• 제목/요약/키워드: Iron Materials

검색결과 1,476건 처리시간 0.029초

Preparation and Characterization of Ophthalmic Hydrophilic Silicone Lens Containing Zinc Oxide and Iron Oxide Nanoparticles

  • Shin, Su-Mi;Sung, A-Young
    • 한국재료학회지
    • /
    • 제31권8호
    • /
    • pp.427-432
    • /
    • 2021
  • This study uses silicone monomer, DMA, crosslinking agent EGDMA, and initiator AIBN as a basic combination to prepare hydrogel lenses using fluorine-based perfluoro polyether and iron oxide and zinc oxide nanoparticles as additives. After manufacturing the lens using iron oxide nanoparticles and zinc oxide nanoparticles, the optical, physical properties, and polymerization stability are evaluated to investigate the possibility of application as a functional hydrogel lens material. As a result of this experiment, it is found that the addition of the wetting material containing fluorine changes the surface energy of the produced hydrogel lens, thereby improving the wettability. Also, the addition of iron oxide and zinc oxide nanoparticles satisfies the basic hydrogel ophthalmic lens properties and slightly increases the UV blocking performance; it also increases the tensile strength by improving the durability of the hydrogel lens. The polymerization stability of the nanoparticles evaluated through the eluate test is found to be excellent. Therefore, it is judged that these materials can be used in various conditions as high functional hydrogel lens material.

산화철 나노 입자의 발열 효과의 제어 (Controlling the Heat Generation Capability of Iron Oxide-Base Nanoparticles)

  • 최진실
    • 한국분말재료학회지
    • /
    • 제28권6호
    • /
    • pp.518-526
    • /
    • 2021
  • This review summarizes the recent progress in iron-oxide-based heat generators. Cancer treatment using magnetic nanoparticles as a heat generator, termed magnetic fluid hyperthermia, is a promising noninvasive approach that has gained significant interest. Most previous studies on improving the hyperthermia effect have focused on the construction of dopant-containing iron oxides. However, their applications in a clinical application can be limited due to extra dopants, and pure iron oxide is the only inorganic material approved by the Food and Drug Administration (FDA). Several factors that influence the heat generation capability of iron-oxide-based nanoparticles are summarized by reviewing recent studies on hyperthermia agents. Thus, our paper will provide the guideline for developing pure iron oxide-based heat generators with high heat dissipation capabilities.

조선후기 산릉공역의 철물 조달과 철제품 제작 -산릉의궤를 중심으로- (A Study on the Procurement of Iron Materials and the Production of Ironwork in Constructions of Royal Tombs in the Later Joseon Period -Focused on Sanneung-uigwes-)

  • 이상명
    • 건축역사연구
    • /
    • 제25권5호
    • /
    • pp.27-40
    • /
    • 2016
  • The purpose of this study was to comprehend the procurement system of iron materials and the production process of ironwork in royal tombs constructions in the later Joseon period. For this purpose, sixteen Sanneung-uigwes were analyzed. The following conclusions have been reached through the study. First, it was procuring five types of iron materials in constructions of royal tombs. Sincheol had been supplied up to the mid-18th century. On the other hand, the amount of jeongcheol was increased rapidly. Because of the procurement system of initial tools was changed from bokjeong(a kind of tribute) to self-production in the Noyaso. Second, the government stockpiles were utilized as much as possible than bokjeong to manage the limited construction period and sudden construction start. Third, before moving the site of tombs, the melting furnace was installed in the Gungisi(armament factory). The amount of the melting furnace was increased from 5 to 8 since producing the initial tools in the Noyaso. Fourth, six kinds of master artisans were worked in the field of producing ironwork. Metal worker was assigned to one person per melting furnace. Fifth, the quality of final iron materials was controlled by use. Since the 19th century, it had been produced enhanced ironwork.

