other education processes throughout the country.

Pb(Mg1/3Nb2/3)O3-PbTiO3계의 조성변화에 의한 다층 콘덴서 물성 (Properties of Multilyer Condensor with Composition Change in the System of Pb(Mg1/3Nb2/3)O3-PbTiO3)

  • 김복희
    • 한국세라믹학회지
    • /
    • 제35권2호
    • /
    • pp.123-128
    • /
    • 1998
  • Multilayer ceramic capacitors(MLCC) were prepared by laminating the layer of composition with dif-ferent Curie temperature to improve temperature coefficient in the Pb(Mg1/3Nb2/3)O3-PbTiO3 binary system. Green sheet was formed by tape casting using Pb(Mg1/3Nb2/3)O3-PbTiO3 and PbTiO3 synthesized with solid state reaction of PBO. Nb2O5 MgO and TiO2. Green sheet with electrode of 70Ag-30Pd was laminated under 300 kg/cm2 at 70$^{\circ}C$ and sintered at 1100$^{\circ}C$ for 2hr. Curie temperatues for MLCC with 10 layers of pure PMN and 0.9PMN-0.1PT were lowered to -22$^{\circ}C$ and 36$^{\circ}C$ respectively. MLCC with 7 layers of PMN and 3 layers of 0.9PMN-0.1PT showed nearly zero temperature coefficient of capacitance in the range of -20∼30$^{\circ}C$ and sum of dissipation factor of each layer.

  • PDF

PZT/BT 박막의 전기적 특성 (Electrical Properties of PZT/BT Mulitilayered Films)

  • 이상헌;남성필;이영희;박재준
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2005년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.189-190
    • /
    • 2005
  • Ploycrystalline $Pb(Zr_{0.5},Ti_{0.5))O_3$ and $BaTiO_3$ powder were prepared by sol-gel process. The alumina substrate were sintered at $1400^{\circ}C$ with bottom electrode of Pt for 2 hours. The Pb(Zr0.5,Ti0.5)O3 / BaTiO3 multilayered thick films with laminating times were fabricated on alumina substrate by screening printing method. The obtained thick films were sintered at $800^{\circ}C$ with upper electrode of Ag paste for 1 hour. Structural properties of Pb(Zr0.5,Ti0.5)O3 / BaTiO3 multilayered thick films were investigated. As a result of the Differential Thermal Analysis(DTA) of Pb(Zr0.5,Ti0.5)O3, exothermic peak was observed at around 650 $^{\circ}C$. The X-ray diffraction (XRD) patterns indicated that BaTiO3 and Pb(Zr0.5,Ti0.5)O3 phases and porosities were formed in the interface of Pb(Zr0.5,Ti0.5)O3 / BaTiO3multilayered thick films.

  • PDF

임의형상가공시스템의 정속위치제어 (A Study on Constant-Speed Position Control of Solid Freeform Fabrication System)

  • 정용래;고민국;김승우
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2002년도 합동 추계학술대회 논문집 정보 및 제어부문
    • /
    • pp.75-78
    • /
    • 2002
  • SFFS(Solid Freeform Fabrication System) is commercializing to rapid prototyping concept in world-wide some corporations including the States, have much technological problems yet and need new mode for agile solid freeform fabrication as well as prototyping. In this paper, we design an automatic control algorithm that the cutting path of laser beam, on the SFFS, is controlled with constant speed. The designed algorithm for constant-speed path control is implemented and experimented in the $CAFL^{VM}$ (Computer Aided Fabrication of Lamination for Various Material) system, the new SFFS which is developed in this paper. Its process is an automated fabrication method in which a 3D object is constructed from STL(SToreoLithography) 2D data, derived from CAD 3D image, by sequentially laminating the part cross-sections. The constant-speed path control is started from the STL data. After STL file is modified in data format to be available for control. The fabrication of the 2D part is, with constant speed, conducted from the 23 position data by laser beam. we confirm its high-performance through experiment results from the application into $CAFL^{VM}$ system.

  • PDF

목재(木材)파아티클과 철선복합(鐵線複合)보오드의 기계적(機械的) 성질(性質)에 관(關)한 연구(硏究) - 휨강도를 중심으로 - (A Study on the Mechanical Properties of the Board Composed of Wood Particle and Steel Wire - Focusing on Bending Strength -)

  • 박헌
    • Journal of the Korean Wood Science and Technology
    • /
    • 제18권4호
    • /
    • pp.9-17
    • /
    • 1990
  • When manufacturing beam by laminating particleboards, the mechanical properties of particleboad-laminated beam would be also improved if the properties, especially mechanical properties of particleboad be reinforced. In this study, steel wires were used to reinforce particleboard. This study was carried out to obtain the basic mechanical properties of the board composed of wood particle and steel wires, focusing on bending strength which is the important factors in laminated beam and it was tried to estimate the relationship between the properties of the particleboard-laminated beam. and the proportion of steel wires to wood particles in particleboards. The result obtained can be summarized as follows: 1. The more steel wires used in boards, the higher value of modulus of rupture in bending was obtained, For example. the density 5 board composed of 14 numbers of steel wires showing 55% improved value than control board. 2. The board with lower density was also made better in higher value of elasticity, the density 0.5 board with 14 numbers of steel wires improved by 170%, the density 0.6 board by 86%, the 0.7 board by 37% and the 0.8 board by 26%. 3. The work to maximum load was improved with more steel wires. for example, the density 0.8 board with 14 numbers of steel wires improved by 31%.