• Title/Summary/Keyword: L-bending

Search Result 452, Processing Time 0.024 seconds

Yield line mechanism analysis of cold-formed channel sections with edge stiffeners under bending

  • Maduliat, S.;Bambach, M.R.;Zhao, X.L.
    • Structural Engineering and Mechanics
    • /
    • v.42 no.6
    • /
    • pp.883-897
    • /
    • 2012
  • Cold-formed channel sections are used in a variety of applications in which they are required to absorb deformation energy. This paper investigates the collapse behaviour and energy absorption capability of cold-formed steel channels with flange edge stiffeners under large deformation major-axis bending. The Yield Line Mechanism technique is applied using the energy method, and based upon measured spatial plastic collapse mechanisms from experiments. Analytical solutions for the collapse curve and in-plane rotation capacity are developed, and used to model the large deformation behaviour and energy absorption. The analytical results are shown to compare well with experimental values. Due to the complexities of the yield line model of the collapse mechanism, a simplified procedure to calculate the energy absorbed by channel sections under large bending deformation is developed and also shown to compare well with the experiments.

Behaviour of flush end-plate beam-to-column joints under bending and axial force

  • da Silva, Luis Simoes;de Lima, Luciano R.O.;da S. Vellasco, Pedro C.G.;de Andrade, Sebastiao A.L.
    • Steel and Composite Structures
    • /
    • v.4 no.2
    • /
    • pp.77-94
    • /
    • 2004
  • Steel beam-to-column joints are often subjected to a combination of bending and axial forces. The level of axial forces in the joint may be significant, typical of pitched-roof portal frames, sway frames or frames with incomplete floors. Current specifications for steel joints do not take into account the presence of axial forces (tension and/or compression) in the joints. A single empirical limitation of 10% of the beam's plastic axial capacity is the only enforced provision in Annex J of Eurocode 3. The objective of the present paper is to describe some experimental and numerical work carried out at the University of Coimbra to try to extend the philosophy of the component method to deal with the combined action bending moment and axial force.

Physical and Mechanical Properties of Sawdust Board Made of Thinning Logs (II) - The Effect of Density and Additive Quantity of Powder Phenolic Resin -

  • Oh, Seung-Won
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.3
    • /
    • pp.17-23
    • /
    • 2003
  • As a fundamental study of developing sawdust board from thinning softwood logs from three species (Pinus densiflora S. et Z., Larix leptolepis G. and Pinus koraiensis S. et Z.), this study examined the effect of board density and resin content on physical and mechanical properties of sawdust board. As the board density increase, thickness swelling, bending strength, and Brinell hardness increased while water absorption decreased. With increasing the resin content, the bending strength and hardness increased while water absorption and thickness swelling decreased. The board made of L. leptolepis was slightly low in its water absorption, and the one made of P. koraiensis was a little high in its bending strength, while there was no definite difference between each kind of trees in their hardness values.

Evaluation of Fretting Fatigue Behavior of Aluminum Alloy(A17050-T7451) Under Cyclic Bending Load (알루미늄 합금(AI7050-T7451)의 반복 굽힘 하중하의 프레팅 피로거동 평가)

  • Kim, Jong-Sung;Yoon, Myung-Jin;Choi, Sung-Jong;Cho, Hyun-Deog
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.9 no.1
    • /
    • pp.25-34
    • /
    • 2010
  • Fretting damage reduces fatigue life of the material due to low amplitude cyclic sliding and changes in the contact surfaces of strongly connected machine and structures such as bolt, key, fixed rivet and connected shaft, which have relative slip of repeatedly very low frequency amplitude. In this study, the fretting fatigue behavior of 7050-T7451 aluminum alloys used mainly in aircraft and automobile industry were evaluated. The plain fatigue test and fretting fatigue test under cyclic bending load carried out commercial bending fatigue tester and specially devised equipments to cause fretting damage. From these experimental work, the following results obtained: (1) The plain fatigue limit for stress ratio R=-l was about 151MPa. (2) In case of fretting fatigue, fatigue limit for stress ratio R=-l about 72MPa, the fatigue limit for R=0 about 81MPa, and the fatigue limit for R=0.3 about 93MPa. (3) The fatigue limit reduction rates by the fretting damage were about 52%(R=-1), 46%(R=0) and 38%(R=0.3) respectively. (4) The fatigue limit reduction rate decreased with stress ratio increase. In fretting bending test, as stress ratio increased, occurrence of initial oblique crack by fretting decreased or phased out, so that fracture surfaces were formed by plain fatigue crack occurrence, and such tendency was notable as stress amplitude increased. (5) Tire tracks and rubbed scars were observed in the fracture surface and contacted surface.