산화철 합성에 미치는 침전제와 초음파의 영향 (Influence of the Precipitation Medium and Ultrasonic Wave on the Synthesis of Iron Oxide)

  • 임종호;김태현;이승원
    • 한국재료학회지
    • /
    • 제16권11호
    • /
    • pp.687-691
    • /
    • 2006
  • Synthesis of Iron oxides by air oxidation of $FeSO_4$ solutions in the presence of NaOH, Diethylenetriamine (DETA), Butylamine (BA) and influence of ultrasonic wave were investigated by XRD, SEM and particle size analyzer. As the DETA addition increased to 0.05 mol, $Fe_3O_4$ was formed with goethite($\alpha$- FeOOH) and $Fe_3O_4$ single phase was formed above 0.18mol of DETA. As the BA addition increased, the XRD peak intensity of (020) face of lepidocrocite($\gamma$-FeOOH) was developed until the formation of $Fe_3O_4$ and reduced the size of the iron oxide particles formed. Ultrasonic wave reduced the size of the iron oxide particles but gave little effects on the iron oxide particles synthesized by amine.

일라이트에 함유된 Fe 불순물 제거 (Removal of Iron Bearing Minerals from Illite)

  • 김윤종;조성백;박현혜;김상배
    • 한국재료학회지
    • /
    • 제16권8호
    • /
    • pp.497-502
    • /
    • 2006
  • Recently, many attention have been focused on illite as a material for the well-being industry. Illite contains various kinds of iron bearing materials and they restrict their usage. In this study, Fe impurities in the illite produced in Yeongdong-gun, Chungcheongbuk-do were characterized and their removal experiments were performed. According to the characterization of illite raw ore, it contained 1.54 wt.%$Fe_2O_3$ due to the existence of iron oxide($Fe_2O_3$) and pyrite($FeS_2$). The raw ore was crushed into 3 mm or less using cone crusher and then ground by rod mill for the liberation of impurity mineral. For the removal of iron bearing minerals, an acid treatment, a flotation, a magnetic separation, and a flotation combined with magnetic separator were performed respectively. When the illite raw ore was treated with magnetic separation and various kinds of acid, 1.54wt.%. $Fe_2O_3$ content was reduced to 0.78 and 1.0 wt.%, respectively. On the other hand $Fe_2O_3$ content was reduced to be 0.52 wt.% after flotation. These results indicate that iron bearing minerals cannot be reduced below 0.3wt.%$Fe_2O_3$. However, combination of magnetic separation and flotation enable us to get 0.24wt.% of illite concentrate. It is concluded that, for the refinement of illite from Yeongdong-gun, the flotation combined with magnetic separation is good for high purity illite.

MOF-Derived FeCo-Based Layered Double Hydroxides for Oxygen Evolution Reaction

  • Fang Zheng;Mayur A. Gaikwad;Jin Hyeok Kim
    • 한국재료학회지
    • /
    • 제33권10호
    • /
    • pp.377-384
    • /
    • 2023
  • Exploring earth-abundant, highly effective and stable electrocatalysts for electrochemical water splitting is urgent and essential to the development of hydrogen (H2) energy technology. Iron-cobalt layered double hydroxide (FeCo-LDH) has been widely used as an electrocatalystfor OER due to its facile synthesis, tunable components, and low cost. However, LDH synthesized by the traditional hydrothermal method tends to easily agglomerate, resulting in an unstable structure that can change or dissolve in an alkaline solution. Therefore, studying the real active phase is highly significant in the design of electrochemical electrode materials. Here, metal-organic frameworks (MOFs) are used as template precursors to derive FeCo-LDH from different iron sources. Iron salts with different anions have a significant impact on the morphology and charge transfer properties of the resulting materials. FeCo-LDH synthesized from iron sulfate solution (FeCo-LDH-SO4) exhibits a hybrid structure of nanosheets and nanowires, quite different from other electrocatalysts that were synthesized from iron chloride and iron nitrate solutions. The final FeCo-LDH-SO4 had an overpotential of 247 mV with a low Tafel-slope of 60.6 mV dec-1 at a current density of 10 mA cm-2 and delivered a long-term stability of 40 h for the OER. This work provides an innovative and feasible strategy to construct efficient electrocatalysts.

