  • Boron nitride films were synthesized with $N_2$ion flux of low energy, up to 100 eV, at different substrate temperatures of no heating, 200, 400, 500, and $800^{\circ}C$, respectively. Boron was supplied by e-beam evaporation at the rate of $1.5\AA$/sec. For all the conditions, hexagonal BN (h-BN) phase was mainly synthesized and high resolution transmission electron microscopy (HRTEM) showed that (002) planes of h-BN phase were aligned vertical to the Si substrate. The maximum alignment occurred around $400^{\circ}C$. In addition to major h-BN phase, transmission electron diffraction (TED) rings identified the formation of cubic BN (c-BN) phase. But HRTEM showed no distinct and continuous c-BN layer. These results suggest that c-BN phase may form in a scattered form even when h-BN phase is mainly synthesized under small momentum transfer by bombarding ions, which are not reconciled with the macro compressive stress model for the c-BN formation.

  • PDF

플라즈마 증착방식에 의해 DLC코팅된 알루미나 세라믹의 코팅박막 특성에 관한 연구 (CHARACTERISTICS OF DIAMONDLIKE CARBON COATED ALUMINA SEALS AT TEMPERATURES UP TO $400^{\circ}C$)

  • 옥철호;김병용;강동훈
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.397-397
    • /
    • 2007
  • Diamondlike carbon (DLC) coatings were deposited on alumina ceramic seals using a plasma immersion ion deposition technique (PIID). Then they were subjected to tribological tests using a pin-on-disc tribometer under a high load (1.3 GPa) and under elevated temperatures up to 400C. Coefficients of friction (COFs) were recorded and compared with that of the untreated alumina while the wear tracks were analyzed using SEM with EDS to characterize the DLC films. To enhance the DLC adhesion to the substrate, various interlayers including Si and Cr were deposited using the PIID process or an ion beam assisted deposition (IBAD) method. It was observed that the DLC coating, if adhering well to the substrate, reduced the COFs significantly, from 0.4-0.8 for the uncoated alumina to about 0.05-0.1, within the tested temperature range. The adhesion was determined by the interlayer type and possibly by the application method. Cr interlayer did not perform as well as the Si interlayer. This could also be due to the fact that the Cr interlayer and the subsequent DLC coating had to be done in two different processing systems, while both the Si interlayer and the subsequent DLC film were deposited in one system without breaking the chamber. The coating failure mode was found to be delamination between the Cr and the alumina substrate. In contrast, the Si interlayer with proper DLC deposition procedures resulted in very good adhesion and hence excellent tribological performance. Further study may lead to future DLC applications of ceramic seals.

  • PDF

이온빔을 이용한 STS304와 알루미나 브레이징 접합효과 (Effects of the Brazing Bonding between Al2O3 and STS304 with an Ion Beams)

  • 박일수
    • 한국산학기술학회논문지
    • /
    • 제16권12호
    • /
    • pp.8679-8683
    • /
    • 2015
  • 세라믹은 고온에서 뛰어난 내마모성, 내부식성을 가지기 때문에 산업적 응용에 있어서 널리 사용된다. 세라믹은 금속과 비교해서 고온에서 더 큰 강도를 가지고 있고, 더 낮은 열전도도 및 열팽창 계수를 가진다. 그러나, 세라믹이 가진 취성의 성질은 전기전자산업과 고온에서의 구조적 적용에의 넓은 적용을 제한한다. Ti 활성금속과 STS304를 IBAD 기술을 이용해서 동시에 증착시켜 STS304 스테인레스강에 $Al_2O_3$(알루미나)의 브레이징 접합강도에 어떤 영향을 미치는지 알아보았으며, 시험편들은 Ti 타겟과 Ti+ STS304 타겟 두 종류를 이용하여 두께를 변화시켜가며 증착하였다. 브레이징 접합을 위한 삽입금속으로는 일반적으로 사용되는 Ag-Cu 공정조성의 합금이 사용되었다. 브레이징 접합품의 강도는 Ag-Cu 삽입금속과 알루미나 사이의 반응층의 두께와 반응 생성물 조직에 의해 결정되며, 본 실험에서는 계면 반응의 메커니즘을 보다 구체화하고 계면 반응에 의한 경사기능성의 접합계면을 더욱 향상시키는 결과를 얻고자 한다.