Biomechanical Behaviors of Disc Degeneration on Bending Loads (굽힘하중에 대한 퇴행성 추간판의 생체역학적 특성 분석)

  • Lee, Hyun-Ok;Lee, Sung-Jae;Shin, Jung-Woog
    • The Journal of Korean Physical Therapy
    • /
    • v.13 no.1
    • /
    • pp.1-18
    • /
    • 2001
  • Aging has been recognized as the primary cause of disc degeneration. A biomechanical characteristics of disc degeneration has been demonstrated that intradiscal pressure is reduced. With the increasing population of elderly people, disc degeneration and associated problems of nerve entrapment are becoming more prevalent. Presently, research on reduced intradiscal pressure associated with degeneration is insufficient. In this study. we used the Finite Element Method (FEM) of computerized simulations to investigate the effects of variation in intradiscal pressure on mechanical behaviours of L4-5 intervertebral disc degeneration. Degeneration was classified using four grades based on initial intradiscal pressure; Normal (135 kPa), mild(107 kPa), moderate (47 kPa) and severe (15 kPa). The predicted results f3r bending loads were as follows; 1 . Range of motion increased progressively with severity of degeneration with flexion and lateral bending moments, but decreased with extension moments. 2. Discal bulging of posterolateral aspect was larger in lateral bending and extension moment. But bulging was increased with severity of degeneration in lateral bending and torsion(same side).3. The rate of increasing intradiscal pressure was decreased in all bending motions with severity of degeneration. In conclusion, lateral bending and extension moment yield greatest bulging in severe degeneration. In torsion, although bending load produces disc bulging, disc bulging was associated more strongly with severity of degeneration than increasing torsional moments. Clinical Implications: Discal bulging may produce nerve root impingement and irritation. The effect of loading and posture on the varying degrees of disc degeneration has important implications especially in the elderly. In the presence of disc degeneration, avoidance of end range postures, especially extension and lateral bending may help reduce discal bulging and in turn, nerve entrapment.

  • PDF

Bending of Korea red pine (Pinus densiflora) by Microwave Irradiation (마이크로파 가열에 의한 소나무재의 곡가공)

  • Jung, Sung-Soo;Lee, Weon-Hee
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.3
    • /
    • pp.17-22
    • /
    • 1999
  • The effect of microwave irradiation on wood bending was investigated in this study. The specimens irradiated with microwave were bent around a form by using pedestal-steel and clamps. The specimens, korea red pine (Pinus densiflora), for this test were water-soaked for 78 hours. Saturated specimens were boiled in water for an hour. The size of specimens was 350mm(L) by 20mm(R) by 10mm(T). These specimens were heated by microwave of 2,450MHz. The most suitable time for microwave irradiation seems to range from 60 to 90 seconds. Wood moisture content decreased remarkably with the increase of irradiation time. When a softened wood piece is bent, its convex side was stretched while the concave side was compressed. It can be compressed considerably, but stretched very little. Therefore the failure will be governed by the tensile breaking strain and occur mainly on the convex face. So we obtained results from three different bending process methods as follows : 1) When bending with a pedestal-steel, convex face had not tensile breakings, but concave face had compression fails. 2) When bending with a clamp, bending time increased more than pedestal-steel and occurred tensile breaking. 3) Bending with a pedestal-steel and a clamp was found to be the most excellent operation method in this study.

  • PDF

Numerical Analysis on the Freezing Process of Internal Water Flow in a L-Shape Pipe (L자형 배관내 물의 결빙에 관한 해석적 연구)

  • Lee, Chung Ho;Suh, Jeong-Se
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.17 no.6
    • /
    • pp.144-150
    • /
    • 2018
  • In this study, the freezing process of L-shaped pipe exposed to the outside was investigated numerically by considering the mushy zone of freezing water. From the numerical results, it was found that the flow was outwardly directed due to the influence of the L-shaped bending part in the outside exposed part of the pipe, and the ice was formed in the shape of longitudinal corrugation on the wall surface of the pipe after the bending part. It is confirmed that this phenomenon is caused by the venturi effect due to the freezing as seen in connection with the velocity distribution in the pipe. It is found that the remelting phenomenon at the end of the freezing section occur simultaneously during the process of forming the ice in the pipe section. In regard of the factors affecting freezing, it was found that the thickness of the freezing layer is increased as the exposed pipe surface temperature is decreased, and the pipe surface temperature had a significant effect on the change of the freezing layer thickness. At the same time, it was found that the freezing layer becomes relatively thin when the water inflow rate is increased. This phenomenon was caused by reducing the exposure time of freezing water due to the vigorous flow convection of the water fluid.