Consolidation of Iron Nanopowder by Nanopowder-Agglomerate Sintering at Elevated Temperature

  • Lee, Jai-Sung;Yun, Joon-Chul;Choi, Joon-Phil;Lee, Geon-Yong
    • 한국분말재료학회지
    • /
    • 제20권1호
    • /
    • pp.1-6
    • /
    • 2013
  • The key concept of nanopowder agglomerate sintering (NAS) is to enhance material transport by controlling the powder interface volume of nanopowder agglomerates. Using this concept, we developed a new approach to full density processing for the fabrication of pure iron nanomaterial using Fe nanopowder agglomerates from oxide powders. Full density processing of pure iron nanopowders was introduced in which the powder interface volume is manipulated in order to control the densification process and its corresponding microstructures. The full density sintering behavior of Fe nanopowders optimally size-controlled by wet-milling treatment was discussed in terms of densification process and microstructures.

Purification of Iron Oxides and Application to Magnetic Hard Ferrite

  • Kim, Jeong-Seog;Chou, Kyoung-Ho;Kim, Jai-Young
    • The Korean Journal of Ceramics
    • /
    • 제2권3호
    • /
    • pp.125-130
    • /
    • 1996
  • Hematite iron ore and waste iron oxide sludge containing about 3-5 wt% $SiO_2$ were purified by three types of method developed on the basis of the Bayer process which is known as the purification process of bauxite ore. The basic principle of the developed methods lies in the fact that the impurities contained in the iron oxides, such as $SiO_2$ and $Al_2O_3$ are soluble in the alkaline reagents. Reaction of the raw materials with KOH was done in pressure vessel, at atmospheric pressure, and by both of these two. By the pressure vessel method $SiO_2$ content was reduced to below 0.5 wt% in the waste iron oxide sludge, while, in iron ore, $SiO_2$ remained at 2-3 wt%. The atmospheric pressure reaction rendered the waste iron oxide sludge $SiO_2$ content below 0.5wt% when the reaction temperature increased to above 90$0^{\circ}C$. The combined method of two previous methods was the most effective process and rendered the refined iron oxide about 300-400ppm of $SiO_2$. Using some refined iron oxides, Ba-ferrite was produced and magnetic properties were measured. The highest quality of magnetic properties obtained in this study were Br=2.09 G, bHc=1.99 KOe, iHc=4.54 KOe, $(BH)_{max}$=1.06 MGOe. Effect of sintering condition and chemical composition will be discussed.

  • PDF

Synthesis of Iron-loaded Zeolites for Removal of Ammonium and Phosphate from Aqueous Solutions

  • Kim, Kwang Soo;Park, Jung O;Nam, Sang Chul
    • Environmental Engineering Research
    • /
    • 제18권4호
    • /
    • pp.267-276
    • /
    • 2013
  • This study presents a comparison of different protocols for the synthesis of iron-loaded zeolites, and the results of their application, as well as that of zeolite-A (Z-A), to the removal of ammonium and phosphate from aqueous media. Zeolites prepared by three methods were evaluated: iron-incorporated zeolites (IIZ), iron-exchanged zeolites (IEZ), and iron-calcined zeolites (ICZ). The optimal iron content for preparing of IIZ, as determined via scanning electron microscopy and X-ray photoelectron spectroscopy analyses, expressed as molar ratio of $SiO_2:Al_2O_3:Fe$, was below 0.05. Ammonia removal revealed that the iron-loaded zeolites have a higher removal capacity than that of Z-A due, not only to ion-exchange phenomena, but also via adsorption. Greater phosphate removal was achieved with IEZ than with ICZ; additionally, no sludge production was observed in this heterogeneous reaction, even though the coagulation process is generally accompanied by the production of a large amount of undesired chemical sludge. This study demonstrates that the developed synthetic iron-loaded zeolites can be applied as a heterogeneous nutrient-removal materials with no sludge production.