The study of determination proper nose properties, used for I..L.M constructing economic long spans bridge. (경제성과 장대경간 구성을 구현할 수 있는 I.L.M교량에 사용되는 추진코의 적정제원 산정에 관한 연구)

  • 박상현;이승주;김찬녕;심재수;황의승
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.853-858
    • /
    • 2001
  • The PSC bridge being built by ILM may have greater bending moment during its construction rather than after completion. When it occurs, Engineer should suggest to reduce stress-resultants than to make bigger cross-section with considering stability ,economics, and proper span-to-depth ratio. The used method is to install extruded nose at the end of girder. It substitutes the weighted segment for the light. From the reference, the stiffness of extruded nose, is 1/10 of the main girder, and the length is 60 to 70% of the length of the span, with little justification. In this study, the proper length and stiffness of the nose element is determined by the parametric study and idealizing procedure. The results about the extruded nose through the mixing of the parameter of its stiffness and length, the proper length of extruded nose is 80% of the longest span and the proper stiffenss is 13% of the bending stiffness of the superstructure and the proper length of extruded nose is 70% of the longest span and the proper stiffness is 9.5% of the bending stiffness of the superstructure.

  • PDF

Effects of Strain Rate and Temperature on Fracture Strength of Ceramic/Metal Joint Brazed with Ti-Ag-Cu Alloy

  • Seo, Do-Won;Lim, Jae-Kyoo
    • Journal of Mechanical Science and Technology
    • /
    • v.16 no.9
    • /
    • pp.1078-1083
    • /
    • 2002
  • Ceramics are significantly used in many industrial applications due to their excellent mechanical and thermal properties such as high temperature strength, low density, high hardness, low thermal expansion, and good corrosion resistive properties, while their disadvantages are brittleness, poor formability and high manufacturing cost. To combine advantages of ceramics with those of metals, they are often used together as one composite component, which necessiates reliable joining methods between metal and ceramic. Direct brazing using an active filler metal has been found to be a reliable and simple technique, producing strong and reliable joints. In this study, the fracture characteristics of Si$_3$N$_4$ ceramic joined to ANSI 304L stainless steel with a Ti-Ag-Cu filler and a Cu (0.25-0.3 mm) interlayer are investigated as a function of strain rate and temperature. In order to evaluate a local strain a couple of strain gages are pasted at the ceramic and metal sides near joint interface. As a result the 4-point bending strength and the deflection of interlayer increased at room temperature with increasing strain rate. However bending strength decreased with temperature while deflection of interlayer was almost same. The fracture shapes were classified into three groups ; cracks grow into the metal-brazing filler line, the ceramic-brazing filler line or the ceramic inside.

Welding behavior between Zn-coated steel plate and free cutting carbon steel rod by Nd:YAG laser beam (Nd:YAG 레이저빔을 이용한 아연도금강판(SECC)과 쾌삭강봉(SUM24L)의 용접에 관한 연구)

  • 노영태;김병철;김도훈;윤갑식
    • Laser Solutions
    • /
    • v.4 no.3
    • /
    • pp.30-39
    • /
    • 2001
  • This work was tamed out to apply a laser welding technique in joining between a Zn coated low carbon steel plate(SECC) and a free cutting carbon steel shaft(SUM24L) with or without W coating. Experiments were carried out and analysed by applying the FD(factorial design)method to obtain the optimum Laser welding condition. Optical microscopy, SEM, TEM and XRD analyses were performed in order to observe the microstructures in the fusion zone and the HAZ. Mechanical properties of the welded specimens were examined by microhardness test, tensile test and twist test. There was no flawed Zn in the fusion zone by EDS analysis. This means that during the welding process, Zn gas could be eliminated by appropriate shielding gas flow rate and butt welding gap. Ni coating itself did not influence on the tensile strength and hardness. However, twist bending strength and the weld depth of the Ni-coated free cutting carbon steel were lower as compared with those of the uncoated free cutting carbon steel. It was attributed to a lower absorbance of laser beam to the shin Ni surface. According to the results of the factorial design tests, the twist bending strength of welded specimens was primarily affected by pulse width, laser power, frequency and speed.